993 resultados para ISOTACTIC POLYSTYRENE


Relevância:

20.00% 20.00%

Publicador:

Resumo:

This study investigates the impact of polystyrene sodium sulfonate (PolyNaSS) grafting onto the osseo-integration of a polyethylene terephthalate artificial ligament (Ligament Advanced Reinforcement System, LARS™) used for Anterior Cruciate Ligament (ACL). The performance of grafted and non-grafted ligaments was assessed in vitro by culturing human osteoblasts under osteogenic induction and this demonstrated that the surface modification was capable of up-regulating the secretion of ALP and induced higher level of mineralisation as measured 6 weeks post-seeding by Micro-Computed Tomography. Grafted and non-grafted LARS™ were subsequently implanted in an ovine model for ACL reconstruction and the ligament-to-bone interface was evaluated by histology and biomechanical testings 3 and 12 months post-implantation. The grafted ligaments exhibited more frequent direct ligament-to-bone contact and bone formation in the core of the ligament at the later time point than the non-grafted specimens, the grafting also significantly reduced the fibrous encapsulation of the ligament 12 months post-implantation. However, this improved osseo-integration was not translated into a significant increase in the biomechanical pull-out loads. These results provide evidences that PolyNaSS grafting improved the osseo-integration of the artificial ligament within the bone tunnels. This might positively influence the outcome of the surgical reconstructions, as higher ligament stability is believed to limit micro-movement and therefore permits earlier and enhanced healing.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

