925 resultados para MORPHOLOGY
Resumo:
The crystallization behavior of crystalline-crystalline diblock copolymer containing poly(ethylene oxide) (PEO) and poly(epsilon-caprolactone) (PCL), in which the weight fraction of PCL is 0.815, has been studied via differential scanning calorimeter (DSC), wide-angle X-ray diffraction (WAXD), and polarized optical microscopy (POM). DSC and WAXD indicated that both PEO and PCL blocks crystallize in the block copolymer. POM revealed a ring-banded spherulite morphology or the PEO-b-PCL diblock copolymer.
Resumo:
The surface morphologies of poly(styrene-b-4vinylpyridine) (PS-b-P4VP) diblock copolymer and homopolystyrene (hPS) binary blend thin films were investigated by atomic force microscopy as a function of total volume fraction of PS (phi(PS)) in the mixture. It was found that when hPS was added into symmetric PS-b-P4VP diblock copolymers, the surface morphology of this diblock copolymer was changed to a certain degree. With phi(PS) increasing at first, hPS was solubilized into the corresponding domains of block copolymer and formed cylinders. Moreover, the more solubilized the hPS, the more cylinders exist. However, when the limit was reached, excessive hPS tended to separate from the domains independently instead of solubilizing into the corresponding domains any longer, that is, a macrophase separation occurred. A model describing transitions of these morphologies with an increase in phi(PS) is proposed. The effect of composition on the phase morphology of blend films when graphite is used as a substrate is also investigated.
Resumo:
Self-assembly thin films of symmetric triblock copolymer after annealing and quenching were examined by an effective Monte Carlo simulation method. The defects in the ordered lamellae of the thin films after quenching, which were dependent on the initialization of copolymer melts, are removed in the thin films after annealing. The mean-square gyration radius and end-to-end distance of copolymer chains in the thin films after annealing are smaller than those in the thin films after quenching because of the complete relaxation of polymer during annealing. We also find that the density of A block in the region near to the surface is higher than that in the interior of the thin films. As a result, it is different from the thin films of symmetric A(n)B(n) diblock copolymer, in which surface ordering forms before the interior, that ordering phenomena occurs first in the interior region in the thin films of symmetric A(n)B(m)A(n). triblocl copolymer.
Resumo:
Surface morphology of polystyrene (PS) films on different substrates by spin-coating before and after annealing was observed using atomic force microscopy (AFM). The effects of polymer molecular weight, substrates, solvents, and annealing conditions on the morphology of the films were investigated. Before annealing, the grain height decreases, and simultaneously the grain diameter increases with molecular weight (M-w) within the measured molecular weight. After annealing. the situation is opposite, i.e., the grain height increases while the grain diameter decreases with M-w. Furthermore, after annealing the smaller surface roughness (Ra) was obtained. It was also found that film surface roughness (Ra) depends on the vapor pressure and dipole moment of different used solvents as well as the substrates. The experimental results show that when the used solvents have similar dipole moment but different vapor pressure, the Ra of PS film decreased with the decreasing vapor pressure of solvents whether on silicon or on mica. And when the used solvents have close vapor pressure but different dipole moment, the Ra decreased with the increasing of solvent dipole moments on both substrates.
Resumo:
We have followed the time development of the microdomain structure in symmetric diblock copolymer poly(styrene-b-methyl methacrylate), P(S-b-MMA), ultrathin films via PMMA-selective solvent vapor treatment by atomic force microscopy (AFM). After preparation on a substrate preferentially attracting the PMMA block, PS forms a continuous layer at a film's free surface. With subsequent solvent vapor treatment, the film gradually shows a well-ordered hexagonally packed nanocylinders structure. It is shown that only when the film thickness is less than the 1/2L(0) (lamellar repeat spacing), and exposed to PMMA block selective solvent for an appropriate time, can the well-ordered hexagonally packed nanocylinders form. On an extended solvent vapor treatment, a mixed morphology containing nanocylinders and stripes appears, followed by the striped morphologies. When the annealing time is long enough, the film comes back to the flat surface again, however, with PMMA instead of PS dominating the free surface.
Resumo:
As one member of high performance fibers, aromatic polyimide fibers possess many advantages, such as high strength, high modulus, high and low temperature resistance, and radiation resistance. However, the preparation of the high performance fibers is so difficult that the commercial fibers have not been produced except P84 with good flame retardancy. In this report, a polyimide was synthesized from 3,3',4,4'-biphenyltetracarboxylic dianhydride (BPDA) and 4,4'-oxydianiline (ODA) and the fibers were prepared from its solution by a dry-jet wet-spinning process. The formation of the as-spun fibers in different coagulation bath composition was discussed. Scanning electron microscope (SEMI) was employed to study the morphology of the as-spun fibers. As a result, the remnant solvent existed in the as-spun fibers generated from coagulation bath of alcohol and water. There were many fibrils and microvoids with the dimension of tens of nanometers in the fibers. One could observe the obvious fibrillation and the drawn fibers.
