996 resultados para Endodontic cements
Resumo:
To investigate the surface hardness (Vickers hardness, HVN) of one light-curing flowable resin composite and five dual-curing resin cements after different polymerization procedures.
Resumo:
The objective of this pilot investigation was to evaluate the utility and precision of already existing limited cone-beam computed tomography (CBCT) scans in measuring the endodontic working length, and to compare it with standard clinical procedures.
Resumo:
The determination of root canal length is a significant outcome predictor for endodontic treatments. The aim of this prospective, controlled clinical study was to analyze endodontic working length measurements in preexisting cone-beam computed tomography (CBCT) scans and to compare them with clinical root canal length determination by using an electronic apex locator (EAL).
Resumo:
This work has investigated the possibility of use bauxite and oyster shell as mineral admixtures,to enhance the properties of metakaolin-based geopolymer cements. Raw materials(metakaolin, bauxite and oyster shell) were characterized in the first time by determination of their chemical and mineralogical compositions, particles size distribution, specific surface area, thermal analysis and then in the second time use to synthesized geopolymers. Different methods of analysis such as Fourier Transform Infrared spectroscopy(FTIR), X-Ray Diffractometry (XRD), and Scanning Electron Microscopy (SEM) were used to assess the variation of setting time, linear shrinkage and 28 days compressive strength of geopolymer pastes. The results of these analysis has showed that bauxite and oyster shells are source of Al2O3 and CaO respectively, and also contain crystalline phases. The geopolymers obtained by mixing metakaolin and bauxite have their setting time between 235 and 420min and their compressive strength between 40 and 57MPa ; for those obtained by mixing metakaolin and oyster shell the setting time is between 330 and 485min and compressive strength between 40 and 58MPa . The addition of a moderate amount (20% by mass) of bauxite or oyster shell led to improve the compressive strength of a metakaolin-based geopolymer of 43% (metakaolin-bauxite-based geopolymers) and 45% (metakaolin-oyster shell-based geopolymers) and decrease the linear shrinkage. More than 20% mineral additive has a deleterious effect on compressive strength and increase the setting time. Keywords: Metakaolin ; Bauxite ; Oyster shell ; synthesis ; Optimization; Geopolymer cements.
Resumo:
OBJECTIVES: The objectives of this in vitro study were (1) to assess the bond strength of the universal cement RelyX Unicem to dentin and to compare it with three conventional resin cements, (2) to test the influence of aging on their bonding capacity and (3) to test the influence of the operator on bonding quality by performing the same test in two different centers. METHODS: 160 third molars, divided into 80 for tests at the University of Zurich (Z) and 80 for tests at the University of Berne (B), were assigned to 2 x 8 subgroups of 10 teeth each. The specimens were prepared with the corresponding bonding agents and acrylic rods were luted either with RelyX Unicem (U), RelyX ARC (A), Multilink (M) or Panavia 21 (P). All specimens were stored in water for 24h (W) and half of the specimens were subjected to 1500 cycles of thermocycling (5 degrees C and 55 degrees C) (T). Bond strength was measured by means of a shear test. RESULTS: After water storage RelyX Unicem exhibited lowest bond strength (UWZ: 9.2+/-1.6 MPa, UWB: 9.9+/-1.2 MPa, AWZ: 15.3+/-6.0 MPa, AWB: 12.2+/-4.3 MPa, MWZ: 15.6+/-3.3 MPa, MWB: 12.4 MPa+/-2.4, PWZ: 13.4+/-2.9 MPa, PWB: 14.9+/-2.6 MPa). Thermocycling affected the bonding performance of all four cements. However, bond strength of RelyX Unicem was least influenced by thermocycling (UTZ: 9.4+/-2.9 MPa, UTB: 8.6+/-1.3 MPa, ATZ: 11.4+/-6.3 MPa, ATB: 13.3+/-3.7 MPa, MTZ: 15.4+/-3.1 MPa, MTB: 10.3+/-2.4 MPa, PTZ: 11.1+/-2.8 MPa, PTB: 11.3+/-2.8 MPa). SIGNIFICANCE: Although the bond strength of RelyX Unicem to dentin was lower in comparison to RelyX ARC, Multilink and Panavia 21, its bond strength was less sensitive to variations in handling and aging.
