861 resultados para Microstructure of titanium


Relevância:

90.00% 90.00%

Publicador:

Resumo:

In this work, we report the synthesis of titanium oxide nanocrystals, especially the rutile TiO2 phase with nanorod morphology, by a method based on peroxotitanium complex decomposition. The results indicate that the anisotropic morphology reported for rutile TiO2 nanocrystals is related to the oriented attachment process. Despite the predominance of rutile nanocrystals at longer treatment times, the nanocrystals were obtained also in the anatase type, according to the degradation time adopted. XANES results evidenced the absence of structural correlation between the peroxytitanium complex and phase evolution, and the coexistence of the two phases strongly suggests a correlation of the oriented attachment mechanism and the rutile phase stabilization.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

We report the preparation and characterization of yttria-stabilized zirconia/nickel oxide composites (YSZ/NiO). This composite is the precursor material of the cermet YSZ/Ni, which is used as solid oxide fuel cell anode material. The performance of the anode is strongly dependent on the microstructural properties of the cermet. Therefore, the control of the microstructure of the YSZ/NiO composite is a key step for the fabrication of high-performance anodes. In this study, the composites were prepared by a modified liquid mixture technique. Scanning electron microscopy analysis evidenced the good dispersion of the phases and that NiO nanoparticles are spread over the YSZ surface. Sintered pellets were studied by X-ray diffraction and impedance spectroscopy. The main results show that the composite is comprised of a well-dispersed mixture of the two phases. The electrical conductivity data show that there is a strong dependence of the transport mechanism on the relative composition of phases. (c) 2005 Elsevier Ltd. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Transmission and scanning electron microscopy techniques were used to study the heterogeneities found in the microstructure of (SnO2Co3O4Nb2O5Fe2O3)-Co-.-Nb-.-Fe-. and (SnO2ZnONb2O5FC2O3)-Zn-.-Nb-.-F-. varistors. Second phases encountered both inside the grains and ingrain boundary regions were identified using energy dispersive spectrometry and electron diffraction patterns. Through the electrical characterisation, the presence of iron oxide among the additives was determined to highlight the non-linear properties of the specimens. A discussion on the influence of second phases on the non-linear features of these systems is also addressed. (C) 2004 Elsevier Ltd. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The effect of the properties of starting boron powders on the superconducting properties of MgB2 has been studied. The 92% and 96% pure powders produce lower surface reactivity and larger particle size than the 99% boron powder, as can be seen from Brunauer - Emmett - Teller (BET) and scanning electron microscopy (SEM) results, indicating that the low purity powders cannot be used to archive the same superconducting properties as those of samples made from pure 99% boron powder. However, the purity of 92% and 96% boron powders can be improved by using a simple chemical process, leading to enhanced magnetic critical current densities J(c). From x-ray diffraction (XRD) measurement, oxide impurity has been observed, which might be originated from the B2O3 phase in the boron powders. In order to get high performance MgB2, it is obviously important to control the phase composition and microstructure of amorphous boron starting powders and solid reaction conditions.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Surface modifications have been applied in endosteal bone devices in order to improve the osseointegration through direct contact between neoformed bone and the implant without an intervening soft tissue layer. Surface characteristics of titanium implants have been modified by addictive methods, such as metallic titanium, titanium oxide and hydroxyapatite powder plasma spray, as well as by subtractive methods, such as acid etching, acid etching associated with sandblasting by either AlO2 or TiO2, and recently by laser ablation. Surface modification for dental and medical implants can be obtained by using laser irradiation technique where its parameters like repetition rate, pulse energy, scanning speed and fluency must be taken into accounting to the appropriate surface topography. Surfaces of commercially pure Ti (cpTi) were modified by laser Nd:YVO4 in nine different parameters configurations, all under normal atmosphere. The samples were characterized by SEM and XRD refined by Rietveld method. The crystalline phases alpha Ti, beta Ti, Ti6O, Ti3O and TiO were formed by the melting and fast cooling processes during irradiation. The resulting phases on the irradiated surface were correlated with the laser beam parameters: the aim of the present work was to control titanium oxides formations in order to improve implants osseointegration by using a laser irradiation technique which is of great importance to biomaterial devices due to being a clean and reproducible process. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Antimony doped tin oxide thin films were deposited on glass by a chemical route derived from Pechini method. Particular emphasis was given to the microstructure of crystallized films. Crystalline phase formation was studied by grazing incident X-ray diffraction and by thermal analyses. Scanning electron microscopy was carried out for microstructure characterization, surface roughness was observed using scanning tunneling microscope and the optical transmittance measurements were performed in the wavelength range of 200-800 nm. (C) 2002 Kluwer Academic Publishers.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The electronic structure of Pb1-xLaxTiO3 (PLT) compounds for x ranging from 0 to 30 at. % of La is investigated by means of soft x-ray absorption near edge structure (XANES) at the Ti L-3,L-2 and O K edges. The greatest modification in the structure of the Ti 2p XANES spectra of the PLT compounds is observed in the region of the high energy peak of the L-3 edge (e(g) states), which exhibits a splitting in the undoped sample. As the amount of lanthanum increases, this splitting becomes less pronounced. This modification is interpreted as a decrease in the degree of disorder of titanium atoms, which is correlated to the substitution of Pb by La atoms. The structural changes observed at the low energy peaks of the O K-edge XANES spectra of the PLT compounds may be interpreted in terms of hybridization between O 2p, Ti 3d, and Pb 6p orbitals. A decrease in the degree of hybridization observed as Pb atoms are replaced by La atoms may be related to the differences in the ferroelectric properties observed between x=0.0 and x=0.30 compounds. (c) 2006 American Institute of Physics.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

