860 resultados para Non-aqueous dispersion, amphiphilic block copolymer polymer, polyurethane porous particle, particle with PDI dye, graphene nanosheet
Resumo:
Poly(acrylic acid) (PAA) was grafted onto both termini of Pluronic F87 (PEO₆₇-PPO₃₉-PEO₆₇) via atom transfer radical polymerization to produce a novel muco-adhesive block copolymer PAA₈₀-b-F₈₇-b-PAA₈₀. It was observed that PAA₈₀-F₈₇-PAA₈₀ forms stable complexes with weakly basic anti-cancer drug, Doxorubicin. Thermodynamic changes due to the drug binding to the copolymer were assessed at different pH by isothermal titration calorimetry (ITC). The formation of the polymer/drug complexes was studied by turbidimetric titration and dynamic light scattering. Doxorubicin and PAA-b-F87-b-PAA block copolymer are found to interact strongly in aqueous solution via non-covalent interactions over a wide pH range. At pH>4.35, drug binding is due to electrostatic interactions. Hydrogen-bond also plays a role in the stabilization of the PAA₈₀-F₈₇-PAA₈₀/DOX complex. At pH 7.4 (α=0.8), the size and stability of polymer/drug complex depend strongly on the doxorubicin concentration. When CDOX <0.13mM, the PAA₈₀-F₈₇-PAA₈₀ copolymer forms stable inter-chain complexes with DOX (110 ~ 150 nm). When CDOX >0.13mM, as suggested by the light scattering result, the reorganization of the polymer/drug complex is believed to occur. With further addition of DOX (CDOX >0.34mM), sharp increase in the turbidity indicates the formation of large aggregates, followed by phase separation. The onset of a sharp enthalpy increase corresponds to the formation of a stoichiometric complex.
Resumo:
The diffusion of water in a phase-separated biodegradable poly(ester urethane) shape-memory polymer with poly(E-caprolactone) (PCL) as the soft segment was investigated using time-resolved FTIR-ATR. On the basis of the band fitting and water ordering in drawn films, the broad water band in the 3800-2800 cm(-1) region was decomposed into four bands located at 3620, 3510, 3400, and 3260 cm(-1), and the first two components at 3620 and 35 10 cm(-1) were assigned to the vibrations of antisymmetric and symmetric stretching of water hydrogen bonded with the C=O group of the soft segment. The other two were associated with water bonded to the urethane hard segments in the forms of N-H:O-H:O=C bridge hydrogen bond and double hydrogen bonds with two C=O groups, respectively. Furthermore, band fitting and two-dimensional correlation analyses revealed that in the diffusion process, water first diffuses into the continuous soft-rich PCL phase and then into the hard-rich urethane domains, forming double hydrogen bonds with two C=O groups prior to the bridge hydrogen bond in the form of N-H:O-H:O=C.
Resumo:
The coupling of drugs to macromolecular carriers received an important impetus from Ringsdorf's notion of polymer-drug conjugates. Several water-soluble polymers, poly(ethylene glycol), poly[N-(2-hydroxypropyl) methacrylamidel, poly(L-glutamic acid) and dextran, are studied intensively and have been utilized successfully in clinical research. The promising results arising from clinical trials with polymer-drug conjugates (e.g., paclitaxel, doxorubicin, camptothecins) have provided a firm foundation for other synthetic polymers, especially biodegradable polymers, used as drug delivery vehicles. This review discusses biodegradable polymeric micelles as an alternative drug-conjugate system. Particular focus is on A-B or B-A-B type biodegradable amphiphilic block copolymer such as polylactide, morpholine-2,5-dione derivatives and cyclic carbonates, which can form a core-shell micellar structure, with the hydrophobic drug-binding segment forming the hydrophobic core and the hydrophilic segment as a hydrated outer shell. Polymeric micelles can be designed to avoid uptake by cells of reticuloendothelial system and thus enhance their blood lifetime via the enhanced permeability and retention effect.
Resumo:
Various metallized nanostructures (such as rings, wires with controllable lengths, spheres) have been successfully fabricated by coating metallic nanolayers onto soft nanotemplates through simple electroless methods. In particular, bimetallic nanostructures have been obtained by using simple methods. The multiple functional polymeric nanostructures, were obtained through the self-assembly of polystyrene/poly(4-vinyl pyridine) triblock copolymer (P4VP-b-PS-b-P4VP) in selective media by changing the common solvent properties. By combining field emission scanning electron microscopy (SEM), atomic force microscopy (AFM) and X-ray photoelectron spectroscopy (XPS) characterization, it was confirmed that polymer/metal and bimetallic (Au@Ag) core-shell nanostructures could be achieved by chemical metal deposition method.
