997 resultados para AMORPHOUS IRON OXYHYDROXIDE


Relevância:

20.00% 20.00%

Publicador:

Resumo:

The rare earth iron garnets Ln3Fe5O12 and Y3AlxFe5-xO12, where x=1.0-5.0, and Y1.5Gd1.5Al0.2Fe4.8O12 have been prepared by the combustion of redox mixtures containing corresponding metal nitrates and oxalyl dihydrazide, i.e. C2H6N4O2 at 350-degrees-C. The solid combustion products are amorphous, submicrometre-sized powders which, on heating at 750-degrees-C for 3 h, yield crystalline single-phase garnets. The particle size of the garnets is below 1 mum and the surface area ranges from 16 to 90 m2 g-1. Yttrium iron garnet could be sintered to a density of more than 95% at 1200-degrees-C for 3 h, giving an average grain size of 3-5 mum.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Trace of iron(III) are determined by differential pulse polarography in a medium of sodium hydroxide and sodium bromate using the catalytic current. Various cations do not interfere. The relative standard deviation is 2%.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Are evaporation of graphite with Fe, Co and Ni yields two distinct types of metal nanoparticles, wrapped in graphitic layers and highly resistant to oxidation. Electron microscopy shows that the metal particles (10-40 nm) in the stub region are encapsulated in carbon onions, the particles in the soot being considerably smaller (2-15 nm). The metal particles in the soot are either ferromagnetic with lowered Curie temperatures or superparamagnetic.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Iron(III) complexes FeL(B)] (1-5) of a tetradentate trianionic phenolate-based ligand (L) and modified dipyridophenazine bases (B), namely, dipyrido-6,7,8,9-tetrahydrophenazine (dpqC in 1), dipyrido3,2-a:2',3'-c]phenazine-2-carboxylic acid (dppzc in 2), dipyrido3,2-a:2',3'-c]phenazine-11-sulfonic acid (dppzs in 3), 7-aminodipyrido3,2-a:2',3'-c]phenazine (dppza in 4) and benzoi]dipyridro3,2-a:2',3'-c]phenazine (dppn in 5), have been synthesized, and their photocytotoxic properties studied along with their dipyridophenazine analogue (6). The complexes have a five. electron paramagnetic iron(III) center, and the Fe(III)/Fe(II) redox couple appears at about 0.69 V versus SCE in DMF-0.1 M TBAP. The physicochemical data also suggest that the complexes possess similar structural features as that of its parent complex FeL(dppz)] with FeO3N3 coordination in a distorted octahedral geometry. The DNA-complex and protein-complex interaction studies have revealed that the complexes interact favorably with the biomolecules, the degree of which depends on the nature of the substituents present on the dipyridophenazine ring. Photocleavage Of pUC19 DNA by the complexes has been studied using visible light of 476, 530, and 647 nm wavelengths. Mechanistic investigations with inhibitors show formation of HO center dot radicals via a photoredox pathway. Photocytotoxicity study of the complexes in HeLa cells has shown that the dppn complex (5) is highly active in causing cell death in visible light with sub micromolar IC50 value. The effect of substitutions and the planarity of the phenazine moiety on the cellular uptake are quantified by determining the total Cellular iron content using the inductively coupled plasma-optical emission spectrometry (ICP-OES) technique. The cellular uptake increases marginally with an increase in the hydrophobicity of the dipyridophenazine ligands whereas complex 3 with dppzs shows very high uptake. Insights into the cell death mechanism by the dppn complex 5, obtained through DAFT nuclear staining in HeLa cells, reveal a rapid programmed cell death mechanism following photoactivation of complex 5 with visible light. The effect of substituent on the DNA photocleavage activity of the complexes has been rationalized from the theoretical studies.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Anomalous X-ray scattering (AXS) has been applied to study the structure of amorphous platinum disulfide, Pt1-xS2, prepared by the precipitation process. The local atomic arrangement in amorphous Pt1-xS2 was determined by the least-squares variational method so as to reproduce the experimental differential interference function at the Pt L(III) absorption edge by the AXS method as well as the ordinary interference function by MoK alpha. The structural unit in amorphous Pt1-xS2 is found to be a PtS6 octahedron, similar to that in crystalline PtS2. These octahedra share both their corners and edges, while only edge-sharing linkages occur in crystalline PtS2.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Amorphous carbon films are prepared by the pyrolysis of Tetra Chloro Phthalic Anhydride (TCPA) at different temperatures (700 degrees C to 900 degrees C). DC Conductivity measurements are done on the films in the temperature range 300K to 4.2K. It shows an activated temperature dependence with a small activation energy (0.02eV to 0.003eV). Variable range hopping is observed at low temperatures. The films are characterised by XRD, SEM, TEM, AFM and microRaman. The electronic structure of the film is used to explain the electrical behaviour.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

