997 resultados para 320-U1333A
Resumo:
The phenomenon of magnetoacoustic emission (MAE) has been ascribed usually to one of two origins: either (1) motion of non-180 degrees domain walls or (2) creation or annihilation of domains. In this paper, we present strong evidence for the argument that the only origin for MAE is motion of non-180 degrees domain walls. The proof is evident as a result of measurements of zero MAE for a wide range of stress in the isotropic zero magnetostrictive polycrystalline alloy of iron with 6.5% silicon. We also explain why it was that the alternative origin was proposed and how the data in that same experiment can be reinterpreted to be consistent with the non-180 degrees wall motion origin. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
The behavior of the Steinmetz coefficient has been described for several different materials: steels with 3.2% Si and 6.5% Si, MnZn ferrite and Ni-Fe alloys. It is shown that, for steels, the Steinmetz law achieves R(2)> 0.999 only between 0.3 and 1.2 T, which is the interval where domain wall movement dominates. The anisotropy of Steinmetz coefficient for non-oriented (NO) steel is also discussed. It is shown that for a NO 3.2% Si steel with a strong Goss component in texture, the power law coefficient and remanence decreases monotonically with the direction of measurement going from rolling direction (RD) to transverse direction (TD), although coercive field increased. The remanence behavior can be related to the minimization of demagnetizing field at the surface grains. The data appear to indicate that the Steinmetz coefficient increases as magnetocrystalline anisotropy constant decreases. (c) 2008 Elsevier B.V. All rights reserved.
Resumo:
An ultra-low carbon steel (30 ppm after decarburization) containing Al and Si was aged for distinct soaking times at 210 degrees C. The core loss increased continuously until around 24 h. After that, only slight changes were verified. It was found that only the hysteresis loss component changed during the aging treatment. By internal friction test and transmission electron microscopy it was seen that carbon precipitation caused the magnetic aging. By scanning electron microscopy it could be concluded that the increase of aging index was attributed to the high number of carbides larger than 0.1 mu m. (C) 2008 Elsevier B. V. All rights reserved.
Resumo:
Magnetic energy losses and permeability have been investigated in laboratory prepared and commercial Mn-Zn sintered ferrites from quasi-static conditions up to 10 MHz. The mechanisms leading to energy dissipation, either due to domain wall displacements or magnetization rotations, have been quantitatively assessed and their respective roles have been clarified. Domain wall processes dissipate energy by pure relaxation effects, while rotations display resonant absorption of energy over a broad range of frequencies. Their specific contributions to the permeability and its frequency dispersion are thus identified and separately evaluated. It is shown that eddy currents are always too weak to appreciably contribute to the losses over the whole investigated frequency range and that rotations are the dominant magnetization and loss producing mechanisms on approaching the MHz range, as predicted by the Landau-Lifshitz-Gilbert equation with distributed anisotropy fields. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
Cold-rolled (0-19% of reduction) 0.5% Si electrical steel sheets were studied in detail, including macro and micro residual stress measurements, crystallographic texture, dc-hysteresis curves and iron losses. Even for the smallest deformation, losses increase significantly, with large increase of the hysteresis losses, whereas the anomalous losses reduce slightly. The residual microstresses are similar to 150-350 MPa, whereas residual macrostresses are compressive, similar to 50 MPa. The large increase of the hysteresis losses is attributed to the residual microstresses. The dislocation density estimated by X-ray diffraction is in reasonable agreement with that predicted from the Sablik et al. model for effect of plastic deformation on hysteresis. The intensity of the texture fibers {1 1 1}< u v w > and < 110 >//RD (RD = rolling direction) increases with the reduction. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
