213 resultados para Photocatalysis
Resumo:
Mesoporous titania–organosilica nanoparticles comprised of anatase nanocrystals crosslinked with organosilica moieties have been prepared by direct co-condensation of a titania precursor, tetrabuthylortotitanate (TBOT), with two organosilica precursors, 1,4-bis(triethoxysilyl) benzene (BTEB) and 1,2-bis(triethoxysilyl) ethane (BTEE), in mild conditions and in the absence of surfactant. These hybrid materials show both high surface areas (200–360 m2 g−1) and pore volumes (0.3 cm3 g−1) even after calcination, and excellent photoactivity in the degradation of rhodamine 6G and in the partial oxidation of propene under UV irradiation, especially after the calcination of the samples. During calcination, there is a change in the TiIV coordination and an increase in the content of Si[BOND]O[BOND]Ti moieties in comparison with the uncalcined materials, which seems to be responsible for the enhanced photocatalytic activity of hybrid titania–silica materials as compared to both uncalcined samples and the control TiO2.
Resumo:
N-doped ZnO/g-C3N4 hybrid core–shell nanoplates have been successfully prepared via a facile, cost-effective and eco-friendly ultrasonic dispersion method for the first time. HRTEM studies confirm the formation of the N-doped ZnO/g-C3N4 hybrid core–shell nanoplates with an average diameter of 50 nm and the g-C3N4 shell thickness can be tuned by varying the content of loaded g-C3N4. The direct contact of the N-doped ZnO surface and g-C3N4 shell without any adhesive interlayer introduced a new carbon energy level in the N-doped ZnO band gap and thereby effectively lowered the band gap energy. Consequently, the as-prepared hybrid core–shell nanoplates showed a greatly enhanced visible-light photocatalysis for the degradation of Rhodamine B compare to that of pure N-doped ZnO surface and g-C3N4. Based on the experimental results, a proposed mechanism for the N-doped ZnO/g-C3N4 photocatalyst was discussed. Interestingly, the hybrid core–shell nanoplates possess high photostability. The improved photocatalytic performance is due to a synergistic effect at the interface of the N-doped ZnO and g-C3N4 including large surface-exposure area, energy band structure and enhanced charge-separation properties. Significantly, the enhanced performance also demonstrates the importance of evaluating new core–shell composite photocatalysts with g-C3N4 as shell material.
Resumo:
In recent years, surface plasmon-induced photocatalytic materials with tunable mesoporous framework have attracted considerable attention in energy conversion and environmental remediation. Herein we report a novel Au nanoparticles decorated mesoporous graphitic carbon nitride (Au/mp-g-C3N4) nanosheets via a template-free and green in situ photo-reduction method. The synthesized Au/mp-g-C3N4 nanosheets exhibit a strong absorption edge in visible and near-IR region owing to the surface plasmon resonance effect of Au nanoparticles. More attractively, Au/mp-g-C3N4 exhibited much higher photocatalytic activity than that of pure mesoporous and bulk g-C3N4 for the degradation of rhodamine B under sunlight irradiation. Furthermore, the photocurrent and photoluminescence studies demonstrated that the deposition of Au nanoparticles on the surface of mesoporous g-C3N4 could effectively inhibit the recombination of photogenerated charge carriers leading to the enhanced photocatalytic activity. More importantly, the synthesized Au/mp-g-C3N4 nanosheets possess high reusability. Hence, Au/mp-g-C3N4 could be promising photoactive material for energy and environmental applications.