In this work the thermal lens, thermal relaxation calorimetry and interferometric methods are applied to investigate the thermo-optical properties of tellurite glasses (in mol%: 80TeO(2)-20 Li2O(TeLi), 80TeO(2)-15Li(2)O-5TiO(2) (TeLiTi-5) and 80TeO(2)-10Li(2)O-10TiO(2) (TeLiTi-10)). Thermal diffusivity, thermal conductivity, specific heat and the temperature coefficients of refractive index, optical path length, thermal expansion and electronic polarizability were determined. The use of three independent methods was useful for a complete characterization of the studied tellurite glasses. In addition, our results showed that the thermal expansion coefficient and the temperature coefficient of the optical path length (dS/dT) were significantly modified with the introduction of titanium, which may be relevant for the application of these glasses in the photonic area. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

This paper describes the preparation and characterization of phenolic resins' thermospheres covered by a magnetic phase of iron oxide. The thermospheres were prepared by allowing phenol and formaldehyde to react under dispersion polymerization conditions and the iron oxide phase was incorporated in situ onto the phenolic resin particles by adding concentrated NH3 to FeCl2 in DMSO. This reaction was conducted at 70 degrees C under nitrogen atmosphere in a controlled temperature vessel, and the modified resin was isolated and dried in vacuo. Both pure and modified resins were characterized by DRX, TG- DTA, and MEV/ EDX. The modified particles were attracted by a magnetic field, indicating the fixation of magnetic iron oxide. No diffraction peaks were observed in DRX analysis; thermal analysis ( DTA) of both pure and modified resins presented exothermic events between 300 and 680 degrees C, and 300 and 570 degrees C, respectively, indicating the microstructure of the resin was modified after the treatment. Thermogravimetric analysis ( TGA) of the pure resin registered a 2.0% residue, compared to 8.0% for the modified resin. These residues correspond to about 7.0% of fixed iron oxide. MEV/ EDX analyses confirm the modification of the resins by the process of fixing iron oxide.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

90.00% 90.00%

Publicador:

Resumo:

