905 resultados para cellulose acetate
Resumo:
Stability and interface properties of cellulose acetate propionate (CAP) and cellulose acetate butyrate (CAB) films adsorbed from acetone or ethyl acetate onto Si wafers have been investigated by means of contact angle measurements and atomic force microscopy (AFM). Surface energy (gamma(total)(S)) values determined for CAP adsorbed from acetone are larger than those from ethyl acetate. In the case of CAB films adsorbed from ethyl acetate and acetone were similar. Dewetting was observed by AFM only for CAP films prepared from ethyl acetate. Positive values of effective Hamaker constant (A(eff)) were found only for CAP prepared from ethyl acetate, corroborating with dewetting phenomena observed by AFM. Oil the contrary, negative values of A(eff) were determined for CAP and CAB prepared from acetone and for CAB prepared from ethyl acetate, Corroborating with experimental observations. Sum frequency generation (SFG) vibrational spectra indicated that CAP and CAB films prepared from ethyl acetate present more alkyl groups oriented perpendicularly to the polymer-air interface than those films prepared from acetone. Such preferential orientation corroborates with macroscopic contact angle measurements. Moreover, SFG spectra showed that acetone hinds strongly to Si wafers, creating a new surface for CAP and CAB films. (C) 2008 Elsevier Inc. All rights reserved.
Resumo:
Spin-coated films of cellulose acetate (CA), cellulose acetate propionate (CAP), cellulose acetate butyrate (CAB) and carboxymethylcellulose acetate butyrate (CMCAB) have been characterized by ellipsometry, atomic force microscopy (AFM) and contact angle measurements. The films were spin-coated onto silicon wafers, a polar surface. Mean thickness values were determined by means of ellipsometry and AFM as a function of polymer concentration in solutions prepared either in acetone or in ethyl acetate (EA), both are good solvents for the cellulose esters. The results were discussed in the light of solvent evaporation rate and interaction energy between substrate and solvent. The effects of annealing and type of cellulose ester on film thickness, film morphology, surface roughness and surface wettability were also investigated.
Resumo:
Cellulose hollow fiber membranes (CHFM) were prepared using a spinning solution containing N-methylmorpholine-N-oxide as solvent and water as a nonsolvent additive. Water was also used as both the internal and external coagulant. It was demonstrated that the phase separation mechanism of this system was delayed demixing. The CHFM was revealed to be homogeneously dense structure after desiccation. The gas permeation properties of CO2, N-2, CH4, and H-2 through CHFM were investigated as a function of membrane water content and operation pressure. The water content of CHFM had crucial influence on gas permeation performance, and the permeation rates of all gases increased sharply with the increase of membrane water content. The permeation rate of CO2 increased with the increase of operation pressure, which has no significant effect on N-2, H-2, and CH4. At the end of this article a detailed comparison of gas permeation performance and mechanism between the CHFM and cellulose acetate flat membrane was given. (C) 2003 Wiley Periodicals, Inc.
Resumo:
The ionic liquid (IL), 1-allyl-3-(1-butyl)imidazolium chloride (AlBuImCl), has been synthesized and its properties determined. Increase in the temperature increased its conductivity and decreased its density, polarity, and viscosity. Microcrystalline cellulose (MCC), dissolves in thisIL by heating at 80 degrees C; this did not affect its degree of polymerization, decreased its index of crystallinity (Ic), and changed in morphology after regeneration. Convenient acylation of MCC was achieved by using 50% excess anhydride at 80 degrees C, for 24 or 48 h for acetic and butyric anhydride, respectively. The composition of the mixed esters depended on the initial ratio of the anhydrides, and their order of addition.
Resumo:
The acylation of three cellulose samples by acetic anhydride, Ac(2)O, in the solvent system LiCl/N,N-dimethylacetamide, DMAc (4 h, 110 A degrees C), has been revisited in order to investigate the dependence of the reaction efficiency on the structural characteristics of cellulose, and its aggregation in solution. The cellulose samples employed included microcrystalline, MCC; mercerized cotton linters, M-cotton, and mercerized sisal, M-sisal. The reaction efficiency expresses the relationship between the degree of substitution, DS, of the ester obtained, and the molar ratio Ac(2)O/AGU (anhydroglucose unit of the biopolymer); 100% efficiency means obtaining DS = 3 at Ac(2)O/AGU = 3. For all celluloses, the dependence of DS on Ac(2)O/AGU is described by an exponential decay equation: DS = DS(o) - Ae(-[(Ac2O/AGU)/B]); (A) and (B) are regression coefficients, and DS(o) is the calculated maximum degree of substitution, achieved under the conditions of each experiment. Values of (B) are clearly dependent on the cellulose employed: B((M-cotton)) > B((M-sisal)) > B((MCC)); they correlate qualitatively with the degree of polymerization of cellulose, and linearly with the aggregation number, N(agg), of the dissolved biopolymer, as calculated from static light scattering measurements: (B) = 1.709 + 0.034 N(agg). To our knowledge, this is the first report on the latter correlation; it shows the importance of the physical state of dissolved cellulose, and serves to explain, in part, the need to use distinct reaction conditions for MCC and fibrous celluloses, in particular Ac(2)O/AGU, time, temperature.
