467 resultados para Metalceramic crowns
Resumo:
Objectives: To determine, by means of static fracture testing the effect of the tooth preparation design and the elastic modulus of the cement on the structural integrity of the cemented machined ceramic crown-tooth complex.
Methods: Human maxillary extracted premolar teeth were prepared for all-ceramic crowns using two preparation designs; a standard preparation in accordance with established protocols and a novel design with a flat occlusal design. All-ceramic feldspathic (Vita MK II) crowns were milled for all the preparations using a CAD/CAM system (CEREC-3). The machined all-ceramic crowns were resin bonded to the tooth structure using one of three cements with different elastic moduli: Super-Bond C&B, Rely X Unicem and Panavia F 2.0. The specimens were subjected to compressive force through a 4 mm diameter steel ball at a crosshead speed of 1 mm/min using a universal test machine (Loyds Instrument Model LRX.). The load at the fracture point was recorded for each specimen in Newtons (N). These values were compared to a control group of unprepared/unrestored teeth.
Results: There was a significant difference between the control group, with higher fracture strength, and the cemented samples regardless of the occlusal design and the type of resin cement. There was no significant difference in mean fracture load between the two designs of occlusal preparation using Super-Bond C&B. For the Rely X Unicem and Panavia F 2.0 cements, the proposed preparation design with a flat occlusal morphology provides a system with increased fracture strength.
Significance: The proposed novel flat design showed less dependency on the resin cement selection in relation to the fracture strength of the restored tooth. The choice of the cement resin, with respect to its modulus of elasticity, is more important in the anatomic design than in the flat design. © 2013 Academy of Dental Materials.
Resumo:
The aim of this study was to perform a photoelastic analysis of stress distribution on straight and angulated implants with different crowns (screwed and cemented). Three models were made of photoelastic resin PL-2: model 1: external hexagon implant 3.75 x 10.00 mm at 0 degrees; model 2: external hexagon implant 3.75 x 10.00 mm at 17 degrees; model 3: external hexagon implant 3.75 x 10.00 mm at 30 degrees. Axial and oblique (45 degrees) load (100 N) was applied with a universal testing machine. The photoelastic fringes on the models were recorded with a digital camera and visualized in a graphic software for qualitative analysis. The axial loading generated the same pattern of stress distribution. The highest stresses were concentrated between medium and apical thirds. The oblique loading generated a similar pattern of stress distribution in the models with similar implant angulation; the highest stress was located on the cervical region opposite to implant angulation and on the apical third. It was concluded that the higher the implant angulation, the higher the stress value, independent of crown type. The screwed prostheses exhibited the highest stress concentration. The oblique load generated higher stress value and concentration than the axial load.
Resumo:
The aim of this study was to evaluate the effect of unilateral angular misfit of 100 Km on stress distribution of implant-supported single crowns with ceramic veneering and gold framework by three-dimensional finite element analysis. Two three-dimensional models representing a maxillary section of premolar region were constructed: group 1 (control)-crown completely adapted to the implant and group 2-crown with unilateral angular misfit of 100 Km. A vertical force of 100 N was applied on 2 centric points of the crown. The von Mises stress was used as an analysis criterion. The stress values and distribution in the main maps (204.4 MPa for group 1 and 205.0 MPa for group 2) and in the other structures (aesthetic veneering, framework, retention screw, implant, and bone tissue) were similar for both groups. The highest stress values were observed between the first and second threads of the retention screw. Considering the bone tissue, the highest stress values were exhibited in the peri-implant cortical bone. The unilateral angular misfit of 100 Km did not influence the stress distribution on the implant-supported prosthesis under static loading.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Restoring a misaligned tooth with an inadequate contact point is a challenge to the practitioner. In some instances, teeth that could be repositioned and adequately restored are extracted. Thus, the aim of this article was to describe a treatment using orthodontic and prosthetic techniques to restore esthetics and function in a patient with a distally drifted maxillary lateral incisor. The patient's functional and esthetic expectations were successfully met with the outlined treatment.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