Resumo:
We report the multiple morphologies and their transformation of polystyrene-block-poly(4-vinylpyridine) (PS-b-P4VP) in low-alkanol solvents. In order to improve the solubility of polystyrene block in alcohol solvents, the solution of block copolymer sample was treated at a higher temperature, and then the influence of rate of decreasing temperature on multiple morphologies (including spheres, rods, vesicles, porous vesicles, large compound vesicles, and large compound micelles) was observed. The transformation of spheres to rods, to tyre-shaped large compound micelles, and to sphere-shaped large compound micelles was also realized. The formation mechanisms of the multiple morphologies and their transformation are discussed briefly.
Resumo:
The graft copolymerization of butyl acrylate onto poly(vinyl alcohol) with eerie ammonium nitrate as redox initiator in a aqueous medium has been investigated. The formation of graft copolymer was confirmed by means of IR, scanning electron microscopy (SEM), and wide-angle X-ray diffraction (WAXD). The percentage of mononer conversion and percentage of grafting varied with concentrations of initiator, nitric acid, monomer, macromolecular backbone (X-n = 1750, M = 80 000), reaction temperature and reaction time. Some inorganic salts and organic solvents have a great influence upon grafting. The reaction mechanism has been explored, and rate equations for the reaction are established. (C) 2000 John Wiley & Sons, Inc.
Resumo:
Beaucoup d'efforts dans le domaine des matériaux polymères sont déployés pour développer de nouveaux matériaux fonctionnels pour des applications spécifiques, souvent très sophistiquées, en employant des méthodes simplifiées de synthèse et de préparation. Cette thèse porte sur les polymères photosensibles – i.e. des matériaux fonctionnels qui répondent de diverses manières à la lumière – qui sont préparés à l'aide de la chimie supramoléculaire – i.e. une méthode de préparation qui repose sur l'auto-assemblage spontané de motifs moléculaires plus simples via des interactions non covalentes pour former le matériau final désiré. Deux types de matériaux photosensibles ont été ciblés, à savoir les élastomères thermoplastiques à base de copolymères à blocs (TPE) et les complexes d'homopolymères photosensibles. Les TPEs sont des matériaux bien connus, et même commercialisés, qui sont généralement composés d’un copolymère tribloc, avec un bloc central très flexible et des blocs terminaux rigides qui présentent une séparation de phase menant à des domaines durs isolés, composés des blocs terminaux rigides, dans une matrice molle formée du bloc central flexible, et ils ont l'avantage d'être recyclable. Pour la première fois, au meilleur de notre connaissance, nous avons préparé ces matériaux avec des propriétés photosensibles, basé sur la complexation supramoléculaire entre un copolymère tribloc simple parent et une petite molécule possédant une fonctionnalité photosensible via un groupe azobenzène. Plus précisément, il s’agit de la complexation ionique entre la forme quaternisée d'un copolymère à blocs, le poly(méthacrylate de diméthylaminoéthyle)-poly(acrylate de n-butyle)-poly(méthacrylate de diméthylaminoéthyle) (PDM-PnBA-PDM), synthétisé par polymérisation radicalaire par transfert d’atomes (ATRP), et l'orange de méthyle (MO), un composé azo disponible commercialement comportant un groupement SO3 -. Le PnBA possède une température de transition vitreuse en dessous de la température ambiante (-46 °C) et les blocs terminaux de PDM complexés avec le MO ont une température de transition vitreuse élevée (140-180 °C, en fonction de la masse molaire). Des tests simples d'élasticité montrent que les copolymères à blocs complexés avec des fractions massiques allant de 20 à 30% présentent un caractère élastomère. Des mesures d’AFM et de TEM (microscopie à force atomique et électronique à ii transmission) de films préparés à l’aide de la méthode de la tournette, montrent une corrélation entre le caractère élastomère et les morphologies où les blocs rigides forment une phase minoritaire dispersée (domaines sphériques ou cylindriques courts). Une phase dure continue (morphologie inversée) est observée pour une fraction massique en blocs rigides d'environ 37%, ce qui est beaucoup plus faible que celle observée pour les copolymères à blocs neutres, dû aux interactions ioniques. La réversibilité de la photoisomérisation a été démontrée pour ces matériaux, à la fois en solution et sous forme de film. La synthèse du copolymère à blocs PDM-PnBA-PDM a ensuite été optimisée en utilisant la technique