Thesis (doctoral)--

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Liquidus isotherms and phase equilibria have been determined experimentally for a pseudo-ternary section of the form MnO-(CaO+MgO)-(SiO2+Al2O3) with a fixed Al-2,O-3,/SiO2, weight ratio of 0.17 and MgO/CaO weight ratio of 0.17 for temperatures in the range 1473-1673 K. The primary phase fields present for the section investigated include manganosite (Mn,Mg,Ca)O; dicalcium silicate alpha-2(Ca,Mg,Mn)O (.) SiO2; merwinite 3CaO(.) ((Mg,Mn)O.2SiO(2); wollastonite [(Ca,Mg,Mn)(OSiO2)-Si-.]; ;tephroite [2(Mn,Mg)O.SiO2]; rhodonite [(Mn,Mg)O. diopside [(CaO,MgO,MnO,Al2O3)(SiO2)-Si-.]; tridymite (SiO2), SiO2] and melilite [2CaO (.) (MgO,MnO,Al2O3).2(SiO2,Al2O3)]. The liquidus temperatures relevant to ferro-manganese and silico-manganese smelting slags have been determined. The liquiclus temperature is shown to be principally dependent on the modified basicity weight ratio (CaO+Mgo)/(SiO2+Al2O3) at low MnO concentrations, and dependent on the mole ratio (CaO+ MgO+MnO)/(SiO2+Al2O3) at higher MnO concentrations.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Phase equilibria have been determined experimentally for pseudo-ternary sections of the form “MnO”- (CaO+MgO)-(SiO2+Al2O3) with a fixed Al2O3/SiO2 weight ratio of 0.17 and MgO/CaO weight ratios of 0.25 and 0.17 respectively for temperatures in the range 1473-1673 K. The primary phase fields present for the MgO/CaO weight ratio of 0.17 include manganosite (Mn,Mg,Ca)O; dicalcium silicate α-2(Ca,Mg,Mn)O·SiO2; merwinite 3CaO⋅(Mg,Mn)O⋅2SiO2; wollastonite [(Ca,Mg,Mn)O·SiO2]; diopside [(CaO,MgO,MnO,Al2O3)·SiO2]; tridymite (SiO2); tephroite [2(Mn,Mg)O·SiO2]; rhodonite [(Mn,Mg)O·SiO2] and melilite [2CaO·(MgO,MnO,Al2O3)·2(SiO2,Al2O3)]. For the section with MgO/CaO weight ratio of 0.25 the anorthite phase (CaO⋅Al2O3⋅2SiO2) is also present. The liquidus temperatures of ferro- and silico-manganese smelting slags have been determined. The liquidus temperatures at low MnO concentrations are shown to be principally dependent on the modified basicity weight ratio (CaO+MgO)/(SiO2+Al2O3).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The Hf isotope composition of seawater does not match that expected from dissolution of bulk continental crust. This mismatch is generally considered to be due to retention of unradiogenic Hf in resistant zircons during incomplete weathering of continental crust. During periods of intense glacial weathering, zircons should break down more efficiently, resulting in the release of highly unradiogenic Hf to the oceans. We test this hypothesis by comparing Nd and Hf isotope time series obtained from NW Atlantic ferromanganese crusts. Both isotope systems show a decrease associated with the onset of northern hemisphere glaciation. The observed changes display distinct trajectories in epsilon Nd- epsilon Hf space, which differ from previously reported arrays of bulk terrestrial material and seawater. Such patterns are consistent with the release of highly unradiogenic Hf from very old zircons, facilitated by enhanced mechanical weathering.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this work, composites were prepared using high energy mechanical milling from the precursors hydroxyapatite - HAp (Ca10(PO4)6(OH)2) and metallic iron ( -Fe ). The main goal here is to study composites in order to employ them in magnetic hyperthermia for cancer therapy. The produced samples were characterized by X-ray di raction (XRD), scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), magnetization curves as a function of applied eld (MxH), and nally measurements of magnetic hyperthermia. The XRD patterns of the milled samples HAp/Fe revealed only the presence of precursor materials. The SEM showed clusters with irregular shapes. The magnetization curves indicated typical cases of weak ferromagnetic behavior. For samples submitted to grinding and annealing, the identi ed phases were: HAp (Ca10(PO4)6(OH)2), hematite (Fe2O3) and Calcium Iron Phosphate (Ca9Fe(PO4)7). Analyzing the results of MxH, there was a reduction of the saturation magnetization, given that the Fe was incorporated into HAp. Hysteresis curves obtained at 300 K are characteristics of samples possessing over a phase. At 77 K, the behavior of the hysteresis curve is in uenced by the presence of hematite, which is antiferromagnetic. Already at T = 4.2 K, it is observed a weak ferromagnetic behavior. Furthermore, there is the e ect of exchange bias. Regarding the magnetic hyperthermia, the results of temperature measurements as a function of the alternating eld are promising for applications in magnetic hyperthermia and other biomedical applications.