Resumo:
In this paper, the binding of neutral red (NR) to bovine serum albumin (BSA) under physiological conditions has been studied by spectroscopy method including fluorescence, circular dichroism (CD) and Fourier transform infrared (FT-IR) spectroscopy. The Stern-Volmer fluorescence quenching constant (K-SV), binding constant (K-b) and the number of binding sites (It) were measured by fluorescence quenching method. Fluorescence experiments were also performed at different ionic strengths. It was found K-SV was ionic strength dependent, which indicated the electrostatic interactions were part of the binding forces. The distance r between donor (BSA) and acceptor (NR) was obtained according to Foster's non-radiative energy transfer theory. CD spectroscopy and FT-IR spectroscopy were used to investigate the structural information of BSA molecules on the binding of NR, and the results showed no change of BSA conformation in our experimental conditions.
Resumo:
A sol-gel technique was used to prepare Gd2Ti2O7:Eu3+-coated submicron silica spheres (SiO2@Gd2Ti2O7:Eu3+). The resulted SiO2@Gd2Ti2O7:Eu3+ core-shell particles were characterized by x-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), scanning electron microscopy (SEM), energy-dispersive x-ray spectra (EDS), transmission electron microscopy (TEM), photoluminescence (PL) spectra, as well as kinetic decays. The XRD results demonstrate that the Gd2Ti2O7:Eu3+ layers begin to crystallize on the SiO2 spheres after annealing at 800 degrees C and the crystallinity increases with raising the annealing temperature. The obtained core-shell phosphors have perfect spherical shape with narrow size distribution (average size similar to 620 nm), non-agglomeration, and smooth surface. The thickness of the Gd2Ti2O7:Eu3+ shells on the SiO2 cores could be easily tailored by varying the number of deposition cycles (60 nm for four deposition cycles). Under the irradiation of 310 nm ultraviolet, the SiO2@GdTi2O7:Eu3+ samples show strong emission of Eu3+.
Resumo:
A uniform nanolayer of europium-doped Gd2O3 was coated on the surface of preformed submicron silica spheres by a Pechini sol-gel process. The resulted SiO2@Gd2O3:Eu3+ core-shell structured phosphors were characterized by X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), field emission scanning electron microscopy (FESEM), transmission electron microscopy (TEM), photoluminescence (PL) spectra as well as kinetic decays. The XRD results show that the Gd2O3:Eu3+ layers start to crystallize on the SiO2 spheres after annealing at 400 degrees C and the crystallinity increases with raising the annealing temperature. The core-shell phosphors possess perfect spherical shape with narrow size distribution (average size: 640 nm) and non-agglomeration. The thickness of the Gd2O3:Eu3+ shells on the SiO2 cores can be adjusted by changing the deposition cycles (70 nm for three deposition cycles). Under short UV excitation, the obtained SiO2@Gd2O3:Eu3+ particles show a strong red emission with D-5(0)-F-7(2) (610 nm) of Eu3+ as the most prominent group.The PL intensity of Eu3+ increases with increasing the annealing temperature and the number of coating cycles.
Resumo:
Ethylenediamine trimolybdate ((C2H10N2)[Mo3O10], denoted as ENTMo) shows unusual photochromic and thermochromic properties. The color of the white ENTMo compounds becomes reddish brown gradually under UV irradiation, and changes gradually to blue-black upon annealing. XRD patterns and FT-IR spectra verify that the crystal structure of the colored samples is almost unchanged except distortion. UV-vis diffuse reflectance spectra (DRS) and ESR spectra of the photochromic and the thermochromic samples could confirm that there must exist difference between thermochromic and photochromic mechanism.
Resumo:
A novel self-assembled layer consisting of water tetramers and nitrate anions has been observed in the [Co(1,10-phenanthroline)(2)(NO3)]center dot(NO)(3)center dot 4H(2)O complex. X-ray crystallography and FT-IR spectroscopy indicate that although the water tetramers exist in an energetically less stable uudd configuration, the anionic host environments may play an important role in the formation and stabilization of the water clusters.