d'échange d'halogène en ATRP, ainsi qu’en apportant d'autres modifications à la recette de polymérisation. Des produits monodisperses ont été obtenus à la fois pour la macroamorceur et le copolymère à blocs. À partir d'un seul copolymère à blocs parent, une série de copolymères à blocs partiellement/complètement quaternisés et complexés ont été préparés. Des tests préliminaires de traction sur les copolymères à blocs complexés avec le MO ont montré que leur élasticité est corrélée avec la fraction massique du bloc dur, qui peut être ajustée par le degré de quaternisation et de complexation. Finalement, une série de complexes d'homopolymères auto-assemblés à partir du PDM et de trois dérivés azobenzènes portant des groupes (OH, COOH et SO3) capables d'interactions directionnelles avec le groupement amino du PDM ont été préparés, où les dérivés azo sont associés avec le PDM, respectivement, via des interactions hydrogène, des liaisons ioniques combinées à une liaison hydrogène à travers un transfert de proton (acidebase), et des interactions purement ioniques. L'influence de la teneur en azo et du type de liaison sur la facilité d’inscription des réseaux de diffraction (SRG) a été étudiée. L’efficacité de diffraction des SRGs et la profondeur des réseaux inscrits à partir de films préparés à la méthode de la tournette montrent que la liaison ionique et une teneur élevée en azo conduit à une formation plus efficace des SRGs.
Resumo:
Well-defined, water-soluble, pH and temperature stimuli-responsive [60]fullerene (C₆₀) containing ampholytic block copolymer of poly((methacrylic acid)-block-(2-(dimethylamino)ethyl methacrylate))-block–C₆₀ (P(MAA-b-DMAEMA)-b-C₆₀) was synthesized by the atom transfer radical polymerization (ATRP) technique. The self-assembly behaviour of the C₆₀ containing polyampholyte in aqueous solution was characterized by dynamic light scattering (DLS), and transmission electron microscopy. This amphiphilic mono-C₆₀ end-capped block copolymer shows enhanced solubility in aqueous medium at room and elevated temperatures and at low and high pH but phase-separates at intermediate pH of between 5.4 and 8.8. The self assembly of the copolymer is different from that of P(MAA-b-DMAEMA). Examination of the association behavior using DLS revealed the co-existence of unimers and aggregates at low pH at all temperatures studied, with the association being driven by the balance of hydrophobic and electrostatic interactions. Unimers and aggregates of different microstructures are also observed at high pH and at temperatures below the lower critical solution temperature (LCST) of PDMAEMA. At high pH and at temperatures above the LCST of PDMAEMA, the formation of micelles and aggregates co-existing in solution is driven by the combination of hydrophobic, electrostatic, and charge-transfer interactions.
Resumo:
The self-assembly into wormlike micelles of a poly(ethylene oxide)-b-poly(propylene oxide)-b-poly(ethylene oxide) triblock copolymer Pluronic P84 in aqueous salt solution (2 M NaCl) has been studied by rheology, small-angle X-ray and neutron scattering (SAXS/SANS), and light scattering. Measurements of the flow curves by controlled stress rheometry indicated phase separation under flow. SAXS on solutions subjected to capillary flow showed alignment of micelles at intermediate shear rates, although loss of alignment was observed for high shear rates. For dilute solutions, SAXS and static light scattering data on unaligned samples could be superposed over three decades in scattering vector, providing unique information on the wormlike micelle structure over several length scales. SANS data provided information on even shorter length scales, in particular, concerning "blob" scattering from the micelle corona. The data could be modeled based on a system of semiflexible self-avoiding cylinders with a circular cross-section, as described by the wormlike chain model with excluded volume interactions. The micelle structure was compared at two temperatures close to the cloud point (47 degrees C). The micellar radius was found not to vary with temperature in this region, although the contour length increased with increasing temperature, whereas the Kuhn length decreased. These variations result in an increase of the low-concentration radius of gyration with increasing temperature. This was consistent with dynamic light scattering results, and, applying theoretical results from the literature, this is in agreement with an increase in endcap energy due to changes in hydration of the poly(ethylene oxide) blocks as the temperature is increased.