Resumo:
INTRODUCTION: This report of 2 cases describes the diagnostic procedures used to identify 2 Stafne's bone cavities (SBC) found in unusually anterior locations in the mandible, both mimicking periapical lesions of endodontic origin. METHODS: In the first patient, a 47-year-old man, an SBC was diagnosed in the area of teeth #27, 28, and 29. In the second patient, a 62-year-old man, the SBC was a fortuitous finding, because this patient was referred for dental implant therapy. RESULTS: In both cases, the final diagnosis was achieved by using limited cone beam computed tomography (CBCT) and magnetic resonance imaging (MRI). In both patients, the lingual bone cavity was found to be occupied by accessory salivary gland tissue. CONCLUSIONS: The combination of CBCT and MRI as noninvasive diagnostic techniques seems ideal to avoid surgical explorations, incisional biopsies, or enucleations of the lesion for diagnostic purposes.
Resumo:
Compression, tension and torsion tests were designed and completed successfully on a brushite and a precipitated hydroxyapatite cement in moist condition. Elastic and strength properties were measured for these three loading cases. For each cement, the full set of strength data was fitted to an isotropic Tsai-Wu criterion and the associated coefficients identified. Since the compressive Young's moduli were about 10% larger than the tensile moduli, the full set of elastic data of each cement was fitted to a conewise linear elastic model. Hysteresis of the stress-strain curves was also observed, indicating dissipation mechanisms within these cement microstructures. A comparison of the measured mechanical properties with human cancellous bone confirmed the indication of brushite as a bone filling material and the potential of the hydroxyapatite cement as a structural biomaterial.
Resumo:
Recent clinical trials have reported favorable early results for transpedicular vertebral cement reinforcement of osteoporotic vertebral insufficiencies. There is, however, a lack of basic data on the application, safety and biomechanical efficacy of materials such as polymethyl-methacrylate (PMMA) and calciumphospate (CaP) cements. The present study analyzed 33 vertebral pairs from five human cadaver spines. Thirty-nine vertebrae were osteoporotic (bone mineral density < 0.75 g/cm2), 27 showed nearly normal values. The cranial vertebra of each pair was augmented with either PMMA (Palacos E-Flow) or experimental brushite cement (EBC), with the caudal vertebra as a control. PMMA and EBC were easy to inject, and vertebral fillings of 20-50% were achieved. The maximal possible filling was inversely correlated to the bone mineral density (BMD) values. Cement extrusion into the spinal canal was observed in 12% of cases. All specimens were subjected to axial compression tests in a displacement-controlled mode. From load-displacement curves, the stiffness, S, and the maximal force before failure, Fmax, were determined. Compared with the native control vertebrae, a statistically significant increase in vertebral stiffness and Fmax was observed by the augmentation. With PMMA the stiffness increased by 174% (P = 0.018) and Fmax by 195% (P = 0.001); the corresponding augmentation with EBC was 120% (P = 0.03) and 113% (P = 0.002). The lower the initial BMD, the more pronounced was the augmentation effect. Both PMMA and EBC augmentation reliably and significantly raised the stiffness and maximal tolerable force until failure in osteoporotic vertebral bodies. In non-porotic specimens, no significant increase was achieved.
Resumo:
OBJECTIVES The aim of this study was to investigate micromechanical properties of five dual-curing resin cements after different curing modes including light curing through glass ceramic materials. MATERIALS AND METHODS Vickers hardness (VH) and indentation modulus (Y HU) of Panavia F2.0, RelyX Unicem 2 Automix, SpeedCEM, BisCem, and BeautiCem SA were measured after 1 week of storage (37 °C, 100 % humidity). The resin cements were tested following self-curing or light curing with the second-generation light-emitting diode (LED) curing unit Elipar FreeLight 2 in Standard Mode (1,545 mW/cm(2)) or with the third-generation LED curing unit VALO in High Power Mode (1,869 mW/cm(2)) or in XtraPower Mode (3,505 mW/cm(2)). Light curing was performed directly or through glass ceramic discs of 1.5 or 3 mm thickness of IPS Empress CAD or IPS e.max CAD. VH and Y HU were analysed with Kruskal-Wallis tests followed by pairwise Wilcoxon rank sum tests (α = 0.05). RESULTS RelyX Unicem 2 Automix resulted in the highest VH and Y HU followed by BeautiCem SA, BisCem, SpeedCEM, and finally Panavia F2.0. Self-curing of RelyX Unicem 2 Automix and SpeedCEM lowered VH and Y HU compared to light curing whereas self-curing of Panavia F2.0, BisCem, and BeautiCem SA led to similar or significantly higher VH and Y HU compared to light curing. Generally, direct light curing resulted in similar or lower VH and Y HU compared to light curing through 1.5-mm-thick ceramic discs. Light curing through 3-mm-thick discs of IPS e.max CAD generally reduced VH and Y HU for all resin cements except SpeedCEM, which was the least affected by light curing through ceramic discs. CONCLUSIONS The resin cements responded heterogeneously to changes in curing mode. The applied irradiances and light curing times adequately cured the resin cements even through 1.5-mm-thick ceramic discs. CLINICAL RELEVANCE When light curing resin cements through thick glass ceramic restorations, clinicians should consider to prolong the light curing times even with LED curing units providing high irradiances.
