872 resultados para expectorant agent


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Thèse numérisée par la Division de la gestion de documents et des archives de l'Université de Montréal

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Thèse numérisée par la Division de la gestion de documents et des archives de l'Université de Montréal

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Mémoire numérisé par la Division de la gestion de documents et des archives de l'Université de Montréal

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Mémoire numérisé par la Division de la gestion de documents et des archives de l'Université de Montréal

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Les accouchements prématurés constituent un problème médical majeur en constante augmentation et ce, malgré tous les efforts mis en œuvre afin de contrer le déclenchement des contractions avant terme. Cette thèse relate du ''design'' rationnel d'un nouvel agent thérapeutique (i.e., tocolytique) qui serait capable de 1) arrêter les contractions, et 2) prolonger la gestation. Pour ce faire, une nouvelle cible, la prostaglandine F2α et son récepteur ont été sélectionnés et le peptidomimétisme a été choisi afin de résoudre cette problématique. L'introduction contient un historique rapide de la conception à la synthèse (''drug design'') du peptide parent, le PDC113, premier peptide a avoir démontré des aptitudes tocolytiques suffisantes pour faire du peptidomimétisme. La deuxième partie de l'introduction présente les concepts du peptidomimétisme appliqués au PDC113 qui ont permis d'accéder au PDC113.824, inhibiteur allostérique du récepteur de la prostaglandine F2α, et explique comment ce mime nous a permis d'élucider les mécanismes de signalisation intracellulaire impliqués dans la contraction musculaire lisse. Cette thèse présente la conception, la synthèse et l'étude structure-activité de mimes de repliement de tour β au sein du mime peptidique original (PDC113.824) dans lequel nous avons remplacé l'azabicycloalkane central (l'indolizidin-2-one) par une série d'autres azabicycloalcanes connus et des acides aza-aminés dont nous avons élaboré la synthèse. Dans un premier temps, une nouvelle stratégie de synthèse en solution de l'aza-glycyl-proline à partir de la diphényle hydrazone et du chloroformate de p-nitrophényle a été réalisée. Cette stratégie a permis d'éliminer les réactions secondaires de cyclisation intramoléculaires communément obtenues lors de l'introduction d'acides aza-aminés avec les protections traditionnelles de type carbamate en présence de phosgène, mais aussi de faciliter l'accès en une étape à des dérivés peptidiques du type aza-glycyle. L'élongation de l'aza-glycyl-proline en solution nous a permis d'accéder à un nouveau mime tetrapeptidique du Smac, un activateur potentiel de l'apoptose au sein de cellules cancéreuses. Par la suite, nous avons développé une stratégie de diversification sélective de l'azote α du résidu azaglycine en utilisant différents types d'halogénures d'alkyle en présence de tert-butoxyde de potassium. Afin de valider le protocole d'alkylation de l'aza-dipeptide, différents halogénures d'alkyle ont été testés. Nous avons également démontré l'utilité des aza-dipeptides résultants en tant que ''building block'' afin d'accéder à une variété d'azapeptides. En effet, l'aza-dipeptide a été déprotégée sélectivement soit en N-terminal soit en C-terminal, respectivement. D'autre part, la libération de l'amine de l'ester méthylique de l'aza-alkylglycyl-proline a conduit à une catégorie de composés à potentiel thérapeutique, les azadicétopipérazines (aza-DKP) par cyclisation intramoléculaire. Enfin, notre intérêt quant au développement d'un nouvel agent tocolytique nous a amené à développer une nouvelle voie de synthèse en solution du PDC113.824 permettant ainsi d'élucider les voies de signalisation intracellulaires du récepteur de la prostaglandine F2α. Afin de valider l'importance de la stéréochimie et d'étudier la relation structure/ activité du mime, nous avons remplacé l'indolizidin-2-one (I2aa) centrale du PDC113.824 par une série d'autres azabicycloalcanes et azadipeptides. Les azabicycloalcanes D-I2aa, quinolizidinone, et indolizidin-9-one ont été synthétisés et incorporés au sein du dit peptide ne donnant aucune activité ni in vitro ni ex vivo, validant ainsi l'importance du tour β de type II' pour le maintien de l'activité biologique du PDC113.824. Finalement, l'insertion d'une série de dérivés aza(alkyl)glycyl-prolyles a mené à de nouveaux inhibiteurs allostériques du récepteur de la PGF2α, l'un contenant l'azaglycine et l'autre, l'azaphénylalanine. Cette thèse a ainsi contribué, grâce à la conception et l'application de nouvelles méthodes de synthèse d'aza-peptides, au développement de nouveaux composés à potentiel thérapeutique afin d'inhiber le travail prématuré.