This research addresses the application of friction stir welding (FWS) of titanium alloy Ti–6Al–4V. Friction stir welding is a recent process, developed in the 1990s for aluminum joining; this joining process is being increasingly applied in many industries from basic materials, such as steel alloys, to high performance alloys, such as titanium. It is a process in great development and has its economic advantages when compared to conventional welding. For high performance alloys such as titanium, a major problem to overcome is the construction of tools that can withstand the extreme process environment. In the literature, the possibilities approached are only few tungsten alloys. Early experiments with tools made of cemented carbide (WC) showed optimistic results consistent with the literature. It was initially thought that WC tools may be an option to the FSW process since it is possible to improve the wear resistance of the tool. The metallographic analysis of the welds did not show primary defects of voids (tunneling) or similar internal defects due to processing, only defects related to tool wear which can cause loss of weld quality. The severe tool wear caused loss of surface quality and inclusions of fragments inside the joining, which should be corrected or mitigated by means of coating techniques on tool, or the replacement of cemented carbide with tungsten alloys, as found in the literature.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Assessment of laser peening induced effects on Ti6Al4V by destructive and non-destructive techniques

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Laser peening has recently emerged as a useful technique to overcome detrimental effects associated to another well-known surface modification processes such as shot peening or grit blasting used in the biomedical field. It is worth to notice that besides the primary residual stress effect, thermally induced effects might also cause subtle surface and subsurface microstructural changes that might influence corrosion resistance. Moreover, since maximum loads use to occur at the surface, they could also play a critical role in the fatigue strength. In this work, plates of Ti-6Al-4V alloy of 7 mm in thickness were modified by laser peening without using a sacrificial outer layer. Irradiation by a Q-switched Nd-YAG laser (9.4 ns pulse length) working in fundamental harmonic at 2.8 J/pulse and with water as confining medium was used. Laser pulses with a 1.5 mm diameter at an equivalent overlapping density (EOD) of 5000 cm-2 were applied. Attempts to analyze the global induced effects after laser peening were addressed by using the contacting and non-contacting thermoelectric power (TEP) techniques. It was demonstrated that the thermoelectric method is entirely insensitive to surface topography while it is uniquely sensitive to subtle variations in thermoelectric properties, which are associated with the different material effects induced by different surface modification treatments. These results indicate that the stress-dependence of the thermoelectric power in metals produces sufficient contrast to detect and quantitatively characterize regions under compressive residual stress based on their thermoelectric power contrast with respect to the surrounding intact material. However, further research is needed to better separate residual stress effects from secondary material effects, especially in the case of low-conductivity engineering materials like titanium alloys.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Pulsed Nd:YAG has been adopted successfully in welding process of thin (0.7 mm) Ti6Al4V. Laser welding of such thin sheet requires a small focal spot, good laser beam quality and fast travel speed, since too much heat generation can cause distortion for thin sheet weld. The microstructures of Ti6Al4V were complex and strongly affected the mechanical properties. These structures include: a´ martensite, metastable ß, Widmanstätten, bimodal, lamellar and equiaxed microstructure. Bimodal and Widmanstätten structures exhibit a good-balance between strength and ductility. The microstructure of pulsed Nd:YAG welded Ti6Al4V was primarily a´ martensite, which showed the lowest ductility but not significantly high strength. A heat treatment at 950 followed by furnace cooling can transform the microstructure in the weld from a´ martensite structure into Widmanstätten structure.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Distortion is one type of defect in the weld, which is troublesome for some reasons, especially in thin plate welding. Distortion was found in fibre laser welding processing for 0.7mm thickness Ti6Al4V plate. The purpose of this paper is to understand and evaluate the effect of distortion on stress level by FEA and tensile test. A group of 0.7mm Ti6Al4V plates welded using continuous wave fibre laser. FEA models were established for fibre laser welded Ti6Al4V in abaqus 6.7. © (2011) Trans Tech Publications.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Tool deflection during milling operation leads to dimensional error, decreasing surface quality and increasing rejection rate. In this study, tool deflection during the milling of the inner surfaces of Ti–6Al–4V prosthetic acetabular shell produced by selective laser melting (SLM) was modelled. The first purpose of this research is to provide a general static cutting tool deflection model for ball nose cutters where deviation of machine components and tool holder are so small as to be considered negligible. This is because the values of machine component and tool holder deflection were lower than standard tolerances (10 μm) and found to be lower than 1/15 of tool deflection. The second and third objectives of this work involve calculating contact surfaces by determining workpiece and tool geometry and choosing second moment of inertia using a novel cross section method (CSM). Static models for three quasi-analytical methods (QAM) that are simple cantilever beam model (SCBM), two-section model (TWSM) and our three section model (THSM) are presented. THSM showed high accuracy which was validated by 3D finite element method (FEM3D) and experimental measurements. The accuracy of tool deflection calculation using THSM by computing, shank, flute and ball head deflection and also utilizing CSM to determine second moment of inertia showed notable improvements.