Resumo:
Objectives The aim of this study was to measure the degree of conversion (DC) of five dual-curing resin cements after different curing modes with a second- and a third-generation light-emitting diode (LED) curing unit. Additionally, irradiance of both light curing units was measured at increasing distances and through discs of two glass ceramics for computer-aided design/manufacturing (CAD/CAM). Materials and methods Irradiance and spectra of the Elipar FreeLight 2 (Standard Mode (SM)) and of the VALO light curing unit (High Power Mode (HPM) and Xtra Power Mode (XPM)) were measured with a MARC radiometer. Irradiance was measured at increasing distances (control) and through discs (1.5 to 6 mm thickness) of IPS Empress CAD and IPS e.max CAD. DC of Panavia F2.0, RelyX Unicem 2 Automix, SpeedCEM, BisCem, and BeautiCem SA was measured with an attenuated total reflectance–Fourier transform infrared spectrometer when self-cured (negative control) or light cured in SM for 40 s, HPM for 32 s, or XPM for 18 s. Light curing was performed directly (positive control) or through discs of either 1.5- or 3-mm thickness of IPS Empress CAD or IPS e.max CAD. DC was analysed with Kruskal–Wallis tests followed by pairwise Wilcoxon rank sum tests (α = 0.05). Results Maximum irradiances were 1,545 mW/cm2 (SM), 2,179 mW/cm2 (HPM), and 4,156 mW/cm2 (XPM), and all irradiances decreased by >80 % through discs of 1.5 mm, ≥95 % through 3 mm, and up to >99 % through 6 mm. Generally, self-curing resulted in the lowest DC. For some cements, direct light curing did not result in higher DC compared to when light cured through ceramic discs. For other cements, light curing through ceramic discs of 3 mm generally reduced DC. Conclusions Light curing was favourable for dual-curing cements. Some cements were more susceptible to variations in curing mode than others. Clinical relevance When light curing a given cement, the higher irradiances of the third-generation LED curing unit resulted in similar DC compared to the second-generation one, though at shorter light curing times.
Resumo:
PURPOSE The purpose of this study was to evaluate the bonding of glass ionomer cements (GICs) to sound and caries-affected dentin by microtensile bond strength (μTBS) and nanoleakage (NL) tests. METHODS Occlusal cavity preparations were made in 36 sound primary molars. Half of the specimens were submitted to a pH-cycling model to create simulated caries-affected dentin. Teeth were randomly restored with one of the three materials: (1) resin-modified GIC with nanoparticles (Ketac N100; KN); (2) resin-modified GIC (Vitremer; VI); and (3) high-viscosity GIC (Ketac Molar Easy Mix; KM). Specimens were tested using a microtensile test (1 mm/minute). One specimen from each tooth was immersed in ammoniacal silver nitrate for 24 hours and revealed after eight hours to assess interfacial NL. The μTBS means were analyzed by 2-way analysis of variance and Tukey's post hoc test. For NL, Kruskal-Wallis and Mann-Whitney tests were used (P<.05). RESULTS No difference was found between sound and caries-affected dentin (P>.05). KM showed the lowest GIC-dentin μTBS values, while VI and KN showed higher values. Infiltration of ammoniacal silver nitrate into the adhesive interface was not affected by sound or caries-affected dentin. CONCLUSION Caries-affected dentin does not jeopardize the bonding of glass ionomer cements to primary tooth dentin.
