976 resultados para random copolymers overall crystallization rate crystal growth rate isothermal crystallization kinetics poly (L-lactide)


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Syndiotactic polystyrene (sPS) nanorods of 200 and 80 nm diameters were prepared by infiltrating porous anodic alumina oxide templates with polymer melt, and the crystallinity and orientation of various forms of sPS crystals in the nanorods were studied by FTIR spectroscopy and electron diffraction. For sPS crystallized from amorphous state at lower temperatures, a-form crystals were found in the nanorods with random orientation and the same degree of crystallinity as that in the bulk. However, for sPS crystallized from molten state at 260 degrees C, while no preferred orientation was found for the chains in the melt, the beta-crystals formed in the nanorods oriented preferentially with the c-axis aligning perpendicular to the axial direction of the nanorod, and the degree of crystallinity was significantly lower than that in the bulk. The crystallinity decrease was more profound for nanorods of smaller diameter. These results were also supported by electron diffraction data and can be attributed to competition between nucleation and crystal growth in the nanotemplates.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The nanocomposites of polyamide1010 (PA1010) filled with carbon nanotubes (CNTs) were prepared by melt mixing techniques. The isothermal melt-crystallization kinetics and nonisothermal crystallization behavior of CNTs/PA1010 nanocomposites were investigated by differential scanning calorimetry. The peak temperature, melting point, half-time of crystallization, enthalpy of crystallization, etc. were measured. Two stages of crystallization are observed, including primary crystallization and secondary crystallization. The isothermal crystallization was also described according to Avrami's approach. It has been shown that the addition of CNTs causes a remarkable increase in the overall crystallization rate of PA1010 and affects the mechanism of nucleation and growth of PA1010 crystals. The analysis of kinetic data according to nucleation theories shows that the increment in crystallization rate of CNTs/PA1010 composites results from the decrease in lateral surface free energy.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Isothermal crystallization and melting behavior of nylon 66 and its blends with poly(ether imide) (PEI) were investigated by differential scanning calorimetry. Crystallization kinetics such as overall rate constant Z and index n were calculated according to Avrami approach. Crystallization in the blend was retarded with respect to that of pure nylon 66 by incorporation of PEI with high glass transition temperature (T-g). The lowest growth rate of the spherulites was observed in the blends containing 10 and 15 wt% fraction of PEI. A transition temperature where positively birefringent spherulites disappear and negative birefringent spherulites develop was measured by thermal analysis. The transition temperature increased with content of PEI in the blends. A suitable range of isothermally crystallization temperatures, 238.5-246 degrees C, is suggested For determining the equilibrium melting points by means of Hoffman-Weeks approach.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The overall isothermal crystallization kinetics for neat polypropylene and grafted polypropylene systems were investigated. The rate constants were corrected assuming the heterogeneous nucleation and three dimensional growth of polypropylene spherulites. A semiempirical equation for the radial growth rate of polypropylene spherulites was developed as a function of temperature, and was used to determine the number of effective nuclei of different temperatures. The number of nuclei in grafted samples was estimated to be 10(2)-10(3) times larger than that of neat polypropylene. (C) 1997 John Wiley & Sons, Inc.