Resumo:

The fracture properties of different concrete-concrete interfaces are determined using the Bazant's size effect model. The size effect on fracture properties are analyzed using the boundary effect model proposed by Wittmann and his co-workers. The interface properties at micro-level are analyzed through depth sensing micro-indentation and scanning electron microscopy. Geometrically similar beam specimens of different sizes having a transverse interface between two different strengths of concrete are tested under three-point bending in a closed loop servo-controlled machine with crack mouth opening displacement control. The fracture properties such as, fracture energy (G(f)), length of process zone (c(f)), brittleness number (beta), critical mode I stress intensity factor (K-ic), critical crack tip opening displacement CTODc (delta(c)), transitional ligament length to free boundary (a(j)), crack growth resistance curve and micro-hardness are determined. It is seen that the above fracture properties decrease as the difference between the compressive strength of concrete on either side of the interface increases. (C) 2010 Elsevier Ltd. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The micro-level properties of different self compacting concrete (SCC) mixes with and without mineral admixures are studied. The study considers SCC as a two phase material consisting of matrix and aggregate. Micro indentation technique is employed to obtain the hardness of individual phases and to compute the micro-property (modulus of elasticity). Using a self consistent homogenization procedure, the micro-property is scaled-up to obtain the macro-property which is shown to agree with the experimentally obtained macro values. It is seen that there exists a smaller interfacial transition zone at different ages of curing across all the mixes due to the presence of more fines in SCC. Also, there is no significant change in the property of the SCC having no fly ash or silica fume beyond 28 days whereas a substantial change in the micro and macro properties are seen in the SCC having fly ash and silica fume.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The flow theory of mechanism-based strain gradient (MSG) plasticity is established in this paper following the same multiscale, hierarchical framework for the deformation theory of MSG plasticity in order to connect with the Taylor model in dislocation mechanics. We have used the flow theory of MSG plasticity to study micro-indentation hardness experiments. The difference between deformation and flow theories is vanishingly small, and both agree well with experimental hardness data. We have also used the flow theory of MSG plasticity to investigate stress fields around a stationary mode-I crack tip as well as around a steady state, quasi-statically growing crack tip. At a distance to crack tip much larger than dislocation spacings such that continuum plasticity still applies, the stress level around a stationary crack tip in MSG plasticity is significantly higher than that in classical plasticity. The same conclusion is also established for a steady state, quasi-statically growing crack tip, though only the flow theory can be used because of unloading during crack propagation. This significant stress increase due to strain gradient effect provides a means to explain the experimentally observed cleavage fracture in ductile materials [J. Mater. Res. 9 (1994) 1734, Scripta Metall. Mater. 31 (1994) 1037; Interface Sci. 3(1996) 169].

Relevância:

80.00% 80.00%

Publicador:

Resumo:

