986 resultados para fracture reduction


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Experimental studies reveal a reduction in the values of permittivity for epoxy nanocomposites; at low filler loadings as compared to neat epoxy over a wide frequency range. This permittivity reduction is attributed to the interaction dynamics between nanoparticles: and epoxy chains at the interface region and interestingly, this interaction has also been found to influence the glass transition temperatures (T-g) of the examined nanocomposite systems. Accordingly, a dual nanolayer interface model for an epoxy based nanocomposite system is analyzed to explain the obtained permittivity characteristics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The grain size dependencies of the yield and fracture stresses in hot rolled Mg-12.7 at % Cd alloy have been measured in the temperature range 77 to 420 K and are found to be in accordance with HalI-Petch type of equations. In hot rolled Mg-12.7 Cd alloy, the HalI-Petch intercept a w is higher than that in hot rolled magnesium, while the slope ky is comparable. The fracture is intercrystalline at 77 K, mixed mode at 300 K and ductile at 420 K. The above flow and fracture behaviours are interpreted in terms of the complimentary effects of texture hardening and solid solution strengthening.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

n this paper, the influence of patch parameters on stress intensity factors in edge cracked plates is studied by employing transmission photoelasticity. Edge cracked plates made of photo-elastic material are patched on one side only by E glass-epoxy and carbon-epoxy unidirectional composites. The patch is located on the crack in such a way that the crack tip is not covered. Magnified isochromatic fringes are obtained by using a projection microscope of magnification 50, converted into a polariscope. Irwin's method is used to compute stress intensity factors from photoelastic data. The reduction in stress intensity factors is presented in graphical form as a function of patch parameters, namely stiffness, location and length. An empirical equation connecting reduction in stress intensity factor and these patch parameters is presented.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This study presents results from an experimental 10-day research charter that was designed to quantify the effects of a) a turtle excluder device (TED) and b) a radial escape section bycatch reduction device (BRD) and c) both devices together, on prawn and bycatch catch rates in the Queensland shallow water eastern king prawn (Penaeus plebejus) trawl fishery. The bycatch was comprised of 250 taxa, mainly gurnards, whiting, lizard fish, flathead, dragonets, portunid crabs, turretfish and flounders. The observed mean catch rates of bycatch and marketable eastern king prawns from the standard trawl net (i.e., net with no TED or BRD) used during the charter were 11.06 (se 0.90) kg per hectare swept by the trawl gear (ha-1) and 0.94 kg ha-1, respectively. For the range of depths sampled (20.1-90.7 m), bycatch catch rates declined significantly at a rate of 0.14 kg ha-1 for every 1 m increase in depth, while prawn catch rates were unaffected. When both the TED and radial escape section BRD were used together they resulted in a 24% reduction in total bycatch catch rate compared to a standard net, but at a 20% reduction in marketable prawn catch rate. The largest reductions were achieved for stout whiting Sillago robusta (57% reduction) and yellowtail scad Trachurus novaezelandiae (32% reduction). Multidimensional scaling and analysis of similarities revealed that bycatch assemblages differed significantly between depths and latitude, but not between the different combinations of bycatch reduction devices. Despite the lowered prawn catch rates, the reduced bycatch catch rates are promising, particularly for S. robusta which is not permitted to be retained by the prawn trawl fleet and yet experiences considerable incidental fishing mortality, and because it is targeted in a separate licensed commercial fishery.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Recent studies (I-7) clearly indicate a strong dependence of fatigue threshold parameter, A K on grain size in several alloy systems. Attempts to explain these observations on the basis of crat~tortuosity (1,8), fracture surface roughness (5,9) and crack closure (6) appear to present a fairly clear picture of the mechanisms that cause a reduction in crack growth rates at threshold. In general, it has been shown that coarse grained microstructures exhibit higher fatigue threshold in low carbon steels (1,5) aluminium alloys (7) and titanium alloys (6). In spite of these observations, there exists (10-1#) considerable uncertainity about the manner in which the AK~L depends on prior austenitic grain size in quenched and tempered steels. Studies in quenched and tempered steels demonstrating both an increase (3,12,14) as well as a decrease (11,12) in AKth with an increase in prior austenitic grain size can be sought to illustrate this point. Occasionally , the absence of any sensitivity of AKth to the variations in prior austenitJc grain size has also been reported (11,13). While a few investigators (5-7) comfortably rationalised the grain size effects on AK~L on the basis of crack closure by a comparison in terms of the closure-free component of the thresho~Ifc~, AK -f such an approach has yet to be extended to high strength steels, An attempt has been made in t~et ,pthrg sent study to explai. n the effect of pri, or austeniti.c grain size on &Kth on the basis of crack closure measurements in a high strength steel.