Although one of the best possibilities for raising the animal protein of the diets of Nigerian is to increase the consumption of fish; particularly through the use of several methods of long term preservation techniques, such as drying, no radical approach has yet emerged. Although, a great deal of the artisanal fish catch is dried for the huge consumer and distant markets, the traditional methods of fish preservation need improvements to cope with demand for increased quantity, shelf-stable, and improved quality of fish products. The paper discusses drying requirements, heat and mass transfer, consumer acceptance, fuel sources, storage and marketing of dried fish products; and suggest ways and means of structurally transforming the artisanal technology of fish drying
Resumo:
A planar waveguide ring resonator was fabricated by organic-inorganic hybrid sol-gel materials; its sensitivity to ethanol vapor was experimentally investigated. It was found that dips in the transmission spectrum of the device shifted to longer wavelengths with increasing the ethanol concentration, and its sensitivity showed a linear relation with the ethanol concentration, showing a coefficient of 1.13 pm/ppm. In addition, the transmission loss of the ring resonator decreased with increasing the ethanol concentration. The measured characteristics suggest that the device may be considered as one of the candidates of alcohol vapor sensors. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
The Er3+-Yb3+ codoped Al2O3 has been prepared by the sol-gel method using the aluminium isopropoxide [Al(OC3H7)(3)]-derived Al2O3 sols with addition of the erbium nitrate [Er(NO3)(3) center dot 5H(2)O] and ytterbium nitrate [Yb(NO3)(3) center dot 5H(2)O]. The phase structure, including only two crystalline types of doped Al2O3 phases, theta and gamma, was obtained for the 1 mol% Er3+ and 5 mol% Yb3+ codoped Al2O3 at the sintering temperature of 1,273 K. By a 978 nm semiconductor laser diodes excitation, the visible up-conversion emissions centered at about 523, 545, and 660 nm were obtained. The temperature dependence of the green up-conversion emissions was studied over a wide temperature range of 300-825 K, and the reasonable agreement between the calculated temperature by the fluorescence intensity ratio (FIR) theory and the measured temperature proved that Er3+-Yb3+ codoped Al2O3 plays an important role in the application of high temperature sensor.
Resumo:
Nanocrystalline La0.8Pb0.2FeO3 has been prepared by the sol-gel method. XRD patterns show that the nanocrystalline La0.8Pb0.2FeO3 is a perovskite phase with the orthorhombic structure and its mean crystallite size is about 19 nm. The influence of Pb ions which replaced the La ions on A-sites can be directly observed from the electrical and sensing properties to H-2 gas. The conductance of La0.8Pb0.2FeO3-based sensor is considerably higher than that of LaFeO3-based sensor, and Pb-doping can enhance the sensitivity to H2 gas. An empirical relationship of R = KCH2alpha with alpha = 0.668 was obtained.
Resumo:
The local structure of Na-Al-P-O-F glasses, prepared by a novel sol-gel route, was extensively investigated by advanced solid-state NMR techniques. Al-21{F-19} rotational echo double resonance (REDOR) results indicate that the F incorporated into aluminophosphate glass is preferentially bonded to octahedral Al units and results in a significant increase in the concentration of six-coordinated aluminum. The extent of Al-F and Al-O-P connectivities are quantified consistently by analyzing Al-27{P-31} and Al-21{F-19} REDOR NMR data. Two distinct types of fluorine species were identified and characterized by various F-19{Al-27}, F-19{Na-23}, and F-19{P-31} double resonance experiments, which were able to support peak assignments to bridging (Al-F-Al, -140 ppm) and terminal (Al-F, -170 ppm) units. On the basis of the detailed quantitative dipole-dipole coupling information obtained, a comprehensive structural model for these glasses is presented, detailing the structural speciation as a function of composition.
