944 resultados para rare-earth doped glasses
Resumo:
The Sr2Mg(BO3)(2) phosphors doped respectively with Tm3+, Tb3+ and Dy3+ as activator were prepared by high temperature solid-state reaction. All the thermo luminescence curves of the phosphors consisted of two isolated peaks and the Dy3+ activated sample exhibited the strongest thermo luminescence intensity. The kinetic parameters of the thermoluminescence of Sr2Mg(BO3)(2):0.04 Dy were calculated employing the peak shape method and 3 dimensional thermo luminescent emission spectra were observed peaking at 480, 579, 662 and 755 nm due to the characteristic transition of Dy3+. In addition, the pre-irradiation heat-treatment and the thermoluminescence dose response of Sr2Mg(BO3)(2):0.04 Dy were investigated.
Resumo:
CaWO4 phosphor films doped with rare-earth ions (Eu3+, Dy-,(3+) Sm3+, Er3+) were prepared by the Pechini sol-gel process. X-ray diffraction (XRD), Fourier transform infrared spectroscopy, thermogravimetric and differential thermal analysis, atomic force microscopy, and photoluminescence spectra, as well as lifetimes, were used to characterize the resulting powders and films. The results of the XRD analysis indicated that the films began to crystallize at 400degreesC and that the crystallinity increased with elevation of the annealing temperature. The doped rare-earth ions showed their characteristic emissions in crystalline CaWO4 phosphor films due to energy transfer from WO42- groups to them. Both the lifetimes and PL intensities of the doped rare-earth ions increased with increasing annealing temperature, from 500 to 900degreesC, and the optimum concentrations for Eu3+, Dy3+, Sm3+, Er3+ were determined as 30, 1.5, 1.5, 0.5 at.% of Ca2+ in CaWO4 films annealed at 900degreesC, respectively.
Resumo:
In this presentation, nanocrystalline YVO4:A (A=Eu3+, Dy3+, SM3+, Er3+) phosphor films and their patterning were fabricated by a Pechini sol-gel process combined with a soft lithography (micro-molding in capillaries). XRD, FT-IR, AFM and optical microscope, absorption spectra, photoluminescence (PL) spectra as well as lifetimes were used to characterize the resulting films. The results of XRD indicated that the films began to crystallize at 400 degrees C and the crystallinity increased with the increase of annealing temperatures. Transparent nonpattemed phosphor films were uniform and crack free, which mainly consisted of grains with an average size of 90nm. Patterned crystalline phosphor film bands with different widths (5-30 mu m) were obtained. The doped rare earth ions (A) showed their characteristic emission in crystalline YVO4 phosphor films due to an efficient energy transfer from vanadate groups to them. The Sm3+ and Er3+ ions also showed upconversion luminescence in YVO4 film host. The optimum concentration for Eu3+ was determined to be 7 mol% and those for Dy3+, Sm3+, Er3+ were 2 Mol% of Y3+ in YVO4 films, respectively.
Resumo:
The solid electrolytes, BaCe(0.8)Ln(0.2)O(2.9) (Ln: Gd, Sm, Eu), were prepared by the sol-gel method. XRD indicated that a pure orthorhombic phase was formed at 900 degrees C. The synthesis temperature by the sol-gel method was about 600 degrees C: lower than the high temperature solid phase reaction method. The electrical conductivity and impedance spectra were measured and the conduction mechanism was studied. The grain-boundary resistance of the solid electrolyte could be reduced or eliminated by the sol-gel method. The conductivity of BaCe0.8Gd0.2O2.9 is 7.87 x 10(-2) S.cm(-1) at 800 degrees C. The open-circuit voltage of hydrogen-oxygen fuel cell using BaCe0.8Gd0.2O2.9 as electrolyte was near to 1 V and its maximum power density was 30 mW.cm(-2).
Resumo:
A novel electrical current applied technique known as flash sintering has been applied to rapidly (within 10 min) densify electrolytes including Ce0.8Gd0.2O1.9 (GDC20), Ce0.9Gd0.1O1.95 (GDC10), and Ce0.8Sm0.2O1.9 (SDC20) for application in Solid Oxide Fuel Cells (SOFCs). The densification temperature for the three electrolytes was 554°C, 635°C, and 667°C, respectively, which is far below conventional sintering temperatures. All specimens after flash sintering maintained the pure fluorite structure and exhibited a well-densified microstructure. To investigate the flash-sintering mechanism, we have applied Joule heating effect with blackbody radiation theory, and found that this theory could reasonably interpret the flash-sintering phenomenon by matching theoretically calculated temperature with the real temperature. More importantly, one of the materials inherent properties, the electronic conductivity, has been found correlated with the onset of flash sintering, which indicates that the electrons and holes are the primary current carriers during the start of flash-sintering process. As a result, potential densification mechanisms have been discussed in terms of spark plasma discharge.
Resumo:
The objective of the present work is to study the effect of rare-earth (RE) doping on the superconducting properties of (Bi,Pb)-2212 system and to develop novel superconductors in the system with improved properties, especially, the self- and in-field critical current densities so as to use them for practical applications. This dissertation describes a range of findings in Bi-based superconductor using the cationic substitution of rare earth (RE) elements. Most of the experiments reported here take advantage of the difference in the valency and ionic radii of dopant and doping site.
Resumo:
The present study is mainly concéntrated on the visible fluorescence of Ho3+ ,nd 3+ and Er 3+rare earths in alkaline earth fluoride hosts(caF2,srF2,BaF2) using a nitrogen laser excitation. A nitrogen laser was fabricated and its parametric studies were first carried out.