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A paradigm shift has taken place in which bone implant materials has gone from being relatively inert to having immunomodulatory properties, indicating the importance of immune response when these materials interact with the host tissues. It has therefore become important to endow the implant materials with immunomodulatory properties favouring osteogenesis and osseointegration. Strontium, zinc and silicon are bioactive elements that have important roles in bone metabolism and that also elicit significant immune responses. In this study, Sr-, Zn- and Si-containing bioactive Sr2ZnSi2O7 (SZS) ceramic coatings on Ti–6Al–4V were successfully prepared by a plasma-spray coating method. The SZS coatings exhibited slow release of the bioactive ions with significantly higher bonding strength than hydroxyapatite (HA) coatings. SZS-coated Ti–6Al–4V elicited significant effects on the immune cells, inhibiting the release of pro-inflammatory cytokines and fibrosis-enhancing factors, while upregulating the expression of osteogenic factors of macrophages; moreover, it could also inhibit the osteoclastic activities. The RANKL/RANK pathway, which enhances osteoclastogenesis, was inhibited by the SZS coatings, whereas the osteogenic differentiation of bone marrow mesenchymal stromal cells (BMSCs) was significantly enhanced by the SZS coatings/macrophages conditioned medium, probably via the activation of BMP2 pathway. SZS coatings are, therefore, a promising material for orthopaedic applications, and the strategy of manipulating the immune response by a combination of bioactive elements with controlled release has the potential to endow biomaterials with beneficial immunomodulatory properties.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Hydroxyapatite (HA) coatings have numerous applications in orthopedics and dentistry, owing to their excellent ability to promote stronger implant fixation and faster bone tissue ingrowth and remodeling. Thermal plasma spray and other plasma-assisted techniques have recently been used to synthesize various calcium phosphate-based bioceramics. Despite notable recent achievements in the desired stoichiometry, phase composition, mechanical, structural, and bio-compatible properties, it is rather difficult to combine all of the above features in a single coating. For example, many existing plasma-sprayed HA coatings fall short in meeting the requirements of grain size and crystallinity, and as such are subject to enhanced resorption in body fluid. On the other hand, relatively poor interfacial bonding and stability is an obstacle to the application of the HA coatings in high load bearing Ti6Al4V knee joint implants. Here, we report on an alternative: a plasma-assisted, concurrent, sputtering deposition technique for high performance biocompatible HA coatings on Ti6Al4V implant alloy. The plasma-assisted RF magnetron co-sputtering deposition method allows one to simultaneously achieve most of the desired attributes of the biomimetic material and overcome the aforementioned problems. This article details the film synthesis process specifications, extensive analytical characterization of the material's properties, mechanical testing, simulated body fluid assessments, biocompatibility and cytocompatibility of the HA-coated Ti6Al4V orthopedic alloy. The means of optimization of the plasma and deposition process parameters to achieve the desired attributes and performance of the HA coating, as well as future challenges in clinical applications are also discussed.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Cell-implant adhesive strength is important for prostheses. In this paper, an investigation is described into the adhesion of bovine chondrocytes to Ti6Al4V-based substrates with different surface roughnesses and compositions. Cells were cultured for 2 or 5 days, to promote adhesion. The ease of cell removal was characterised, using both biochemical (trypsin) and mechanical (accelerated buoyancy and liquid flow) methods. Computational fluid dynamics (CFD) modelling has been used to estimate the shear forces applied to the cells by the liquid flow. A comparison is presented between the ease of cell detachment indicated using these methods, for the three surfaces investigated. © 2008 Materials Research Society.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

No presente trabalho, foram realizados ensaios de tribocorrosão no aço inoxidável AISI 304L, no titânio comercialmente puro (CPTi) e na liga de titânio Ti6Al4V em solução aquosa de 0,90% m/v NaCl. Amostras de ligas de titânio com tratamento térmico superficial de refusão a laser também foram utilizadas. Um tribômetro do tipo pino-no-disco com contracorpo de alumina foi usado. Técnicas eletroquímicas in situ de monitoramento em circuito aberto, espectroscopia de impedância eletroquímica, curvas de polarização e amperimetria de resistência nula foram empregadas. Os resultados obtidos indicam que o desgaste tribocorrosivo das ligas de titânio é mais intenso do que o observado no aço inoxidável, apresentando perfis de superfície mais irregulares. A análise da impedância eletroquímica mostrou que todos os materiais utilizados apresentam uma rápida recuperação da camada passiva, exibindo módulos e fases um pouco menores do que os medidos antes do desgaste. Sob atrito, os diagramas de impedância apresentam uma forte redução do módulo. Sob desgaste, o expoente α do elemento de fase constante (CPE) atinge seu valor mais baixo, enquanto o parâmetro γ é máximo. As curvas de polarização exibem potenciais menores e densidades de corrente de corrosão maiores durante o desgaste. O tratamento de refusão a laser, embora mude a microestrutura e a dureza superficial das amostras, não indica uma mudança aparente nos parâmetros eletroquímicos sob tribocorrosão, bem como do coeficiente de atrito. Nos ensaios de amperimetria de resistência nula, foi possível estimar a corrente mensurada no ARN por meio do emprego de um circuito elétrico equivalente. A densidade espectral de potência dos sinais de potencial e de corrente exibe a frequência de rotação (1,25 Hz) e seus harmônicos. Para baixas frequências (abaixo de 10 mHz), o decaimento obedece à relação 1 ⁄ e 1⁄ para os sinais de potencial e corrente, respectivamente.