Square and two-level pulse width modulation (PWM) magnetic induction waveforms are investigated and their effect on electrical steels losses as a function of the grain size is determined. The increase of hysteresis losses-as compared to that resulting from sinusoidal voltages-occurs only for two-level PWM waveforms. Total losses are lower for square waveform, and the difference between losses under square and sinusoidal waveform increase with increasing grain size, result explained with the loss separation model. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
Effects of titanium carbide (TiC) addition on structural and magnetic properties of isotropic (Pr,Nd)-Fe-B nanocrystalline magnetic materials have been investigated. In this work, we investigate the effect of TiC addition on a (Pr,Nd)-poor and B-rich composition, as well as on a B-poor and (Nd, Pr)-rich composition. Rapidly solidified (Pr, Nd)-Fe-B alloys were prepared by melt-spinning. The compositions studied were (Pr(1-x)Nd(x))(4)Fe(78)B(18) (x = 0, 0.5, and 1) with addition of 3 at% TiC. Unlike the (Pr(x)Nd(1-x))(9.5)Fe(84.5)B(6) materials that present excellent values for coercive. field and energy product, the (Pr,Nd)-poor and B-rich composition alloys with TiC addition present lower values. Rietveld analysis of X-ray data and Mossbauer spectroscopy revealed that samples are predominantly composed of Fe(3)B and alpha-Fe. For the RE-rich compositions (Pr(x)Nd(1-x))(9.5)Fe(84.5)B(6) (x = 0.1, 0.25, 0.5, 0.75, and 1) with the addition of 3 at% TiC, the highest coercive field and energy product (8.4 kOe and 14.4 MGOe, respectively) were obtained for the composition Pr(9.5)Fe(84.5)B(6). (c) 2008 Elsevier B.V. All rights reserved.
Resumo:
The development and fabrication of a thermo-electro-optic sensor using a Mach-Zehnder interferometer and a resistive micro-heater placed in one of the device`s arms is presented. The Mach-Zehnder structure was fabricated on a single crystal silicon substrate using silicon oxynitride and amorphous hydrogenated silicon carbide films to form an anti-resonant reflective optical waveguide. The materials were deposited by Plasma enhanced chemical vapor deposition technique at low temperatures (similar to 320 degrees C). To optimize the heat transfer and increase the device response with current variation, part of the Mach-Zehnder sensor arm was suspended through front-side bulk micromachining of the silicon substrate in a KOH solution. With the temperature variation caused by the micro-heater, the refractive index of the core layer of the optical waveguide changes due to the thermo-optic effect. Since this variation occurs only in one of the Mach-Zehnder`s arm, a phase difference between the arms is produced, leading to electromagnetic interference. In this way, the current applied to the micro-resistor can control the device output optical power. Further, reactive ion etching technique was used in this work to define the device`s geometry, and a study of SF6 based etching rates on different composition of silicon oxynitride films is also presented. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Electric arc furnace (EAF) dust is a waste generated in the EAF during the steel production process. Among different wastes, EAF dust represents one of the most hazardous, since it contains heavy metals such as Zn, Fe, Cr, Cd and Pb. The goal of the present work is to characterise the waste through chemical analysis, particle size distribution, X-ray diffraction (XRD), scanning electron microscopy coupled with energy dispersive spectroscopy detection and thermal analysis. The waste sample is composed essentially of spherical particles and has a very small particle size and the majority of the identified elements were Fe, Zn, Ca, Cr, Mn, K and Si. The XRD has presented compounds such as ZnO, ZnFe2O4, Fe2O3, MnO, SiO2, FeFe2O4 and MnAl2O4. According to the thermal analysis results, up to 1000 degrees C the total weight loss was similar to 5%. The results of waste characterisation are very important to these further investigations.