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Quantitative data on the crystallization kinetics of polymorphic polymers can be derived from the investigation of gross spherulitic morphology formed in isothermal conditions. Depending on distance between centers, and the time lag between their formation and relative growth rates, various types of boundary lines can be generated by the impinging of two spherical bodies whose radii increase linearly with time, In polymorphic polymers, different types of spherulites often develop simultaneously at different rates from sporadic or predetermined nuclei. In same cases, the so-called growth transformation, in which a nucleus of the fast growing specie is formed at the tip of an advancing lamella of the slower crystal form, provides an alternative mode of nucleation, It is shown that if only one event of growth transformation takes place at the front of a slow growing body, the fast growing spherulite swallows the parent one and the resultant shape of interspherulitic boundary is described by two symmetrical logarithmic spirals whose parameters can be extracted from micrographs taken at the end of crystallization. These concepts are applied to determine the radial growth rate of gamma form spherulites of polypivalolactone in a wide range of temperatures through analysis of the alpha/gamma interspherulitic profiles formed in isothermal conditions and direct measurement of the growth rate of the alpha counterparts at the same temperature.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A study has been made of the crystallization behavior of polypropylene (PP) filled with rare earth oxides under isothermal conditions. These rare earth oxides include lanthanum oxide (La2O3), yttrium oxide (Y2O3), and a mixture of rare earth oxides containing 70% Y2O3 (Y2O3-0.70). A differential scanning calorimeter was used to monitor the energetics of the crystallization process from the melt. During isothermal crystallization, dependence of the relative degree of crystallinity on time was described by the Avrami equation. It has been shown that the addition of any of the three rare earth oxides causes a considerable increase in the overall crystallization rate of PP but does not influence the mechanism of nucleation and growth of the PP crystals. The analysis of kinetic data according to nucleation theories shows that the increase in crystallization rate of PP in the composites is due to the decrease in surface energy of the extremity surfaces. The relative contents of the beta-form in the composites are somewhat higher than that in the plain PP. However, the contents of the beta-form in the plain PP and the composites are all very low relative to those of the alpha-form and the influence of the formation of the beta-form on the crystallization kinetics can be neglected.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Lysozyme is a naturally occurring enzyme in egg white and has high commercial importance due to its antimicrobial properties. The main objective of this work was to study the growth rate of lysozyme crystals isolated from egg for the first 72 hours and verify the results with McCabe’s constant crystal growth theory. Hanging drop crystallization method was used to form high purity lysozyme crystals from the embryonic stage. To this end, this work differs from an earlier work of Forsythe et al., who used seed crystals in the size range of 10 µm - 40 µm for face growth measurements at different pH values. The maximum crystal size recorded in the present work was 392.86 µm, which is within the typical size range of 50 µm - 500 µm for which constant crystal growth is expected to hold according to McCabe’s ?L law. Electron micrographs (SEM) revealed the structure and dimensions of the crystals while SDS-Page was used to measure the purity of the crystals. The SEM results showed that that lysozyme growth rate was linear and agreed with McCabe’s constant growth theory, producing a growth rate of 1.77 x 10-3 µm .s-1

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The quality of single crystal diamond obtained by microwave CVD processes has been drastically improved in the last 5 years thanks to surface pretreatment of the substrates [A. Tallaire, J. Achard, F. Silva, R.S. Sussmann, A. Gicquel, E. Rzepka, Physica Status Solidi (A) 201, 2419-2424 (2004); G. Bogdan, M. Nesladek, J. D'Haen, J. Maes, V.V. Moshchalkov, K. Haenen, M. D'Olieslaeger, Physica Status Solidi (A) 202, 2066-2072 (2005); M. Yamamoto, T. Teraji, T. Ito, Journal of Crystal Growth 285, 130-136 (2005)]. Additionally, recent results have unambiguously shown the occurrence of (110) faces on crystal edges and (113) faces on crystal corners [F. Silva, J. Achard, X. Bonnin, A. Michau, A. Tallaire, O. Brinza, A. Gicquel, Physica Status Solidi (A) 203, 3049-3055 (2006)]. We have developed a 3D geometrical growth model to account for the final crystal morphology. The basic parameters of this growth model are the relative displacement speeds of (111), (110) and (113) faces normalized to that of the (100) faces, respectively alpha, beta, and gamma. This model predicts both the final equilibrium shape of the crystal (i.e. after infinite growth time) and the crystal morphology as a function of alpha, beta, gamma, and deposition time.

