999 resultados para Zirconium alloys


Relevância:

60.00% 60.00%

Publicador:

Resumo:

"Contract No. W-7405-eng-92."

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Plate-shaped products resulting from martensitic, diffusional, and mixed mode transformations in zirconium-base alloys are compared. in the present study. These alloys are particularly suitable for the comparison in view of the fact that the lattice correspondence between the parent beta (bcc) and the product alpha (hcp) or gamma-hydride (fct) phases are remarkably similar for different types of transformations. Crystallographic features such as orientation relations, habit planes, and interface structures associated with these transformations have been compared:, with a view toward examining whether the transformation mechanisms have characteristic imprints on these experimental observables. Martensites exhibiting dislocated lath, internally twinned plate, and self-accommodating three-plate cluster morphologies have been encountered in Zr-2.5Nb alloy. Habit planes corresponding to all these morphologies have been found to be consistent with the predictions based on the invariant plane strain (IFS) criterion. Different morphologies have been found to reflect the manner in which the neighboring martensite variants are assembled. Lattice-invariant shears (LISs) for all these cases have been identified to be either {10 (1) over bar 1}(alpha) ((1) over bar 123)(alpha) slip or twinning on (10 (1) over bar 1)(alpha) planes. Widmanstatten alpha precipitates, forming in a step-quenching treatment, have been shown to have a lath morphology, the alpha/beta interface being decorated with a periodic array of (c + a) dislocations at a spacing of 8 to 10 nm. The line vectors of these dislocations are nearly parallel to the invariant lines. The alpha precipitates, forming in the retained beta phase on aging, exhibit an internally twinned structure with a zigzag habit plane. Average habit planes for the morphologies have been found to lie near the {103}(beta) - {113}(beta) poles, which are close to the specific variant of the {112}(beta) plane, which transforms into a prismatic plane of the type {1 (1) over bar 00}(alpha). The crystallography of the formation of the gamma-hydride phase (fct) from both the alpha and beta phases is seen to match the IFS predictions. While the beta-gamma transformation can be treated approximately as a simple shear on the basal plane involving a change in the stacking sequence, the alpha-gamma transformation call be conceptually broken into a alpha --> beta transformation following the Burgers correspondence and the simple beta-gamma shear process. The active eutectoid decomposition in the Zr-Cu system, beta --> alpha + beta', has been described in terms of cooperative growth of the alpha phase from the beta phase through the Burgers correspondence and of the partially ordered beta' (structurally similar to the equilibrium Zr2Cu phase) through an ordering process. Similarities and differences in crystallographic features of these transformations have been discussed. and the importance of the invariant line vector in deciding the geometry of the corresponding habit planes has been pointed out.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Development of new biodegradable implants and devices is necessary to meet the increasing needs of regenerative orthopedic procedures. An important consideration while formulating new implant materials is that they should physicochemically and biologically mimic bone-like properties. In earlier studies, we have developed and characterized magnesium based biodegradable alloys, in particular magnesium-zirconium (Mg-Zr) alloys. Here we have reported the biological properties of four Mg-Zr alloys containing different quantities of strontium or calcium. The alloys were implanted in small cavities made in femur bones of New Zealand White rabbits, and the quantitative and qualitative assessments of newly induced bone tissue were carried out. A total of 30 experimental animals, three for each implant type, were studied, and bone induction was assessed by histological, immunohistochemical and radiological methods; cavities in the femurs with no implants and observed for the same period of time were kept as controls. Our results showed that Mg-Zr alloys containing appropriate quantities of strontium were more efficient in inducing good quality mineralized bone than other alloys. Our results have been discussed in the context of physicochemical and biological properties of the alloys, and they could be very useful in determining the nature of future generations of biodegradable orthopedic implants.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Factors that influence alloying zirconium to magnesium with a Mg-33.3Zr master alloy and the subsequent grain refinement are discussed based on a large number of experiments conducted at the laboratory scale (up to 30 kg of melt). It is shown that the zirconium particles released from the Zirmax(R) master alloy must be brought into thorough contact with the melt by an appropriate stirring process in order to attain a good dissolution of zirconium. The influence of alloying temperature on the recovery of zirconium was found to be negligible in the range from 680 to 780 degreesC. An ideal zirconium alloying process should end up with both high soluble and high total zirconium in the melt in order to achieve the best grain refinement in the final alloy. The distribution of zirconium in the final alloy microstructure is inhomogeneous and almost all of the zirconium in solution is concentrated in zirconium-rich cores in the microstructure.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