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Les biofilms sont des communautés structurées de micro-organismes enrobées dans une matrice extracellulaire. Les biofilms sont impliqués dans la persistance de plusieurs maladies infectieuses et la matrice extracellulaire du biofilm protège les bactéries contre les cellules du système immunitaire de l'hôte, les antibiotiques et les désinfectants. Récemment notre laboratoire a démontré que le zinc inhibe la formation de biofilm chez Actinobacillus pleuropneumoniae, une bactérie pathogène du porc. Le but de cette étude est d'évaluer l'effet du zinc sur la croissance et la formation du biofilm chez différentes bactéries pathogènes du porc, telles que Bordetella bronchiseptica, Escherichia coli, Haemophilus parasuis, Salmonella, Staphylococcus aureus et Streptococcus suis. Les bactéries ont été cultivées dans des plaques de 96 puits sous condition optimale de formation de biofilm et les biofilms ont été colorés au cristal violet. La présence du biofilm a été confirmée par microscopie confocale à balayage laser à l’aide du marqueur fluorescent FilmTracerTM FM ® 1-43. À des concentrations micromolaires, le zinc inhibe faiblement la croissance bactérienne et bloque d'une manière dose-dépendante la formation de biofilm d’A. pleuropneumoniae, Salmonella Typhimurium et H. parasuis. De plus, la formation de biofilm de E. coli, S. aureus et S. suis a été faiblement inhibée par le zinc. Nos résultats indiquent que le zinc a un effet inhibiteur sur la formation de biofilm de la plupart des pathogènes bactériens d'origine porcine. Cependant, le mécanisme sous-jacent de l'activité anti-biofilm du zinc reste à être caractérisé.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We consider envy-free (and budget-balanced) rules that are least manipulable with respect to agents counting or with respect to utility gains. Recently it has been shown that for any profile of quasi-linear preferences, the outcome of any such least manipulable envy-free rule can be obtained via agent-k-linked allocations. This note provides an algorithm for identifying agent-k-linked allocations.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Isora fibre-reinforced natural rubber (NR) composites were cured at 80, 100, 120 and 150°C using a low temperature curing accelerator system. Composites were also prepared using a conventional accelerator system and cured at 150°C. The swelling behavior of these composites at varying fibre loadings was studied in toluene and hexane. Results show that the uptake of solvent and volume fraction of rubber due to swelling was lower for the low temperature cured vulcanizates which is an indication of the better fibre/rubber adhesion. The uptake of aromatic solvent was higher than that of aliphatic solvent, for all the composites. As the fibre content increased, the solvent uptake decreased, due to the superior solvent resistance of the fibre and good fibre-rubber interactions. The bonding agent improved the swelling resistance of the composites due to the strong interfacial adhesion. Due to the improved adhesion between the fibre and rubber, the ratio of the change in volume fraction of rubber due to swelling to the volume fraction of rubber in the dry sample (V,) was found to decrease in the presence of bonding agent. At a fixed fibre loading, the alkali treated fibre composite showed a lower percentage swelling than untreated one for both systems showing superior rubber-fibre interactions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A series of short-isora-fiber-reinforced natural rubber composites were prepared by the incorporation of fibers of different lengths (6, 10, and 14 mm) at 15 phr loading and at different concentrations (10, 20, 30, and 40 phr) with a 10 mm fiber length. Mixes were also prepared with 10 mm long fibers treated with a 5% NaOH solution. The vulcanization parameters, processability, and