Resumo:
The objective of this study was to evaluate the performance and to estimate costs of two round baling systems for harvesting understory biomass. One system was a cutter-shredderbaler prototype (Bio-baler). The other system required two successive operations. The first operation was cutting and shredding with a Supertrak tractor equipped with a Fecon mulcher head. The second operation was baling with a Claas baler. The machines were evaluated in three different pine stands on the Osceola National Forest in Florida, United States. Data collection included time study, fuel consumption and bale measurements. Material was collected from a sample of bales for heat and moisture content determination. On the most representative site (Site 2), the Bio-baler recovered 8.05 green t ha(-1) while the mulcher and the Claas baler recovered 9.75 green t ha(-1) (43 and 52 percent of original understory biomass, respectively). Productivity was 0.30 ha h(-1) for the Bio-baler and 0.51 ha h(-1) for the Claas baler. Density of the bales was 321 green kg m(-3) for the Bio-baler and 373 green kg m(-3) for the Claas baler. Average net heat content was 6263 MJ bale(-1) for the Bio-baler and 6695 MJ bale(-1) for the Claas baler with biomass containing 38 percent of moisture content on a wet basis. cost per unit area was less with the Bio-baler (US$320.91 ha(-1)) than with the mulcher-baler system (US$336.62-US$596.77 ha(-1)). Published by Elsevier Ltd.
Resumo:
In order to further address the known interaction between ethylene and components of the oxidative system, we have used the ethylene-insensitive Never ripe (Nr) tomato (Solanum lycopersicum L) mutant, which blocks ethylene responses. The mutant was compared to the control Micro-Tom (MT) cultivar subjected to two stressful situations: 100 mM NaCl and 0.5 mM CdCl(2). Leaf chlorophyll, lipid peroxidation and antioxidant enzyme activities in roots, leaves and fruits, and Na and Cd accumulation in tissues were determined. Although we verified a similar growth pattern and Na and Cd accumulation for MT and Nr, the mutant exhibited reduced leaf chlorophyll degradation following stress. In roots and leaves, the patterns of catalase (CAT), glutathione reductase (GR), ascorbate peroxidase (APX), guaiacol peroxidase (GPOX), superoxide dismutase (SOD) enzyme activity as well as malondialdehyde (MDA) and hydrogen peroxide (H(2)O(2)) production under the stressful conditions tested were very similar between MT and Nr mutant. However, Nr fruits showed increased H(2)O(2) production, reduced and enhanced APX activity in NaCl and CdCl(2), respectively, and enhanced GPOX in NaCl. Moreover, through non-denaturing PAGE, a similar reduction of SOD I band intensity in both, control MT and Nr mutant, treated with NaCl was observed. In leaves and fruits, a similar SOD activity pattern was observed for all periods, genotypes and treatments. Overall the results indicate that the ethylene signaling associated with NR receptor can modulate the biochemical pathways of oxidative stress in a tissue dependent manner, and that this signaling may be different following Na and Cd exposure. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
The natural chlorophyll degradation results in noncolored chlorophyll catabolites (NCCs), but there are controversies if these are the final products. The formation and degradation of NCCs during soybean seed (Glycine max L. Merrill) maturation and two drying temperatures were investigated. Soybean was harvested at six maturation stages. The effect of postharvest drying at 40 and 60 degrees C on the NCC formation was analyzed by high-performance liquid chromatography (HPLC), and results were expressed as areas under the curve. All samples contained fractions with an absorption maximum at 320 nm, typical for NCC. The amounts of NCC increased until 114 days after planting and were significantly lower in advanced maturation stages. These results indicate that the NCC in soybeans might not be the final products of chlorophyll degradation. Their reduction in advanced maturation stages may be due to further metabolization. Heating soybeans at 40 and 60 degrees C promoted unnatural chlorophyll degradation and impaired the formation of NCC.
