Self-organized InGaAs QDs are intensively studied for optoelectronic applications. Several approaches are in study to reach the emission wavelengths needed for these applications. The use of antimony (Sb) in either the capping layer or into the dots is one example. However, these studies are normally focused on buried QD (BQD) where there are still different controversial theories concerning the role of Sb. Ones suggest that Sb incorporates into the dot [1], while others support the hypothesis that the Sb occupies positions surrounding the dot [2] thus helping to keep their shape during the capping growth.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Quantum dot infrared photodetectors (QDIPs) are very attractive for many applications such as infrared imaging, remote sensing and gas sensing, thanks to its promising features such as high temperature operation, normal incidence response and low dark current [1]. However, the key issue is to obtain a high-quality active region which requires an optimization of the nanostructure. By using GaAsSb capping layer, InAs QDs have improved their optical emission in the range between 1.15 and 1.3 m (at Sb composition of 14 %), due to a reduction of a compressive strain in QD and an increment of a QD height [2]. In this work, we have demonstrated strong and narrow intraband photoresponses at ~ 5 m from GaAsSb-capped InAs/GaAs QDIPs under normal light-incidence.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Diluted nitride self-assembled In(Ga)AsN quantum dots (QDs) grown on GaAs substrates are potential candidates to emit in the windows of maximum transmittance for optical fibres (1.3-1.55 μm). In this paper, we analyse the effect of nitrogen addition on the indium desorption occurring during the capping process of InxGa1−xAs QDs (x = l and 0.7). The samples have been grown by molecular beam epitaxy and studied through transmission electron microscopy (TEM) and photoluminescence techniques. The composition distribution inside the dots was determined by statistical moiré analysis and measured by energy dispersive X-ray spectroscopy. First, the addition of nitrogen in In(Ga)As QDs gave rise to a strong redshift in the emission peak, together with a large loss of intensity and monochromaticity. Moreover, these samples showed changes in the QDs morphology as well as an increase in the density of defects. The statistical compositional analysis displayed a normal distribution in InAs QDs with an average In content of 0.7. Nevertheless, the addition of Ga and/or N leads to a bimodal distribution of the Indium content with two separated QD populations. We suggest that the nitrogen incorporation enhances the indium fixation inside the QDs where the indium/gallium ratio plays an important role in this process. The strong redshift observed in the PL should be explained not only by the N incorporation but also by the higher In content inside the QDs

Relevância:

10.00% 10.00%

Publicador:

Resumo:

SUMMARY Concentration Photovoltaic Systems (CPV) have been proposed as an alternative to conventional systems. During the last years, there has been a boom of the CPV industry caused by the technological progress in all the elements of the system. and mainly caused by the use of multijunction solar cells based on III-V semiconductors, with efficiencies exceeding to 43%. III-V solar cells have been used with high reliability results in a great number of space missions without concentration. However, there are no previous results regarding their reliability in concentration terrestrial applications, where the working conditions are completely different. This lack of experience, together with the important industrial interest, has generated the need to evaluate the reliability of the cells. For this reason, nowadays there are several research centers around the undertaking this task. The evaluation of the reliability of this type of devices by means of accelerated tests is especially problematic when they work at medium or high concentration, because it is practically impossible to emulate real working conditions of the cell inside climatic chambers. In fact, as far as we know, the results that appear in this Thesis are the first estimating the Activation Energy of the failure mechanism involved, as well as the warranty of the III-V concentrator solar cells tested here. To evaluate the reliability of III-V very high concentrator solar cells by means of accelerated tests, a variety of activities, described in this Thesis have been carried out. The First Part of the memory presents the theoretical part of the Doctoral Thesis. After the Introduction, chapter 2 presents the state of the art in degradation and reliability of CPV systems and solar cells. Chapter 3 introduces some reliability definitions and the application of specific statistical functions to the evaluation of the reliability and parameters. From these functions, important parameters will be calculated to be used later in the experimental results of Thesis. The Second Part of the memory contains the experimental. Chapter 4 shows the types of accelerated tests and the main goals pursuit with them when carried out over CPV systems and solar cells. In order to evaluate quantitatively the reliability of the III-V concentrator solar cells used in these tests, some modifications have been introduced which discussion will be tackled here. Based on this analysis the working plan of the tests carried out in this Doctoral Thesis is presented. Chapter 5 