By carrying out contact-arc vaporization of graphite in a partial atmosphere of Fe(CO)5, an iron-adduct with C60 has been obtained. The adduct has been characterized by various techniques including mass spectrometry, Fe-57 Mossbauer spectroscopy and Fe K-EXAFS. Properties of this adduct are compared with those of an adduct prepared by solution method where Fe is clearly outside the cage. Results suggest that FeC60 obtained from the gas phase reaction has the Fe atom in the cage.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fe/AlOOH gels calcined and reduced at different temperatures have been investigated by a combined use of Mossbauer spectroscopy, x-ray diffraction, and electron microscopy in order to obtain information on the nature of the iron species formed as well as the various reduction processes. Calcination at or below 1070 K mainly gives reducible Fe3+ while calcination at higher temperatures gives substitutional Fe3+ in the form of Al2-xFexO3. The Fe3+ species in the calcined samples are, by and large, present in the form of small superparamagnetic particles. Crystallization of Al2O3 from the gels is catalyzed by Fe2O3 as well as FeAl2O4. Fe (20 wt. %)/AlOOH gels calcined at or below 870 K give FeAl2O4 when reduced in hydrogen at 1070 K or lower and a ferromagnetic Fe0-Al2O3 composite (with the metallic Fe particles >100 angstrom) when reduced at 1270 K. Samples calcined at 1220 K or higher give the Fe0-Al2O3 composite when reduced in the 870-12,70 K range, but a substantial proportion of Fe3+ remains unreduced in the form of Al2-xFexO3, showing thereby the extraordinary stability of substitutional Fe3+ to reduction even at high temperatures. Besides the ferromagnetic Fe0-Al2O3 composite, high-temperature reduction of Al2-xFexO3 yields a small proportion of superparamagnetic Fe0-Al2O3 wherein small metallic particles (<100 angstrom) are embedded in the ceramic matrix. In order to preferentially obtain the Fe0-Al2O3 composite on reduction, Fe/AlOOH gels should be calcined at low temperatures (less-than-or-equal-to 1100 K); high-temperature calcination results in Al2-xFexO3. Several modes of formation of FeAl2O4 are found possible during reduction of the gels, but a novel one is that involving the reaction, 2Fe3+ + Fe0 --> 3Fe2+.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Passivation of point and extended defects in GaSb has been observed as a result of hydrogenated amorphous silicon (a-Si:H) treatment by the glow discharge technique. Cathodoluminescence (CL) images recorded at various depths in the samples clearly show passivation of defects on the surface as well as in the bulk region. The passivation of various recombination centers in the bulk is attributed to the formation of hydrogen-impurity complexes by diffusion of hydrogen ions from the plasma a-Si:H acts as a protective cap layer and prevents surface degradation which is usually encountered by bare exposure to hydrogen plasma. An enhancement in luminescence intensity up to 20 times is seen due to the passivation of nonradiative recombination centers. The passivation efficiency is found to improve with an increase in a-Si:H deposition temperature. The relative passivation efficiency of donors and acceptors by hydrogen in undoped and Te-compensated p-GaSb has been evaluated by CL and by the temperature dependence of photoluminescence intensities. Most notably, effective passivation of minority dopants in tellurium compensated p-GaSb is evidenced for the first time. (C) 1996 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Amorphous conducting carbon films are prepared by plasma assisted chemical vapour deposition and their d.c. conductivity (similar to 100 Scm(-1)) is studied from 300K down to 4.2K. The films were irradiated by high energy ion beam(I+13, 170 MeV) with a dose of 10(13) ions/cm(2). As a result a marked decrease in conductivity by two to three orders in magnitude was observed. The structural changes and the defects in the films caused by ion irradiation are studied using photoluminescence, persistent photoconductivity, and ESR spectroscopy.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