Resumo:
I. The target molecules are classified as 1-aryl 2-cyclopropyl substituted ethylene. In the ground state, these molecules have a number of conformers, which are in equilibrium through rotation about single bonds. Once excited, the conformers have fixed conformation and are no longer in equilibrium and can be distinguished by their UV-vis as well as fluorescence spectra. The synthetic strategy involves standard steps. Both 2-methylanthracene and 2-methylnaphthalene were brominated using N-bromosuccinimide to give the bromomethyl adduct, which then was reacted with triphenylphosphine to form the phosphonium salt. This was followed by the formation of the phosphorus ylide, which upon treatment with cyclopropanecarboxaldehyde gave the product.^ II. The degradation of three aliphatic haloethers: bis-(2-chloroethyl) ether, bis-(2-chloroisopropyl) ether, and bis-(2-chloroethoxy)methane and two aromatic haloethers: 4-chlorodiphenyl ether and 4-bromodiphenyl ether was studied. Product studies have been conducted on the titanium dioxide photocatalysis of these compounds including mass balance, monitoring and identifying intermediates to establish the reaction pathways to deduce a mechanism for their degradation. The extent of mineralization was determined from the measurement of halogen anion (Cl$\sp-$/Br$\sp-$) as well as total organic carbon. The relative rates of disappearance of the individual haloethers appear to be related to the hydrophobic character of the given compound. Reaction mechanisms involving hydroxyl radical are proposed to explain the observed results. ^
Resumo:
We thank the European Commission for financial support through the European Project Light2CAT, funded by the European Union’s Seventh Framework Programme (FP7) under the grant agreement no. 283062 Eco-Innovation, Theme Environment
Resumo:
A well-organised reduced graphene oxide (RGO) and silver (Ag) wrapped TiO2 nano-hybrid was successfully achieved through a facile and easy route. The inherent characteristics of the synthesized RGO-Ag/TiO2 were revealed through crystalline phase, morphology, chemical composition, Raman scattering, UV-visible absorption, and photoluminescence analyses. The adopted synthesis route significantly controlled the uniform formation of silver nanoparticles and contributed for the absorption of light in the visible spectrum through localized surface plasmon resonance effects. The wrapped RGO nanosheets triggered the electron mobility and promoted visible light shift towards red spectrum. The accomplishment of synergised effect of RGO and Ag well degraded Bisphenol A under visible light irradiation with a removal efficiency of 61.9%.
Resumo:
The thesis is divided into two main parts. In the first one organocatalysis is briefly introduced. Then, new enantiopure trityl pyrrolidines modified with an ionic tag are described. All the catalysts are tested in the benchmark Michael addition reaction to prove their activity and stereoselectivity. In the second part, photocatalysis is first introduced. Then, four different research projects are described. At first, the construction of a hybrid metal-organo-photoredox catalyst is described. The hybrid photocatalysts obtained were employed in the benchmark photoredox alkylation of aldehydes. Then, the use of visible light and a photocatalytic system for the cyclization of iodoaryl vinyl derivatives to tetrahydroquinoline structures is described. In addition, the reaction can also be performed using flow-chemistry. Finally, a mechanistic proposal based on some mechanistic studies is described. Third, a new photoredox catalyzed transformation for the synthesis of 2,3-dihydrofurans is reported. Depending on the involved starting materials, different pathways have arisen. A mechanistic proposal based on reported literatures and experimental data is described. At last, a new photoredox catalyzed transformation for the synthesis of 2-aminofurans is described. Electrophilic radical addition on allenamides and subsequential intramolecular cyclization are exploited. The reaction proceeds under very mild conditions and in 2-aminofurans are obtained in good to high yield. It represents one of the few applications of allenamides in photoredox catalysis. A mechanistic proposal is described. Finally, preliminary investigations on the applicability of the developed transformation under flow chemistry conditions.
Resumo:
The photocatalytic degradation of phenol in aqueous suspensions of TiO2 under different salt concentrations in an annular reactor has been investigated. In all cases, complete removal of phenol and mineralization degrees above 90% were achieved. The reactor operational parameters were optimized and its hydrodynamics characterized in order to couple mass balance equations with kinetic ones. The photodegradation of the organics followed a Langmuir-Hinshelwood-Hougen-Watson lumped kinetics. From GC/MS analyses, several intermediates formed during oxidation have been identified. The main ones were catechol, hydroquinone, and 3-phenyl-2-propenal, in this order. The formation of negligible concentrations of 4-chlorophenol was observed only in high salinity medium. Acute toxicity was determined by using Artemia sp. as the test organism, which indicated that intermediate products were all less toxic than phenol and a significant abatement of the overall toxicity was accomplished, regardless of the salt concentration.