Resumo:
OBJECTIVE Fractured endodontic instruments inhibit optimal cleaning and filling of dental root canals, which may result in a less favorable prognosis for the tooth. Several techniques are available to remove fractured instruments; however, healthy tooth substance often must be destroyed in the process. This study was intended to evaluate Nd:YAG laser treatment as a method to remove fractured stainless steel instruments without destroying healthy tooth substance. METHOD AND MATERIALS Stainless steel endodontic instruments were fractured in 33 unprocessed root canals of mandibular central and lateral incisors and premolars in vitro. A brass tube charged with solder was placed at the coronal end of the fractured instrument and laser energy was used to melt the solder, connecting the fractured instrument with the brass tube. The success rates of connecting and removal of fractured instruments from the root channel were recorded for each case. RESULTS Connecting was achieved in every case in which more than 1.5 mm of the fractured instrument was tangible (22 out of 22). In cases where less than 1.5 mm was tangible, the rate for successful connection decreased to 4 out of 11 (36.4%). Fractured endodontic instruments were removed successfully in 17 out of 22 cases (77.3%) in which more than 1.5 mm was tangible. If less than 1.5 mm was tangible, the removal success rate decreased to 3 out of 11 cases (27.3%). CONCLUSION Our data support Nd:YAG laser-mediated connecting of a brass tube to a fractured endodontic instrument as a feasible and tissue conserving removal approach when more than 1.5 mm of the instrument is tangible.
Resumo:
PURPOSE To determine the impact of long-term storage on adhesion between titanium and zirconia using resin cements. MATERIALS AND METHODS Titanium grade 4 blocks were adhesively fixed onto zirconia disks with four resin cements: Panavia F 2.0 (Kuraray Europe), GC G-Cem (GC Europe), RelyX Unicem (3M ESPE), and SmartCem 2 (Dentsply DeguDent). Shear bond strength was determined after storage in a water bath for 24 h, 16, 90, and 150 days at 37°C, and after 6000 cycles between 5°C and 55°C. Fracture behavior was evaluated using scanning electron microscopy. RESULTS After storage for at least 90 days and after thermocycling, GC G-Cem (16.9 MPa and 15.1 MPa, respectively) and RelyX Unicem (10.8 MPa and 15.7 MPa, respectively) achieved higher shear bond strength compared to SmartCem 2 (7.1 MPa and 4.0 MPa, respectively) and Panavia F2 (4.1 MPa and 7.4 MPa, respectively). At day 150, GC G-Cem and RelyX Unicem caused exclusively mixed fractures. SmartCem 2 and Panavia F2 showed adhesive fractures in one-third of the cases; all other fractures were of mixed type. After 24 h (GC G-Cem: 26.0, RelyX Unicem: 20.5 MPa, SmartCem 2: 16.1 MPa, Panavia F2: 23.6 MPa) and 16 days (GC G-Cem: 12.8, RelyX Unicem: 14.2 MPa, SmartCem 2: 9.8 MPa, Panavia F2: 14.7 MPa) of storage, shear bond strength was similar among the four cements. CONCLUSION Long-term storage and thermocycling differentially affects the bonding of resin cement between titanium and zirconia.
Resumo:
PURPOSE The purpose of this study was to analyze the removal of implant-supported crowns retained by three different cements using an air-accelerated crown remover and to evaluate the patients' response to the procedure. MATERIALS AND METHODS This controlled clinical trial was conducted with 21 patients (10 women, 11 men; mean age: 51 ± 10.2 years) who had received a total of 74 implants (all placed in the posterior zone of the mandible). Four months after implant surgery, the crowns were cemented on standard titanium abutments of different heights. Three different cements (two temporary: Harvard TEMP and Improv; and one definitive: Durelon) were used and randomly assigned to the patients. Eight months later, one blinded investigator removed all crowns. The number of activations of the instrument (CORONAflex, KaVo) required for crown removal was recorded. The patients completed a questionnaire retrospectively to determine the impact of the procedure and to gauge their subjective perception. A linear regression model and descriptive statistics were used for data analysis. RESULTS All crowns could be retrieved without any technical complications or damage. Both abutment height (P = .019) and cement type (P = .004) had a significant effect on the number of activations, but the type of cement was more important. An increased total number of activations had no or only a weak correlation to the patients' perception of concussion, noise, pain, and unwillingness to use the device. CONCLUSIONS Cemented implant crowns can be removed, and the application of an air-accelerated device is a practicable method. A type of cement with appropriate retention force has to be selected. The impact on the patients' subjective perception should be taken into account.