Resumo:
The self adhesion behaviour of thermoplastic polyurethane (TPU) in itself and its composite with short Kevlar fibre with respect to contact time, temperature, pressure, and fibre loading has been studied. The adhesion strength showed two linear increments of different slopes with respect to the square root of time: with temperature and pressure of contact, the adhesion strength was improved. The maximum strength was obtained with 20 phr of short fibre in only one of the mating substrates in the peel test sample. The duration for wetting and diffusion was shifted to longer time intervals with fibres loaded in both the substrates.
Resumo:
The effect of an external flaw on the tensile strength of short kevlar fiber-thermoplastic composites has been studied with respect to fiber content, fiber orientation, location of the external flaw, and the temperature of test. The composites showed a three-step reduction in tensile strength with increasing flaw size. The critical flaw-length region was shifted to higher flaw-size levels with increasing fiber content. With increasing temperature, the critical flaw length was increased in the case of unfilled TPU, whereas it remained more or less constant in the case of short kevlar fiber-filled-TPU composite.
Resumo:
The flammability of short Kevlar aramide fiber-thermoplastic polyurethane (TPU) has been investigated with respect to fiber loading and various flame retardant additives such as halogen containing polymers, antimony oxide/chlorine donor combination, zinc borate, and aluminum hydroxide. Smoke generation was reduced drastically, while the oxygen index was reduced marginally in the presence of short fibers. The best improvement in the oxygen index was obtained with antimony oxide/chlorinated paraffin wax combination, in the weight ratio 1:6. A 70 phr loading of aluminum hydroxide improved LOI and reduced smoke generation.
Resumo:
The thermal degradation of short kevlar fibre-thermoplastic polyurethane (TPU) composites has been studied by Thermogravimetric Analysis (TGA) and Differential Scanning Calorimetry (DSC). TGA showed that the thermal degradation of TPU takes place in two steps with peak maxima (T1max and T2ma,) at 383°C and 448°C, respectively. In the presence of 10-40 phr of short kevlar fibres, T1_ and T2max were shifted to lower temperatures. The temperature of onset of degradation was increased from 245 to 255°C at 40 parts per hundred rubber (phr) fibre loading. Kinetic studies showed that the degradation of TPU and kevlar-TPU composite follows first-order reaction kinetics. The DSC study showed that there is an improvement in thermal stability of TPU in the presence of 20 phr of short kevlar fibres.
Resumo:
Cellulose was extracted from lignocellulosic fibers and nanocrystalline cellulose (NC) prepared by alkali treatment of the fiber, steam explosion of the mercerized fiber, bleaching of the steam exploded fiber and finally acid treatment by 5% oxalic acid followed again by steam explosion. The average length and diameter of the NC were between 200-250 nm and 4-5 nm, respectively, in a monodisperse distribution. Different concentrations of the NC (0.1, 0.5, 1.0, 1.5, 2.0 and 2.5% by weight) were dispersed non-covalently into a completely bio-based thermoplastic polyurethane (TPU) derived entirely from oleic acid. The physical properties of the TPU nanocomposites were assessed by Fourier Transform Infra-Red spectroscopy (FTIR), Thermo-Gravimetric Analysis (TGA), Differential Scanning Calorimetry (DSC), X-Ray Diffraction (XRD), Dynamic Mechanical Analysis (DMA) and Mechanical Properties Analysis. The nanocomposites demonstrated enhanced stress and elongation at break and improved thermal stability compared to the neat TPU. The best results were obtained with 0.5% of NC in the TPU. The elongation at break of this sample was improved from 178% to 269% and its stress at break from 29.3 to 40.5 MPa. In this and all other samples the glass transition temperature, melting temperature and crystallization behavior were essentially unaffected. This finding suggests a potential method of increasing the strength and the elongation at break of typically brittle and weak lipid-based TPUs without alteration of the other physico-chemical properties of the polymer. (C) 2012 Elsevier Ltd. All rights reserved.
