417 resultados para Porcelain veneer
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Purpose: To evaluate the effects of two surface treatments, aging, and two resin cements on shear bond strength between dentin and yttrium-stabilized tetragonal zirconia polycrystal ceramic (Y-TZP).Materials and Methods: Eighty human molars were embedded in acrylic resin and sectioned 3 mm below the occlusal plane. These teeth and 80 cylindrical Y-TZP specimens (height, 4 mm; diameter, 3.4 mm) were divided into eight groups (n=10) using the following factors: Y-TZP surface treatment (Vi: low-fusing porcelain [vitrification] + hydrofluoric acid etching + silanization or Si: tribochemical silicatization); cementation strategies (PF: Pan avia or CC: Clearfil); and storage (nonaging or aging). Bonding surfaces of 40 Y-TZP specimens received Vi treatment, and the rest received Si treatment. Half of the ceramic-tooth assemblies were cemented with Panavia, the rest with Clearfil. Shear tests were executed using 0.4-mm-thick wire at 0.5 mm/min. Data were analyzed by three-way analysis of variance and Tukey test (alpha=0.05). Fractures were analyzed.Results: Y-TZP surface treatments did not affect bond strength (p=0.762, Vi = Si), while resin cements (p<0.001, Panavia > Clearfil) and aging (p=0.006, nonaging > aging) showed a significant effect. Most failures were in adhesive at dentin-cement interfaces; no failure occurred between zirconia and cement.Conclusion: When Y-TZP ceramic is bonded to dentin, the weakest interface is that between dentin and resin cement. The resin cement/Y-TZP interface was less susceptible to failures, owing to Y-TZP surface treatments.
Resumo:
Aiming to investigate in vitro the behavior of esthetic veneers placed in crows and made of the laboratory resins Artglass and Targis when submitted to insertion and removal of circunferential cobalt-chromium clasps, 24 veneer crowns were made (twelve with Artglass (Heraeus Kulzer) and twelve with Targis (Ivoclar Vivadent)), as well as the respective cobalt-chromium clasps. The crowns were then submitted to five thousand cycles of clasps insertion and removal, using a proper device. Using the verification of the force necessary to remove the clasps over the crowns during the experiment, the clasps and crowns mass variation, and the macroscopic inspection of the veneers, one may conclude that the veneers did not show a significant variation of the force required to remove the clasps over the crowns; they show a little amount of abrasion, possible to detect using a visual inspection and they show a little and variable amount of mass loss, less for that made with Artglass (average of 0,002g) and greater for that made with Targis (average of 0,006g)
Resumo:
Pós-graduação em Odontologia Restauradora - ICT
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Pós-graduação em Odontologia Restauradora - ICT
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Purpose: To evaluate the survival rate, success rate, load to fracture, and finite element analysis (FEA) of maxillary central incisors and canines restored using ceramic veneers and varying preparation designs.Methods and Materials: Thirty human maxillary central incisors and 30 canines were allocated to the following four groups (n=15) based on the preparation design and type of tooth: Gr1 = central incisor with a conservative preparation; Gr2 = central incisor with a conventional preparation with palatal chamfer; Gr3 = canine with a conservative preparation; Gr4 = canine with a conventional preparation with palatal chamfer. Ceramic veneers (lithium disilicate) were fabricated and adhesively cemented (Variolink Veneer). The specimens were subjected to 4 x 106 mechanical cycles and evaluated at every 500,000 cycles to detect failures. Specimens that survived were subjected to a load to fracture test. Bidimensional models were modeled (Rhinoceros 4.0) and evaluated (MSC.Patrans 2005r2 and MSC.Marc 2005r2) on the basis of their maximum principal stress (MPS) values. Survival rate values were analyzed using the Kaplan-Meier test (alpha = 0.05) and load to fracture values were analyzed using the Student t-test (alpha = 0.05).Results: All groups showed 100% survival rates. The Student t-test did not show any difference between the groups for load to fracture. FEA showed higher MPS values in the specimens restored using veneers with conventional preparation design with palatal chamfer.Conclusion: Preparation design did not affect the fracture load of canines and central incisors, but the veneers with conventional preparation design with palatal chamfer exhibited a tendency to generate higher MPS values.
Resumo:
This study evaluated the effect of the core substrate type (dentin and composite resin) on the retention of crowns made of yttrium oxide stabilized tetragonal zirconia polycrystal (Y-TZP), submitted to three inner surface conditionings. For this purpose, 72 freshly extracted molars were embedded in acrylic resin, perpendicular to the long axis, and prepared for full crowns: 36 specimens had crown preparations in dentin; the remaining 36 teeth had the crowns removed, and crown preparations were reconstructed with composite resin plus fiber posts with dimensions identical to the prepared dentin. The preparations were impressed using addition silicone, and 72 Y-TZP copings for the tensile test were produced. Cementation was performed with a dual-cured cement containing phosphate monomers. For cementation, the crown preparation (dentin or resin) was conditioned with the adhesive system, and the ceramic was subjected to one of three surface treatments: isopropyl alcohol, tribochemical silica coating, or thin low-fusing glassy porcelain layer application plus silanization. After 24 hours, all specimens were submitted to thermocycling (6000 cycles) and placed in a special tensile testing device in a universal testing machine to determine failure loads. The failure modes of all samples were analyzed under a stereomicroscope. Two-way analysis of variance showed that the surface treatment and substrate type (alpha=0.05) affected the tensile retention results. The dentin substrate presented the highest tensile retention values, regardless of the surface treatment. When the substrate was resin, the tribochemical silica coating and low-fusing glaze application plus silanization groups showed the higher retention values.
Resumo:
The aim of this study was to verify through microtensile test the influence of time and concentration of surface conditioning with hydrofluoric acid and its interference in the adhesion of dual resin cement to porcelain.We used 32 bodies of glass-ceramic lithium disilicate system IPS e.max Press LT with dimensions of 6mm thick, 8 mm in length and 8 mm in length, which will be molded to obtain composite resin blocks corresponding to blocks ceramics. Ceramic and resin blocks were divided into 16 groups (n = 4) and numbered according to the concentration of hydrofluoric acid (2.5%, 5%, 7.5% and 10%) and conditioning time (20 seconds, 40 seconds, 1 minute and 2 minutes). The blocks were cleaned in ultrasonic apparatus with distilled water and dried with compressed air, subjected to acid etching and air-jet washed with water, dried with compressed air and received application of silane agent Monobond-S, followed by adhesive Excite ( Ivoclar Vivaden). Each ceramic block was bonded to the corresponding block of resin through the resin cement Multilink Automix. The specimens were cut to obtain nine micro samples for each set of ceramic-resin with 1 mm X 1 mm X 12 mm in length, which were submitted to microtensile test. The results were analyzed with descriptive statistics and analysis of variance with significance level of 5%, revealing that there were statistically significant (p = 0.000001 <0.05). From the Tukey test can be concluded that etching with hydrofluoric acid and 2.5% for 120 seconds gave the best bond strength, however, no statistical difference between the conditioning with the same acid in the concentration of 5.0% for 20 to 40 seconds
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)