126 resultados para Polyimides
Resumo:
A novel synthesis of asymmetric bis(chlorophthalimide)s (3,4-BCPIs) has been established. The polymerizations of them produced higher molecular weight (0.38-0.51 dL/g) polyimides containing biphenyl units than those of isomeric polymers derived from symmetric bis(chlorophthalimide)s (4,4'-BCPIs) and 3,3'-BCPIs. The distribution of the formed biphenyl units of head to tail, head to head, and tail to tail in the chain of the polymers was about 58.0:21.0:21.0, determined by C-13 NMR spectra of the polymers. The composition of model compounds, determined by HPLC, was well consistent with the 13C NMR spectrum result. Comparing with polymers derived from 4,4'-BCPIs and 3,3'-BCPIs, the polymers derived from 3,4-BCPIs showed better solubilities in N,N-dimethylacetamide (DMAc), N,N-dimethyl-formamide (DMF), and N-methylpyrrolinone (NMP). Flexible films could be cast from the polymer solution with the inherent viscosities of above 0.35 dL/g. The polymer derived from asymmetric bis(chlorophthimide)s gave the highest T-g among the isomeric polymers.
Resumo:
A new synthetic route to 2,2',3,3'-BTDA (where BTDA is benzophenonetetracarboxylic dianhydride), an isomer of 2,3',3',4'-BTDA and 3,3',4,4'-BTDA, is described. Single-crystal X-ray diffraction analysis of 2,2',3,3'-BTDA has shown that this dianhydride has a bent and noncoplanar structure. The polymerizations of 2,2',3,3'-BTDA with 4,4'-oxydianiline (ODA) and 4,4'-bis(4-aminophenoxy)benzene (TPEQ) have been investigated with a conventional two-step process. A trend of cyclic oligomers forming in the reaction of 2,2',3,3'-BTDA and ODA has been found and characterized with IR, NMR, matrix-assisted laser desorption/ionization time-of-flight mass spectrometry, and elemental analyses. Films based on 2,2',3,3'-BTDA/TPEQ can only be obtained from corresponding polyimide (PI) solutions prepared by chemical imidization because those from their polyamic acids by thermal imidization are brittle. PIS from 2,2',3,3'-BTDA have lower inherent viscosities and worse thermal and mechanical properties than the corresponding 2,3',3',4'-BTDA- and 3,3',4,4'-BTDA-based PIs. PIs from 2,2',3,3'-BTDA and 2,3',3',4'-BTDA are amorphous, whereas those from 3,3',4,4'-BTDA have some crystallinity, according to wide-angle X-ray diffraction.
Resumo:
Cis-1,2,3,4-cyclohexanetetracarboxylic dianhydride (cis-1,2,3,4-CHDA) was synthesized. It was found that under such conditions as heating or boiling in acetic anhydride, cis-1,2,3,4-CHDA could be converted to its trans-isomer. The process of thermal isomerization was monitored by H-1 NMR spectra and the mechanism of conversion was proposed. Their absolute structures of cis- and trans-1,2,3,4-CHDAs were elucidated by single crystal X-ray diffraction. The polycondensations of cis- and trans-1,2,3,4-CHDAs with aromatic diamines such as 4,4'-oxydianiline (ODA), 4,4'-methylenedianiline (MDA), 4,4'-diamino-3,3'-dimethyldiphenylmethane (DMMDA), 4,4'-bis(4-aminophenoxy)benzene (TPEQ), 2,2-bis[4-(4-aminophenoxy)phenyl] propane (BAPP) were studied. It is easy to obtain higher molecular weight polyimides from trans-1,2,3,4-CHDA using conventional one-step or two-step methods. However, higher molecular weight polyimides derived from cis-1,2,3,4-CHDA could not be prepared by the usual methods (solid content ca. 10%) owing to the trend of forming cyclic oligomers.