Resumo:
The stability of ternary blends of two immiscible homopolymers and a block copolymer compatiblizer depends crucially on the effective interaction between the copolymermonolayers that form between the unlike homopolymer domains. Here, the interaction is calculated for blends involving A and B homopolymers of equal size with ABABdiblock copolymers of symmetric composition using both self-consistent field theory (SCFT) and strong-segregation theory (SST). If the homopolymers are larger than the copolymer molecules, an attractive interaction is predicted which would destroy the blend. This conclusion coupled with considerations regarding the elastic properties of the monolayer suggests that the optimum size of the homopolymer molecules is about 80% that of the copolymer molecule. A detailed examination of the theory demonstrates that the attraction results from the configurational entropy loss of the homopolymer molecules trapped between the copolymermonolayers. We conclude by suggesting how the monolayers can be altered in order to suppress this attraction and thus improve compatiblization.
From amphiphilic block copolymers to ferrocenyl-functionalized polymers for biosensoric applications
Resumo:
The present thesis can be divided in three main parts. In all parts new polymer architecturesrnwere synthesized and characterized concerning their special features.rnThe first part will emphasize the advantage of a polystyrene-block-(hyperbranchedrnpolyglycerol) copolymer in comparison to an analogue polystyrene-block-(linear polyglycerol)rncopolymer. Therefore a synthethic route to prepare linear block copolymersrnhas been developed. Two strategies were examined. One strategy was based on thernclassic, sequential anionic polymerization; the second strategy was based on arn“Click-Chemistry” coupling reaction. In a following step glycidol was hypergraftedrnfrom these block copolymers by applying a hypergrafting reaction with glycidol. Thernbehavior of the amphiphilic block copolymers synthesized was studied in differentrnsolvents. Furthermore the polarity of the solvent was changed to form the correspondingrninverse micelles. DLS, SLS, SEC-MALLS-VISCO, AFM and Cyro TEMrnmeasurements were performed to obtain a visual image from the appearance of thernaggregates. It was found that a linear-hyperbranched architecture is necessary, ifrnwell defined, monodisperse aggregates are required, e.g. for the preparation of orderedrnnanoarrays. Linear-linear block copolymers formed only polydisperse aggregates.rnAdditionally it was found that size distribution could be improved dramaticallyrnby passing the aggregates through a SEC column with large pores. The SEC columnsrnacted like a template in which the aggregates adopt a more stable conformation.rnIn the second part anionic polymerization was employed to synthesize silaneendfunctionalizedrnmacromonomers with different molecular weights based on polybutadienernand polyisoprene. These were polymerized by a hydrosilylation reaction inrnbulk to obtain branched polymers, using Karstedt’s catalyst. Surprisingly the additionrnof monofunctional silanes during the polymerization had only a minimal effect concerningrnthe degree of polymerization. It was possible to introduce silanes without increasingrnthe overall number of reaction steps by a very convenient “pseudo-copolymerization”rnmethod. All branched polymers were analyzed by SEC, SEC-MALLS,rnSEC-viscometry, 1H-NMR-spectroscopy and DSC concerning their branching ratio.rnThe branching parameters for the branched polymers exhibited similar characteristicsrnas hyperbranched polymers based on AB2 monomers. Detailed kinetic study showedrnthat the polymerization occurred very rapidly in comparison to the hydrosilylation polymerizationrnof classical AB2 type carbosilanes monomers.rnThe last part will deal with ferrocenyl-functionalized polymers. On the one hand,rnferrocenyl-functionalized polyglycerols (PG) were studied. Esterification of PGs withrndifferent molecular weight using ferrocenemonocarboxylic acid gave the ferrocenylrnfuntionalized polymers in high yields. On the other hand three different block copolymersrnwere prepared with different ratios of styrene to butadiene units (10:1, 4:1, 2:1).rnThe double bonds of the 1,2-PB block were hydrosilylated using silanes bearing onern(HSiMe2Fc) or two (HSiMeFc2) ferrocene units. High degrees of functionalizationrnwere obtained (up to 83 %). In this manner, six different ferrocenyl-rich block copolymersrnwith different fractions of ferrocene were prepared and analyzed, employingrnNMR-spectroscopy, SEC, SEC/MALLS/viscometry, DLS and cyclic voltammetry. Thernredox properties of the studied polymers varied primarily with the nature of the silanernunit attached. Additionally, the redox properties in solution of the studied polymersrnwere influenced by the block length ratio of the block copolymers. Unexpectedly, withrnincreasing block length of the ferrocenyl block the fraction of active ferrocenes decreased.rnNevertheless, in case of thin monolayer films this behaviour was not observed.rnAll polymers (PG and PS-b-PB based) exhibited good electrochemical propertiesrnin a wide range of solvents, which rendered them very interesting for biosensoricrnapplications.
