903 resultados para PEG-PCL copolymer
Resumo:
Three comb polymers (CP) based on modified alternating methyl vinyl ether/maleic anhydride copolymer with oligo-oxyethylene side chains of the type -O(CH2CH2O)(n)CH3 were synthesized and characterized, and the ionic conductivity of CP/salt complexes is reported. The conductivity of these complexes was about 10(-5)-10(-6) S cm(-1) at room temperature. The conductivity, which displayed non-Arrhenius behaviour, was analysed using the Vogel-Tammann-Fulcher equation. The conductivity maxima appear at lower salt concentration, when CP has longer side chains. Infrared (i.r.) was used to study the cation-polymer interaction. I.r. results also indicate that the ester in CP might decompose at 140 degrees C and reproduce the maleic anhydride ring. (C) 1997 Elsevier Science Ltd.
Resumo:
The contact angles theta of polar liquids on PP-g-AM copolymer (AM content 0.19, 0.26, and 0.37 wt%) were measured. The critical surface tension gamma(c) of PP-g-AM films were evaluated by the Zisman plot (cos theta versus gamma(L)), the Young-Dupre-Good-Girifalco plot (1 + cos theta) versus 1/gamma(L)(0.5), and the log(1 + cos theta) versus log gamma(L) plot. The gamma(L) values estimated by the plot log(1 + cos theta) versus log gamma(L) were smaller than those obtained by the other plots.
Resumo:
Comb-like polymers (CPs) based on modified alternating methyl vinyl ether/maleic anhydride copolymer with oligo(oxyethylene) side chains of the type -O(CH2CH2O)(n)CH3 were synthesized and characterized, and complexed with lithium salts to form amorphous polymer electrolytes. Maximum conductivity close to 1.38 x 10(-4) S/cm was achieved at room temperature and at a [Li]/[EO] ratio (EO = ethylene oxide) of about 0.066. The temperature dependence of ionic conductivity suggested that the ion transport was controlled by segmental motion of the polymer, shown by linear curves obtained in Vogel-Tammann-Fulcher plots. The ionic conductivity maximum moved to a higher salt concentration as the temperature increased, indicating that a larger number of charge carriers can be transferred through polymer chains, of which free volume is increased at higher temperature. IR results indicated that the ester in CPs might decompose at 140 degrees C and reproduce the maleic anhydride ring.
Resumo:
Comb-like polymers (CP) based on modified alternating methyl vinyl ether/maleic anhydride copolymer with oligo-oxyethylene side chains of the type -O(CH2CH2O)(n)CH3 have been synthesized and characterized, and complexed with lithium salts to form amorphous polymer electrolytes. CP/salt complexes showed conductivity up to 10(-5)Scm(-1) at room temperature. The temperature dependence of ionic conductivity suggests that the ion transport is controlled by segmental motion of the polymer, shown by linear curves obtained in Vogel-Tammann-Fulcher plots. The ionic conductivity maximum moves to a higher salt concentration as the temperature increases. IR results indicate that the ester in CP might decompose at 140 degrees C and reproduce the maleic anhydride ring.
Resumo:
An ethylene-propylene copolymer (EPM) has been functionalized with acrylic acid (AA) by means of a radical-initiated melt process. Different degrees of grafting have been obtained by varying the overall composition of the reaction mixture. The influence of the grafting degree on the structure has been investigated by differential scanning calorimetry (DSC), Fourier-transform infrared analysis (FTIR), and wide-angle x-ray scattering (WAXS) techniques. The results of the structural investigations suggest that the grafting preferentially occurs onto the ethylene sequences of EPM. After acrylic acid was grafted onto EPM, the grafted AA acted as nucleation agent; it caused an increase of crystallization temperature of propylene sequences of EPM-g-AA.