presents a new methodology as well as the necessary instrumentation to carry out the tests described here. This new methodology takes into account the adaptation, improvement and novel techniques needed to test concentrator solar cells. The core of this memory is chapter 6, which presents the results of the characterization of the cells during the accelerated life tests and the analysis of the aforementioned results with the purpose of getting quantitative values of reliability in real working conditions. The acceleration factor of the accelerated life tests, under nominal working conditions has been calculated. Accordingly, the validity of the methodology as well as the calculations based on the reliability assessment, have also been demonstrated. Finally, quantitative values of degradation, reliability and warranty of the solar cells under field nominal working conditions have been calculated. With the development of this Doctoral Thesis the reliability of very high concentrator GaAs solar cells of small area has been evaluated. It is very interesting to generalize the procedures described up to this point to III-V multijunction solar cells of greater area. Therefore, chapter 7 develops this generalization and introduces also a useful thermal modeling by means of finite elements of the test cells’ circuits. In the last chapter, the summary of the results and the main contributions of this Thesis are outlined and future research activities are identified. RESUMEN Los Sistemas Fotovoltaicos de Concentración (SFC) han sido propuestos como una alternativa a los sistemas convencionales de generación de energía. Durante los últimos años ha habido un auge de los SFC debido a las mejoras tecnológicas en todos los elementos del sistema, y principalmente por el uso de células multiunión III-V que superan el 43% de rendimiento. Las células solares III-V han sido utilizadas con elevada fiabilidad en aplicaciones espaciales sin concentración, pero no existe experiencia de su fiabilidad en ambiente terrestre a altos niveles de concentración solar. Esta falta de experiencia junto al gran interés industrial ha generado la necesidad de evaluar la fiabilidad de las células, y actualmente hay un significativo número de centros de investigación trabajando en esta área. La evaluación de la fiabilidad de este tipo de dispositivos mediante ensayos acelerados es especialmente problemática cuando trabajan a media o alta concentración por la casi imposibilidad de emular las condiciones de trabajo reales de la célula dentro de cámaras climáticas. De hecho, que sepamos, en los resultados de esta Tesis se evalúa por primera vez la Energía de Activación del mecanismo de fallo de las células, así como la garantía en campo de las células de concentración III-V analizadas. Para evaluar la fiabilidad de células solares III-V de muy alta concentración mediante ensayos de vida acelerada se han realizado diversas actividades que han sido descritas en la memoria de la Tesis. En la Primera Parte de la memoria se presenta la parte teórica de la Tesis Doctoral. Tras la Introducción, en el capítulo 2 se muestra el estado del arte en degradación y fiabilidad de células y Sistemas Fotovoltaicos de Concentración. En el capítulo 3 se exponen de forma resumida las definiciones de fiabilidad y funciones estadísticas que se utilizan para la evaluación de la fiabilidad y sus parámetros, las cuales se emplearán posteriormente en los ensayos descritos en este Tesis. La Segunda Parte de la memoria es experimental. En el capítulo 4 se describen los tipos y objetivos de los ensayos acelerados actualmente aplicados a SFC y a las células, así como las modificaciones necesarias que permitan evaluar cuantitativamente la fiabilidad de las células solares de concentración III-V. En base a este análisis se presenta la planificación de los trabajos realizados en esta Tesis Doctoral. A partir de esta planificación y debido a la necesidad de adaptar, mejorar e innovar las técnicas de ensayos de vida acelerada para una adecuada aplicación a este tipo de dispositivos, en el capítulo 5 se muestra la metodología empleada y la instrumentación necesaria para realizar los ensayos de esta Tesis Doctoral. El núcleo de la memoria es el capítulo 6, en él se presentan los resultados de caracterización de las células durante los ensayos de vida acelerada y el análisis de dichos resultados con el objetivo de obtener valores cuantitativos de fiabilidad en condiciones reales de trabajo. Se calcula el Factor de Aceleración de los ensayos acelerados con respecto a las condiciones nominales de funcionamiento a partir de la Energía de Activación obtenida, y se demuestra la validez de la metodología y cálculos empleados, que son la base de la evaluación de la fiabilidad. Finalmente se calculan valores cuantitativos de degradación, fiabilidad y garantía de las células en condiciones nominales en campo durante toda la vida de la célula. Con el desarrollo de esta Tesis Doctoral se ha evaluado la fiabilidad de células III-V de área pequeña, pero es muy interesante generalizar los procedimientos aquí desarrollados para las células III-V comerciales de área grande. Por este motivo, en el capítulo 7 se analiza dicha generalización, incluyendo el modelado térmico mediante elementos finitos de los circuitos de ensayo de las células. En el último capítulo se realiza un resume del trabajo y las aportaciones realizadas, y se identifican las líneas de trabajo a emprender en el futuro.