994 resultados para Roasting (Metallurgy)


Relevância:

20.00% 20.00%

Publicador:

Resumo:

It has been experimentally established that nickel and cobalt can be extracted from their ferrites with sodium sulphate melt containing femc ions. The kinetics of extraction from synthetic ferrites using a melt of sodium and ferric sulphates of eutectic composition has been studied as a function of the particle size of the ferrite and temperature in the range 900 to 1073 K. The divalent ions in the ferrite exchange with the ferric ion in the melt, leaving a residue of hematite.The rate of reaction conforms to the Crank-Ginstling-Brounshtein diffusion model. The reaction rate is governed by the counter-diffusion of ~ e an~d ~+i ' +(or co2+) ions in the hematite lattice. Analytical expressions for the rate constants have been derived from the experimental data as a function of particle size and temperature. The activation energy for the extraction of nickel from nickel ferrite is 154(+10) kJ mol-' and the corresponding value for cobalt is 142(+10)kJ mol;'. In sulphation roasting of minerals containing nickel, the yield of nickel is generally limited to 75% due to the formation of insoluble ferrites. The use of melts based on sodium sulphate provides a possible route for enhancing the recovery of nickel to approximately 98%.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The solid-solution-particle reinforced W(Al)-Ni composites were successfully fabricated by using mechanical alloying (MA) and hot-pressing (HP) technique when the content of Ni is between 45 wt% and 55 wt%. Besides, samples of various original component ratio of Al50W50 to Ni have been fabricated, and the corresponding microcomponents and mechanical properties such as microhardness, ultimate tensile strength and elongation were characterized and discussed. The optimum ultimate tensile strength under the experiment conditions is 1868 MPa with elongation of 10.21 % and hardness of 6.62 GPa. X-ray diffraction (XRD), FE-SEM and energy dispersive analysis of X-rays (EDS) were given to analysis the components and morphology of the composite bulk specimens.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

After thermal treatment of a mixture of glucose and glycine for 2 h at 125 degreesC, about 60% of the starting material was converted into nonsoluble, black pigments, whereas 40% of the mixture was still water-soluble. Dialysis of the latter fraction revealed 30.4% of low molecular weight compounds (LMWs; MW <10 000 De) and 10.0% high-molecular weight products [HMWs; MW greater than or equal to 10000 Dal. The water-soluble Maillard reaction products (MRPs) were separated by gel permeation chromatography and ultrafiltration, revealing that 60% of the water-soluble products of the total carbohydrate/amino acid mixture had MWs <1 000 Da and consisted mainly of non-coloured reaction products. MRPs with MWs between 1000 and 30000 Da were Found in comparatively low yields (about 1.3%). In contrast, about 31.1% of the MRPs exhibited MWs > 30000 Da, amongst which 14.5% showed MWs > 100000 Da, thus indicating an oligomerisation of LMWs to melanoidins under roasting conditions. To investigate the physiological effects of these MRPs, xenobiotic enzyme activities were analysed in intestinal Caco-2 cells. For Phase-I NADPH-cytochrome c-reductase, the activity in the presence of the LMW and HMW fraction was decreased by 13% and 22%: respectively. Phase-II glutathione-S-transferase activity decreased by 15% and 18%, respectively, after incubation with the LMW and the HMW fractions. Considering the different yields, 30% and 10%, respectively, of the LMW and the HMW fractions, the total amount of the LMW fraction present in the glucose-glycine mixture is more active in modulating three enzyme activities than that of the HMW fraction.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Colombian Arabica coffee beans were roasted to give light, medium, and dark samples. Their aqueous extracts were analyzed by gel filtration chromatography, UV-visible spectrophotometry, capillary electrophoresis, and the ABTS(.+) assay. A progressive decrease in antioxidant activity (associated mainly with chlorogenic acids in the green beans) with degree of roasting was observed with the simultaneous generation of high (HMM) and low molecular mass (LMM) compounds possessing antioxidant activity. Maximum antioxidant activity was observed for the medium-roasted coffee; the dark coffee had a lower antioxidant activity despite the increase in color. Analysis of the gel filtration chromatography fractions showed that the LMM fraction made a greater contribution to total antioxidant activity than the HMM components.

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This study presents the in-vivo evaluation of Ti-13Nb-13Zr alloy implants obtained by the hydride route via powder metallurgy. The cylindrical implants were processed at different sintering and holding times. The implants` were characterized for density, microstructure (SEM), crystalline phases (XRD), and bulk (EDS) and surface composition (XPS). The implants were then sterilized and surgically placed in the central region of the rabbit`s tibiae. Two double fluorescent markers were applied at 2 and 3 weeks, and 6 and 7 weeks after implantation. After an 8-week healing period, the implants were retrieved, non-decalcified section processed, and evaluated by electron, UV light (fluorescent labeling), and light microscopy (toluidine blue). BSE-SEM showed close contact between bone and implants. Fluorescent labeling assessment showed high bone activity levels at regions close to the implant surface. Toluidine blue staining revealed regions comprising osteoblasts at regions of newly forming/formed bone close to the implant surface. The results obtained in this study support biocompatible and osseoconductive properties of Ti-13Nb-13Zr processed through the hydride powder route. (c) 2007 Published by Elsevier B.V.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Micro-porous nickel (Ni) with an open cell structure was fabricated by a special powder metallurgical process, which includes the adding of a space-holding material. The average pore size of the micro-porous Ni samples approximated 30 μm and 150 μm, and the porosity ranged from 60 % to 80 %. The porous characteristics of the Ni samples were observed using scanning electron microscopy (SEM) and the mechanical properties were evaluated using compressive tests. For comparison, porous Ni samples with a macro-porous structure prepared by both powder metallurgy
(pore size 800 μm) and the traditional chemical vapour deposition (CVD) method (pore size 1300 μm) were also presented. Results indicated that the porous Ni samples with a micro-porous structure exhibited different deformation behaviour and dramatically increased mechanical properties,
compared to those of the macro-porous Ni samples.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The microstructural evolution and characteristics of the Ti–16Sn–4Nb powder particles and bulk alloys sintered from the powders ball-milled for various periods of time were studied. Results indicated that ball milling to 8 h led to the development of a supersaturated hcp α-Ti and partial amorphous phase due to the solid solution of Sn and Nb into Ti lattice. The bulk Ti–16Sn–4Nb alloy made from the powders ball milled for a short time, up to 2 h, exhibited a primary α and a Widmanstätten structure consisting of interlaced secondary α and β. With an increase in ball milling time up to 10 h, the microstructure evolved into a fine β phase dispersed homogeneously within α phase matrix. The microhardness values of the bulk alloy in both α- and β-phases increased with the increasing of the ball milling time and reached a plateau value at 8 h and longer, i.e. 687 and 550 HV for α- and β-phases, respectively. Likewise, the microhardness of the α phases was always higher than that of the β phases in the bulk alloys made from the powders ball milled for the same milling time.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Porous Ti-Mo alloy samples with different porosities from 52% to 72% were successfully fabricated by the space-holder sintering method. The pore size of the porous Ti-Mo alloy samples were ranged from 200 to 500 μm. The plateau stress and elastic modulus of the porous Ti-Mo alloy samples increases with the decreasing of the porosity. Moreover, an apatite coating on the Ti-Mo alloy after an alkali and heat treatment was obtained through soaking into a simulated body fluid (SBF). The porous Ti-Mo alloy provides promising potential for new implant materials with new bone tissue ingrowth ability, bioactivity and mechanical properties mimicking those of natural bone.