An optimized operating point, deduced from the model, has been validated experimentally by measuring the growth rate in (100), (111), (110), and (113) orientations. Furthermore, the evolution of alpha, beta, gamma as a function of methane concentration in the gas discharge has been established. From these results, crystal growth strategies can be proposed in order, for example, to enlarge the deposition area. In particular, we will show, using the growth model, that the only possibility to significantly increase the deposition area is, for our growth conditions, to use a (113) oriented substrate. A comparison between the grown crystal and the model results will be discussed and characterizations of the grown film (Photoluminescence spectroscopy, EPR, SEM) will be presented. (C) 2008 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Polystyrene latex particles modified at the surface with different hydrophilic functional groups were prepared by miniemulsion polymerization and applied to control the crystallization of zinc oxide in aqueous medium. The effects of both latex structure and concentration on the crystal growth, morphology, crystalline structure, and properties of the resulting zinc oxide were analyzed. Depending on the latex additive used, micro- and submicrosized crystals with a broad variety of morphologies were obtained. Among the studied latexes, the carboxyl-derived particles were shown to be a convenient system for further quantitative investigations. In this case, as the additive concentration increases, the aspect ratio of the crystals decreases systematically. Latex particles are assumed to adsorb preferentially onto the fast growing {001} faces of ZnO, interacting with the growth centers and reducing the growth rate in [001]. When zinc oxide is precipitated in the presence of latex, the polymer particles become incorporated into the growing crystals and polymer–inorganic hybrid materials are obtained. These materials are composed of an inorganic and largely undisturbed crystalline matrix in which organic latex particles are embedded. Increasing amounts of latex become incorporated into the growing crystals at increasing overall concentration in the crystallizing system. Photoluminescence (PL) spectra were measured to obtain information on defect centers. Emission spectra of all samples showed a narrow UV peak and a broad band in the green-yellow spectral region. The former emission is attributed to exciton recombination, whereas the latter seems to be related with deep-level donors. Latex appears to be a quencher of the visible emission of zinc oxide. Thus, compared to pure zincite, ZnO–latex hybrid materials show a significantly lower PL intensity in the visible range of the spectrum. Under continuous photoexcitation, a noticeable dynamic behavior of the PL is observed, which can be related to a photodesorption of adsorbed oxygen. These surface-adsorbed oxygen species seem to play a crucial role for the optical properties of the materials and may mediate the tunneling of electrons from the conduction band to preexisting deep-level traps, probably related to intrinsic defects (oxygen vacancies or interstitial zinc). The polymer particles can block the sites where oxygen adsorbs, and the disappearance of the “electron-shuttle” species leads to the observed quenching of the visible emission. Electron paramagnetic resonance (EPR) provided additional information about crystal defects with unpaired electrons. Spectra of all samples exhibit a single signal at g ≈ 1.96, typical for shallow donors. Contrary to the results of other authors, no correlation was possible between the EPR signal and the visible range of PL spectra, which suggests that centers responsible for the visible emission and the EPR signal are different.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Protein crystallization has gained a new strategic and commercial relevance in the postgenomic era due to its pivotal role in structural genomics. Producing high quality crystals has always been a bottleneck to efficient structure determination, and this problem is becoming increasingly acute. This is especially true for challenging, therapeutically important proteins that typically do not form suitable crystals. The OptiCryst consortium has focused on relieving this bottleneck by making a concerted effort to improve the crystallization techniques usually employed, designing new crystallization tools, and applying such developments to the optimization of target protein crystals. In particular, the focus has been on the novel application of dual polarization interferometry (DPI) to detect suitable nucleation; the application of in situ dynamic light scattering (DLS) to monitor and analyze the process of crystallization; the use of UV-fluorescence to differentiate protein crystals from salt; the design of novel nucleants and seeding technologies; and the development of kits for capillary counterdiffusion and crystal growth in gels. The consortium collectively handled 60 new target proteins that had not been crystallized previously. From these, we generated 39 crystals with improved diffraction properties. Fourteen of these 39 were only obtainable using OptiCryst methods. For the remaining 25, OptiCryst methods were used in combination with standard crystallization techniques. Eighteen structures have already been solved (30% success rate), with several more in the pipeline.