In this paper, we describe a wide-angle laser beam scanner and the rigorous result of the wide-angle laser beam scanner was obtained with the help of the vector refraction theory. Using the rigorous results, the distortion of the beam shape was discussed. The distortion of the beam shape is varying with the different relative angles of the double prisms. According to the conservation of the energy, the distribution of the laser intensity is changed too. (c) 2005 Elsevier GmbH. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We describe the rigorous results of a wide-angle laser beam scanner, obtained with the help of the vector refraction theory. Using the rigorous results, the distortion of the beam shape is discussed. The distortion to the beam varies with the different relative angles of double prisms. The scanner expands the beam in some directions while it contracts the beam in other directions. According to the conservation of energy, the distribution of the laser intensity is changed as well. (c) 2006 Society of Photo-Optical Instrumentation Engineers.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The structural evolution of an ice-quenched high-density polyethylene (HDPE) subjected to uniaxial tensile deformation at elevated temperatures was examined as a function of the imposed strains by means of combined synchrotron small-angle X-ray scattering (SAXS) and wide-angle X-ray scattering (WAXS) techniques. The data show that when stretching an isotropic sample with the spherulitic structure, intralamellar slipping of crystalline blocks was activated at small deformations, followed by a stress-induced fragmentation and recrystallization process yielding lamellar crystallites with their normal parallel to the stretching direction. Stretching of an isothermally crystallized HDPE sample at 120 degrees C exhibited changes of the SAXS diagram with strain similar to that observed for quenched HDPE elongated at room temperature, implying that the thermal stability of the crystal blocks composing the lamellae is only dependent on the crystallization temperature.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Based on the X-ray scattering intensity theory and using the approximate expression for the atomic scattering factor, the correction factors for three crystalline peaks and an amorphous peak of Nylon 1212 were calculated and the formula of degree of crystallinity of Nylon 1212 was derived by a graphic multipeak resolution method. The degree of crystallinity calculated from the WARD method is compatible with those obtained by density and calorimetry methods.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A novel wide angle spectrometer has been implemented with a highly oriented pyrolytic graphite crystal coupled to an image plate. This spectrometer has allowed us to look at the energy resolved spectrum of scattered x rays from a dense plasma over a wide range of angles ( ~ 30°) in a single shot. Using this spectrometer we were able to observe the temporal evolution of the angular scatter cross section from a laser shocked foil. A spectrometer of this type may also be useful in investigations of x-ray line transfer from laser-plasmas experiments.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A unique in situ multiaxial deformation device has been designed and built specifically for simultaneous synchrotron small angle X-ray scattering (SAXS) and wide angle X-ray scattering (WAXS) measurements. SAXS and WAXS patterns of high-density polyethylene (HDPE) and HDPE/clay nanocomposites were measured in real time during in situ multiaxial deformation at room temperature and at 55 degrees C. It was observed that the morphological evolution of polyethylene is affected by the existence of clay platelets as well as the deformation temperature and strain rate. Martensitic transformation of orthorhombic into monoclinic crystal phases was observed under strain in HDPE, which is delayed and hindered in the presence of clay nanoplatelets. From the SAXS measurements, it was observed that the thickness of the interlamellar amorphous region increased with increasing strain, which is due to elongation of the amorphous chains. The increase in amorphous layer thickness is slightly higher for the nanocomposites compared to the neat polymer. (C) 2011 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 49: 669-677, 2011

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This paper proposes a hybrid scanning antenna architecture for applications in mm-wave intelligent mobile sensing and communications. We experimentally demonstrate suitable W-band leaky-wave antenna prototypes in substrate integrated waveguide (SIW) technology. Three SIW antennas have been designed that within a 6.5 % fractional bandwidth provide beam scanning over three adjacent angular sectors. Prototypes have been fabricated and their performance has been experimentally evaluated. The measured radiation patterns have shown three frequency scanning beams covering angles from 11 to 56 degrees with beamwidth of 10?±?3 degrees within the 88-94 GHz frequency range.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The paper presents an analysis of WAXS (wide-angle X-ray scattering) data which aids an understanding of the structure of non-crystalline polymers. Experimental results are compared with calculations of scattering from possible models. Evidence is presented which supports the view that the chains in molten PE do not lie parallel but have a conformation in accord with the predictions of energy calculations. However, the evidence indicates that in “molten” PTFE the chains lie parallel over distances well in excess of their diameters. WAXS-based proposals are made for the conformations of a-PMMA and a-PS.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Molecular orientation parameters have been measured for the non-crystalline component of crosslinked natural rubber samples deformed in uniaxial tension as a function of the extension ratio and of temperature. The orientation parapeters 〈P2(cosα)〉 and 〈P4(cosα)〉 were obtained by an analysis of the anisotropy of the wide-angle X-ray scattering functions. For the measurements made at high temperatures the level of crystallinity detected was negligible and the orientation-strain behaviour could be compared directly with the predictions of molecular models of rubber elasticity. The molecular orientation behaviour with strain was found to be at variance with the estimates of the affine model particularly at low and moderate strains. Extension of the crosslinked rubber at room temperature led to strain-crystallization and measurements of both the molecular orientation of the non-crystalline chains and the degree of crystallinity during extension and relaxation enabled the role of the crystallites in the deformation process to be considered in detail. The intrinsic birefringence of the non-crystalline component was estimated, through the use of the 〈P2(cosα)〉 values obtained from X-ray scattering measurements, to be 0.20±0.02.