在压头尖端曲率半径取100nm的前提下,采用Chen和Wang的应变梯度理论,对微压痕实验进行了系统的数值分析.首先通过拟合载荷-位移实验曲线的后半段来确定材料的屈服应力和幂硬化指数值,然后用有限元方法数值模拟压痕实验,并将计算得到的整段载荷-位移曲线及硬度-位移曲线和实验结果进行了比较.结果表明应变梯度理论所预测的计算结果和实验结果很好地符合,包括压痕深度在亚微米和微米范围内的整段曲线.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Pizgrischite, (Cu,Fe)Cu14PbBi17S35, is a new mineral species named after the type locality, Piz Grisch Mountain, Val Ferrera, Graubunden, Switzerland. This sulfosalt occurs as thin, striated, metallic lead-grey blades measuring up to I cm in length, embedded in quartz and associated with tetrahedrite, chalcopyrite, pyrite, sphalerite, emplectite and derivatives of the aikinite-bismuthinite series. In plane-polarized light, the new species is brownish grey with no perceptible pleochroism; under crossed nicols in oil immersion, it presents a weak anisotropy with dark brown tints. Minimum and maximum reflectance values (in %) in air are: 40.7-42.15 (470 nm), 41.2-43.1 (546 nm), 41.2-43.35 (589 nm) and 40.7-43.3 (650 nm). Cleavage is perfect along 001 I and well developed on {010}. Abundant polysynthetic twinning is observed on (010). The mean micro-indentation hardness is 190 kg/mm(2) (Mohs hardness 3.3), and the calculated density is 6.58 g/cm(3). Electron-microprobe analyses yield (wt%; mean result of seven analyses): Cu 16.48, Pb 2.10, Fe 0.77, Bi 60.70, Sb 0.35, S 19.16, Se 0.04, total 99.60. The resulting empirical chemical formula is (Cu15.24Fe0.80Pb0.60)(Sigma 16.64)(Bi17.07Sb0.17)(Sigma 17.24)(S35.09Se0.03)(Sigma 35.12), in accordance with the formula derived from the single-crystal refinement of the structure, (Cu,Fe)Cu14PbBi17S35. Pizgrischite is monoclinic, space group C2/m, with the following unit-cell parameters: a 35.054(2), b3.91123(I), c43.192(2) angstrom, beta 96.713(4)degrees, V5881.24 angstrom(3), Z=4. The strongest seven X-ray powder-diffraction lines [d in angstrom (I)(hkl)] are: 5.364(40)((6) over bar 04), 4.080(50)((8) over bar 05), 3.120(40)(118), 3.104(68)((3) over bar 18), 2.759(53) ((9) over bar 11),2.752(44)(910) and 1.956(100)(020). The crystal structure is an expanded monoclinic derivative of kupcikite. Pizgrischite belongs to the cuprobismutite series of bismuth sulfosalts but, sensu stricto, it is not a homologue of cuprobismutite. At the type locality. pizarischite is the result of the Alpine metamorphism under greenschist-facies conditions of pre-Tertiary hydrothermal Cu-Bi mineralization.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