Resumo:
In the present study the effect of relative humidity (RH) during spin-coating process on the structural characteristics of cellulose acetate (CA), cellulose acetate phthalate (C-A-P), cellulose acetate butyrate (CAB) and carboxymethyl cellulose acetate butyrate (CMCAB) films was investigated by means of atomic force microscopy (AFM), ellipsometry and contact angle measurements. All polymer solutions were prepared in tetrahydrofuran (THF), which is a good solvent for all cellulose esters, and used for spin-coating at RH of (35 +/- A 5)%, (55 +/- A 5)% or (75 +/- A 5)%. The structural features were correlated with the molecular characteristics of each cellulose ester and with the balance between surface energies of water and THF and interface energy between water and THF. CA, CAB, CMCAB and C-A-P films spin-coated at RH of (55 +/- A 5)% were exposed to THF vapor during 3, 6, 9, 60 and 720 min. The structural changes on the cellulose esters films due to THF vapor exposition were monitored by means of AFM and ellipsometry. THF vapor enabled the mobility of cellulose esters chains, causing considerable changes in the film morphology. In the case of CA films, which are thermodynamically unstable, dewetting was observed after 6 min exposure to THF vapor. On the other hand, porous structures observed for C-A-P, CAB and CMCAB turned smooth and homogeneous after only 3 min exposure to THF vapor.
Resumo:
Films of cellulose acetate butyrate (CAB) and carboxymethylcellulose acetate butyrate (CMCAB) were deposited from ethyl acetate solutions onto bare silicon wafers (Si/SiO2) or amino-terminated surfaces (APS) by means of equilibrium adsorption. All surfaces were characterized by means of ellipsometry, atomic force microscopy (AFM) and contact angle measurements. The presence of amino groups on the support surface favored the adsorption of CAB and CMCAB, inducing the orientation almost polar groups to the surface and the exposition of alkyl group to the air. Such molecular orientation caused increase of the dispersive component of surface energy (gamma(d)(s)) and decrease of the polar component of surface energy (gamma(p)(s)) of cellulose esters in comparison to those values determined for films deposited onto bare Si/SiO2 wafers. Adsorption behavior of jacalin or concanavalin A onto CAB and CMCAB films was also investigated. The adsorbed amounts of lectins were more pronounced on cellulose esters with high (gamma(p)(s)) and total surface energy (gamma(t)(s)) values. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Thermal behavior of mixtures composed of cellulose acetate butyrate (CAB), carboxymethylcellulose acetate butyrate (CMCAB), or cellulose acetate phthalate (CAPh), and sorbitan-based surfactants was investigated as a function of mixture composition by means of differential scanning calorimetry (DSC). Surfactants with three different alkyl chain lengths, namely, polyoxyethylenesorbitan monolaurate (Tween 20), polyoxyethylenesorbitan monopalmitate (Tween 40), and polyoxyethylene sorbitan monostearate (Tween 60) were chosen. DSC measurements revealed that Tween 20, 40, and 60 act as plasticizers for CAB, CMCAB, and CAPh (except for Tween 60), leading to a dramatic reduction of glass transition temperature (T-g). The dependence of experimental T-g values on the mixture composition was compared with theoretical predictions using the Fox equation. Plasticization was strongly dependent on mixture composition, surfactant hydrophobic chain length, and type of cellulose ester functional group.
Resumo:
Triggered biodegradable composites made entirely from renewable resources are urgently sought after to improve material recyclability or be able to divert materials from waste streams. Many biobased polymers and natural fibers usually display poor interfacial adhesion when combined in a composite material. Here we propose a way to modify the surfaces of natural fibers by utilizing bacteria (Acetobacter xylinum) to deposit nanosized bacterial cellulose around natural fibers, which enhances their adhesion to renewable polymers. This paper describes the process of modifying large quantities of natural fibers with bacterial cellulose through their use as substrates for bacteria during fermentation. The modified fibers were characterized by scanning electron microscopy, single fiber tensile tests, X-ray photoelectron spectroscopy, and inverse gas chromatography to determine their surface and mechanical properties. The practical adhesion between the modified fibers and the renewable polymers cellulose acetate butyrate and poly(L-lactic acid) was quantified using the single fiber pullout test. © 2008 American Chemical Society.