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Maize (Zea mays L.) is a chill-susceptible crop cultivated in northern latitude environments. The detrimental effects of cold on growth and photosynthetic activity have long been established. However, a general overview of how important these processes are with respect to the reduction of productivity reported in the field is still lacking. In this study, a model-assisted approach was used to dissect variations in productivity under suboptimal temperatures and quantify the relative contributions of light interception (PARc) and radiation use efficiency (RUE) from emergence to flowering. A combination of architectural and light transfer models was used to calculate light interception in three field experiments with two cold-tolerant lines and at two sowing dates. Model assessment confirmed that the approach was suitable to infer light interception. Biomass production was strongly affected by early sowings. RUE was identified as the main cause of biomass reduction during cold events. Furthermore, PARc explained most of the variability observed at flowering, its relative contributions being more or less important according to the climate experienced. Cold temperatures resulted in lower PARc, mainly because final leaf length and width were significantly reduced for all leaves emerging after the first cold occurrence. These results confirm that virtual plants can be useful as fine phenotyping tools. A scheme of action of cold on leaf expansion, light interception and radiation use efficiency is discussed with a view towards helping breeders define relevant selection criteria. This paper originates from a presentation at the 5th International Workshop on Functional–Structural Plant Models, Napier, New Zealand, November 2007.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Oxygen Consumption by alternative oxidase (AOX), present in mitochondria of many angiosperms, is known to be cyanide-resistant in contrast to cytochrome oxidase. Its activity in potato tuber (Solarium tuberosum L.) was induced following chilling treatment at 4 degrees C.About half of the total O-2 consumption of succinate oxidation in such mitochondria was found to be sensitive to SHAM, a known inhibitor of AOX activity. Addition of catalase to the reaction mixture of AOX during the reaction decreased the rate of SHAM-sensitive oxygen consumption by nearly half, and addition at the end of the reaction released nearly half of the consumed oxygen by AOX, both typical of catalase action on H2O2. These findings with catalase suggest that the product of reduction of AOX is H2O2 and not H2O, as previously Surmised. In potatoes Subjected to chill stress (4 degrees C) for periods of 3, 5 and >= 8 days the activity of AOX in mitochondria increased progressively with a corresponding increase in the AOX protein detected by immunoblot of the protein.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Three anaerobic ponds used to store and treat piggery wastes were fully covered with permeable materials manufactured from polypropylene geofabric, polyethylene shade cloth and supported straw. The covers were assessed in terms of efficacy in reducing odour emission rates over a 40-month period. Odour samples were collected from the surface of the covers, the surface of the exposed liquor and from the surface of an uncovered (control) pond at one of the piggeries. Relative to the emission rate of the exposed liquor at each pond, the polypropylene, shade cloth and straw covers reduced average emission rates by 76%, 69% and 66%, respectively. At the piggery with an uncovered control pond, the polypropylene covers reduced average odour emission rates by 50% and 41%, respectively. A plausible hypothesis, consistent with likely mechanisms for the odour reduction and the olfactometric method used to quantifying the efficacy of the covers, is offered.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this study, reduction and desorption of oxides of nitrogen (NOx) were conducted using an electrical discharge plasma technique. The study was carried out using a simulated gas mixture to explore the possibility of re-generation of used adsorbents by a nonthermal plasma desorption technique. Three different types of corona electrodes, namely, pipe, helical wire, and straight wire, were used for analyzing their effectiveness in NOx reduction/desorption. The pipe-type corona electrode exhibited a nitric oxide (NO) conversion of 50%, which is 1.5 times that of the straight-wire-type electrode at an energy density of 175J/L. The helical-wire-type corona electrode exhibited a NOx desorption efficiency almost 4 times that of the pipe-type electrode,indicating the possibility that corona-generated species play a crucial role in desorption.