Resumo:
This work reports the first instance of self-organized thermoset blends containing diblock copolymers with a crystallizable thermoset-immiscible block. Nanostructured thermoset blends of bisphenol A-type epoxy resin (ER) and a low-molecular-weight (M-n = 1400) amphiphilic polyethylene-block-poly(ethylene oxide) (EEO) symmetric diblock copolymer were prepared using 4,4'-methylenedianiline (MDA) as curing agent and were characterized by transmission electron microscopy (TEM), atomic force microscopy (AFM), small-angle X-ray scattering (SAXS), and differential scanning calorimetry (DSC). All the MDA-cured ER/EEO blends do not show macroscopic phase separation but exhibit microstructures. The ER selectively mixes with the epoxy-miscible PEO block in the EEO diblock copolymer whereas the crystallizable PE blocks that are immiscible with ER form separate microdomains at nanoscales in the blends. The PE crystals with size on nanoscales are formed and restricted within the individual spherical micelles in the nanostructured ER/EEO blends with EEO content up to 30 wt %. The spherical micelles are highly aggregated in the blends containing 40 and 50 wt % EEO. The PE dentritic crystallites exist in the blend containing 50 wt % EEO whereas the blends with even higher EEO content are completely volume-filled with PE spherulites. The semicrystalline microphase-separated lamellae in the symmetric EEO diblock copolymer are swollen in the blend with decreasing EEO content, followed by a structural transition to aggregated spherical micellar phase morphology and, eventually, spherical micellar phase morphology at the lowest EEO contents. Three morphological regimes are identified, corresponding precisely to the three regimes of crystallization kinetics of the PE blocks. The nanoscale confinement effect on the crystallization kinetics in nanostructured thermoset blends is revealed for the first time. This new phenomenon is explained on the basis of homogeneous nucleation controlled crystallization within nanoscale confined environments in the block copolymer/thermoset blends.
Resumo:
Synthesis of high quality boron carbide (B4C) powders is achieved by carbothermal reduction of boron oxide (B2O3) from a condensed boric acid (H3BO3)/polyvinyl acetate (PVAc) product. Precursor solutions are prepared via free radical polymerisation of vinyl acetate (VA) monomer in methanol in the presence of dissolved H3BO3. A condensed product is then formed by flash evaporation under vacuum. As excess VA monomer is removed at the evaporation step, the polymerisation time is used to manage availability of carbon for reaction. This control of carbon facilitates dispersion of H3BO3 in solution due to the presence of residual VA monomer. B4C powders with very low residual carbon are formed at temperatures as low as 1,250 °C with a 4 hour residence time.
Resumo:
Diketopyrrolopyrole-naphthalene polymer (PDPP-TNT), a donor-acceptor co-polymer, has shown versatile behavior demonstrating high performances in organic field-effect transistors (OFETs) and organic photovoltaic (OPV) devices. In this paper we report investigation of charge carrier dynamics in PDPP-TNT, and [6,6]-phenyl C71 butyric acid methyl ester (PC71BM) bulk-heterojunction based inverted OPV devices using current density-voltage (J-V) characteristics, space charge limited current (SCLC) measurements, capacitance-voltage (C-V) characteristics, and impedance spectroscopy (IS). OPV devices in inverted architecture, ITO/ZnO/PDPP-TNT:PC71BM/MoO3/Ag, are processed and characterized at room conditions. The power conversion efficiency (PCE) of these devices are measured ∼3.8%, with reasonably good fill-factor 54.6%. The analysis of impedance spectra exhibits electron’s mobility ∼2 × 10−3 cm2V−1s−1, and lifetime in the range of 0.03-0.23 ms. SCLC measurements give hole mobility of 1.12 × 10−5 cm2V−1s−1, and electron mobility of 8.7 × 10−4 cm2V−1s−1.