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Environmental liabilities from accidents in the retail petroleum industry, especially in urban areas, have represented a serious problem whose impact reaches the underground, people's health and even economic losses with the remediation process. In U.S.A. are estimated hundreds of billions of dollars invested in soil remediation processes. The results of the reports and investigative reports of liabilities in fuel stations distributed in the urban area of Natal-RN were used to estimate the local scenario of contamination. This database has been possible to determine the main contaminants (BTEX, PAHs, TOC), affected neighborhoods and types of potentially more impacted soils. Experiments were carried out in order to reverse contamination of this scenario, where the soil type was a factor in the planning, because it influences directly on the effectiveness of remediation techniques studied: Oxidation by hydrogen peroxide and oxidation by sodium persulphate. These oxidants are activated forming free radicals (HO•-, SO4 •-, HO2 • , O2 •-, S2O8 -2, etc) responsible for to mineralize the hydrocarbons and other organic compounds (releasing O2 e CO2). In the activation process, the ferrous ions (II) and ferric (III) were studied as well as hydrogen peroxide activation technique with sodium persulfate, the latter being presented the best efficiency among all the study, when activated with Fe+3. In addition to defining the most efficient technique, the aim of this study was to evaluate the influence of different soils among oxidative techniques, characterizing the effect of the concentration of these oxidants and also the concentration of the catalysts. Exists in most scenarios evaluated the presence of intrinsic total iron soil matrix. The so-called latosols present microaggregates reddish indicating the presence of these reactive species like iron and clayey aspect. The kinetic study was conducted by experimental design and monitoring of the percentage of total carbon (SSM-5000A) in the solid and liquid phases, knowing that 82.4% of the diesel molecule is carbon. Yet organic carbon and pH of liquid samples were analyzed for technical, characterizing the influence of soil type and its operating condition. The Fenton-like technique H2O2 e Fe+2 presented satisfactory oxidation, including sandy soil, but well below the best result. The sodium persulphate only activated with temperature, even in the most favorable soil, did not provide good efficiency. The best technique in the study had the concentration profile with 2,2x10- 1mol.L-1 of Na2S2O8 activated with 6,53x10-1mol.L-1 of H2O2 and 2,5x10-2 Fe3+mol.L-1 which reduced in less than a day 96 contamination in red soil, initially with 66,667 mg of diesel per kg of clean soil

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Tailings dams are structures that aims to retain the solid waste and water from mining processes. Its analysis and planning begins with searching of location for deployment, step on which to bind all kinds of variables that directly or indirectly influence the work, such as geological, hydrological, tectonic, topographic, geotechnical, environmental, social characteristics, evaluation security risks, among others. Thus, this paper aims to present a study on the most appropriate and secure type of busbar to design a layout structure of iron ore tailings, taking into account all the above mentioned variables. The case study involves the assessment of sites for location of dams of tailings disposal beneficiation of iron mine to be built in Bonito, in the municipality of Jucurutu in Seridó Potiguar. For site selection among alternatives, various aspects of the current state of the art were considered, one that causes the least environmental impact, low cost investment, adding value to the product and especially the safety of the implanted structure mitigates the concern about induced earthquakes as a result of liquefaction wastes somatized by dams in the region, as the tilling of Mina Bonito is located practically in the hydraulic basin dam Armando Ribeiro in environmental protection (APA). The methodology compares induced by dams in the semiarid region with the characteristics of the waste disposal and sterile seismicity, taking into account the enhancement of liquefaction by the action of seismicity in the Mina Bonito region. With the fulcrum in the methodology, we indicated the best busbar type for disposal of tailings from iron ore or combination of them, to be designed and built in semiarid particularly for Mina Bonito. Also presents a number of possible uses for the tailings and in engineering activities, which may cause processing to the common good.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The goal set for this work was to synthesize and to characterize new iron and copper complexes with the Schiff base 3-MeOsalen and ligands of biological relevance, whose formulas are [Fe(3-MeOsalen)NO2], [Fe(3-MeOsalen)(etil2-dtc)], [Fe(3-MeOsalen)NO] and Na[Cu(3-MeOsalen)NO2]. The compounds were characterized by vibrational spectroscopy in the infrared region (IV) and Electronic spectroscopy in the ultraviolet and visible region (Uv-Vis). From the analysis of infrared spectra, they proved to formation of precursor complexes, as evidenced by changes in the vibrationals frequencies ν(C=N) e ν(C-O) and the emergence of vibrationals modes metal-oxygen and metal-nitrogen. For nitro complexes of iron and copper were observed ν(NO2)ass around 1300 cm-1 e ν(NO2)sim in 1271 cm-1 , indicating that the coordination is done via the nitrogen