[Fe(N2H5)2(H2O)2Cl2].Cl2, M(r) = 299.65, monoclinic, P2(1)/c, a = 8.027 (1), b = 5.725 (2), c = 11.430 (2) angstrom, beta = 97.08 (1)-degrees, V = 521.3 (2) angstrom 3, Z = 2, D(m) = 1.92, D(x) = 1.910 g cm-3, lambda(Mo K-alpha) = 0.71069 angstrom, mu = 24.5 cm-1, F(000) = 304, T = 295 K, final R = 0.0242 and wR = 0.0292 for 1411 significant [F(o) > 5.0-sigma(F(o))] reflections. The crystal contains discrete Cl- ions and complex [Fe(N2H5)2(H2O)2Cl2]2+ cations. In the complex cation, the Fe atom is bonded to two hydrazinium cations, two Cl atoms and two water molecules. The coordinated atoms are trans to each other. The ions are connected by both N-H...Cl and O-H...Cl type hydrogen bonds.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Laser processing of structure sensitive hypereutectic ductile iron, a cast alloy employed for dynamically loaded automative components, was experimentally investigated over a wide range of process parameters: from power (0.5-2.5 kW) and scan rate (7.5-25 mm s(-1)) leading to solid state transformation, all the way through to melting followed by rapid quenching. Superfine dendritic (at 10(5) degrees C s(-1)) or feathery (at 10(4) degrees C s(-1)) ledeburite of 0.2-0.25 mu m lamellar space, gamma-austenite and carbide in the laser melted and martensite in the transformed zone or heat-affected zone were observed, depending on the process parameters. Depth of geometric profiles of laser transformed or melt zone structures, parameters such as dendrile arm spacing, volume fraction of carbide and surface hardness bear a direct relationship with the energy intensity P/UDb2, (10-100 J mm(-3)). There is a minimum energy intensity threshold for solid state transformation hardening (0.2 J mm(-3)) and similarly for the initiation of superficial melting (9 J mm(-3)) and full melting (15 J mm(-3)) in the case of ductile iron. Simulation, modeling and thermal analysis of laser processing as a three-dimensional quasi-steady moving heat source problem by a finite difference method, considering temperature dependent energy absorptivity of the material to laser radiation, thermal and physical properties (kappa, rho, c(p)) and freezing under non-equilibrium conditions employing Scheil's equation to compute the proportion of the solid enabled determination of the thermal history of the laser treated zone. This includes assessment of the peak temperature attained at the surface, temperature gradients, the freezing time and rates as well as the geometric profile of the melted, transformed or heat-affected zone. Computed geometric profiles or depth are in close agreement with the experimental data, validating the numerical scheme.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A novel technique to generate forward phase conjugate wave by two-wave mixing (TWM) in photorefractive iron-doped lithium niobate crystal has been demonstrated. An optical beam from a positive transparency was forward phase conjugated by TWM technique. The experimental scheme was then extended to a specific interferometric application.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Porous, large surface area, metastable zirconias, are of importance to catalytic, electrochemical, biological, and thermal insulation applications. Combustion synthesis is a very commonly used method for producing such zirconias. However, its rapid nature makes control difficult. A simple modification has been made to traditional solution combustion synthesis to address this problem. It involves the addition of starch to yield a starting mixture with a ``dough-like'' consistency. Just 5 wt% starch is seen to significantly alter the combustion characteristics of the ``dough.'' In particular, it helps to achieve better control over reaction zone temperature that is significantly lower than the one calculated by the adiabatic approximation typically used in self-propagating high-temperature synthesis. The effect of such control is demonstrated by the ability to tune dough composition to yield zirconias with different phase compositions from the relatively elusive ``amorphous'' to monoclinic (> 30 nm grain size) and tetragonal pure zirconia (< 30 nm grain size). The nature of this amorphous phase has been investigated using infrared spectroscopy. Starch content also helps tailor porosity in the final product. Zirconias with an average pore size of about 50 mu m and specific surface area as large as 110 m2/g have been obtained.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Four types of cationic collectors were tested and evaluated for their performance in the reverse flotation of silica from the spiral preconcentrate of Kudremukh iron ore. A stagewise flotation was conducted by adding the reagent in three stages. Starch was used to depress hematite. Silica flotation was found to be very sensitive to the amount of cationic reagent added. The performance of the reagents was evaluated based on the percentage of silica and iron in the concentrate and percent recovery of iron obtained in the concentrate. Tests of significance, namely, t-test and F-test were performed to select the best two reagents for further investigations.