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Los sistemas de concentración fotovoltaica (CPV) parecen ser una de las vías más prometedoras para generar electricidad a gran escala a precios competitivos. La investigación actual se centra en aumentar la eficiencia y la concentración de los sistemas para abaratar costes. Al mismo tiempo se investiga sobre la fiabilidad de los diferentes componentes que integran un sistema de concentración, ya que para que los sistemas de concentración sean competitivos es necesario que tengan una fiabilidad al menos similar a los sistemas basados en células de silicio. En la presente tesis doctoral se ha llevado a cabo el estudio de aspectos avanzados de células solares multi-unión diseñadas para trabajar a concentraciones ultra-altas. Para ello, se ha desarrollado un modelo circuital tridimensional distribuido con el que simular el comportamiento de las células solares triple-unión bajo distintas condiciones de funcionamiento, así mismo se ha realizado una caracterización avanzada de este tipo de células para comprender mejor su modo de operación y así poder contribuir a mejorar su eficiencia. Finalmente, se han llevado a cabo ensayos de vida acelerados en células multiunión comerciales para conocer la fiabilidad de este tipo de células solares. Para la simulación de células solares triple-unión se ha desarrollado en la presente tesis doctoral un modelo circuital tridimensinal distribuido el cuál integra una descripción completa de la unión túnel. De este modo, con el modelo desarrollado, hemos podido simular perfiles de luz sobre la célula solar que hacen que la densidad de corriente fotogenerada sea mayor a la densidad de corriente pico de la unión túnel. El modelo desarrollado también contempla la distribución lateral de corriente en las capas semiconductoras que componen y rodean la unión túnel. Por tanto, se ha podido simular y analizar el efecto que tiene sobre el funcionamiento de la célula solar que los concentradores ópticos produzcan perfiles de luz desuniformes, tanto en nivel de irradiancia como en el contenido espectral de la luz (aberración cromática). Con el objetivo de determinar cuáles son los mecanismos de recombinación que están limitando el funcionamiento de cada subcélula que integra una triple-unión, y así intentar reducirlos, se ha llevado a cabo la caracterización eléctrica de células solares monouni ón idénticas a las subcelulas de una triple-unión. También se ha determinado la curva corriente-tensión en oscuridad de las subcélulas de GaInP y GaAs de una célula dobleunión mediante la utilización de un teorema de reciprocidad electro-óptico. Finalmente, se ha analizado el impacto de los diferentes mecanismos de recombinación en el funcionamiento de la célula solar triple-unión en concentración. Por último, para determinar la fiabilidad de este tipo de células, se ha llevado a cabo un ensayo de vida acelerada en temperatura en células solares triple-unión comerciales. En la presente tesis doctoral se describe el diseño del ensayo, el progreso del mismo y los datos obtenidos tras el análisis de los resultados preliminares. Abstract Concentrator photovoltaic systems (CPV) seem to be one of the most promising ways to generate electricity at competitive prices. Nowadays, the research is focused on increasing the efficiency and the concentration of the systems in order to reduce costs. At the same time, another important area of research is the study of the reliability of the different components which make up a CPV system. In fact, in order for a CPV to be cost-effective, it should have a warranty at least similar to that of the systems based on Si solar cells. In the present thesis, we will study in depth the behavior of multijunction solar cells under ultra-high concentration. With this purpose in mind, a three-dimensional circuital distributed model which is able to simulate the behavior of triple-junction solar cells under different working conditions has been developed. Also, an advanced characterization of these solar cells has been carried out in order to better understand their behavior and thus contribute to improving efficiency. Finally, accelerated life tests have been carried out on commercial lattice-matched triple-junction solar cells in order to determine their reliability. In order to simulate triple-junction solar cells, a 3D circuital distributed model which integrates a full description of the tunnel junction has been developed. We have analyzed the behavior of the multijunction solar cell under light profiles which cause the current density photo-generated in the solar cell to be higher than the tunnel junction’s peak current density. The advanced model developed also takes into account the lateral current spreading through the semiconductor layers which constitute and surround the tunnel junction. Therefore, the effects of non-uniform light profiles, in both irradiance and the spectral content produced by the concentrators on the solar cell, have been simulated and analyzed. In order to determine which recombination mechanisms are limiting the behavior of each subcell in a triple-junction stack, and to try to reduce them when possible, an electrical characterization of single-junction solar cells that resemble the subcells in a triplejunction stack has been carried out. Also, the dark I-V curves of the GaInP and GaAs subcells in a dual-junction solar cell have been determined by using an electro-optical reciprocity theorem. Finally, the impact of the different recombination mechanisms on the behavior of the triple-junction solar cell under concentration has been analyzed. In order to determine the reliability of these solar cells, a temperature accelerated life test has been carried out on commercial triple-junction solar cells. In the present thesis, the design and the evolution of the test, as well as the data obtained from the analysis of the preliminary results, are presented.