Resumo:
Fourier-transform (FT)-Raman and -infrared (IR) spectroscopy were employed to investigate the function of the aqueous 2-hydroxyethylmethacrylate/glutaraldehyde solution (Gluma) as a desensitizer. 2-Hydroxyethylmethacrylate (HEMA), glutaraldehyde (GA), and the mixture of HEMA/GA (i.e. Gluma) were used to interact with dentin, collagen, hydroxyapatite (HAP), and bovine serum albumin (BSA) individually. All the interactions were monitored by an FT-Raman spectrometer. FT-IR spectroscopy was also used in this study. The results show that HEMA could be absorbed by dentin and collagen; GA could cross-link collagen and BSA; and when BSA was added to Gluma, polymerization of HEMA occurred. The results suggest that Gluma acts as a desensitizer whereby, first, GA reacts with part of the serum albumin in dentinal fluid, which induces a precipitation of serum albumin, then, second, a reaction of GA with serum albumin induces polymerization of HEMA. The function of Gluma as a desensitizer to block dentinal tubules occurs via these two reactions.
Resumo:
SiO2@Gd2MoO6:EU3+ core-shell phosphors were prepared by the sol-gel process. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), field emission scanning electron microscopy (FESEM), energy-dispersive X-ray spectra (EDS), transmission electron microscopy ITEM), photoluminescence (PL) spectra as well as kinetic decays were used to characterize the resulting SiO2@Gd2MoO6:Eu3+ core-shell phosphors. The XRD results demonstrate that the Gd2MoO6:Eu3+ layers on the SiO2 spheres begin to crystallize after annealing at 600 degrees C and the crystallinity increases with raising the annealing temperature. The obtained core-shell phosphors have a near perfect spherical shape with narrow size distribution (average size ca. 600 nm), are not agglomerated, and have a smooth surface. The thickness of the Gd2MoO6:Eu3+ shells on the SiO2 cores could be easily tailored by varying the number of deposition cycles (50 nm for four deposition cycles). The Eu3+ shows a strong PL luminescence (dominated by D-5(0)-F-7(2) red emission at 613 nm) under the excitation of 307 nm UV light.
Resumo:
Europium-doped nanocrystalline GdVO4 phosphor layers were coated on the surface of preformed submicron silica spheres by sol-gel method. The resulted SiO2@Gd0.95Eu0.05VO4 core-shell particles were characterized by X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), scanning electron microscopy (FESEM), energy-dispersive X-ray spectra (EDS), transmission electron microscopy (TEM), photoluminescence (PL) spectra, low voltage cathodoluminescence (CL), time resolved PL spectra and kinetic decays. The XRD results demonstrate that the Gd0.95Eu0.05VO4 layers begin to crystallize on the SiO2 spheres after annealing at 600 C and the crystallinity increases with raising the annealing temperature. The obtained core-shell phosphors have spherical shape, narrow size distribution (average size ca. 600 nm), non-agglomeration. The thickness of the Gd0.95Eu0.05VO4 shells on the SiO2 cores could be easily tailored by varying the number of deposition cycles (50 nm for four deposition cycles). PL and CL show that the emissions are dominated by D-5(0)-F-7(2) transition of Eu3+ (618 nm, red).
Resumo:
Rare-earth ion (Eu3+, Tb3+, Ce3+)- doped LaPO4 nanocrystalline thin films and their patterning were fabricated by a Pechini sol-gel process combined with soft lithography on silicon and silica glass substrates. X-Ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), thermogravimetric and differential thermal analysis (TG-DTA), atomic force microscopy (AFM), scanning electron microcopy (SEM), optical microscopy, absorption and photoluminescence (PL) spectra as well as lifetimes were used to characterize the resulting films. The results of XRD indicate that the films begin to crystallize at 700 degreesC and the crystallinity increases with increasing annealing temperature. The morphology of the thin film depends on the annealing temperature and the number of coating layers. The 1000 degreesC annealed single layer film is transparent to the naked eye, uniform and crack-free with a thickness of about 200 nm and an average grain size of 100 nm. Patterned thin films with different strip widths ( 5 - 50 mm) were obtained by micromolding in capillaries ( soft lithography). The doped rare earth ions show their characteristic emission in the nanocrystalline LaPO4 films, i.e., Eu3+ D-5(0)-F-7(J) (J = 1, 2, 3, 4), Tb3+ D-5(3,4) - F-7(J) ( J = 6, 5, 4, 3, 2) and Ce3+ 5d-4f transition emissions, respectively. Both the lifetimes and the PL intensities of Eu3+ and Tb3+ increase with increasing annealing temperature, and the optimum concentrations for them were determined to be 5 mol% and 16 mol% of La3+ in LaPO4 thin films, respectively. An energy transfer phenomenon from Ce3+ to Tb3+ has been observed in LaPO4 nanocrystalline thin films, and the energy transfer efficiency depends on the doping concentration of Tb3+ if the concentration of Ce3+ is fixed.
