837 resultados para Rubber composites
Resumo:
Conducting polymers are excellent microwave absorbers and they show technological advantage when compared with inorganic electromagnetic absorbing materials, being light weight , easily processable, and the ability of changing the electromagnetic properties with nature and amount of dopants, synthesis conditions, etc. In this paper we report the synthesis, dielectric properties, and expected application of conducting composites based on polyaniline (PAN). Cyclohexanone soluble conducting PAN composites of microwave conductivity 12.5 S/m was synthesized by the in situ polymerization of aniline in the presence of emulsion grade polyvinyl chloride. The dielectric properties of the composites, especially the dielectric loss, conductivity, dielectric heating coefficient , absorption coefficient, and penetration depth, were studied using a HP8510 vector network analyzer. The microwave absorption of the composites were studied at different frequency bands i.e, S, C, and X bands (2-12 GHz). The absorption coefficient was found to be higher than 200 m -' and it can be used for making microwave absorbers in space applications
Resumo:
The effect of various processing parameters, such as nip gap, friction ratio and roll temperature, on the tensile properties of short Kevlar aramid fibre-thermoplastic polyurethane composite has been investigated and the tensile and tear fracture surfaces have been characterised using a scanning electron microscope. A nip gap of 0.45 mm, a friction ratio of 1.15 and a roll temperature of 62°C was found to give optimum mechanical properties. Scanning electron microscopy study revealed a higher extent of fibre orientation in the milling direction in the above condition.
Resumo:
The effect of an external flaw on the tensile strength of short kevlar fiber-thermoplastic composites has been studied with respect to fiber content, fiber orientation, location of the external flaw, and the temperature of test. The composites showed a three-step reduction in tensile strength with increasing flaw size. The critical flaw-length region was shifted to higher flaw-size levels with increasing fiber content. With increasing temperature, the critical flaw length was increased in the case of unfilled TPU, whereas it remained more or less constant in the case of short kevlar fiber-filled-TPU composite.
Resumo:
Blends of styrene butadiene rubber (SBR) with maleic anhydride grafted whole tire reclaim (MA-g-WTR) have been prepared and the cure and mechanical properties have been studied with respect to the reclaim content. The grafting was carried out in the presence of dicumylperoxide (DCP) in a Brabender Plasticorder at 150'C. The presence of anhydride group on the WTR was confirmed by infrared spectrometry (IR) study. The properties were compared with those of the blends containing unmodified WTR. Though the cure time was marginally higher, the mechanical properties of the blends containing grafted WTR were better than that of the unmodified blends.
Resumo:
Blends of nitrile rubber and reclaimed rubber containing different levels of a coupling agent, Si 69 (bis(3- triethoxysilyl propyl)(tetrasulphide) were prepared and the cure characteristic's and mechanical properties were studied. Optimum loading of Si-69 was found to be a function of blend ratio. 3 phi- of Si 69 in a 70:30. Blend was found to be the optimum combination with respect to the mechanical properties. The rate and state of cure were also affected bv the conp/ing agent. Tensile strength, tear strength and abrasion resistance were improved in the presence of coupling agent. While the state of cure improved, the cure rate and scorch time decreased with increasing silane content. Ageing studies showed that the blends containing the coupling agent were inferior to the unmodified blends.
Resumo:
Chloroprene rubber was blended with whole tire reclaimed rubber (WTR) in presence of different levels of a coupling agent Si69 [bis- (3-(triethoxysilyl)propy1)tetrasuIfide] and the cure characteristics and mechanical properties were studied. The rate and state of cure were also affected by the coupling agent. While the cure time was increased, the cure rate and scorch time were decreased with increasing silane content. Tensile strength, tear strength, and abrasion resistance were improved in the presence of coupling agent. Compression set and resilience were adversely affected in presence of silane-coupling agent.Aging studies showed that the blends containing the coupling agent were inferior to the unmodified blends.
Resumo:
Blends of Acrylonitrile rubber with Maleic anhydride grafted Whole Tyre Reclaim WTR (MA-g-WTR) have been prepared and the cure and mechanical properties have been studied with respect to reclaim content. Control compounds containing unmodified WTR were also prepared for comparison. Grafting was confirmed by IR studies. Blends containing grafted WTR showed higher minimum torque and (max-min) torque. They also showed longer cure time, scorch time and lower cure rate. Grafting of the WTR with maleic anhydride also resulted in the improved tensile strength, abrasion resistance, compression set and resilience. However, the heat build up under dynamic loading was marginally higher for the blends containing grafted reclaimed rubber.