Resumo:
A novel diamine, 3,3'-bis(N-aminophthalimide) (BAPI), was prepared from 3,3'-bis(N-phenylphthalimide). Its structure was determined via IR, H-1 NMR, N-15 NMR, elemental analysis, and single-crystal X-ray diffraction analysis. A series of homo- and copolyimides were synthesized by a conventional one-step method in p-chlorophenol. The characteristic IR absorption bands of hydrazine-based imide groups were near 1780, 1750, 1350, 1100, and 730 cm(-1). The polymers showed good solubility in polar aprotic solvents and phenols at room temperature. The temperatures of 5% weight loss (T-5%) of the polyimides ranged from 495 to 530 degrees C in air. DMTA analyses indicated that the glass-transition temperatures (Tgs) of the polyimides were in the range 371-432 degrees C. These polymers had cutoff wavelengths between 350 and 400 nm. The polyimide films of 6FDA/BAPI and 4,4'-HQPDA/BAPI were colorless; other films were pale yellow or yellow.
Resumo:
3,3',4,4'-Diphenylthioether dianhydride (4,4'-TDPA), 2,3,3',4'-diphenylthioether dianhydride (3,4'-TDPA), and 2,2',3,3-diphenylthioether dianhydride (3,3'TDPA) were synthesized from 3-chlorophthalic anhydride and 4-chlorophthalic anhydride. A series of polyimides derived from the isomeric diphenylthioether dianhydrides with several diamines were prepared. The properties, such as the solubility, thermal and mechanical behavior, dynamic mechanical behavior, wide-angle X-ray diffraction, and permeability to some gases, were compared among the isomeric polyimides. Both 3,3'-TDPA- and 3,4-TDPA-based polyimides had good solubility in polar aprotic solvents and phenols. The 5% weight loss temperatures of all the obtained polyimides was near 500 degrees C in nitrogen. The glass-transition temperatures decreased according to the order of the polyimides based on 3,3'-TDPA, 3,4'-TDPA, and 4,4'-TDPA. The 3,4'-TDPA-based polyimides had the best permeability and lowest permselectivity, whereas the 4,4'-TDPA-based polyimides had the highest permselectivity and the lowest permeability of the three isomers. Furthermore, the rheological properties of thermoplastic polyimide resins based on the isomeric dipbenylthioether dianhydrides were investigated, and they showed that polyimide 3,4'-TDPA/4,4-oxydianiline had the lowest melt viscosity among the isomers; this indicated that the melt processibility had been greatly improved.
Resumo:
A new fluorinated diamine monomer, [1,4-bis(4-amino-3-trifluoromethylphenoxy)benzene (2)], and a known isomeric analog 1,4-bis(4-amino-2-trifluoromethylphenoxy)benzene (3) were synthesized. A series of organosoluble polyimides Ia-d and IIa were prepared from the diamines (2, 3) and dianhydrides (a-d) by a high-temperature one-step method. The effects of the trifluoromethyl substituents on the properties of polyimides were evaluated through the study of their soluble, thermal, optical, and gas permeability properties. Polyimides (Ia-d) had glass transition temperatures between 229 and 279 degrees C, and the temperatures at 5% weight loss ranged from 510 to 533 degrees C under nitrogen. These polyimides could be cast into flexible and tough membranes from DMAc solutions. The membranes had tensile strengths in the range of 137-169 MPa, tensile modulus in the range of 1.6-2.2 GPa and elongations at break from 11% to 14%. The polyimide la with trifluoromethyl groups ortho to the imide nitrogen exhibited enhanced gas permeability, solubility, transparency, and thermal stability compared with the isomeric polyimide IIa with the CF3 group meta to the imide nitrogen.