Resumo:
Organically modified silica xerogels (OMSX) and Eu3+ (Tb3+)-doped OMSX were prepared by the reaction of (3-aminopropyl) triethoxysilane (APS) with 3-isocyanatepropyltriethoxysilane (ICPTES) followed by the subsequent hydrolysis and condensation in the presence of Eu3+ (Tb3+) via sol-gel method, which were characterized by FT-IR, XRD, fluorescence excitation and emission spectra. The as-formed OMSX shows a strong blue emission with the maximum excitation and emission wavelength at 351 and 420 nm, respectively. Due to the spectral overlap between the emission band of OMSX and f-f absorption lines of Eu3+ and Tb3+ in the UV-blue region, an energy transfer was observed from OMSX host to Eu3+ and Tb3+ in OMSX/Eu3+ and OMSX/Tb3+, respectively. Excitation at 350-360 nm resulted in a very weak emission around 420 nm from OMSX host and strong emission of Eu3+ and Tb3+ in OMSX/Eu3+ and OMSX/Tb3+, respectively. The emission spectra of Eu3+ and Tb3+ consist of D-5(0)-F-7(J) (J = 0, 1, 2, 3, 4) and D-5(4)-F-7(J) (J = 6, 5, 4, 3), respectively. Furthermore, the predicted structure of OMSX/Eu3+ and OMSX/Tb3+ is presented.
Resumo:
The electrochemical properties Of PW12O403- (abbreviated as PW12) anion in poly(ethylene glycol) (PEG) have been studied by cyclic voltammetry, complex impedance and FT-IR spectroscopy. The PW12 anion in PEG-LiClO4 electrolyte shows reasonable facile electrochemistry, and the diffusion coefficients Of PW12 were measured with microelectrode. It is shown that ionic conductivity of polymer electrolytes based on low molecular weight PEG can be improved by the addition of PW12. The increase of conductivity is coupled with decrease of transient cross-links density of polymer chains which is evidenced by the downshift of C-O-C stretching mode. The phenomena are explained in view of ion-ion and ion-polymer interactions.
Resumo:
The electrochemical behavior of alpha-Keggin-type nanoparticles, Co(en)(3)(PMo12O40) (abbreviated as PMo12-Co), have been studied in poly(ethylene glycol) for four different molecular weights (PEG, average MW 400, 600, 1000, and 2000 g mol(-1)) and containing LiClO4 (O/Li=100/1) supporting electrolyte. The diffusion coefficients of the PMo12-Co nanoparticles were determined using a microelectrode by chronoamperometry for PEG of different molecular weights that were used to describe the diffusion behavior of PMo12-Co nanoparticles in different phase states. Moreover, the conductivity of the composite system increases upon addition of PMo12-Co nanoparticles, which was measured by an a.c. impedance technique. FT-IR spectra and DSC were used to follow the interactions of PEG-LiClO4-PMo12-Co, and well described the reason that the PMo12-Co nanoparticles could promote the conductivity of the PEG-LiClO4-PMo12-Co system.
Resumo:
采用纳米微粒直接分散法合成了纳米 Ce O2 /阴离子聚氨酯复合材料 ,粘度分析表明 ,随着纳米Ce O2 含量的增加 ,复合材料的粘度降低 ;FT- IR分析表明 ,Ce O2 的吸收峰出现蓝移现象 ;TEM和光散射粒径分析表明 ,复合粒子仍以纳米量级存在 ,平均粒径为 35 nm,且呈单分散状态 ,Ce O2 纳米粒子均匀分散在聚氨酯中。并且对复合粒子形成机理及稳定性进行了初步探讨
Resumo:
A biodegradable two block copolymer, poly(epsilon-caprolactone)-b- poly(gamma-benzyl-L-glutamic acid) (PCL-PBLG) was synthesized successfully by ring-opening polymerization of N-carboxyanhydride of gamma-benzyl-L-glutamate (BLG-NCA) with aminophenyl-terminated PCL as a macroinitiator. The aminophenethoxyl-terminated PCL was prepared via hydrogenation of a 4-nitrophenethoxyl-teminated PCL, which was novelly obtained from the polymerization of c-caprolactone (CL) initiated by amino calcium 4-nitrobenzoxide. The structures of the block copolymer and its precursors from the initial step of PCL were confirmed and investigated by H-1 NMR, FT-IR, GPC, and FT-ICRMS analyses and DSC measurements.
Resumo:
采用独特的二次溶解和沉淀的萃取方法,将PP b PE中的不可溶物与可溶物分离,并通过1 3C NMR,DSC,FT IR进行结构与性能的研究