Resumo:
A new preparation route towards rare-earth (RE) doped polycrystalline lead lanthanum zirconate titanate (PLZT) ceramics (RE = Y(3+), Nd(3+), Yb(3+)), based on the use of doped lanthanum oxide or zirconia, is reported. Structural characterization by X-ray powder diffraction reveals that secondary phase formation can be substantially diminished in comparison to conventional preparation methods. The distribution of the rare-earth dopants was investigated as a function of concentration by static (207)Pb spin echo NMR spectra, using Fourier Transformation of Carr-Purcell-Meiboom-Gill spin echo trains. For the Nd- and Yb-doped materials, the interaction of the (207)Pb nuclei with the unpaired electron spin density results in significant broadening and shifting of the NMR signal, whereas these effects are absent in the diamagnetic Y(3+) doped materials. Based on different concentration dependences of the NMR lineshape parameters, we conclude that the structural role of the Nd(3+) dopants differs significantly from that of Yb(3+). While the Nd(3+) ions appear to be statistically distributed in the PLZT lattice, incorporation of Yb(3+) into PLZT appears to be limited by the appearance of doped cubic zirconia as a secondary phase. (C) 2009 Elsevier Masson SAS. All rights reserved.
Resumo:
To facilitate the design of laser host materials with optimized emission properties, detailed structural information at the atomic level is essential, regarding the local bonding environment of the active ions (distribution over distinct lattice sites) and their extent of local clustering as well as their population distribution over separate micro- or nanophases. The present study explores the potential of solid state NMR spectroscopy to provide such understanding for rare-earth doped lead lanthanum zirconate titanate (PLZT) ceramics. As the NMR signals of the paramagnetic dopant species cannot be observed directly, two complementary approaches are utilized: (1) direct observation of diamagnetic mimics using Sc-45 NMR and (2) study of the paramagnetic interaction of the constituent host lattice nuclei with the rare-earth dopant, using Pb-207 NMR lineshape analysis. Sc-45 MAS NMR spectra of scandium-doped PLZT samples unambiguously reveal scandium to be six-coordinated, suggesting that this rare-earth ion substitutes in the B site. Static Pb-207 spin echo NMR spectra of a series of Tm-doped PLZT samples reveal a clear influence of paramagnetic rare-earth dopant concentration on the NMR lineshape. In the latter case high-fidelity spectra can be obtained by spin echo mapping under systematic incrementation of the excitation frequency, benefiting from the signal-to-noise enhancement afforded by spin echo train Fourier transforms. Consistent with XRD data, the Pb-207 NMR lineshape analysis suggests that statistical incorporation into the PLZT lattice occurs at dopant levels of up to 1 wt.% Tm3+, while at higher levels the solubility limit is reached. (C) 2008 Elsevier Masson SAS. All rights reserved.
Resumo:
This paper presents and discusses some of the results of the effects of processing on rare earth-doped nanosize SnO2. Several relevant factors that may influence the characteristics of the final product are studied. The influence of two preparation routes and two heat-treatment conditions on the incorporation of dopants is investigated. The route whereby a soluble salt is used as the dopant source is found to provide the highest degree of dopant incorporation, even under the least favorable heat-treatment conditions.
Resumo:
Monodisperse spheres of silica and latex were obtained by a surfactant free styrene polimerization and the Stober method respectively. Controlling settling either by centrifugation or by dip-coating colloidal crystals could be obtained. Silica inverse opals were prepared by using the latex colloidal crystals as templates and TEOS/ethanol solution. Eu3+ containing silica spheres were obtained dispersing silica spheres in Eu(NO3)(3) isopropanol solutions. Emission spectra suggest the formation of an amorphous Eu3+ containing phase well adhered at the spheres surface. The utilization of solutions of trifluoroacetates salts of Pb2+ and Eu3+ was observed to destroy the silica spherical pattern when samples are treated at 1000degreesC. In that case nanocrystals of PbF2 and amorphous silica were obtained after heat treatment.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
In this work we present results on the preparation of planar waveguides based on HfO2 and HfO2-SiO2. Stable sols containing europium and erbium doped HfO2 nanoparticles have been prepared and characterized. The nanosized sol was either deposited (spin-coating) on quartz substrates or embedded in (3-glycidoxipropil)trimethoxisilane (GPTS) used as a hybrid host for posterior deposition. The refractive index dispersion and luminescence characteristics were determined for the resulting HfO2 films. The optical parameters of the waveguides such as refractive index, thickness and propagation losses were measured for the hybrid composite. The planar waveguides present thickness of a few micra and support well confined propagating modes.
Resumo:
In this work we report on visible upconversion emission in Er 3+-, and Ho3+-doped PbGeO3-PbF 2-CdF2-based transparent glass ceramics under 980 nm infrared excitation. In erbium-doped vitroceramic samples, blue(410 ran), green(530, and 550 nm) and red(660 nm) emission signals were generated, which were identified as due to the 2H9/2, 2H 11/2, 4S3/2, and 4F9/2 transitions to the 4I15/2 ground-state, respectively. Intense red(650 nm) upconversion emission corresponding to the 5F5 - 5I8 transition and very small blue(490 nm) and green(540 nm) signals assigned to the 5F 2,3 - 5I8 and 4S2, 5F4 - 5I8 transitions, respectively, were observed in the holmium-doped samples. The 540 nm is the dominant upconversion signal in Ho3+-doped vitroceramics under 850 nm excitation. The dependence of the upconversion processes upon pump power and doping concentration are also investigated, and the main routes for the upconversion excitation processes are also identified. The comparison of the upconversion process in transparent glass ceramics and the precursor glass was also examined and the results revealed that the former present higher upconversion efficiencies.