965 resultados para Chalcohalide glasses
Resumo:
New lithium-barium-lead-bismuth glasses with low OH- concentration have been obtained. The role of the different components in the glass formation has been explored from the thermal, density, and refractive index measurements. The T-g, T-x, and T-x-T-g values of these glasses are in the range of 358-400, 453-575, and 87-197 degreesC, respectively. The densities (p) and refractive indices of these glasses are mainly affected by Bi2O3 and PbO contents. A wide transmitting window from visible to infrared (IR) regions for some compositions of these glasses has been observed, which makes them appealing candidates for different optical applications such as upconverting phosphors, new laser materials, optical waveguides, and crystal-free fibre drawing. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
The upconversion properties of Er3+/Yb3+ codoped tellurite glasses and glass fibers with D-shape cladding under 980 mu excitation were investigated. Intense emission bands centered at 531, 546 and 658 nm corresponding to the transitions Er3+: H-2(11/2) -> I-4(15/2) , S-4(3/2) -> I-4(15/2) and F-4(9/2) -> I-4(15/2), respectively, were observed at room temperature. Compared with that in Er3+/Yb3+ codoped tellurite bulk glass, the upconversion luminescence becomes more efficient in the fiber geometry. The dependence of upconversion intensities on fiber geometry and possible upconversion mechanism are discussed and evaluated. The presented Er3+/Yb3+ codoped tellurite fibers with intense upconversion luminescence can be used as potential host materials for upconversion fiber lasers. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
High-uniform nanowires with diameters down to 50 nm are directly taper-drawn from bulk glasses. Typical loss of these wires goes down to 0.1 dB/mm for single-mode operation. Favorable photonic properties such as high index for tight optical confinement in tellurite glass nanowires and photoluminescence for active devices in doped fluoride and phosphate glass nanowires are observed. Supporting high-index tellurite nanowires with solid substrates (such as silica glass and MgF2 crystal) and assembling low-loss microcoupler with these wires are also demonstrated. Photonic nanowires demonstrated in this work may open up vast opportunities for making versatile building blocks for future micro- and nanoscale photonic circuits and components. (c) 2006 Optical Society of America.
Resumo:
Tm3+/Yb3+-codoped heavy metal oxide-halide glasses have been synthesized by conventional melting and quenching method. Structural properties were obtained based on the Raman spectra, indicating that halide ion has an important influence on the phonon density and maximum phonon energy of host glasses. Intense blue and weak red emissions centered at 477 and 650 nm, corresponding to the transitions (1)G(4) -> H-3(6) and (1)G(4) -> H-3(4), respectively, were observed at room temperature. The possible up-conversion mechanisms are discussed and estimated. With increasing halide content, the up-conversion luminescence intensity and blue luminescence lifetimes of Tm3+ ion increase notably. Our results show that with the substitution of halide ion for oxygen ion, the decrease of phonon density and maximum phonon energy of host glasses both contribute to the enhanced up-conversion emissions. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
A series of five different concentration erbium-doped tellurite glasses with various hydroxl groups were prepared. Infrared spectra of glasses were measured. In order to estimate the exact content of OH- groups in samples, various absorption coefficients of the OH- vibration band were analyzed under the different oxygen bubbling times. The absorption spectra of the glasses were measured, and the Judd-Ofelt intensity parameters Omega(i) of samples with the different erbium ions concentration and OH- contents were calculated on the basis of the Judd-Ofelt theory. The peak stimulated emission cross-section of (I13/2 ->I15/2)-I-4-I-4 transition of the samples was finally calculated by using the McCumber theory. The fluorescence spectra of Er3+:I-4(13/2)->I-4(15/2) transition and the lifetime of Er3+:I-4(13/2) level of the samples were measured. The effects of OH- groups on the spectroscopic properties of Er3+ doped samples with the different concentrations were discussed. The results showed that the OH- groups had great influences on the Er3+ lifetime and the fluorescence peak intensity. The OH- group is a main influence factor of fluorescence quenching when the doping concentration of Er2O3 is smaller than 1.0 mol%, but higher after this concentration, the energy transfer of Er3+ ions turns into the main function of the fluorescence quenching. And basically, there is no influence on the other spectroscopic properties (FWHM, absorption spectra, peak stimulated emission cross section, etc.).