Resumo:
The silicon backbone conformation in poly(di-n-butylsilane) (PDBS) has been shown to be a 7/3 helix at ambient conditions, which is in marked contrast to the near-planar conformation of its homologous polymers with side chain lengths of one to three or six to eight carbon atoms. In this work, both the 7/3 helical and near-planar chain conformations are achieved by controlling the solvent evaporation rate around room temperature. The chain conformation and crystal structure obtained in this method have been correlated to the crystal morphology by wide-angle X-ray diffraction, transmission electron microscopy, electron diffraction, optical microscopy, atomic force microscopy, and UV absorption spectrum. The lath-shaped single crystals obtained at 12 degreesC correspond to an orthorhombic form with near-planar chain conformation whereas the lozenge-shaped single crystals obtained at 30 degreesC (in coexistence with the lath-shaped crystals) are orthohexagonal with a 7/3 helix.
Resumo:
The effects of the molecular weight of polystyrene (PS) component on the phase separation of PS/poly(4-vinylpyridine) (PS/P4VP) blend films on homogeneous alkanethiol self-assembled monolayer (SAM) and heterogeneous SAM/Au substrates have been investigated by means of atomic force microscopy (AFM). For the PS (22.4k)/P4VP (60k) system, owing to the molecular weight of PS component is relatively small, the well-aligned PS and P4VP stripes with good thermal stability are directed by the patterned SAM/Au surfaces. With the increase of the molecular weight of PS component (for the PS (582k)/P4VP (60k) system), the diffusion of P4VP is hindered by the high viscosity of PS during the fast spin-coating process. The phase separation behavior of PS/P4VP on the SAM/Au patterned substrates is similar to that on the homoueneous SAM and cannot be easily directed by the patterned SAM surfaces even though the characteristic length of the lateral domain morphology is commensurate with the stripe width.
Resumo:
We have studied the surface morphology of symmetric poly(styrene)-block-poly(methyl methacrylate) diblock copolymer thin films after solvent vapor treatment selective for poly(methyl methacrylate). Highly ordered nanoscale depressions or striped morphologies are obtained by varying the solvent annealing time. The resulting nanostructured films turn out to be sensitive to the surrounding medium, that is, their morphologies and surface properties can be reversibly switchable upon exposure to different block-selective solvents.
Resumo:
Vaterite-type YBO3:Eu3+ crystals with interesting flower and hedgehog fungus-like structures composed of nanosheets were obtained by controlled crystallization of Y2O3 and Eu2O3 in H3BO3 solutions under acidic hydrothermal (HT) conditions. Nanosheets of uniform thicknesses were formed by preferential crystal growth along the (100) crystallographic plane and specific three-dimensional structures were further developed through a homocentric growth mechanism. Optical emission measurements showed that the HT-grown nanosheet crystals exhibited a higher ratio of the emitted red-to-orange light ratio than crystals grown from solid-state reactions. The photoluminescence intensity and emission lifetimes were also studied as a function of the Eu3+ dopant concentration and the HT synthesis temperature. The effect of some additives: a chelating ligand, a surfactant and a polymer, on the YBO3:Eu3+ crystals morphology was also investigated.
Resumo:
Nanocomposites based on poly(hydroxybutyrate-co-hydroxyvalerate) (PHBV) and multi-walled carbon nanotubes (MWNTs) were prepared by solution processing. Ultrasonic energy was used to uniformly disperse MWNTs in solutions and to incorporate them into composites. Microscopic observation reveals that polymer-coated MWNTs dispersed homogenously in the PHBV matrix. The thermal properties and the crystallization behavior of the composites were characterized by thermogravimetric analysis, differential scanning calorimetry and wide-angle X-ray diffraction, the nucleant effect of MWNTs on the crystallization of PHBV was confirmed, and carbon nanotubes were found to enhanced the thermal stability of PHBV in nitrogen.
Resumo:
Poly(ethylene glycol) -poly(epsilon-caprolactone) diblock copolymers PEG-PCL were synthesized by ring-opening polymerization of c-caprolactone using monomethoxy poly(ethylene glycol) as the macroinitiator and calcium ammoniate as the catalyst. Obvious mutual influence between PEG and PCL crystallization was studied by altering the relative block length. Fixing the length of the PEG block (M-n = 5000) and increasing the length of the PCL block, the crystallization temperature of the PCL block rose gradually from I to about 35 degreesC while that of the PEG block dropped from 36 to -6.6 degreesC. Meanwhile, the melting temperature of the PCL block went up from 30 to 60 degreesC, while that of the PEG block declined from 60 to 41 degreesC. If the PCL block was longer than the PEG block, the former would crystallize first when cooling from a molten state and led to obviously imperfect crystallization of PEG and vice versa. And they both crystallized at the same temperature, if their weight fractions were equal. We found that the PEG block could still crystallize at -6.6 degreesC even when its weight fraction is only 14%. A unique morphology of concentric spherulites was observed for PEG5000-PCL5000.
Resumo:
Crystallization behavior, structural development and morphology evolution in a series of diblock copolymers Of poly(L-lactide)-blockpoly(ethylene glycol) (PLLA-b-PEG) were investigated via differential scanning calorimetry, wide-angle X-ray diffraction, polarized optical microscopy and atomic force microscopy. In these copolymers, both blocks are crystallizable and biocompatible. It was interesting that these PLLA-b-PEG diblock copolymers could form spherulites with banded textures, which was undercooling dependent. Single crystals with an abundance of screw dislocations were also observed via AFM. Such results indicated that these ringed spherulites and single crystals were formed during the crystallization of the PLLA blocks.