Early season ozone uptake is important for determining ozone tolerance in two trembling aspen clones
Resumo:
There is substantial genetic variability in response to ozone amongst and within tree species. Aspen is a highly variable species with a wide range of responses to ozone. Aspen response to elevated O3 levels is being investigated at the Aspen FACE site near Rhinelander, WI where five aspen clones of varying O3 tolerance have been fumigated with elevated O3 over the past decade. In this study, we examined the physiological differences in two of the aspen clones that differed significantly in their O3 tolerance with 8L being tolerant and 42E being sensitive. Throughout the 2007 and 2008 growing seasons we periodically estimated instantaneous photosynthetic rates, ACi responses and light response curves. The results of our study suggest that aspen clone 8L’s tolerance is due in part to decreased stomatal conductance early in the season, which lowered ozone uptake. Later during the season O3 uptake was comparable for the two clones. Our results also suggest the response of Vcmax, TPU, Rd, Gm, light compensation point and quantum flux to elevated O3 did not differ significantly between the two clones. Ozone uptake is important for ozone tolerance in clone 8L early in the season but cannot explain late season tolerance. Photosynthetic parameters for the two clones were similar, so clone 8L’s ozone tolerance is not due to a more efficient photosynthetic system.
Resumo:
A series of TPU nanocomposites were prepared by incorporating organically modified layered silicates with controlled particle size. To our knowledge, this is the first study into the effects of layered silicate diameter in polymer nanocomposites utilizing the same mineral for each size fraction. The tensile properties of these materials were found to be highly dependent upon the size of the layered silicates. A decrease in disk diameter was associated with a sharp upturn in the stress-strain curve and a pronounced increase in tensile strength. Results from SAXS/SANS experiments showed that the layered silicates did not affect the bulk TPU microphase structure and the morphological response of the host TPU to deformation or promote/hinder strain-induced soft segment crystallization. The improved tensile properties of the nanocomposites containing the smaller nanofillers resulted from the layered silicates aligning in the direction of strain and interacting with the TPU sequences via secondary bonding. This phenomenon contributes predominantly above 400% strain once the microdomain architecture has largely been disassembled. Large tactoids that are unable to align in the strain direction lead to concentrated tensile stresses between the polymer and filler, instead of desirable shear stresses, resulting in void formation and reduced tensile properties. In severe cases, such as that observed for the composite containing the largest silicate, these voids manifest visually as stress whitening.
Preparation and property testing of compatibilized poly(l-lactide)/thermoplastic polyurethane blends
Resumo:
Poly(l-lactide) (PLL) has been blended with a polycaprolactone-based thermoplastic polyurethane (TPU) elastomer as a toughening agent and a poly(l-lactide-co-caprolactone) (PLLCL) copolymer as a compatibilizer. Both 2-component (PLL/TPU) and 3-component (PLL/TPU/PLLCL) blends were prepared by melt mixing, characterized, hot-pressed into thin sheets and their tensile properties tested. The results showed that, although the TPU could toughen the PLL, the blends were largely immiscible leading to phase separation. However, addition of the PLLCL copolymer improved blend compatibility. The best all-round properties were found for the 3-component blend of composition PLL/TPU/PLLCL = 90/10/10 parts by weight.
Resumo:
Il poliuretano termoplastico (TPU) è un materiale polimerico molto versatile che, se formulato in maniera opportuna può assumere un’ampia gamma di caratteristiche chimico-fisiche e proprietà meccaniche. Per questo motivo negli ultimi decenni sono state studiate estesamente le sue applicazioni e i metodi di sintesi. Il lavoro presentato ha come scopo la valutazione delle proprietà reologiche dei fusi polimerici di una serie di TPUs, mediante l'ausilio di un reometro capillare. A tal proposito lo scopo del progetto è stato quello di incrementare la conoscenza dei fenomeni reologici che avvengono in un fuso polimerico in fase di lavorazione per ottenere un determinato prodotto finito e commercializzabile e che sanciscono l'effettiva realizzazione del processo in funzione delle caratteristiche del TPU in questione. Con l’utilizzo del reometro capillare si ha la possibilità di simulare le condizioni termiche e di stress meccanico delle più comuni tecnologie di formatura dei materiali polimerici: dall’estrusione allo stampaggio ad iniezione, passando per lo stampaggio a compressione. Questa importante caratteristica strumentale risulta utile in fase di assistenza al cliente, in modo da proporre una tipologia di materiale adatta alla tecnologia disponibile e, in alcuni casi, suggerire le condizioni più opportune per la lavorazione dello stesso.