Resumo:
This paper presents the study of photochemical behavior of polycyclic aromatic hydrocarbons (PAHs), potential pollutants in secondary reactions in aerosols, through Raman spectroscopy compared with its electrochemical behavior. The PAHs studied include pyrene, anthracene, phenanthrene and fluorene. These were adsorbed onto TiO2 and irradiated with ultraviolet light (254 nm). Their electrochemical oxidation was studied by in situ Surface-enhanced Raman Scattering (SERS) and led to the formation of carbonyl-containing products. Oxidized intermediates bearing the C=O group were also formed during photodegradation. The joint analysis of the photodegradation data with those produced by electrochemical means - using spectroscopic techniques for the identification and characterization of the products - revealed the formation of identical products for anthracene, but not for pyrene. A reasonable explanation for this difference in results is that photochemical and electrochemical oxidation reactions proceed via different mechanisms. While photocatalytic degradation over TiO2 is initiated by hydroxyl radicals, electrochemical oxidation is initiated by the direct electron transfer from adsorbed PAH to the electrode, generating PAH cation radicals that undergo subsequent reactions.
Combined photocatalytic and fungal processes for the treatment of nitrocellulose industry wastewater
Resumo:
The objective of this work was to characterize the delignification effluent originating from the delignification industry and evaluate the combination of the fungus and photocatalytic process (TiO(2)/UV system) for the treatment of this effluent. The delignification effluent has proven harmful to the environment because it presents high color (3516 CU), total phenol (876 mg/L and TOC (1599 mg/L) and is also highly toxic even in a low concentration. The results of photocatalysis were 11%, 25% and 13% higher for reductions in color, total phenol and TOC, respectively. The combined treatments presented benefits when compared to the non-combined treatments. Fungus and photocatalysis in combination proved to be the best treatment, reducing the color, total phenol, toxicity (inhibition of Escherichia coli growth) and TOC by 94.2%, 92.6%, 4.9% and 62%, respectively. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
TiO2 in anatase crystal phase is a very effective catalyst in the photocatalytic oxidation of organic compounds in water. To improve the recovery rate of TiO2 photocatalysts, which in most cases are in fine powder form, the chemical vapor deposition (CVD) method was used to load TiO2 onto a bigger particle support, silica gel. The amount of titania coating was found to depend strongly on the synthesis parameters of carrier gas flow rate and coating time. XPS and nitrogen ads/desorption results showed that most of the TiO2 particles generated from CVD were distributed on the external surface of the support and the coating was stable. The photocatalytic activities of TiO2/silica gel with different amounts of titania were evaluated for the oxidation of phenol aqueous solution and compared with that of Degussa P25. The optimum titania loading rate was found around 6 wt % of the TiO2 bulk concentration. Although the activity of the best TiO2/silica gel sample was still lower than that of P25, the synthesized TiO2/silica gel catalyst can be easily separated from the treated water and was found to maintain its TiO2 content and catalytic activity.
Resumo:
Coating anatase TiO2 onto three different particle supports, activated carbon (AC), gamma -alumina (Al2O3) and silica gel (SiO2), by chemical vapor deposition (CVD) was studied. The effect of the CVD synthesis conditions on the loading rate of anatase TiO2 was investigated. It was found that introducing water vapor during CVD or adsorbing water before CVD was crucial to obtain anatase TiO2 on the surface of the particle supports. The evaporation temperature of precursor, deposition temperature in the reactor, flow rate of carrier gas, and the length of coating time were also important parameters to obtain more uniform and repeatable TiO2 coating. High inflow precursor concentration, high CVD reactor temperature and long coating time tended to cause block problem. Coating TiO2 onto small particles by CVD involved both chemical vapor deposition and particle deposition. It was believed that the latter was the reason for the block problem. In addition, the mechanism of CVD process in this study included two parts, pyrolysis and hydrolysis, and one of them was dominant in the CVD process under different synthesis route. Among the three types of materials, silica gel, with higher surface hydroxyl groups and macropore surface area, was found to be the most efficient support in terms of both anatase TiO2 coating and photocatalytic reaction. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
The gel point of a dicyanate ester resin (Arocy B-10 (4-4'-dicyanato-2,2'-diphenylpropane)) heated following irradiation in the presence of the catalyst tricarbonyl cyclopentadienyl manganese (CpMn(CO)(3)) was studied using differential scanning calorimetry (d.s.c.) and dynamic rheological techniques over the temperature range 110-140 degrees C. The gel times of another commercial cyanate ester (RTX366) were also studied using independent rheological techniques, and the results agreed within experimental error. Gel times decreased linearly with increasing catalyst level and with increasing temperature according to an Arrhenius relation with activation energy of 68 +/- 6 kJmol(-1). The gel conversion was calculated by correlation of the rheological gel data to d.s.c. data to be 0.57 +/- 0.02, and differences between techniques, and between theoretical predictions, are discussed. Evidence is produced that the photocatalysed polymerization results in a greater rate of cyclotrimerization, less intramolecular cyclization and a more rigid network than the uncatalysed or metal salt-catalysed high-temperature polymerization. (C) 1997 Elsevier Science Ltd.