Resumo:
Divalent metal fluorides MF2 (M=Sr, Mg, Ca) in oxyfluoride tellurite glasses TeO2-BaF2-LaF3 were synthesized. The densities, refractive indices and characteristic temperatures of synthesized glasses were measured. The influence of divalent metal fluorides MF2 (M=Sr, Mg, Ca) on the thermal stability of oxyfluoride tellurite glasses TeO2-BaF2-LaF3 were studied. Results show that the replacement of BaF2 by SrF2 and MgF2 can enhance the thermal stability against crystallization of the glass. A glass system with good thermal stability was produced, which could be a potential candidate for the host materials of the fiber devices.
Thermal stability and frequency up-conversion properties of Er3+-doped oxyfluoride tellurite glasses
Resumo:
Effect of Yb2O3 content on upconversion luminescence and mechanisms in Yb3+-sensitized Tm3+-doped oxyhalide tellurite glasses were investigated under 980 nm excitation. Intense blue and relatively weak red upconversion emission centered at 476 and 649nm corresponding to the transitions (1)G(4) -> H-3(6) and (1)G(4) -> H-3(4) of Tm3+, respectively, are simultaneously observed at room temperature. The results show that upconversion blue and red emission intensities of Tm3+ first increase, reach its maximum at Yb2O3% = 3 mol%, and then decrease with increasing Yb2O3 content. The effect of Yb2O3 content on upconversion intensity is discussed, and possible effect mechanisms are evaluated. The investigated results were conducing to increase upconversion luminescence efficiency of Tm3+. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Novel oxyfluoride glasses are developed with the composition of 30SiO(2)-15Al(2)O(3)-28PbF(2)-22CdF(2)-0.1TmF(3)-xYbF(3) -(4.9-x) AlF3(x = 0, 0.5, 1.0, 1.5, 2.0) in mol fraction. Furthermore, the upconversion luminescence characteristics under a 970nm excitation are investigated. Intense blue, red and bear infrared luminescences peaked at 453nm, 476nm, 647nm and 789nm, which correspond to the transitions of Tm3+: D-1(2) -> F-3(4), (1)G(4) -> H-3(6), (1)G(4) -> F-3(4), and H-3(4) -> H-3(6), respectively, are observed. Due to the sensitization of Yb3+ ions, all the upconversion luminescence intensities are enhanced considerably with Yb3+ concentration increasing. The upconversion mechanisms are discussed based on the energy matching rule and quadratic dependence on excitation power. The results indicate that the dominant mechanism is the excited state absorption for those upconversion emissions.
Resumo:
Fluorophosphate glasses codoped with Tm3+ and Yb3+ were prepared and their thermal stability, phonon states, and upconversion properties were studied. It is found that the increment of phosphate content is good for the thermal stability but increases the phonon density of states. However, the phonon density of states of these fluorophosphate glasses is very low due to the low phosphate content in their composition. The upconversion luminescence spectra were measured under excitation of 970 nm laser diode, and the intense blue (476 nm) and near infrared (794 nm) emission were simultaneous obtained at room temperature. The sensitizing mechanisms of Yb3+ to Tm3+ for blue and red emission contain both sequential and cooperative sensitization. The near infrared emission is a two-photon upconversion process. These researches suggest that when the phosphate content in the composition is low enough, fluorophosphate glass can be suitable host material of Tm3+ codoped with Yb3+ for blue and near infrared upconversion luminescence. (c) 2005 Elsevier B.V All rights reserved.