stress-strain properties of these composites were analyzed. Properties such as tensile strength, tear strength, and tensile modulus were found to be at maximum for composites containing longitudinally oriented fibers 10 mm in length. Mixes containing fiber loadings of 30 phr with bonding agent (resorcinol-formaldehyde [RF] resin) showed mechanical properties superior to all other composites. Scanning electron microscopy (SEM) studies were carried out to investigate the fiber surface morphology, fiber pullout, and fiber-rubber interface. SEM studies showed that the bonding between the fiber and rubber was improved with treated fibers and with the use of bonding agent.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Tribasic lead sulphate is tried as a practical curing agent for polychloroprene. The cure characteristics of the compounds as well as the technical properties of the vulcanizates show that it can act as a potential curative.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Blends of nitrile rubber and reclaimed rubber containing different levels of a coupling agent, Si 69 (bis(3- triethoxysilyl propyl)(tetrasulphide) were prepared and the cure characteristic's and mechanical properties were studied. Optimum loading of Si-69 was found to be a function of blend ratio. 3 phi- of Si 69 in a 70:30. Blend was found to be the optimum combination with respect to the mechanical properties. The rate and state of cure were also affected bv the conp/ing agent. Tensile strength, tear strength and abrasion resistance were improved in the presence of coupling agent. While the state of cure improved, the cure rate and scorch time decreased with increasing silane content. Ageing studies showed that the blends containing the coupling agent were inferior to the unmodified blends.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Chloroprene rubber was blended with whole tire reclaimed rubber (WTR) in presence of different levels of a coupling agent Si69 [bis- (3-(triethoxysilyl)propy1)tetrasuIfide] and the cure characteristics and mechanical properties were studied. The rate and state of cure were also affected by the coupling agent. While the cure time was increased, the cure rate and scorch time were decreased with increasing silane content. Tensile strength, tear strength, and abrasion resistance were improved in the presence of coupling agent. Compression set and resilience were adversely affected in presence of silane-coupling agent.Aging studies showed that the blends containing the coupling agent were inferior to the unmodified blends.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The rheological characteristics of short Nylon-6 fiber-reinforced Styrene Butadiene rubber (SBR) in the presence of epoxy resin-based bonding agent were studied with respect to the effect of shear rate, fiber concentration , and temperature on shear viscosity and die swell using a capillary rheonzeter. All the composites containing bonding agent showed a pseudoplastic nature, which decreased with increasing temperature. Shear viscosity was increased in the presence of fibers. The temperature sensitivity of the SBR matrices was reduced on introduction of fibers. The temperature sensitivity of the melts was found to be lower at higher shear rates. Die swell was reduced in the presence of fibers. Relative viscosity of the composites increased with shear rate. In the presence of epoxy resin bonding agent the temperature sensitivity of the mixes increased. Die swell was larger in the presence of bonding agent.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The cure characteristics and mechanical properties of short nylon fiber- styrene /whole tyre reclaim (SBR/WTR) composites with and without an interfacial bonding agent based on 4,4 diphenyl methane diisocyanate and polyethylene glycol (MDI/PEG) have been studied. An 80:40 blend of SBR/ WTR reinforced with 20 phr of short nylon fiber has been selected and the MDI/ PEG ratio has been changed from 0.67:1 to 2:1. The minimum and maximum torques increased with isocyanate concentration. The scorch time and cure time showed an initial reduction. The cure rate showed an initial improvement. Tensile strength, tear strength and abrasion resistance increased with MDI/PEG ratio, these values were higher in longitudinal direction. Resilience and compression set increased with isocyanate concentration.