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The cold crucible, or induction skull melting process as is otherwise known, has the potential to produce high purity melts of a range of difficult to melt materials, including Ti–Al and Ti6Al4V alloys for Aerospace, Ti–Ta and other biocompatible materials for surgical implants, silicon for photovoltaic and electronic applications, etc. A water cooled AC coil surrounds the crucible causing induction currents to melt the alloy and partially suspend it against gravity away from water-cooled surfaces. Strong stirring takes place in the melt due to the induced electromagnetic Lorentz forces and very high temperatures are attainable under the right conditions (i.e., provided contact with water cooled walls is minimised). In a joint numerical and experimental research programme, various aspects of the design and operation of this process are investigated to increase our understanding of the physical mechanisms involved and to maximise process efficiency. A combination of FV and Spectral CFD techniques are used at Greenwich to tackle this problem numerically, with the experimental work taking place at Birmingham University. Results of this study, presented here, highlight the influence of turbulence and free surface behaviour on attained superheat and also discuss coil design variations and dual frequency options that may lead to winning crucible designs.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The cold crucible, or induction skull melting process as is otherwise known, has the potential to produce high purity melts of a range of difficult to melt materials, including Ti–Al and Ti6Al4V alloys for Aerospace, Ti–Ta and other biocompatible materials for surgical implants, silicon for photovoltaic and electronic applications, etc. A water cooled AC coil surrounds the crucible causing induction currents to melt the alloy and partially suspend it against gravity away from water-cooled surfaces. Strong stirring takes place in the melt due to the induced electromagnetic Lorentz forces and very high temperatures are attainable under the right conditions (i.e., provided contact with water cooled walls is minimised). In a joint numerical and experimental research programme, various aspects of the design and operation of this process are investigated to increase our understanding of the physical mechanisms involved and to maximise process efficiency. A combination of FV and Spectral CFD techniques are used at Greenwich to tackle this problem numerically, with the experimental work taking place at Birmingham University. Results of this study, presented here, highlight the influence of turbulence and free surface behaviour on attained superheat and also discuss coil design variations and dual frequency options that may lead to winning crucible designs.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Models and software products have been developed for modelling, simulation and prediction of different correlations in materials science, including 1. the correlation between processing parameters and properties in titanium alloys and ?-titanium aluminides; 2. time–temperature–transformation (TTT) diagrams for titanium alloys; 3. corrosion resistance of titanium alloys; 4. surface hardness and microhardness profile of nitrocarburised layers; 5. fatigue stress life (S–N) diagrams for Ti–6Al–4V alloys. The programs are based on trained artificial neural networks. For each particular case appropriate combination of inputs and outputs is chosen. Very good performances of the models are achieved. Graphical user interfaces (GUI) are created for easy use of the models. In addition interactive text versions are developed. The models designed are combined and integrated in software package that is built up on a modular fashion. The software products are available in versions for different platforms including Windows 95/98/2000/NT, UNIX and Apple Macintosh. Description of the software products is given, to demonstrate that they are convenient and powerful tools for practical applications in solving various problems in materials science. Examples for optimisation of the alloy compositions, processing parameters and working conditions are illustrated. An option for use of the software in materials selection procedure is described.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The relationship between heat-treatment parameters and microstructure in titanium alloys has so far been mainly studied empirically, using characterization techniques such as microscopy. Calculation and modeling of the kinetics of phase transformation have not yet been widely used for these alloys. Differential scanning calorimetry (DSC) has been widely used for the study of a variety of phase transformations. There has been much work done on the calculation and modeling of the kinetics of phase transformations for different systems based on the results from DSC study. In the present work, the kinetics of the transformation in a Ti-6Al-4V titanium alloy were studied using DSC, at continuous cooling conditions with constant cooling rates of 5 °C, 10 °C, 20 °C, 30 °C, 40 °C, and 50 °C/min. The results from calorimetry were then used to trace and model the transformation kinetics in continuous cooling conditions. Based on suitably interpreted DSC results, continuous cooling–transformation (CCT) diagrams were calculated with lines of isotransformed fraction. The kinetics of transformation were modeled using the Johnson–Mehl–Avrami (JMA) theory and by applying the "concept of additivity." The JMA kinetic parameters were derived. Good agreement between the calculated and experimental transformed fractions is demonstrated. Using the derived kinetic parameters, the transformation in a Ti-6Al-4V alloy can be described for any cooling path and condition. An interpretation of the results from the point of view of activation energy for nucleation is also presented.