BackgroundEndodontic treatment, involves removal of the dental pulp and its replacement by a root canal filling. Restoration of root filled teeth can be challenging due to structural differences between vital and non-vital root filled teeth. Direct restoration involves placement of a restorative material e.g. amalgam or composite directly into the tooth. Indirect restorations consist of cast metal or ceramic (porcelain) crowns. The choice of restoration depends on the amount of remaining tooth which may influence long term survival and cost. The comparative in service clinical performance of crowns or conventional fillings used to restore root filled teeth is unclear.ObjectivesTo assess the effects of restoration of endodontically treated teeth (with or without post and core) by crowns versus conventional filling materials.Search methodsWe searched the following databases: the Cochrane Oral Health Group's Trials Register, CENTRAL, MEDLINE via OVID, EMBASE via OVID, CINAHL via EBSCO, LILACS via BIREME and the reference lists of articles as well as ongoing trials registries. There were no restrictions regarding language or date of publication. Date of last search was 13 February 2012.Selection criteriaRandomised controlled trials (RCTs) or quasi-randomised controlled trials in participants with permanent teeth which have undergone endodontic treatment. Single full coverage crowns compared with any type of filling materials for direct restoration, as well as indirect partial restorations (e.g. inlays and onlays). Comparisons considered the type of post and core used (cast or prefabricated post), if any.Data collection and analysisTwo review authors independently assessed trial quality and extracted data.Main resultsOne trial judged to be at high risk of bias due to missing outcome data, was included. 117 participants with a root filled premolar tooth restored with a carbon fibre post, were randomised to either a full coverage metal-ceramic crown or direct adhesive composite restoration. At 3 years there was no reported difference between the non-catastrophic failure rates in both groups. Decementation of the post and marginal gap formation occurred in a small number of teeth.Authors' conclusionsThere is insufficient evidence to support or refute the effectiveness of conventional fillings over crowns for the restoration of root filled teeth. Until more evidence becomes available clinicians should continue to base decisions on how to restore root filled teeth on their own clinical experience, whilst taking into consideration the individual circumstances and preferences of their patients.
Resumo:
Objectives: To compare the fracture resistance of bovine teeth after intracoronal bleaching with sodium percarbonate (SPC) or sodium perborate (SP) mixed with water or 20% hydrogen peroxide (HP). Materials and methods: Fifty extracted bovine teeth were divided into four experimental groups (G1G4) and one control (n = 10) after endodontic treatment. Following root canal obturation, a glass ionomer barrier was placed at the cementoenamel junction. After that, the pulp chambers were filled with: G1 SP with water; G2 SP with 20% HP; G3 SPC with water; and G4 SPC with 20% HP. No bleaching agent was used in the control group. Coronal access cavities were sealed with glass ionomer and specimens were immersed in artificial saliva. The bleaching agents were replaced after 7 days, and teeth were kept in artificial saliva for an additional 7 days, after which the pastes were removed and the coronal access cavities were restored with glass ionomer. Crowns were subjected to compressive load at a cross head speed of 0.5 mm min-1 applied at 135 degrees to the long axis of the root by an EMIC DL2000 testing machine, until coronal fracture. Data were statistically analysed by anova and Tukey test. Results: No differences in fracture resistance were observed between the experimental groups (P > 0.05). However, all experimental groups presented lower fracture resistance than the control group (P < 0.05). Conclusion: SPC and SP led to equal reduction on fracture resistance of dental crowns, regardless of being mixed with water or 20% HP.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Objective. To determine the influence of cement thickness and ceramic/cement bonding on stresses and failure of CAD/CAM crowns, using both multi-physics finite element analysis and monotonic testing.Methods. Axially symmetric FEA models were created for stress analysis of a stylized monolithic crown having resin cement thicknesses from 50 to 500 mu m under occlusal loading. Ceramic-cement interface was modeled as bonded or not-bonded (cement-dentin as bonded). Cement polymerization shrinkage was simulated as a thermal contraction. Loads necessary to reach stresses for radial cracking from the intaglio surface were calculated by FEA. Experimentally, feldspathic CAD/CAM crowns based on the FEA model were machined having different occlusal cementation spaces, etched and cemented to dentin analogs. Non-bonding of etched ceramic was achieved using a thin layer of poly(dimethylsiloxane). Crowns were loaded to failure at 5 N/s, with radial cracks detected acoustically.Results. Failure loads depended on the bonding condition and the cement thickness for both FEA and physical testing. Average fracture loads for bonded crowns were: 673.5 N at 50 mu m cement and 300.6 N at 500 mu m. FEA stresses due to polymerization shrinkage increased with the cement thickness overwhelming the protective effect of bonding, as was also seen experimentally. At 50 mu m cement thickness, bonded crowns withstood at least twice the load before failure than non-bonded crowns.Significance. Occlusal "fit" can have structural implications for CAD/CAM crowns; pre-cementation spaces around 50-100 mu m being recommended from this study. Bonding benefits were lost at thickness approaching 450-500 mu m due to polymerization shrinkage stresses. (C) 2012 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)