La germination des spores est une étape essentielle dans le cycle de vie de la majorité des champignons filamenteux. Les champignons mycorhiziens à arbuscules (CMA) forment un certain nombre de propagules infectieuses différentes qui augmentent leur potentiel à coloniser les racines. Parmi elles se trouvent les spores extraracinaires et intraracinaires. La paroi cellulaire des spores joue un rôle majeur dans la survie de ces propagules en étant une barrière physique et osmotique. Puisque une cellule peut faire des ajustements considérables dans la composition et la structure de sa paroi, en réponse aux conditions environnementales, il est possible que les parois des spores intraracinaires et extraracinaires montrent des propriétés mécaniques et osmotiques différentes affectant leur germination et leur survie. Pourtant, contrairement à la connaissance de la génétique moléculaire et de la formation de la paroi cellulaire des CMA, peu d’information est disponible au sujet de ces propriétés mécaniques. Les informations sur la germination des CMA dans des conditions hypertoniques sont aussi rares, et les modèles expérimentaux ne séparent généralement pas les effets directs de la forte pression osmotique externe sur la germination des champignons et les effets attribuables aux plantes. Cette étude avait pour but de répondre à deux importantes séries de questions concernant le comportement des spores mycorhiziennes. Nous avons d'abord déterminé la relation entre la composition de la paroi cellulaire, la structure et les propriétés mécaniques du champignon modèle Glomus irregulare (isolat DAOM 197198). La micro-indentation a été utilisée pour mesurer quantitativement les propriétés mécaniques de la paroi cellulaire. La composition (contenu de chitine et de glomaline) de la paroi cellulaire a été quantifiée par immunofluorescence tandis que la microscopie optique a été utilisée pour mesurer l'épaisseur de la paroi cellulaire. La densité locale en glomaline et l’épaisseur de la paroi étaient significativement plus élevées pour les parois des spores extraracinaires alors que la densité locale en chitine et la rigidité n’ont pas montré de variations entre les spores extraracinaires et intraracinaires. La grande variabilité dans les paramètres étudiés nous a empêchés de cibler un facteur principal responsable de la force totale de la paroi lors de la compression. La diminution des concentrations de chitine et de glomaline a été corrélée à l'évolution de la paroi du champignon au cours de son cycle de vie. On a aussi observé une composition différentielle des couches de la paroi: les polymères de chitine et de glomaline furent localisés principalement dans les couches externes et internes de la paroi, respectivement. Dans la deuxième partie de notre travail, nous avons exploré les effets directs d'engrais, par rapport à leur activité de l'eau (aw), sur la germination des spores et la pression de turgescence cellulaire. Les spores ont été soumises à trois engrais avec des valeurs de aw différentes et la germination ainsi que la cytorrhyse (effondrement de la paroi cellulaire) des spores ont été évaluées après différents temps d'incubation. Les valeurs de aw des engrais ont été utilisées comme indicateurs de leurs pressions osmotiques. L'exposition des spores de Glomus irregulare au choc osmotique causé par les engrais dont les valeurs de aw se situent entre 0,982 et 0,882 a provoqué des changements graduels au niveau de leur cytorrhyse et de leur germination. Avec l'augmentation de la pression de turgescence externe, la cytorrhyse a augmenté, tandis que le taux de germination a diminué. Ces effets ont été plus prononcés à des concentrations élevées en éléments nutritifs. La présente étude, bien qu’elle constitue une étape importante dans la compréhension des propriétés mécaniques et osmotiques des spores de CMA, confirme également que ces propriétés dépendent probablement de plusieurs facteurs, dont certains qui ne sont pas encore identifiés.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Polydimethylsiloxane (PDMS) is the elastomer of choice to create a variety of microfluidic devices by soft lithography techniques (eg., [1], [2], [3], [4]). Accurate and reliable design, manufacture, and operation of microfluidic devices made from PDMS, require a detailed characterization of the deformation and failure behavior of the material. This paper discusses progress in a recently-initiated research project towards this goal. We have conducted large-deformation tension and compression experiments on traditional macroscale specimens, as well as microscale tension experiments on thin-film (≈ 50µm thickness) specimens of PDMS with varying ratios of monomer:curing agent (5:1, 10:1, 20:1). We find that the stress-stretch response of these materials shows significant variability, even for nominally identically prepared specimens. A non-linear, large-deformation rubber-elasticity model [5], [6] is applied to represent the behavior of PDMS. The constitutive model has been implemented in a finite-element program [7] to aid the design of microfluidic devices made from this material. As a first attempt towards the goal of estimating the non-linear material parameters for PDMS from indentation experiments, we have conducted micro-indentation experiments using a spherical indenter-tip, and carried out corresponding numerical simulations to verify how well the numerically-predicted P(load-h(depth of indentation) curves compare with the corresponding experimental measurements. The results are encouraging, and show the possibility of estimating the material parameters for PDMS from relatively simple micro-indentation experiments, and corresponding numerical simulations.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Scanning electrochemical microscopy (SECM) in surface generation/tip collection mode is investigated as an assessment tool for studying the corrosion behaviour of magnesium in simulated biological fluid. The technique provides a local map of hydrogen (H2) evolution which alone can be used as a direct measure of corrosion. The H2 generated during corrosion of magnesium is oxidized at the probe(i.e. a Pt ultra micro-electrode);with the magnitude of the current generated due to oxidation being indicative of the intensity of H2 evolution at a local scale on the magnesium surface. This method was calibrated using a cathodically polarized Pt disk to simulate H2 evolution in a controlled condition on a homogeneous surface. Potential interference from dissolving Mg or high local pH was also investigated. The technique was implemented for studying H2 evolution at the surface of AZ31 as a model Mg alloy.SECM results combined with SEM-EDX and profilometry data revealed that local domains of higher H2 evolution on the surface of AZ31 are in close proximityof the observed pitting sites.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Titanium alloys of Ti-Si-B system were manufactured by blended elemental powder method using Ti, Si and B powders as starting materials. It was found that uniaxial and isostatic pressing followed by hot pressing at around 1000°C, for 20 minutes, provided good densification of such alloys. The physicochemical studies were performed by means of scanning electron microscopy, X-ray diffraction, atomic force microscopy and microindentation/wear tests. The investigations revealed a multiphase microstructure formed mainly by α-titanium, Ti6Si2B, Ti5Si3, TiB and Ti3Si phases. The phase transformations after pressureless sintering at 1200°C was also studied by X-ray diffraction for the Ti-18Si-6B composition. As stated in some other researches, these intermetallics in the α-titanium matrix provide high wear resistance and hardness, with the best wear rate of 0.2 mm3/N.m and the highest hardness of around 1300 HV. © (2012) Trans Tech Publications, Switzerland.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Pós-graduação em Engenharia Mecânica - FEIS