A new zirconium-rich magnesium-zirconium master alloy (designated AM-cast) has been developed by the CRC for Cast Metals Manufacturing in collaboration with Australian Magnesium Corporation for use as a grain refiner for magnesium alloys that do not contain aluminium. This work describes the microstructural characteristics of this new grain refiner and its grain refining ability when added to different magnesium alloys under various conditions (alloying temperature from 680 °C to 750 °C; weight of melt from 1 kg to 150 kg and sample thickness from 7 mm to 62 mm). Owing to its highly alloyable microstructure, AM-cast can be readily introduced into molten magnesium at any temperature when assisted by a few minutes of stirring or puddling. Little sludge has been found at the bottom of the alloying vessel in these trials due to the fine zirconium particles contained in the master alloy. The recovery of zirconium is normally in the range from 40% to 60% with respect to 1% zirconium addition as the master alloy. It is shown that this new master alloy is an excellent grain refiner for aluminium-free magnesium alloys.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The precipitation reactions occurring in a series of copper-based alloys selected from the system copper-chromium-zirconium have been studied by resistometric and metallographic techniques. A survey of the factors influencing the development of copper-based alloys for high strength, high conductivity applications is followed by a more general review of contemporary materials, and illustrates that the most promising alloys are those containing chromium and zirconium. The few systematic attempts to study alloys from this system have been collated, discussed, and used as a basis for the selection of four alloy compositions viz:- Cu - 0.4% Cr Cu - 0.24. Zr Cu - 0. 3% Cr - 0.1% Zr Cu - 0.2% Cr - 0.2% Zr A description of the experimental techniques used to study the precipitation behaviour of these materials is preceeded by a discussion of the currently accepted theories relating to precipitate nucleation and growth. The experimental results are presented and discussed for each of the alloys independently, and are then treated jointly to obtain an overall assessment of the way in which the precipitation kinetics, metallography and mechanical properties vary with alloy composition and heat treatment. The metastable solid solution of copper-chromium is found to decompose by the rejection of chromium particles which maintain a coherent interface and a Kurdjumov-Sachs type crystallographic orientation relationship with the copper matrix. The addition of 0.1% zirconium to the alloy retards the rate of transformation by a factor of ten and modifies the dispersion characteristics of the precipitate without markedly altering the morphology. Further additions of zirconium lead to the growth of stacking faults during ageing, which provide favourable nucleation sites for the chromium precipitate. The partial dislocations bounding such stacking faults are also found to provide mobile heterogeneous nucleation sources for the precipitation reactions occurring in copper-zirconium.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The successful applications of magnesium (Mg) alloys as biodegradable orthopedic implants are mainly restricted due to their rapid degradation rate in the physiological environment, leading to a loss of mechanical integrity. This study systematically investigated the degradation behaviors of novel Mg-Zr-Sr alloys using electrochemical techniques, hydrogen evolution, and weight loss in simulated body fluid (SBF). The microstructure and degradation behaviors of the alloys were characterized using optical microscopy, XRD, SEM, and EDX. The results indicate that Zr and Sr concentrations in Mg alloys strongly affected the degradation rate of the alloys in SBF. A high concentration of 5 wt% Zr led to acceleration of anodic dissolution, which significantly decreased the biocorrosion resistance of the alloys and their biocompatibility. A high volume fraction of Mg17Sr2 phases due to the addition of excessive Sr (over 5 wt%) resulted in enhanced galvanic effects between the Mg matrix and Mg17Sr2 phases, which reduced the biocorrosion resistance. The average Sr release rate is approximately 0.15 mg L-1 day-1, which is much lower than the body burden and proves its good biocompatibility. A new biocorrosion model has been established to illustrate the degradation of alloys and the formation of degradation products on the surface of the alloys. It can be concluded that the optimal concentration of Zr and Sr is less than 2 wt% for as-cast Mg-Zr-Sr alloys used as biodegradable orthopedic implants.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The microstructural changes of Al-22 wt%U and Al-46 wt%U alloys containing 3 wt% Zr were investigated after heat treatment at 620 degrees C for 1 to 45 days, Though it is reported that addition of similar to 3 wt% Zr stabilizes the (U,Zr)Al-3 phase at room temperature, the present investigation shows that the (U,Zr)Al-3 phase is not stable but slowly transforms to the U0.9Al4 phase, The high temperature creep curves generated for these ternary alloys showed a wavy pattern which also suggests that the (U,Zr)Al-3 phase is not stable.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The influence of pH on the corrosion behaviour of two aluminium-lithium-copper-magnesium-zirconium (8090 and 2091) alloys was studied and compared with a standard aircraft alloy, 2014 (Al-4.4% Cu) and 99.9% pure Al. In constant exposure and potentiodynamic polarization studies conducted in 3.5% NaCl solution having different pH values, all the alloys exhibited high corrosion rates in acidic and alkaline environments, with a minimum in less hostile environments close to neutral pH. The pitting potentials for aluminium-lithium alloys were slightly lower than those for 2014 and pure Al. The effect of pH on the passive current density was also less for aluminium-lithium alloys.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Strontium modified barium zirconium titanate with general formula Ba1-xSrxZr0.05Ti0.95O3 ceramics have been prepared by solid state and high energy ball milling technique. The X-ray diffraction and Rietveld refinement studies show that all the compositions have single phase symmetry. The composition BaZr0.05Ti0.95O3 shows orthorhombic symmetric with space group Amm2. The structure changes from orthorhombic to tetragonal with strontium doping up to x = 0.3 and with further addition, changes to cubic. The scanning electron micrographs show that the grain size decreases with increase in strontium content. The temperature dependent dielectric behavior shows three phase transition in the parent material which merges with an increase in Sr content The transition temperature and dielectric constant decreases with an increase in Sr concentration. The phase transition becomes more diffused with increment in doping concentration. The ferroelectric behavior of the ceramics is studied by the hysteresis loop. The optical behavior is studied by the UV-visible spectroscopy and found that the optical band gap increases with Sr concentration. (C) 2015 Elsevier B.V. All rights reserved.