It has been observed that poly(styrene peroxide) with a high molecular weight is thermally less stable than the same polymer with a low molecular weight. This has been explained as being due to the strain on the O-O bond due to the greater polymer chain length.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effect of cobalt salicylate on the oxidative degradation and ignition of polystyrene has been studied. It was found that cobalt salicylate sensitizes both the degradation and ignition of polystyrene by facilitating electron-transfer processes in the propagation step. From thermochemical and kinetic studies it was found that the cobalt ion, owing to its ability to exist in variable valence states, promotes electron transfer in the propagation step of polymer degradation, increasing the rate of propagation and consequently the overall rate. Using solid-phase thermal ignition theory, an attempt has been made to explain the sensitization of ignition by the cobalt ion.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Vacuum pyrolysis of ammonium perchlorate (AP) and ammonium perchlorate/polystyrene (PS) propellant has been studied by differential thermal analysis (DTA) in order to observe the effect of transition metal oxides on sublimation. Sublimation and decomposition being competitive processes, their proportions depend on the pressure of the pyrolysis chamber. The enthalpies for complete decomposition and complete sublimation are available from the literature and by using these data together with DTA area measurements, the extents of sublimation and decomposition have been calculated for AP and the propellant system. The effect of the metal ions on the extent and rate of sublimation depends on their nature. For AP the extent of sublimation increases with a decrease in particle size. For the propellants the powder sublimes more readily than the bulk material, but in the presence of metal ions the bulk material sublimes more readily than the powder. To substantiate this finding, the effect of MnO2 on AP sublimation as a function of particle size was examined, and it was observed that the extent of sublimation decreases as the particle size decreases.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effect of transition metal oxides (Fe2O3, MnO2, Ni2O3 and Co2O3) on polystyrene/ammonium perchlorate propellant systems has been examined. The mechanism of action of the oxides in increasing the burning rate was examined by studying the effect of the oxides on the thermal decomposition and combustion of the oxidizer and the propellant. It has been concluded that one of the mechanisms by which the oxides act is by promoting the charge-transfer process, which is indicated by the enhancement of the electron-transfer process in ammonium perchlorate and by the correlation between the redox potential of the metal ions and the corresponding burning rates of the propellant.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The annealing behavior of isotactic polybutene-1 (PB-1) has been studied by differential scanning calorimetry and wide-angle x-ray diffraction. On annealing at 110°C, PB-1 yields thick crystals melting at -140°C which are mainly of Form I. An increase in the heat of fusion (ΔHf) and crystallinity is found for annealing times up to 12 h at 110°C; at longer times these properties decrease with increasing annealing time. The increases in ΔHf and crystallinity are attributed to increases in the lamellar thickness in the chain direction and in crystal perfection, and subsequent decreases to degradation of the polymer.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An electric field (100 V/cm at 230°C and 150°C) has been applied to ammonium perchlorate (AP)/polystyrene (PS) propellant mixtures in order to understand the low temperature decomposition behavior of the propellant. The charge-carrying species is anionic in nature at 230°C, which could be ClO4−, but is cationic at 150°C, which could be either NH4+ or H+. These results are parallel to that observed for pure ammonium perchlorate (AP) pellets [1]. The burning rate (r' ) of the propellant was found to follow the same trend as that for the thermal decomposition of the propellant on application of an electric field. At 150°C Image was higher at the −ve electrode than at the +ve electrode, but at 230°C just the opposite was observed. Kinetic studies have confirmed that the decomposition of the orthorhombic AP follows two mechanism corresponding to E = 30 kcal mol−1 (180–230°C) and E = 15 kcal mol−1 (150–180°C).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Polystyrene peroxide has been synthesized and its decomposition has been studied by thermogravimetry and differential thermal analysis. Polystyrene peroxide has been found to decompose exothermically at about 110°C. The activation energy for the decomposition was estimated to be 30 kcal/mole both by the Jacobs and Kureishy method and by fitting the α versus time curves to the first-order kinetic equation. This suggests that the rate-controlling step in the decomposition of polystyrene peroxide is cleavage of the O---O bond.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The thermal degradation of polystyrene peroxide was carried out using differential scanning calorimetry. The activation energy (E) was found to be 136 kJ mole–1 at all extents of decomposition. TheE value was found to correspond to-O-O-dissociation. The order of reaction was found to decrease from 2 to 1 as the decomposition progresse.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An electric field (100 V/cm at 230°C and 150°C) has been applied to ammonium perchlorate (AP)/polystyrene (PS) propellant mixtures in order to understand the low temperature decomposition behavior of the propellant. The charge-carrying species is anionic in nature at 230°C, which could be ClO4−, but is cationic at 150°C, which could be either NH4+ or H+. These results are parallel to that observed for pure ammonium perchlorate (AP) pellets [1]. The burning rate (Image ) of the propellant was found to follow the same trend as that for the thermal decomposition of the propellant on application of an electric field. At 150°C Image was higher at the −ve electrode than at the +ve electrode, but at 230°C just the opposite was observed. Kinetic studies have confirmed that the decomposition of the orthorhombic AP follows two mechanism corresponding to E = 30 kcal mol−1 (180–230°C) and E = 15 kcal mol−1 (150–180°C).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Some aspects of the pyrolysis of polystyrene peroxide (PSP) have been examined. Low-temperature decomposition studies at 60°C and 70°C have been carried out to elucidate the ageing behaviour of PSP. The exothermic decomposition was found to be complete in 44 h at 70°C suggesting that all peroxide bonds have broken. Enthalpy measurements of the aged samples were carried out as a function of storage time. Ageing was also followed by infrared spectroscopy, and the intensity of the peroxide absorption around 1050 cm−1 was found to decrease with ageing time. Benzaldehyde formed as a result of PSP pyrolysis is readily converted into benzoic acid, which crystallizes during the ageing process. Pyrolysis—gas chromatographic studies have shown that up to 450°C the basic decomposition mechanism (i.e., the formation of benzaldehyde and formaldehyde as the major products) does not change. No effect of pressure on the decomposition exotherm in differential thermal analysis was observed, suggesting that peroxide composition involves only condensed phase reactions. Hydroquinone, p-aminophenol and cadmium sulphide were found to retard the thermal decomposition of PSP, suggesting that these compounds would be potential antioxidants for polymers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The importance of the study of thermal degradation of polymeric fuels arises from their role in the combustion of solid propellants. Estimation of the condensed-phase heat release during combustion can be facilitated by the knowledge of the enthalpy change associated with the polymer degradation process. Differential scanning calorimetry has been used to obtain enthalpy data. Kinetic studies on the polymeric degradation process have been carried out with the following objectives. The literature values of activation energies are quite diverse and differ from author to author. The present study has tried to locate possible reasons for the divergence in the reported activation energy values. A value of 30 kcal has been obtained and found to be independent of the technique employed. The present data on the kinetics support to chain-end initiation and unzipping process. The activation energies are further found to be independent of the atmosphere in which the degradation of polymer fuel is carried out. The degradation in air, N2, and O2 all yield a value of 30 kcal/mole for the activation energies.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Mass histories of polystyrene spheres (initial diameter 2–5 mm) burning in simulated air have been obtained by quenching combustion after variable times and weighing the residues. The flame positions and temperature histories of the spheres have also been recorded. A simple analytical model — an extension of quasi-steady combustion theory of liquid droplets — is shown to describe the combustion process reasonably well. Though the combustion process is broadly similar to that of liquid spheres, flame diameter is relatively smaller, particle temperature higher, and decomposition reactions occur in the condensed phase.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Poly(styrene peroxide) has been prepared and characterized. Nuclear magnetlc resonance (NMR) spectra Of the polymer show the shift Of aliphatic protons. Differential scanning calorimetric (DSC) and differential thermal analysis (DTA) results show anexothermic peak around 110 OC which is characteristic of peroxide decomposition.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Composites of Polystyrene-multi wall carbon nanotubes (PS-MWNTs) were prepared with loading up to 7 wt% of MWNTs by simple solvent mixing and drying technique. MWNTs with high aspect ratio similar to 4000 were used to make the polymer composites. A very high degree of dispersion of MWNTs was achieved by ultrasonication technique. As a result of high dispersion and high aspect ratio of the MWNTs electrical percolation was observed at rather low weight fraction similar to 0.0021. Characterization of the as prepared PS-MWNTs composites was done by Electron microscopy (EM), X-ray diffraction technique (XRD) and Thermogravimetery analysis (TGA).