Resumo:
Ammonium perchlorate (AP) has been coated with polystyrene (PS), cellulose acetate (CA), Novolak resin and polymethylmethacrylate (PMMA) by a solvent/nonsolvent method which makes use of the coacervation principle. The effect of polymer coating on AP decomposition has been studied using thermogravimetry (TG) and differential thermal analysis (DTA). Polymer coating results in the desensitization of AP decomposition. The observed effect has been attributed to the thermophysical and thermochemical properties of the polymer used for coating. The effect of polystyrene coating on thermal decomposition of aluminium perchlorate trihydrazinate and ammonium nitrate as well as on the combustion of AP-CTPB composite propellants has been studied.
Resumo:
A kind of optical pH sensor was demonstrated that is based on a pH-sensitive fluorescence dye-doped (eosin) cellulose acetate (CA) thin-film modified microstructured polymer optical fiber (MPOF). It was obtained by directly inhaling an eosin-CA-acetic acid mixed solution into array holes in a MPOF and then removing the solvent (acetic acid). The sensing film showed different fluorescence intensities to different pH solutions in a pH range of 2.5-4.5. Furthermore, the pH response range could be tailored through doping a surfactant, hexadecyl trimethyl ammonium bromide (CTAB), in the sensing film. (c) 2007 Optical Society of America.
Resumo:
The mono- and bimetallic catalytic polymeric hollow-fiber reactors were established with catalytic polymeric cellulose acetate (CA) hollow fibers prepared by supporting the polymer-anchored mono- or bimetallic catalyst in/on the inner wall of the hollow fibers. The selective hydrogenation of cyclopentadiene to cyclopentene was efficiently carried out in the above catalytic polymeric hollow-fiber reactors, especially in the NaBH4 reduced bimetallic PVP-Pd-0.5Co/CA hollow-fiber reactor under mild conditions of 40 degrees C and 0.1 MPa. It was found that there was a remarkable synergic effect of palladium and cobalt reduced by NaBH4 in the bimetallic PVP-Pd-0.5Co/CA hollow-fiber reactor, which results in a 97.5% conversion of cyclopentadiene and a 98.4% selectivity for cyclopentene. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Various metal-chitosan nanocomposites were synthesized, including silver (Ag), gold (Au), platinum (Pt), and palladium (Pd) in aqueous solutions. Metal nanoparticles were formed by reduction of corresponding metal salts with NaBH4 in the presence of chitosan. And chitosan molecules adsorbing onto the surface of as-prepared metal nanoparticles formed the corresponding metal-chitosan nanocomposites. Transmission electron microscopy (TEM) images and UV-vis spectra of the nanocomposites revealed the presence of metal nanoparticles. Comparison of all the resulting particles size, it shows that silver nanoparticles are much larger than others (Au, Pt and Pd). In addition, the difference in particles size leads to develop different morphologies in the films cast from prepared metal-chitosan nanocomposites. Polarized optical microscopy (POM) images show a batonet-like structure for Ag-chitosan nanocomposites film, while for the films cast from other metal (Au, Pt, and Pd)-chitosan nanocomposites, some branched-like structures with a few differences among them were observed under POM observation.
Resumo:
Mixtures of methanol/MTBE were separated with polyimide/sulfonated poly(ether-sulfone) hollow-fiber membranes. The separation was attempted by vapor permeation instead of pervaporation, which had been used by most researchers. The separation properties of the hollow-fiber membranes and operating conditions are discussed. The results showed that separation factors of the blended polyimide/sulfonated poly(ether-sulfone) hollow-fiber membranes were extremely high for the methanol/MTBE mixtures.
Resumo:
The porosity and the hydrophobicity of membranes are two essential requirements for membrane distillation (MD) of aqueous solutions. So far, the hydrophobic porous membranes used in MD studies have been prepared from hydrophobic materials. In this work, hydrophilic cellulose acetate and cellulose nitrate membranes were modified into hydrophobic membranes by radiation grafting polymerization and plasma polymerization, and used in MD studies successfully. The results indicated that modified membranes with good performance in MD can be obtained if the modifying conditions are controlled appropriately. Especially plasma polymerization, in which many particular kinds of monomer could be polymerized onto the surface of porous materials, has become an efficient method to prepare hydrophobic porous membrane with high performance from hydrophilic membranes. It will stimulate the development and practical application of MD.