Resumo:
The modification of ethylene-propylene copolymer (EPM) has been accomplished by melt grafting of maleic anhydride (MAH) molecules promoted by radical initiators. The resulting EPM-g-MAH and EPM have been used to obtain binary nylon 1010/EPM or nylon 1010/EPM-g-MAH blends by melt mixing. It was found that the EPM-g-MAH copolymer used as the second component has a profound effect upon the properties of the resulting blends. This behavior has been attributed to a series of chemical and physicochemical interactions taking place between the two components. The interactions are due to the presence of the anhydride functionality on the copolymer and do not occur when this functionality is absent. The interaction has been confirmed by Fourier-transform infrared spectroscopy, differential scanning calorimetry, dynamic mechanical analysis, and scanning electron microscopic.
Resumo:
The crystallization and unusual crystalline morphologies of compatible mixtures of tetrahydrofuran-methyl methacrylate diblock copolymer with tetrahydrofuran homopolymer were studied. It is shown that the PTHF [poly(tetrahydrofuran)] block of the copolymer cocrystalizes with the PTHF homopolymer in the PTHF microphase of the blend. However, the degree of crystallinity of the PTHF block is always lower than that of the PTHF homopolymer in the PTHF microphase. The crystallizability of the PTHF microphase increases appreciably with increasing PTHF microphase size and PTHF homopolymer weight fraction in the microphase. The morphology study of the blends shows that the crystalline morphology is strongly dependent on blend composition, copolymer composition and PTHF block length, as well as crystallization temperature. When alternating PTHF and PMMA [poly(methyl methacrylate)] lamellae are formed, the macroscopic crystalline morphology could be only observed when the thickness of the PTHF lamellae is large enough (similar to 20 nm). In the blend where PMMA spherical or cylindrical microphases are formed, the crystalline morphology changes dramatically with the change in the PTHF microdomain size and PMMA interdomain distance. Many unusual crystalline morphologies have been observed. A study of the solution-crystallized morphology of the blends at different temperatures shows that the morphology is also strongly dependent on the isothermal crystallization temperature, suggesting that the PMMA microdomains may have different effects on the morphology formation when the blend is crystallized at different rates.
Resumo:
The overall isothermal crystallization kinetics for neat polypropylene and grafted polypropylene systems were investigated. The rate constants were corrected assuming the heterogeneous nucleation and three dimensional growth of polypropylene spherulites. A semiempirical equation for the radial growth rate of polypropylene spherulites was developed as a function of temperature, and was used to determine the number of effective nuclei of different temperatures. The number of nuclei in grafted samples was estimated to be 10(2)-10(3) times larger than that of neat polypropylene. (C) 1997 John Wiley & Sons, Inc.
Resumo:
Comb-like polymers (CP) based on modified alternating methyl vinyl ether/maleic anhydride copolymer with oligo-oxyethylene side chains of the type-O(CH2CH2O)(n)CH3 have been synthesized and characterized, and complexed with LiNO3 to form an amorphous polymer electrolyte. CP/salt complexes showed conductivity up to 10(-5) S/cm at room temperature. The temperature dependence of ionic conductivity suggests that the ion transport is controlled by segmental motion of the polymer, shown by linear curves obtained in Vogel-Tammann-Fulcher plots. The ionic conductivity maximum moves to a higher salt concentration as the temperature increases. IR results also indicate that the ester in CP might decompose at 140 degrees C and reproduce the maleic anhydride ring.
Resumo:
Grafting of acrylamido tertiary butyl sulfonic acid (ATBS) onto ethylene-polypropylene copolymer (EPM) was carried out by using a reactive processing method. The grafting copolymer was characterized by means of WAXD, FT-IR, ESCA, and DSC. Improved thermal stability was observed for graft copolymer. Effects of the monomer and the initiator concentrations, reactive temperature, and time on grafting degree were investigated. (C) 1997 John Wiley & Sons, Inc.