Resumo:
A Series of novel homo- and copolyimides containing pyridine units were prepared from the heteroaromatic diamines, 2,5-bis (4-aminophenyl) pyridine and 2-(4aminophenyl)-5-aminopyridine, with pyromelltic dianhydride (PMDA), and 3,3',4,4'-biphenyl tertracarboxylic dianhydride (BPDA) via a conventional two-step thermal imidizaton method. The poly(amic acid) precursors have inherent viscosities of 1.60-9.64 dL/g (c = 0.5 g/dL in DMAC, 30 degrees C) and all of them can be cast and thermally converted into flexible and tough polyimide films. All of the polyimides show excellent thermal stability and mechanical properties. The polyimides have 10% weight loss temperature in the range of 548-598 degrees C in air. The glass transition temperatures of the PMDA-based samples are in the range of 395-438 degrees C, while the BPDA-based polyimides show two glass transition temperatures (T(g)1 and T(g)2), ranging from 268 to 353 degrees C and from 395 to 418 degrees C, respectively. The flexible films possess tensile modulus in the range of 3.42-6.39 GPa, strength in the range of 112-363 MPa and an elongation at break in the range of 1.2-69%. The strong reflection peaks in the wide-angle X-ray diffraction patterns indicate that the polyimides have a high packing density and crystallinity.
Resumo:
2-(4-Aminophenyl)-5-aminopyrimidine (4) is synthesized via a condensation reaction of vinamidium salts and amidine chloride salts, followed by hydrazine palladium catalyzed reduction. A series of novel homo- and copolyimides containing pyrimidine unit are prepared from the diamine and 1,4-phenylenediamine (PDA) with pyromellitic dianhydride (PMDA) or 3,3',4,4'-biphenyl tertracarboxylic dianhydride (BPDA) via a conventional two-step thermal imidization method. The poly(amic acid) precursors had inherent viscosities of 0.97-4.38 dL/g (c = 0.5 g/dL, in DMAc, 30 degrees C) and all of them could be cast and thermally converted into flexible and tough polyimide films. All of the polyimides showed excellent thermal stability and mechanical properties. The glass transition temperatures of the resulting polyimides are in the range of 307-434 degrees C and the 10% weight loss temperature is in the range of 556-609 degrees C under air. The polyimide films possess strength at break in the range of 185-271 MPa, elongations at break in the range of 6.8-51%, and tensile modulus in the range of 3.5-6.46 GPa. The polymer films are insoluble in common organic solvents, exhibiting high chemical resistance.
Resumo:
A facile method for the synthesis of biphenyl polyimides, which involves the nickel-catalyzed coupling of aromatic dichlorides containing imide structure in the presence of zinc and triphenylphosphine, has been developed. The polymerizations proceeded smoothly under mild conditions and produced biphenyl polyimides with inherent viscosities of 0.13-0.98 dL/g. The polymerizations of bis(4-chlorophthalimide)s with bulky side substituents gave high molecular weight polymers. Low molecular weight polymers from bis(4-chlorophthalimide)s containing rigid diamine moieties and bis(3-chlorophthalimide)s were obtained because of the formations of polymer precipitate and cyclic oligoimides, respectively. The effects of various factors, such as amount of catalyst, solvent volume, ligand, reaction temperature, and time, on the polymerization were studied. The random copolymerization of two bis(chlorophthalimide)s in varying proportions produced medium molecular weight material. The TgS of prepared polyimides were observed at 245-311 degreesC, and the thermogravimetry of polymers showed 10% weight loss in nitrogen at 470-530 degreesC.
Resumo:
A series of polyimides (PIs) based on 2,3,3',4'-benzophenonetetracarboxylic dianhydride (2,3,3',4'-BTDA) and 3,3',4,4'-BTDA were prepared by the conventional two-step process. The properties of the 2,3,3',4'-BTDA based polyimides were compared with those of polyimides prepared from 3,3',4,4'-BTDA. It was found that PIs from 2,3,3,4'-BTDA have higher glass transition temperature and better solubility without sacrificing their thermal properties. Furthermore the theological properties of PMR-15 type polyimide resins based on 2,3,3',4'-BTDA showed lower melt viscosity and wider melt flow region (flow window) compared with those from 3,3',4,4'-BTDA. The structure-property relations resulted from isomerism were discussed.
