Orthogonal designs are used to investigate the main factors when doing experiments in which pulse bias is superimposed on d.c. bias during cathodic are deposition of TiN. Pulse peak, duty cycle, frequency, direct voltage, are current and pressure all are investigated when coating TiN on HSS substrates. Roughness, surface micrograph, microhardness and thickness are tested. By analysis of variance, it is shown that pressure and frequency are the main factors. R-a and droplet density of the film with (d.c. + pulse) bias decrease. A simple explanation for the result is suggested.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The properties of a highly sp3 bonded form of amorphous carbon denoted ta-C deposited from a filtered cathodic vacuum arc (FCVA) are described as a function of ion energy and deposition temperature. The sp3 fraction depends strongly on ion energy and reaches 85% at an ion energy of 100 eV. Other properties such as density and band gap vary in a similar fashion, with the optical gap reaching a maximum of 2.3 eV. These films are very smooth with area roughness of order 1 nm. The sp3 fraction falls suddenly to almost zero for deposition above about 200 °C.