Resumo:
Two kinds of silanes, 3-glycidoxypropyltrimethoxysilane (GLYMO) and 3-trimethoxysililpropylmethacrylate (TMSPM), were used to prepare ormosil waveguide films by the sol-gel method. Thirty percent Ti(OBu)(4) and 70% silane were contained in the precursor sets. The properties of films were measured by scanning electron microscopy (SEM), Fourier transform infrared spectroscopy (FTIR), UV/VIS/NIR spectrophotometer (UV-vis), atomic force microscopy (AFM), m-line and scattering-detection method. The films from GLYMO and TMSPM precursors exhibit similar thickness (2.58 mu m for GLYMO, 2.51 mu m for TMSPM) and refractive index (1.5438 for GLYMO, 1.5392 for TMSPM, lambda=632.8 nm), but the film from TMSPM precursor has higher propagation loss (1.024 dB/cm, lambda=632.8 nm) than the film prepared from GLYMO (0.569 dB/cm, lambda=632.8 nm). Furthermore, the film prepared from TMSPM is easy to be opaque and cracks during coating whereas the same phenomenon was not found for the film prepared with GLYMO. It is confirmed that GLYMO is a better precursor than TMSPM for waveguide film preparation. (C) 2005 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
Resumo:
Sol-gel derived TiO2/SiO2/ormosil hybrid planar waveguides have been deposited on soda-lime glass slides and silicon substrates, films were heat treated at 150 degreesC for 2 h or dried at room temperature. Different amounts of water were added to sols to study their impacts on microstructures and optical properties of films. The samples were characterized by m-line spectroscopy, Fourier transform infrared spectroscopy (FT-IR), UV/VIS/NIR spectrophotometer (UV-vis), atomic force microscopy (AFM), thermal analysis instrument and scattering-detection method. The refractive index was found to have the largest value at the molar ratio H2O/OR = 1 in sol (OR means -OCH3, -OC2H5 and -OC4H9 in the sol), whereas the thickest film appears at H2O/OR = 1/2. The rms surface roughness of all the films is lower than 1.1 nm, and increases with the increase of water content in sol. Higher water content leads to higher attenuation of film. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
EU3+ -doped Y3Al5O12 (YAG:Eu3+) phosphors were synthesized by a facile sol-gel combustion method. In this process, citric acid traps the constituent cations and reduces the diffusion length of the precursors. YAG phase is obtained through sintering at 900 degrees C for 2h. There were no intermediate phases such as YAlO3 (YAP) and Y4Al2O9 (YAM) observed. The charge transfer band of nanocrystalline phosphors shows a shift toward the high-energy side, compared with that of amorphous ones due to lower covalency of Eu-O bond for nanocrystalline phosphors. The higher concentration quenching in YAG:EU3+ nanophosphors may be caused by the confinement effect on resonant energy transfer of nanocrystalline. It also indicates that the sol-gel combustion synthesis method provides a good distribution of Eu3+ activators in YAG host. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
High-quality Ce3+-doped Y3Al5O12 (YAG:Ce3+) phosphors were synthesized by a facile sol-gel combustion method. In this sol-gel combustion process, citric acid acts as a fuel for combustion, traps the constituent cations and reduces the diffusion length of the precursors. The XRD and FT-IR results show that YAG phase can form through sintering at 900 degrees C for 2 h. This temperature is much lower than that required to synthesize YAG phase via the solid-state reaction method. There were no intermediate phases such as YAlO3 (YAP) and Y4Al2O9 (YAM) observed in the sintering process. The average grain size of the phosphors sintered at 900-1100 degrees C is about 40 nm. With the increasing of sintering temperature, the emission intensity increases due to the improved crystalline and homogeneous distribution of Ce3+ ions. A blue shift has been observed in the Ce3+ emission spectrum of YAG:Ce3+ phosphors with increasing sintering temperatures from 900 to 1200 degrees C. It can be explained that the decrease of lattice constant affects the crystal field around Ce3+ ions. The emission intensity of 0.06Ce-doped YAG phosphors is much higher than that of the 0.04Ce and 0.02Ce ones. The red-shift at higher Ce3+ concentrations may be Ce-Ce interactions or variations in the unit cell parameters between YAG:Ce3+ and YAG. It can be concluded that the sol-gel combustion synthesis method provides a good distribution of Ce3+ activators at the molecular level in YAG matrix. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Y4Al2O9:EU3+ phosphor was synthesized through a sol-gel combustion method. The Y4Al2O9 phase can form through sintering at 800 degrees C. This temperature is much lower than that required via the solid state reaction method. The average grain size of the phosphor was about 30 run. Compared with the amorphous phosphor, the charge transfer band of crystalline phosphor shows a blue shift. The emission Of Y4Al2O9:Eu3+ indicates the existence of two luminescent centers, in agreement with the crystal structure of Y4Al2O9. Higher doping concentration could be realized in Y4Al2O9 nanocrystal host lattice. This indicates that the sol-gel combustion synthesis method can increase emission intensity and quenching concentration due to a good distribution of EU3+ activators in Y4Al2O9 host. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Au colloids were prepared by irradiation with a Nd:YAG laser. Au nanoparticles were characterized by absorption spectra, transmission electron microscopy (TEM) and X-ray diffraction (XRD) analysis. It is found that the wavelength of the laser has no effect on the size but the number of the Au nanoparticles. By irradiating a transparent silica gel doped with gold ions with the focused laser in the gel and subsequent exposing in air, a space-selective pattern of letter "P" consisting of Au nanoparticles was observed inside the silica gel.