In this paper an unprecedent thermo-reversible sol-gel transition for titania nanoparticles dispersed in a solution of p-toluene sulfonic acid (PTSH) in isopropanol is reported. The sol formed by the thermo-hydrolysis at 60 degrees C of titanium tetraisopropoxide (Ti((OPr)-Pr-i)(4)) reversibly changes into a turbid gel upon cooling to room temperature. Turbidimetric measurements performed for samples containing different nominal acidity ratios (A = [PTSH]/[Ti]) have evidenced that the gel transformation temperature increases from 20 to 35 degrees C as the [PTSH]/[Ti] ratio increases from 0.2 to 2.0. SAXS results indicate that the thermo-reversible gelation is associated to a reversible aggregation of a monodisperse set of titania nanoparticles with average gyration radius of approximate to 2 nm. From the different PTSH species evidenced by Raman spectroscopy and TG/DTA of dried gels we proposed that the then-no-reversible gelation in this systems is induced by the formation of a supramolecular network, in which the protonated surface of nanoparticles is interconnected through cooperative hydrogen bonds between -SO3 groups of p-toluene sulfonic acid. (C) 2009 Elsevier Ltd. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Objectives: This study evaluated the marginal gaps on several surfaces of onlays created with the Cerec 3D system using one intraoral and two extraoral optical impression methods. Methods: A human molar (#19) was mounted with its adjacent teeth on a typodont (Frasaco) and prepared for a MODL onlay. The typodont was assembled in the mannequin head in order to simulate clinical conditions. The same operator took 36 individual optical impressions using a CEREC 3D camera. For group 1 (IP), a thin layer of titanium dioxide powder (CEREC powder-VITA) was applied directly onto the surface of the preparation for imaging (n=12). For group 2 (EP), a sectional impression was taken with hydrocolloid Identic Syringable (Dux Dental), a die made with polyvinylsiloxane KwikkModel Scan (R-dental Dentalerzeugnisse GmbH) and powdered with titanium dioxide for imaging (n=12). For group 3 (ES), a sectional impression was taken with PVS and a sectional stock tray, a die fabricated in stone (Diamond die- HI-TEC Dental Products) and the die being imaged without powdering (n=12). One operator designed and machined the onlays in Vita Blocks Mark II for Cerec (VITA) using a CEREC 3D. The marginal gaps (pm) were measured with an optical microscope (50x) at 12 points, three on each surface of the MODL. The results were analyzed by two-way ANOVA/Tukey's (p=0.05). Results: The overall mean marginal gaps (mu m) for the three methods were: IP=111.6 (+/- 34.0); EP=161.4 (+/- 37.6) and ES=116.8 (+/- 42.3). IP and ES were equal, but both were significantly less than EP. The pooled mean marginal gaps (mu m) for the occlusal = 110.5 (+/- 39) and lingual = 111.5 (+/- 30.5) surfaces were equivalent and significantly less than the distal = 136.5 (+/- 42.5) and mesial = 161.1 (+/- 43.3). Conclusion: The marginal gap of CEREC 3D onlay restorations was not different when the optical impression was taken intraorally vs extraorally using a stone cast that does not require powdering. The lingual and occlusal surfaces showed the lowest gaps.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

90.00% 90.00%

Publicador:

Resumo:

In orofacial implantology there are many types of implants for the different systems. Among these is the implant surface type, e.g., a screw type, cylindrical and laminar. Furthermore, the implants are different in their dimensions, their metal composition, their surface condition, such as smooth, grit or layered surfaces and in their methods of application. Two different self-tapping implants, one smooth and the other grit-blasted, are screwed into the bone, and another one with a plasma of titanium coating, which is also in a screw form but with greater spaces between the screw threads are compared. The greatest amount of bone deposition in the bone/implant interface was encountered in the latter one, the smooth surfaced implant being in second place. All of these systems can alter the implant healing process and to demonstrate this, we injected bone markers in the rabbits over different periods of time so as to observe the different areas of bone deposition in the tibias where the implants had been inserted. The bone tracers used were Alizarin, Calcein and Xylenol-orange. The amount of deposition was calculated by using the method of surface morphometry.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Co3O4 can be used as electrocatalyst for oxygen evolution reaction. The macro and microstructure of the oxide, obtained by compacting and sintering lithium-doped Co3O4 powder in atmosphere of dry air and in conditions of controlled temperature and time was analyzed by metallographic techniques. The porous material was characterized by XRD, SEM and EDS combined techniques. For working temperatures up to 1200°C, the pellet was consituted of particles with varying sizes over a wide range of particle size and, at higher temperatures CoO is formed and polymorphic transformation was observed. The materials were also characterized electrochemically in alkaline media by open circuit potential and potentiodynamic I/E measurements. The results were compared to those previously prepared by others by thermal deposition.