Tm3+/Yb3+-codoped gernianate-niobic (GN) and germanium-bismuth (GB) glasses have been synthesized by conventional ruching and quenching method. Intense blue and weak red emissions centered at 477 and 650 nm, corresponding to the transitions (1)G(4)->H-3(6) and (1)G(4)->H-3(4), respectively, were observed at room temperature. The possible Up-conversion mechanisms are discussed and estimated. GN glass showed a weaker up-conversion emission than GB glass, which is inconsistent with the prediction from the difference of maximum phonon energy between GN and GB glasses. In this paper, Raman spectroscopy was employed to investigate the origin of the difference in up-conversion luminescence in the two glasses. Compared with phonon side-band spectroscopy, Raman spectroscopy extracts more information including both phonon energy and phonon density. For the first time, our results reveal that, besides the maximum phonon energy, the phonon density of host glasses is also an important factor in determining the up-conversion efficiency. (c) 2005 Elsevier Ltd. All rights reserved.
Resumo:
Tm3+-doped oxide-chloride germanate and tellurite glasses have been synthesized by conventional melting method. Intense up-conversion luminescence emissions were simultaneously observed at room temperature in these glasses. The possible up-conversion mechanisms are discussed and estimated. However, in these Tm3+-doped glasses, tellurite glass showed weaker up-conversion emissions than germanate glass, which is inconsistent with the prediction from the difference of maximum phonon energy between tellurite and germanate glasses. In this paper, Raman spectroscopy was employed to investigate the origin of the difference in up-conversion luminescence in the two glasses. Our results confirm that, besides the maximum phonon energy, the phonon density of host glasses is also an important factor in determining the up-conversion efficiency. (c) 2005 Elsevier Ltd. All rights reserved.
Resumo:
Ytterbium-sensitized erbium-doped oxide-halide tellurite and germanate-niobic-lead glasses have been synthesized by conventional melting method. Intense green and red emissions centered at 525, 546 and 657 nm, corresponding to the transitions H-2(11/2) -> I-4(15/2), S-4(3/2) -> I-4(15/2) and F-4(9/2) -> I-4(15/2), respectively, were simultaneously observed at room temperature in these glasses. The quadratic dependence of the 525, 546 and 657 nm emissions on excitation power indicates that a two-photon absorption process occurs. Tellurite glass showed a weaker up-conversion emission than germanate-niobic-lead glass, which is inconsistent with the prediction from the difference of maximum phonon energy between tellurite and germanate-mobic-lead glasses. In this paper, Raman spectroscopy was employed to investigate the origin of the difference in up-conversion luminescence in the two glasses. Compared with phonon side-band spectroscopy, Raman spectroscopy extracts more information including both phonon energy and phonon density. Our results reveal that the phonon density and the maximum phonon energy of host glasses are both important factors in determining the up-conversion efficiency. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
研究了掺铒磷酸盐玻璃波导放大器的特性。利用重叠因子将980nm光抽运的掺铒玻璃波导放大器四能级模型的速率-传输方程进行化简,在考虑上转换效应和放大自发发射的情况下.利用数值模拟的方法,得到了掺铒玻璃波导放大器的增益与Er^3+离子浓度、抽运功率、波导长度等参量之间的关系曲线;同时模拟出放大自发发射曲线并与实验测量结果进行比较。结果表明在考虑上转换效应和放大自发发射的情况下,理论结果和实验测量结果是一致的。同时看到,选择合适的铒离子浓度是制作掺铒玻璃波导放大器的关键;并且为了全面发挥掺铒玻璃波导放大器的性能
Resumo:
A waveguide amplifier is fabricated by Ag+-Na+ two-step ion exchange on Er/Yb-doped phosphate glass. The spectroscopic performance of glass and the properties of channel waveguide are characterized. A double-pass configuration is adopted to measure the gain and noise figure (NF) of the waveguide amplifier, and the comparison of gain and NF for the single and double-pass configuration of the waveguide amplifier is presented. The results show that the double-pass configuration can make the gain increase from 8.8dB (net gain 2.2dB/cm) of the single-pass one to 14.6 dB (net gain 3.65 dB/cm) for small input power at 1534 nm, and the NF are all lower than 5.5dB for both the configurations.
Resumo:
This paper reports on the optical spectroscopic properties and thermal stability of Er3+-doped TeO2-BaO (Li2O,NaO)-La2O3 glasses for developing 1.5-mu m fiber amplifiers. Upon excitation at 977 nm laser diode, an intense 1.53-mu m infrared fluorescence has been observed with a broad full width at half maximum (FWHM) of about 60 nm for the Er3+-doped TeO2-BaO (Li2O, Na2O)-La2O3 glass with 10 mol% of BaO. The calculated fluorescence lifetime and the emission cross-sections of the 1.53-mu m transition are 2.91 ms and similar to 9.97 x 10(-21) cm(2), respectively. It is noted that the gain bandwidth, a, x FWHM, of the TeO2-BaO-La2O3Er2O3 glass is about 600, which is significantly higher than that in silicate and phosphate glasses. Meanwhile, it is interesting to note that the TeO2-BaO-La2O3-Er2O3 glass has shown a high glass thermal stability and good infrared transmittance. As a result, TeO2-BaO (Li2O, Na2O)-La2O3 glass with 10 mol% of BaO has been considered to be more useful as a host for broadband optical fiber amplifier. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
One of the key systems of a Wave Energy Converter for extraction of wave energy is the Power Take-Off (PTO) device. This device transforms the mechanical energy of a moving body into electrical energy. This paper describes the model of an innovative PTO based on independently activated double-acting hydraulic cylinders array. The model has been developed using a simulation tool, based on a port-based approach to model hydraulics systems. The components and subsystems used in the model have been parameterized as real components and their values experimentally obtained from an existing prototype. In fact, the model takes into account most of the hydraulic losses of each component. The simulations show the flexibility to apply different restraining torques to the input movement depending on the geometrical configuration and the hydraulic cylinders on duty, easily modified by a control law. The combination of these two actions allows suitable flexibility to adapt the device to different sea states whilst optimizing the energy extraction. The model has been validated using a real test bench showing good correlations between simulation and experimental tests.
Resumo:
The up-conversion luminescence of Yb3+-doped yttriurn lanthanum oxide transparent ceramic was investigated. It was ascribed to cooperative luminescence originated from the coupled states of the Yb3+ ion pairs. The proper doping of La2O3 can remove the cooperative luminescence of Yb3+ ion. But excessive La2O3 (at least 10 at.%) the cooperative up-conversion of Yb3+:Y2O3 is obtained again, and the intensity of up-conversion luminescence strengthens with the increase of La2O3 content. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
High optical quality Lu2SiO5 (LSO) and (Lu0.5Gd0.5)(2)SiO5 (LGSO) laser crystals codoped with Er3+ and Yb3+ have been fabricated by the Czochralski method. Intense upconversion (UC) and infrared emission (1543 nm) are observed under excitation of 975 nm. The luminescence processes are explained and the emission efficiencies are quantitatively obtained by measuring the UC efficiency and calculating the emission cross section. The temperature-dependent optical properties of the crystals are also investigated. Our study indicates that Er3+-Yb3+ : LSO and Er3+-Yb3+: LGSO crystals are promising gain media for developing the solid-state 1.5 mu m optical amplifiers and tunable UC lasers. (c) 2008 American Institute of Physics.