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A variety of materials were trialed as supported permeable covers using a series of laboratory-scale anaerobic digesters. Efficacy of cover performance was assessed in terms of impact on odour and greenhouse gas emission rate, and the characteristics of anaerobic liquor. Data were collected over a 12-month period. Initially the covers reduced the rate of odour emission 40-100 times relative to uncovered digesters. After about three months, this decreased to about a threefold reduction in odour emission rate, which was maintained over the remainder of the trial. The covers did not alter methane emission rates. Carbon dioxide emission rates varied according to cover type. Performance of the covers was attributed to the physical characteristics of the cover materials and changes in liquor composition. The reductions in odour emission indicate that these covers offer a cost-effective method for odour control.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The efficacy of supported covers was investigated under field conditions using a series of prototypes deployed on an anaerobic pond treating typical piggery waste. Research focused on identifying effective cover support materials and deployment methods, quantifying odour reduction, and estimating the life expectancy of various permeable cover materials. Over a 10-month period, median odour emission rates were five to eight times lower from supported straw cover surfaces and a non-woven, spun fibre polypropylene weed control material than from the adjacent uncovered pond surface. While the straw covers visually appeared to degrade very rapidly, they continued to reduce odour emissions effectively. The polypropylene cover appeared to offer advantages from the perspectives of cost, reduced maintenance and ease of manufacture.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Anatomically precontoured plates are commonly used to treat periarticular fractures. A well-fitting plate can be used as a tool for anatomical reduction of the fractured bone. Recent studies highlighted that some plates fit poorly for many patients due to considerable shape variations between bones of the same anatomical site. While it is impossible to design one shape that fits all, it is also burdensome for the manufacturers and hospitals to produce, store and manage multiple plate shapes without the certainty of utilization by a patient population. In this study, we investigated the number of shapes required for maximum fit within a given dataset, and if they could be obtained by manually deforming the original plate. A distal medial tibial plate was automatically positioned on 45 individual tibiae, and the optimal deformation was determined iteratively using finite element analysis simulation. Within the studied dataset, we found that: (i) 89% fit could be achieved with four shapes, (ii) 100% fit was impossible through mechanical deformation, and (iii) the deformations required to obtain the four plate shapes were safe for the stainless steel plate for further clinical use. The proposed framework is easily transferable to other orthopaedic plates.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A technique to quantify in real time the microstructural changes occurring during mechanical nanoscale fatigue of ultrathin surface coatings has been developed. Cyclic nanoscale loading, with amplitudes less than 100 nm, is achieved with a mechanical probe miniaturized to fit inside a transmission electron microscope (TEM). The TEM tribological probe can be used for nanofriction and nanofatigue testing, with 3D control of the loading direction and simultaneous TEM imaging of the nano-objects. It is demonstrated that fracture of 10-20 nm thick amorphous carbon films on sharp gold asperities, by a single nanoscale shear impact, results in the formation of < 10 nm diameter amorphous carbon filaments. Failure of the same carbon films after cyclic nanofatigue, however, results in the formation of carbon nanostructures with a significant degree of graphitic ordering, including a carbon onion.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The fatigue and fracture performance of a cracked plate can be substantially improved by providing patches as reinforcements. The effectiveness of the patches is related to the reduction they cause in the stress intensity factor (SIF) of the crack. So, for reliable design, one needs an accurate evaluation of the SIF in terms of the crack, patch and adhesive parameters. In this investigation, a centrally cracked large plate with a pair of symmetric bonded narrow patches, oriented normally to the crack line, is analysed by a continuum approach. The narrow patches are treated as transversely flexible line members. The formulation leads to an integral equation which is solved numerically using point collocation. The convergence is rapid. It is found that substantial reductions in SIF are possible with practicable patch dimensions and locations. The patch is more effective when placed on the crack than ahead of the crack. The present analysis indicates that a little distance inwards of the crack tip, not the crack tip itself, is the ideal location, for the patch.