873 resultados para Titanium carbide
Resumo:
The distribution of dissolved, soluble and colloidal fractions of Al and Ti was assessed by ultrafiltration studies in the upper water column of the eastern tropical North Atlantic. The dissolved fractions of both metals were found to be dominated by the soluble phase smaller than 10 kDa. The colloidal associations were very low (0.2–3.4%) for Al and not detectable for Ti. These findings are in some contrast to previous estimations for Ti and to the predominant occurrence of both metals as hydrolyzed species in seawater. However, low tendencies to form inorganic colloids can be expected, as in seawater dissolved Al and dissolved Ti are present within their inorganic solubility levels. In addition, association with functional organic groups in the colloidal phase is unlikely for both metals. Vertical distributions of the dissolved fractions showed surface maxima with up to 43 nM of Al and 157 pM of Ti, reflecting their predominant supply from atmospheric sources to the open ocean. In the surface waters, excess dissolved Al over dissolved Ti was present compared to the crustal source, indicating higher solubility and thus elevated inputs of dissolved Al from atmospheric mineral particles. At most stations, subsurface minima of Al and Ti were observed and can be ascribed to scavenging processes and/or biological uptake. The dissolved Al concentrations decreased by 80–90% from the surface maximum to the subsurface minimum. Estimated residence times in the upper 100 m of the water column ranged between 1.6 and 4 years for dissolved Al and between 14 and 17 years for dissolved Ti. The short residence times are in some contrast to the low colloidal associations of Al and Ti and the assumed role of colloids as intermediates in scavenging processes. This suggests that either the removal of both metals occurs predominantly via direct transfer of the hydrolyzed species into the particulate fraction or that the colloidal phase is rapidly turned over in the upper water column.
Resumo:
Marine bivalves (Mytilus galloprovincialis) were exposed to titanium dioxide (10 mg L-1) either as engineered nanoparticles (nTiO(2); fresh, or aged under simulated sunlight for 7 days) or the bulk equivalent. Inductively coupled plasma-optical emission spectrometry analyses of mussel tissues showed higher Ti accumulation (>10-fold) in the digestive gland compared to gills. Nano-sized TiO2 showed greater accumulation than bulk, irrespective of ageing, particularly in digestive gland (>sixfold higher). Despite this, transcriptional expression of metallothionein genes, histology and histochemical analysis suggested that the bulk material was more toxic. Haemocytes showed significantly enhanced DNA damage, determined by the modified comet assay, for all treatments compared to the control, but no significant differences between the treatments. Our integrated study suggests that for this ecologically relevant organism photocatalytic ageing of nTiO(2) does not significantly alter toxicity, and that bulk TiO2 may be less ecotoxicologically inert than previously assumed.
Resumo:
High-resolution synchrotron X-ray diffraction was used to study the phase transformations in titanium alloys. Three titanium alloys were investigated: Ti-6Al-4V, Ti-6Al-2Sn-4Zr-2Mo-0.08Si and beta21s. Both room and high temperature measurements were performed. The room temperature experiments were performed to study the structure of the alloys after different heat treatments, namely as received (AR), furnace cooling (FC), water quenching (WQ) and water quenching followed by ageing. The alpha, alpha', alpha'' and beta phases were observed in different combinations depending on the heat treatment conditions and the alloy studied. A multicomponent hexagonal close packed (hcp) alpha phase, with different c and the same a lattice parameters, was detected in Ti-6Al-4V after FC. High temperature synchrotron X-ray diffraction was used for 'in situ' study of the transformations on the sample surface at elevated temperatures. The results were used to trace the kinetics of surface oxidation and the concurrent phase transformations taking place under different conditions. The influence of the temperature and oxygen content on the lattice parameters of the alpha phase was derived and new data obtained on the coefficients of thermal expansion in the different directions of the hcp alpha phase, for Ti-6Al-4V and Ti-6Al-2Sn-4Zr-2Mo-0.08Si.
Resumo:
Dielectronic recombination (DR) has been studied in highly charged He-like Ti ions using an electron beam ion trap. X-rays emitted from radiative recombination (RR) and DR were observed as the electron beam energy was scanned through the resonances. Differential DR resonant strengths were determined by normalizing the DR x-ray intensity to the RR intensity using theoretical RR cross sections. KLn (2 less than or equal to n less than or equal to 5) resonant strengths were determined for He-like Ti ions. The differential resonant strengths were calibrated without reference to any theoretical DR calculations while the electron energy scale was derived with reference to the well-known energy for ionization of the He-like and H-like ions from the ground state. Calibration in this way facilitates a more exacting comparison between theory and experiment than has been reported previously. To facilitate this comparison, total and differential theoretical resonance strengths were calculated. These calculations were found to be in good agreement with the measured results.