Relevância:

40.00% 40.00%

Publicador:

Resumo:

A dynamical instability is observed in experimental studies on micro-channels of rectangular cross-section with smallest dimension 100 and 160 mu m in which one of the walls is made of soft gel. There is a spontaneous transition from an ordered, laminar flow to a chaotic and highly mixed flow state when the Reynolds number increases beyond a critical value. The critical Reynolds number, which decreases as the elasticity modulus of the soft wall is reduced, is as low as 200 for the softest wall used here (in contrast to 1200 for a rigid-walled channel) The instability onset is observed by the breakup of a dye-stream introduced in the centre of the micro-channel, as well as the onset of wall oscillations due to laser scattering from fluorescent beads embedded in the wall of the channel. The mixing time across a channel of width 1.5 mm, measured by dye-stream and outlet conductance experiments, is smaller by a factor of 10(5) than that for a laminar flow. The increased mixing rate comes at very little cost, because the pressure drop (energy requirement to drive the flow) increases continuously and modestly at transition. The deformed shape is reconstructed numerically, and computational fluid dynamics (CFD) simulations are carried out to obtain the pressure gradient and the velocity fields for different flow rates. The pressure difference across the channel predicted by simulations is in agreement with the experiments (within experimental errors) for flow rates where the dye stream is laminar, but the experimental pressure difference is higher than the simulation prediction after dye-stream breakup. A linear stability analysis is carried out using the parallel-flow approximation, in which the wall is modelled as a neo-Hookean elastic solid, and the simulation results for the mean velocity and pressure gradient from the CFD simulations are used as inputs. The stability analysis accurately predicts the Reynolds number (based on flow rate) at which an instability is observed in the dye stream, and it also predicts that the instability first takes place at the downstream converging section of the channel, and not at the upstream diverging section. The stability analysis also indicates that the destabilization is due to the modification of the flow and the local pressure gradient due to the wall deformation; if we assume a parabolic velocity profile with the pressure gradient given by the plane Poiseuille law, the flow is always found to be stable.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The influence of the indenter shapes and various parameters on the magnitude of the capillary force is studied on the basis of models describing the wet adhesion of indenters and substrates joined by liquid bridges. In the former, we consider several shapes, such as conical, spherical and truncated conical one with a spherical end. In the latter, the effects of the contact angle, the radius of the wetting circle, the volume of the liquid bridge, the environmental humidity, the gap between the indenter and the substrate, the conical angle, the radius of the spherical indenter, the opening angle of the spherical end in the truncated conical indenter are included. The meniscus of the bridge is described using a circular approximation, which is reasonable under some conditions. Different dependences of the capillary force on the indenter shapes and the geometric parameters are observed. The results can be applicable to the micro- and nano-indentation experiments. It shows that the measured hardness is underestimated due to the effect of the capillary force. (c) 2008 Elsevier Ltd. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Models describing wet adhesion between indenters and substrates joined by liquid bridges are investigated. The influences of indenter shapes and various parameters of structures on capillary force are focused. In the former, we consider several shapes, such as conical, spherical and truncated conical indenter with a spherical end. In the latter, the effects of the contact angle, the environmental humidity, the gap between the indenter and the substrate, etc. are included. Different dependences of the capillary force on the indenter shapes and the geometric parameters are observed. Most interesting finding is that applying the present results to micro- and nano-indentation experiments shows the size effect in indentation hardness not produced but underestimated by the effects of capillary force.(4 refs)

Relevância:

40.00% 40.00%

Publicador:

Resumo:

A novel micro-spray-assembly process and an automatic device to fabricate multilayer ultra-thin film are introduced. Employing self-assembly monolayer (SAM) technique, ultra-thin film can be assembled by utilizing the micro-spray-assembly device. The thickness and roughness of each monolayer can be controlled by varying various materials attributes, i.e., deposition time, ionic strength, pH value, molecular concentration and by selecting different manufacturing parameters of the automatic device such as spraying rate, size of micro-drop, N2 flow rate, temperature of N2 flow.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)