Resumo:
The microphase transition in a styrene-butadiene-styrene triblock copolymer was studied by rheometric mechanical spectroscopy. A high-temperature-melt rheological transition from the highly elastic, nonlinear viscous behavior typical of a multiphase structure to linear viscous behavior with insignificant elasticity typical of a single-phase structure was observed. The transition temperature is determined according to the discontinuity of the rheological properties across the transition region, which agrees well with the results obtained from the small angle X-ray scattering data and the expectation of the random phase approximation theory. Maybe for the first time, microphase dissolution was investigated theologically. The storage modulus (G') and the loss modulus (G '') increase with time during the process. An entanglement fluctuation model based on the segmental density fluctuations is presented to explain the rheological behavior in this dissolution process. (C) 1997 John Wiley & Sons.
Resumo:
The melting points(T-m), crystalline temperature(T-c) and crystallinity(chi(c)) of propylene/alpha-olefin (pentene-l, octene-1 and decene-1) copolymers have been investigated, The results show that the T-m, T-c and chi(c) of the copolymers are lower than those of propylene homopolymer, indicating that lower alpha-olefin incorporation in copolymer has strongly hampered the crystallization of propylene, From critical crystalline sequence length of several propylene/alpha-olefin copolymers, it can be seen that a long chain alpha-olefin has much stronger effect on crystallization of PP than a short alpha-olefin does.
Resumo:
The thermal properties of ethylene-propylene copolymer grafted with glycidyl methacrylate (EP-g-GMA) were investigated by using differential scanning calorimetry (DSC). Compared to the plain ethylene-propylene copolymer (EP), peak values of melting temperature (T-m) of the propylene sequences in the grafted EP changed a little, crystallization temperature (T-c) increased about 8-12 degrees C, and melting enthalpy (Delta H-m) increased about 4-6 J/g. The isothermal and nonisothermal crystallization kinetics of grafted and ungrafted samples was carried out by DSC. Within the scope of the researched crystallization temperature, the Avrami exponent (n) of ungrafted sample is 1.6-1.8, and those of grafted samples are all above 2. The crystallization rates of propylene sequence in EP-g-GMA were faster than that in the plain EP and increased with increasing of grafted monomer content. It might be attributed to the results of rapid nucleation rate. (C) 1996 John Wiley & Sons, Inc.
Resumo:
A comb polymer with oligo-oxyethylene side chains of the type -(CH2CB2O)(12)CH3 was prepared from methyl vinyl ether/maleic anhydride copolymer and poly (ethylene glycol) methyl ether. The polymer can dissolve LiClO4 salt to form homogeneous amorphous polymer electrolyte. The ac ion conduction was measured using the complex impedance method, and conductivities were investigated as functions of temperatures and salt concentration. The complexes were first found to have two classes of glass transition which increase with increasing salt content, The optimum conductivity attained at 25 degrees C is in the order of 5.50 x 10(-6)Scm(-1). IR spectroscopy was used to study the cation-polymer interaction.
Resumo:
The crystallization and melting behaviours of a multiblock copolymer comprising poly(ether ether ketone) (PEEK) and poly(ether sulfone) (PES) blocks whose number average molecular weights <((M)over bar (n)'s)> were 10 000 and 2900, respectively, were studied. The effect of thermal history on crystallization was investigated by wide-angle X-ray diffraction measurement. A differential scanning calorimeter was used to detect the thermal transitions and to monitor the energy evolved during the isothermal crystallization process from the melt. The results suggest that the crystallization of the copolymer becomes more difficult as compared with that of pure PEEK. The equilibrium melting point of the copolymer was found to be 357 degrees C, about 30 degrees C lower than that of pure PEEK. During the isothermal crystallization, relative crystallinity increased with crystallization time, following an Avrami equation with exponent n approximate to 2. The fold surface free energy for the copolymer crystallized from the melt was calculated to be 73 erg cm(-2), about 24 erg cm(-2) higher than that of pure PEEK. Copyright (C) 1996 Elsevier Science Ltd.