Resumo:
Culture conditions (pH, time, temperature, inoculum size, orbital agitation speed and substrate concentration) for an extracellular collagenase produced by Candida albicans URM3622 were studied using three experimental designs (one 2(6-2) fractionary factorial and two 2(3) full factorial). The analysis of the 2(6-2) fractionary design data indicated that agitation speed and substrate concentration had the most significant effect on collagenase production. Based on these results, two successive 2(3) full factorial design experiments were run in which the effects of substrate concentration, orbital agitation speed and pH were further studied. These two sets of experiments showed that all variables chosen were significant for the enzyme production, with the maximum collagenolytic activity of 6.8 +/- 0.4 U achieved at pH 7.0 with an orbital agitation speed of 160 rpm and 2% substrate concentration. Maximum collagenolytic activity was observed at pH 8.2 and 45 degrees C. The collagenase was stable within a pH range of 7.2-8.2 and over a temperature range of 28-45 degrees C. These results clearly indicate that C. albicans URM3622 is a potential resource for collagenase production and could be of interest for pharmaceutical, cosmetic and food industry. Crown Copyright (C) 2008 Published by Elsevier B.V. All rights reserved.
Resumo:
Published studies on the association between cancer and paracoccidioidomycosis consist either isolated cases or clinical data based on hospital cohorts of paracoccidioidomycosis. The frequency of neoplasia in series of >= 80 patients with paracoccidioidomycosis ranges from 0.16 to 14.1%, mean of 3.96%. There are only two retrospective controlled studies, one of them showing greater incidence of carcinoma in biopsy and necropsy samples of paracoccidioidomycosis (12 cases in 147 patients with the mycosis: 8.2%) than in the necropsies of the control group (320 cases in 7,302 necropsies: 4.9%). In the other, 22,409 autopsies were reviewed and 4,372 cases of cancer were found; of the 85 patients with paracoccidioidomycosis, 12 were diagnosed with cancer. No differences were observed in the frequency of malignancies between the group of patients with paracoccidioidomycosis (14.1%) and the control group (19.5%). Considering all the reported cases, carcinoma was more frequent than hematological malignancies, and was more often found at the same site or in a neighboring site affected by the mycosis, usually occurring after the diagnosis of the mycosis. Commonly, the basic cause of death was related to secondary infections or neoplasia. Lymphoma was associated with poorly organized rich in fungi granuloma. The clinical course and mortality were related to the cancer evolution or secondary infections and was worse in lymphoid series, metastatic carcinoma or in patients under cytotoxic chemotherapy. Additionally, as in several cases the clinical and histopathological data may mimick neoplasia, the correct diagnosis of both diseases is essential to guarantee an early and safe intervention.
Resumo:
In this study was developed a new nano drug delivery system (NDDS) based on association of biodegradable surfactants with biocompatible magnetic fluid of maguemita citrate derivative. This formulation consists in a magnetic emulsion with nanostructured colloidal particles. Preliminary in vitro experiments showed that the formulation presents a great potential for synergic application in the topical release of photosensitizer drug (PS) and excellent target tissue properties in the photodynamic therapy (PDT) combined with hyperthermia (HPT) protocols. The physical chemistry characterization and in vitro assays were carried out by Zn(II) Phtalocyanine (ZnPc) photosensitizer incorporated into NDDS in the absence and the presence of magnetic fluid, showed good results and high biocompatibility. In vitro experiments were accomplished by tape-stripping protocols for quanti. cation of drug association with different skin tissue layers. This technique is a classical method for analyses of drug release in stratum corneum and epidermis+ dermis skin layers. The NDDS formulations were applied directly in pig skin (tissue model) fixed in the cell`s Franz device with receptor medium container with a PBS/EtOH 20% solution (10mM, pH 7.4) at 37 degrees C. After 12 h of topical administration stratum corneum was removed from fifty tapes and the ZnPc retained was evaluated by solvent extraction in dimetil-sulphoxide under ultrasonic bath. These results indicated that magnetic nanoemulsion (MNE) increase the drug release on the deeper skin layers when compared with classical formulation in the absence of magnetic particles. This could be related with the increase of biocompatibility of NDDS due to the great affinity for the polar extracelullar matrix in the skin and also for the increase in the drug partition inside of corneocites wall. (C) 2008 Elsevier B.V. All rights reserved.