atom. The complex spectrum [Fe(3-MeOsalen)(etil2-dtc)] exhibited two bands, the ν(C-NR2) in 1508 cm-1 e ν(C-S) in 997 cm-1 , the relevant vibrational modes of coordinating ligand in the bidentate form. For the complex [Fe(3-MeOsalen)NO] was observed a new intense band in 1670 cm-1 related to the ν(NO). With the electronic spectra, the formation of complexes was evidenced by shifts of bands intraligands transitions and the emergence of new bands such as LMCT (p Cl-  d* Fe3+) in [Fe(3-MeOsalen)Cl] and the d-d in [Cu(3-MeOsalen)H2O]. As for the [Fe(3-MeOsalen)NO2] has highlighted the absence of LMCT band present in the precursor complex as for the [Cu(3-MeOsalen)NO2] found that the displacement of the band hipsocrômico d-d on 28 nm. The electronic spectrum of [Fe(3-MeOsalen)(etil2-dtc)] presented LMCT band shifts and changes in intraligantes transitions. With regard to [Fe(3-MeOsalen)NO], revealed a more energetic transitions intraligands regions from the strong character π receiver NO and MLCT band of transition dπFe(II)π*(NO).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This work describes the synthesis and aplication of homogeneous and heterogenized iron catalysts in the alkylation reaction of toluene with propene, empolying experimental design. The homogenous complex was obtained trough the synthesis of the organic ligand folowed by the complexation of the iron(II) chloride. As to the heterogenized complexes, first were synthetized the inorganic supports (SBA-15, MCM-41 and Al-MCM-41). Then, it was synthetized the ligand again, that through funcionalization with chloropropyltrimethoxysilane (CPTMS), was anchored on the support previously calcinated. To these anchored ligands, was complexed the iron(II) chloride, previously solubilizated in tetrahydrofuran (THF). The organic ligand characterization was accomplished trough nuclear magnetic resonance (NMR) and Infrared spectroscopy (IV). The supports were characterized with x-ray diffraction (DRX), texture analysis with nitrogen adsorption/desorption (before and after the anchoring), termogravimetric analysis (TG) and infrared (IV). The metalic content was quantified trough the atomic absorption spectrophotometry (AAS). The complexes were tested in catalytic reactions emolying ethylaluminium sesquichloride (EASC) as co-catalyst in steel reactor, under mecanic stirring. The reaction conditions ranged from 4 to 36 ◦C, with many aluminum/iron ratios. The catalysts were actives in homogeneous and heterogenized ways. The homogenous catalytic complex showed a maximum turnover frequency (TOF) of 8.63 ×103 · h −1 , while, in some conditions, the anchored complexes showed better results, with TOF of until 8.08 ×103 · h −1 . Aditionally, it was possible to determine an equation, to the homogenous catalyst, that describes the product quantity in function of reacional temperature and aluminum/iron ratio.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Mining in Brazil has a key role in economic and social development, contributing directly to improve the lives of the population. However, the mining activity even if done responsibly and with a proper study of waste management to reduce the impact of its effects, may cause harmful damage to the environment. Other forms of pollution are also caused due to mining activity. The visual pollution caused by the waste storage at open sky, in addition to the noise pollution caused by the excessive noise of the machines both in the extraction of ore, as in processing. An alternative way to lessen the environmental impacts caused by mining is the use of waste in layers that will compose the pavements along the highways. Thus, this work sets out to give a proper disposal of the wastes from the processing of iron ore, resulting from the mining activity of the group of mining Mhag Services and Mining S/A, in the mine of Bonito, located in Jucurutu, a town in the state of Rio Grande do Norte. The residues of the iron ore were stabilized with a granular soil from the city of Macaiba, also in the state of Rio Grande do Norte, which is being used in the duplication of the BR-304 referring to the entitled passage of Reta Tabajara. The present work was developed in three stages, being the first one divided by the chemical and mineralogical tests, by the tests of physical characterization and by the tests of paving for the residues of the iron ore. The second stage corresponds to the same tests being performed for granular soil. The third stage includes the essays abovementioned for three different mixtures of iron ore waste and granular soil, being they: 15% of iron-ore waste and 85% of granular soil, 25% of iron-ore waste and 75% of granular soil, 50% of iron-ore waste and 50% of granular soil. The technical feasibility of using waste from the iron ore beneficiation was checked, compressed in the intermediate energy and modified for use in base layers, sub-base, reinforcement subgrade and subgrade. The incorporation of the residues originating from the improvement of the iron ore in highways will provide an alternative to the use of aggregate conventionally used in the paving, besides preserving the environment.