Resumo:
Er2O3-doped TeO2-ZnO-La2O3 modified tellurite glasses were prepared by the conventional melt-quenching method, and the Er3+ : I-4(13/2) -> I-4(15/2) fluorescence properties have been studied for different Er3+ concentrations. Infrared spectra were measured in order to estimate the exact content of OH- groups in samples. Based on the electric dipole-dipole interaction theory, the interaction parameter, C-Er,(Er), for the migration rate of Er3+ : I-4(13/2) -> I-4(13/2) in modified tellurite glass was calculated. Finally, the concentration quenching mechanism using a model based on energy transfer and quenching by hydroxyl (OH-) groups was presented. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
A comprehensive study on the thermal stability and spectroscopic properties of Er3+/Yb3+-codoped Al(PO3)(3)-based fluorophosphate glasses is reported of the 1.5μ m fibre amplifiers in this paper. From optical absorption spectra, the Judd-Ofelt parameters of Er3+ in the glasses and several important optical properties, such as the radiative transition probability, the branching ratio and the spontaneous emission probability, have been calculated by using Judd-Ofelt theory. The fluorophosphate glass exhibits broadband near-infrared emission at 1.53μ m with a full width at half-maximum over 63nm, and a large calculated stimulated-emission cross-section of 6.85 x 10(-21)cm(2).
Resumo:
The thermal stability and structure of RF-RF2-AIF(3)-Al(PO3)(3) fluorophosphate glasses were investigated. Analyses of infrared absorbance spectra and Raman spectra reveal that with increasing number of alkali and alkaline earth fluoride components, the sum of P-O-P bond and O-P-O bond increases and glass network is strengthened. Consequently, the inhibition to nucleation and crystallization processes is improved, which is proved by the increment of thermal stability factors AT and S determined by differential scanning calorimetry. In addition, it was found that LiF has poor ability to form glass in univalent alkali fluorides and MgF2 has comparative strong ability to form glass in bivalent alkaline earth fluorides. (c) 2006 Published by Elsevier B.V.
Resumo:
Tm3+-Yb3+ codoped oxyfluoride silicate glasses suitable for upconversion laser has been fabricated. In this paper, effect of CdF2 addition on thermal stability and upconversion luminescence properties in Tm3+-Yb3+ codoped oxyfluoride silicate glasses have been systematically investigated. The experimental results indicate that, with the substitution CdF2 for PbF2, the glass thermal stability increases and the UV cutoff edge moves to short-wave band slightly. With increasing CdF2 content, the blue and red upconversion luminescence intensity increases slightly at first, and then increases rapidly. While the near infrared (NIR) upconversion emission intensity increases notably at first and then increases slightly. However, the blue and NIR luminescence intensity are much stronger than that of red, indicating these oxyfluoride silicate glasses are more preferable for blue and NIR emissions than red emission. The possible upconversion mechanisms for the blue, red and NIR fluorescence are also estimated and evaluated. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Tm3+/Yb3+-codoped gernianate-niobic (GN) and germanium-bismuth (GB) glasses have been synthesized by conventional ruching and quenching method. Intense blue and weak red emissions centered at 477 and 650 nm, corresponding to the transitions (1)G(4)->H-3(6) and (1)G(4)->H-3(4), respectively, were observed at room temperature. The possible Up-conversion mechanisms are discussed and estimated. GN glass showed a weaker up-conversion emission than GB glass, which is inconsistent with the prediction from the difference of maximum phonon energy between GN and GB glasses. In this paper, Raman spectroscopy was employed to investigate the origin of the difference in up-conversion luminescence in the two glasses. Compared with phonon side-band spectroscopy, Raman spectroscopy extracts more information including both phonon energy and phonon density. For the first time, our results reveal that, besides the maximum phonon energy, the phonon density of host glasses is also an important factor in determining the up-conversion efficiency. (c) 2005 Elsevier Ltd. All rights reserved.