Resumo:
Nesta tese é descrita a preparação de nanotubos de titanatos (TNT) via síntese hidrotérmica alcalina, usando uma nova metodologia que evita a utilização de TiO2 cristalino como precursor. Foi estudada a influência da substituição sódio/protão na estrutura, morfologia e propriedades ópticas dos materiais preparados. Os resultados mostraram que a substituição Na+ → H+ resulta numa redução na distância intercamadas dos TNTs, tendo sido medidos valores entre 1.13±0.03 nm e 0.70±0.02 nm para aquele parâmetro. O comportamento óptico dos TNTs foi estudado na região UV-vis, estimando-se um hiato óptico de energia 3.27±0.03 eV para a amostra com maior teor de sódio enquanto que para a amostra protonada foi determinado um valor de 2.81±0.02 eV. Estes valores mostram que a troca iónica Na+ → H+ teve influência no desvio da banda de absorção dos TNTs para a região do visível próximo. A actividade fotocatalítica dos TNTs na degradação do corante rodamina 6G (R6G) foi posteriormente estudada. Verificou-se que, apesar de a amostra com maior teor de sódio ter sido a que exibiu maior capacidade para adsorver o R6G, foi a amostra protonada que apresentou a actividade catalítica mais elevada na fotodegradação deste corante. Numa segunda fase, e com o objectivo de preparar novos materiais nanoestruturados fotosensíveis, procedeu-se à decoração dos TNTs protonados com semicondutores (SC) nanocristalinos usando um método novo. Para o efeito os TNTs foram decorados com nanocristalites de ZnS, CdS e Bi2S3. Foi estudada a influência do tipo de semicondutor na estrutura, morfologia e propriedades ópticas dos SC/TNTs obtidos. Verificou-se que, para qualquer dos semicondutores usados no processo de decoração, a estrutura dos TNTs é preservada e não ocorre segregação do SC. Verificou-se ainda que a morfologia dos nanocompósitos preparados depende fortemente da natureza do semicondutor. No que respeita ao comportamento óptico destes materiais, foram determinados hiatos ópticos de energia 3.67±0.03 eV, 2.47±0.03 eV e 1.35±0.01 eV para as amostras ZnS/TNT, CdS/TNT e Bi2S3/TNT, respectivamente. Estes resultados mostram que através do processo de decoração de TNTs com semicondutores podem ser preparados materiais nanocompósitos inovadores, com propriedades ópticas novas e/ou pré-definidas numa gama alargada do espectro electromagnético.
Resumo:
Titanate nanotubes (TNT) with different sodium contents have been synthesised using a hydrothermal approach and a swift and highly controllable post-washing processes. The influence of the sodium/proton replacement on the structural and morphological characteristics of the prepared materials was analysed. Different optical behaviour was observed depending on the Na+/H+ samples’ content. A band gap energy of 3.27±0.03 eV was estimated for the material with higher sodium content while a value of 2.81±0.02 eV was inferred for the most protonated material, which therefore exhibits an absorption edge in the near visible region. The point of zero charge of the materials was determined and the influence of the sodium content on the adsorption of both cationic and anionic organic dyes was studied. The photocatalytic performance of the TNT samples was evaluated in the rhodamine 6G degradation process. Best photodegradation results were obtained when using the most protonated material as catalyst, although this material has shown the lowest R6G adsorption capability.