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this work, a fiber-based optical powering (or power-by-light) system capable of providing more than 1 W is developed. The prototype was used in order to power a shunt regulator for controlling the activation and deactivation of solar panels in satellites. The work involves the manufacture of a light receiver (a GaAs multiple photovoltaic converter (MPC)), a power conditioning block, and a regulator and the implementation and characterization of the whole system. The MPC, with an active area of just 3.1 mm2, was able to supply 1 W at 5 V with an efficiency of 30%. The maximum measured device efficiency was over 40% at an input power (Pin) of 0.5 W. Open circuit voltage over 7 V was measured for Pin over 0.5 W. A system optoelectronic efficiency (including the optical fiber, connectors, and MPC) of 27% was measured at an output power (Pout) of 1 W. At Pout = 0.2 W, the efficiency was as high as 36%. The power conditioning block and the regulator were successfully powered with the system. The maximum supplied power in steady state was 0.2 W, whereas in transient state, it reached 0.44 W. The paper also describes the characterization of the system within the temperature range going from -70 to +100?°C.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Arsenic alloying is observed for epitaxial layers nominally intended to be In0.75Ga0.25N. Voids form beneath their interfaces with GaAs substrates, acting as sources of Ga + As out-diffusion into the growing epilayers. As a result, heteroepitaxial single-phase quaternary InxGa1-xAsyN1-y, films are formed with x similar to 0.55 and 0.05 menor que y menor que 0,10. While an undoped epilayer retains the wurtzite structure, a Mn-doped sample showed randomly spaced dopant segregations, which, together with a slightly higher As concentration, led to a transformation from the hexagonal to the twinned cubic phase.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We demonstrate site-controlled growth of epitaxial Ag nanocrystals on patterned GaAs substrates by molecular beam epitaxy with high degree of long-range uniformity. The alignment is based on lithographically defined holes in which position controlled InAs quantum dots are grown. The Ag nanocrystals self-align preferentially on top of the InAs quantum dots. No such ordering is observed in the absence of InAs quantum dots, proving that the ordering is strain-driven. The presented technique facilitates the placement of active plasmonic nanostructures at arbitrarily defined positions enabling their integration into complex devices and plasmonic circuits.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The behavior of quantum dot, quantum wire, and quantum well InAs/GaAs solar cells is studied with a very simplified model based on experimental results in order to assess their performance as a function of the low bandgap material volume fraction fLOW. The efficiency of structured devices is found to exceed the efficiency of a non-structured GaAs cell, in particular under concentration, when fLOW is high; this condition is easier to achieve with quantum wells. If three different quasi Fermi levels appear with quantum dots the efficiency can be much higher.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We report growth of InAs/GaAs quantum dots (QDs) by molecular beam epitaxy with low density of 2 μm−2 by conversion of In nanocrystals deposited at low temperatures. The total amount of InAs used is about one monolayer, which is less than the critical thickness for conventional Stranski–Krastanov QDs. We also demonstrate the importance of the starting surface reconstruction for obtaining uniform QDs. The QD emission wavelength is easily tunable upon post-growth annealing with no wetting layer signal visible for short anneals. Microphotoluminescence measurements reveal well separated and sharp emission lines of individual QDs.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The use of GaAsSbN capping layers on InAs/GaAs quantum dots (QDs) has recently been proposed for micro- and optoelectronic applications for their ability to independently tailor electron and hole confinement potentials. However, there is a lack of knowledge about the structural and compositional changes associated with the process of simultaneous Sb and N incorporation. In the present work, we have characterized using transmission electron microscopy techniques the effects of adding N in the GaAsSb/InAs/GaAs QD system. Firstly, strain maps of the regions away from the InAs QDs had revealed a huge reduction of the strain fields with the N incorporation but a higher inhomogeneity, which points to a composition modulation enhancement with the presence of Sb-rich and Sb-poor regions in the range of a few nanometers. On the other hand, the average strain in the QDs and surroundings is also similar in both cases. It could be explained by the accumulation of Sb above the QDs, compensating the tensile strain induced by the N incorporation together with an In-Ga intermixing inhibition. Indeed, compositional maps of column resolution from aberration-corrected Z-contrast images confirmed that the addition of N enhances the preferential deposition of Sb above the InAs QD, giving rise to an undulation of the growth front. As an outcome, the strong redshift in the photoluminescence spectrum of the GaAsSbN sample cannot be attributed only to the N-related reduction of the conduction band offset but also to an enhancement of the effect of Sb on the QD band structure.