Resumo:
2,2',3,3'-Oxydiphthalic dianhydride (2,2',3,3'-ODPA) and 2,3,3',4'-ODPA were synthesized from 3-chlorophthalic anhydride with 2,3-xylenol and 3,4-xylenol, respectively. Their structures were determined via single-crystal X-ray diffraction. A series of polyimides derived from isomeric ODPAs with several diamines were prepared in dimethylacetamide (DMAc) with the conventional two-step method. Matrix-assisted laser desorption/ionization time-of-flight spectra showed that the polymerization of 2,2',3,3'-ODPA with 4,4'-oxydianiline (ODA) has a greater trend to form cyclic oligomers than that of 2,3,3',4'-ODPA. Both 2,2',3,3'-ODPA and 2,3,3',4'-ODPA based polyimides have good solubility in polar aprotic solvents such as DMAc, dimethylformamide, and N-methylpyrrolidone. The 5% weight-loss temperatures of all polyimides were obtained near 500 degreesC in air. Their glass-transition temperatures measured by dynamic mechanical thermal analysis or differential scanning calorimetry decreased according to the order of polyimides on the basis of 2,2',3,3'-ODPA, 2,3,3',4'-ODPA, and 3,3',4,4'-ODPA. The wide-angle X-ray diffraction of all polyimide films from isomeric ODPAs and ODA showed some certain extent of crystallization after stretching. Rheological properties revealed that polyimide (2,3,3',4'-ODPA/ODA) has a comparatively lower melt viscosity than its isomers, which indicated its better melt processability.
Resumo:
The synthesis of mellophanic dianhydride (MPDA), an isomer of pyromellitic dianhydride (PMDA), was studied. A trend of forming cyclic oligomers in the reactions of MPDA with 4,4'-oxydianiline (ODA) or 4,4'-methylenedianiline (MDA) in DMAC was found. The cyclic dimer from MPDA/MDA was isolated and fully characterized, including an X-ray crystallographic analysis. The reactions of MPDA with aromatic diamines were found much more complicated than those of PMDA. A model study was performed to clarify the reactions. Several byproducts were isolated and characterized, so that, in an usual two-step process to prepare polyimides, imide, amide linkage, and carboxylic group may be involved in the polymer structure. The water, either existing in solvent or being generated during the imidization, is the main reason for the side reactions. The properties of some polyimides derived from MPDA and diamines were tested and compared with those of the isomeric polyimides derived from PMDA.
Resumo:
A series of homopolyimides and copolyimides was synthesized by the solution condensation of biphenyltetracarboxylic dianhydride (BPDA) isomers and various diamines followed by chemical imidization. These polyimides had intermediate to high molecular weights with inherent viscosities of 0.34-1.01 dL/g for homopolyimides and 0.48-1.02 dL/g for copolyimides. Thermogravimetric analysis indicated that the aromatic polyimides were stable up to 500degreesC, and the 5% weight loss temperatures were recorded in the range of 506-597degreesC in an air atmosphere and in the range of 517-601degreesC in a nitrogen atmosphere, depending on the diamines used. The glass transition temperatures of aromatic homopolyimides were above 271degreesC, while the glass transition temperatures of the copolyimides increased with an increase in the 2, 2', 3, 3'-BPDA-component. The effects of the chemical structure of the polymer chain on the solubility were investigated. It was found that the solubility of BPDA-based polyimides could be improved by the introduction of flexible units, nonlinear and non-coplanar units, and copolymerization. The polyimides with nonlinear and non-coplanar units derived from 2, 2', 3, 3'-BPDA appeared to have prominently enhanced solubility in polar aprotic solvents and polychlorocarbons when compared with the homopolyimide derived from 3, 3', 4, 4'-BPDA.
Resumo:
3,3'-Dioxo-1.1'(3H.3'H)spirobi[isobenzofuran]-5,6,5',6 acid 1 was resolved successfully and the corresponding optically active polyimides PI were synthesized. The properties of the optically active PI and the racemic one were investigated. The results showed that the specific rotation of(-)-PI was about two times to that of the: (+)-PI, and the regularity of the optically active PI was higher than that of the racemic one.
Resumo:
The effect of organic solvents on the electrochemical behavior of the soluble polyimide(PI) was studied by using cyclic voltammetry. It was found that PI can undergo electrochemical reaction in some solvents, while the electrochemical response can not be observed in other solvents. The results of IR spectra indicate that the effect of the solvents on the electrochemical behavior of PI is due to the different interactions between PI and the solvent.