Resumo:
Mechanical properties and thermal degradation of natural rubber compounds containing castor oil were studied to evaluate its suitability as plasticizer. Naphthenic oil was used as a reference plasticizer. The cure time was marginally lower in the case of castor oil mixes, probably due to the presence offree fatty acids in it. The tear strength and modulus were better in the case of mixes containing castor oil, while most of the other mechanical properties were comparable to the mixes containing naphthenic oil. The heat build up and compression set were higher than that of the naphthenic oil mixes. Thermal studies showed an increase of 8 °C in the temperature of initiation of degradation and an increase of 6 °C in the temperature at which the peak rate of degradation occurred. The peak rate of degradation was comparable to that of the reference compound
Resumo:
Mechanical properties and thermal degradation characteristics of natural rubber compounds captaining coconut oil were compared with that of a control compound containing naphthenic oil. Cure time was marginally lower in the case of coconut oil mixes, probably due to the presence of free fatty acids. Tensile strength , tear strength, resilience and abrasion resistance were better than the naphthenic oil-based compounds . Compression set and hardness were marginally inferior The coconut oil mixes had a crosslink density comparable to that of the reference compound. Thermal studies showed that the temperature of initiation of degradation was increased by 10°C and the temperature at which the peak rate of degradation occured was increased by 7°C. The peak rate of degradation was compa rable to the control compound.
Resumo:
The rheological characteristics of short Nylon-6 fiber reinforced styrene butadiene rubber (SBR) were studied using a capillary rheometer. The study was done with respect to the effect of shear rate, fiber concentration, and temperature on shear viscosity and die swell. All the melts showed pseudoplastic nature, which decreased with increasing temperature. Shear viscosity increased in the presence of fibers. Introduction of fiber reduces the temperature sensitivity of the rubber matrix. A reduction in die swell was found in presence of fibers.
Resumo:
The effect of diphenylmethane diisocyanate (MDI) -polyethyleneglycol (PEG) resin on the cure characteristics and mechanical properties of nitrile rubber/whole tyre eclaim-short nylon fiber composite-was studied. At a constant loading of 5 phr, the resin composition was varied. The minimum torque .,id (maximum - minimum) torque increased with isocyanate concentration. Scorch time and cure time showed a reduction on introduction of bonding agent. Properties like tensile strength, tear strength, and abrasion resistance increased with increase in MDI/PEG ratio, and these properties are higher in the longitudinal direction of fiber orientation. Compression set increased with isocyanate concentration and the resilience remain unchanged.
Resumo:
Cure characteristics and mechanical properties of acrylonitrile butadiene rubber/reclaimed rubber blends were studied. Minimum torque, (ma)dmum -minimum) torque, scorch time, cure time and cure rate decreased in presence of reclaimed rul3ber. Tensile strength, elongation at break and compression set increased'with increase in reclaim content. Resilience and abrasion resistance decreased with reclaim loading. Heat build up was higher for the blends. The ageing resistance of the blends was inferior to that of the gum compound.
Resumo:
Cure characteristics and mechanical properties of styrene butadiene rubber reclaimed rubber blends were studied. The blends showed improved processability, as indicated by the minimum torque values. Cure characteristics like minimum torque, (maximum-minimum) torque, cure time and cure rate decreased in the presence of reclaimed rubber. Tensile strength, tear strength, elongation at break were higher for blends. Resilience decreased with reclaim content. Compression set and abrasion loss were higher in the blends.
Resumo:
The cure characteristics of short fiber-polyurethane elastomer were studied with respect to different fiber-matrix bonding agents. A hexamethylenetetramine- resorcinol -hydrated silica based bonding agent was found to affect the stability of the composite. A new bonding agent, TP resin, based on polymeric toluenediisocyanate and polypropylene glycol has been developed. Cure characteristics of the composite with and without TP resin at different fiber loadings were also compared. Minimum torque, scorch time and optimum cure time increased with fiber content. Maximum torque was consistently higher with TP resin at all fiber loadings.
Resumo:
The thermal degradation of short kevlar fibre-thermoplastic polyurethane (TPU) composites has been studied by Thermogravimetric Analysis (TGA) and Differential Scanning Calorimetry (DSC). TGA showed that the thermal degradation of TPU takes place in two steps with peak maxima (T1max and T2ma,) at 383°C and 448°C, respectively. In the presence of 10-40 phr of short kevlar fibres, T1_ and T2max were shifted to lower temperatures. The temperature of onset of degradation was increased from 245 to 255°C at 40 parts per hundred rubber (phr) fibre loading. Kinetic studies showed that the degradation of TPU and kevlar-TPU composite follows first-order reaction kinetics. The DSC study showed that there is an improvement in thermal stability of TPU in the presence of 20 phr of short kevlar fibres.