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The photoluminescence efficiency of GaAsSb-capped InAs/GaAs type II quantum dots (QDs) can be greatly enhanced by rapid thermal annealing while preserving long radiative lifetimes which are ∼20 times larger than in standard GaAs-capped InAs/GaAs QDs. Despite the reduced electron-hole wavefunction overlap, the type-II samples are more efficient than the type-I counterparts in terms of luminescence, showing a great potential for device applications. Strain-driven In-Ga intermixing during annealing is found to modify the QD shape and composition, while As-Sb exchange is inhibited, allowing to keep the type-II structure. Sb is only redistributed within the capping layer giving rise to a more homogeneous composition.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

IBPOWER is a Project awarded under the 7th European Framework Programme that aims to advance research on intermediate band solar cells (IBSCs). These are solar cells conceived to absorb below bandgap energy photons by means of an electronic energy band that is located within the semiconductor bandgap, whilst producing photocurrent with output voltage still limited by the total semiconductor bandgap. IBPOWER employs two basic strategies for implementing the IBSC concept. The first is based on the use of quantum dots, the IB arising from the confined energy levels of the electrons in the dots. Quantum dots have led to devices that demonstrate the physical operation principles of the IB concept and have allowed identification of the problems to be solved to achieve actual high efficiencies. The second approach is based on the creation of bulk intermediate band materials by the insertion of an appropriate impurity into a bulk semiconductor. Under this approach it is expected that, when inserted at high densities, these impurities will find it difficult to capture electrons by producing a breathing mode and will cease behaving as non-radiative recombination centres. Towards this end the following systems are being investigated: a) Mn: In1-xGax N; b) transition metals in GaAs and c) thin films.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The present work aims to assess Laser-Induced Plasma Spectrometry (LIPS) as a tool for the characterization of photovoltaic materials. Despite being a well-established technique with applications to many scientific and industrial fields, so far LIPS is little known to the photovoltaic scientific community. The technique allows the rapid characterization of layered samples without sample preparation, in open atmosphere and in real time. In this paper, we assess LIPS ability for the determination of elements that are difficult to analyze by other broadly used techniques, or for producing analytical information from very low-concentration elements. The results of the LIPS characterization of two different samples are presented: 1) a 90 nm, Al-doped ZnO layer deposited on a Si substrate by RF sputtering and 2) a Te-doped GaInP layer grown on GaAs by Metalorganic Vapor Phase Epitaxy. For both cases, the depth profile of the constituent and dopant elements is reported along with details of the experimental setup and the optimization of key parameters. It is remarkable that the longest time of analysis was ∼10 s, what, in conjunction with the other characteristics mentioned, makes of LIPS an appealing technique for rapid screening or quality control whether at the lab or at the production line.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

ZnTe doped with high concentrations of oxygen has been proposed in previous works as intermediate band (IB) material for photovoltaic applications. The existence of extra optical transitions related to the presence of an IB has already been demonstrated in this material and it has been possible to measure the absorption coefficient of the transitions from the valence band (VB) to the IB. In this work we present the first measurement of the absorption coefficient associated to transitions from the IB to the conduction band (CB) in ZnTe:O. The samples used are 4 ?m thick ZnTe layers with or without O in a concentration ~ 1019 cm-3, which have been grown on semi-insulating GaAs substrates by molecular beam epitaxy (MBE). The IB-CB absorption coefficient peaks for photon energies ~ 0.4 eV. It is extracted from reflectance and transmittance spectra measured using Fourier Transform Infrared (FTIR) spectroscopy. Under typical FTIR measurement conditions (low light intensity, broadband spectrum) the absorption coefficient in IB-to-CB transitions reaches 700 cm-1. This is much weaker than the one observed for VB-IB absorption. This result is consistent with the fact that the IB is expected to be nearly empty of electrons under equilibrium conditions in ZnTe(:O). The absorption for VB to IB transitions is also observed in the same samples through reflectance measurements performed in the visible range using a monochromator. These measurements are compared with the quantum efficiency (QE) from solar cells fabricated under similar conditions.