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Calcitic belemnite rostra are usually employed to perform paleoenvironmental studies based on geochemical data. However, several questions, such as their original porosity and microstructure, remain open, despite they are essential to make accurate interpretations based on geochemical analyses.This paper revisits and enlightens some of these questions. Petrographic data demonstrate that calcite crystals of the rostrum solidum of belemnites grow from spherulites that successively develop along the apical line, resulting in a “regular spherulithic prismatic” microstructure. Radially arranged calcite crystals emerge and diverge from the spherulites: towards the apex, crystals grow until a new spherulite is formed; towards the external walls of the rostrum, the crystals become progressively bigger and prismatic. Adjacent crystals slightly vary in their c-axis orientation, resulting in undulose extinction. Concentric growth layering develops at different scales and is superimposed and traversed by a radial pattern, which results in the micro-fibrous texture that is observed in the calcite crystals in the rostra.Petrographic data demonstrate that single calcite crystals in the rostra have a composite nature, which strongly suggests that the belemnite rostra were originally porous. Single crystals consistently comprise two distinct zones or sectors in optical continuity: 1) the inner zone is fluorescent, has relatively low optical relief under transmitted light (TL) microscopy, a dark-grey color under backscatter electron microscopy (BSEM), a commonly triangular shape, a “patchy” appearance and relatively high Mg and Na contents; 2) the outer sector is non-fluorescent, has relatively high optical relief under TL, a light-grey color under BSEM and low Mg and Na contents. The inner and fluorescent sectors are interpreted to have formed first as a product of biologically controlled mineralization during belemnite skeletal growth and the non-fluorescent outer sectors as overgrowths of the former, filling the intra- and inter-crystalline porosity. This question has important implications for making paleoenvironmental and/or paleoclimatic interpretations based on geochemical analyses of belemnite rostra.Finally, the petrographic features of composite calcite crystals in the rostra also suggest the non-classical crystallization of belemnite rostra, as previously suggested by other authors.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Purpose: This randomized, multicenter trial compared first-line trastuzumab plus docetaxel versus docetaxel alone in patients with human epidermal growth factor receptor 2 (HER2)-positive metastatic breast cancer (MBC). Patients and Methods: Patients were randomly assigned to six cycles of docetaxel 100 mg/m 2 every 3 weeks, with or without trastuzumab 4 mg/kg loading dose followed by 2 mg/kg weekly until disease progression. Results: A total of 186 patients received at least one dose of the study drug. Trastuzumab plus docetaxel was significantly superior to docetaxel alone in terms of overall response rate (61% v 34%; P = .0002), overall survival (median, 31.2 v 22.7 months; P = .0325), time to disease progression (median, 11.7 v 6.1 months; P = .0001), time to treatment failure (median, 9.8 v 5.3 months; P = .0001), and duration of response (median, 11.7 v 5.7 months; P = .009). There was little difference in the number and severity of adverse events between the arms. Grade 3 to 4 neutropenia was seen more commonly with the combination (32%) than with docetaxel alone (22%), and there was a slightly higher incidence of febrile neutropenia in the combination arm (23% v 17%). One patient in the combination arm experienced symptomatic heart failure (1%). Another patient experienced symptomatic heart failure 5 months after discontinuation of trastuzumab because of disease progression, while being treated with an investigational anthracycline for 4 months. Conclusion: Trastuzumab combined with docetaxel is superior to docetaxel alone as first-line treatment of patients with HER2-positive MBC in terms of overall survival, response rate, response duration, time to progression, and time to treatment failure, with little additional toxicity. © 2005 by American Society of Clinical Oncology.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

An innovative approach to precise tailoring of surface density, shapes, and sizes of single-crystalline α-Fe 2O 3 nanowires and nanobelts by controlling interactions of reactive oxygen plasma-generated species with the Fe surface is proposed. This strongly nonequilibrium, rapid, almost incubation-free, high-rate growth directly from the solid-solid interface can also be applied to other oxide materials and is based on deterministic control of the density of oxygen species and the surface conditions, which determine the nanostructure nucleation and growth.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Differential scanning calorimetry (DSC) has been used to obtain kinetic and nucleation parameters for polymer crystallization under a non-isothermal mode of operation. The available isothermal nucleation growth-rate equation has been modified for non-isothermal kinetic analysis. The values of the nucleation constant (K g ) and surface free energies (sgr, sgr e ) have been obtained for i-polybutene-1, i-polypropylene, poly(L-lactic acid), and polyoxymethylene and are compared with those obtained from isothermal kinetic analysis; a good agreement in both is seen.