958 resultados para Castor polyurethane


Relevância:

30.00% 30.00%

Publicador:

Resumo:

Vegetable-based polyurethane (PU) was prepared in the thin film form by spin coating. This polymer is synthesised from castor oil, which can be extracted from the seeds of a native plant in Brazil called mamona. This polymer is biocompatible and is being used as material for artificial bone. The PU was characterised by dielectric spectroscopy in a wide range of frequency (10(-5) Hz to 10(5) Hz) and by thermally stimulated discharge current (TSDC) measurements. The glass transition temperature (T-g=39degreesC) was determined and using the initial rise method the activation energy was found to be 1.58 eV. (C) 2003 Kluwer Academic Publishers.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Flexible and free-standing films of piezoelectric composites made up of lead zirconate titanate (PZT) ceramic powder dispersed in a castor oil-based polyurethane (PU) matrix were obtained by spin coating and characterised as materials for sensor applications. The piezoelectric coefficients d(31) and d(33) were measured with the usual technique. The piezoelectric charge constant d(33) yields values up to less than or equal to 24 pC/N, even at lower PZT content (33 vol%). Some desirable properties like piezoelectricity, flexibility and good mechanical resistance show this new material to be a good alternative for use as sensors and actuators.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Composite made of Lead Zirconate Titranate (PZT) ceramic powder and castor oil based polyurethane (PU) were prepared in the thin film form with 0-3 connectivity by spin coating. The composite films were obtained in the thickness range of 100 mum to 300 mum using 33-vol.% of ceramic. The samples mechanical resistance. The material was characterised by dielectric spectroscopy, thermally stimulated discharge current (TSDC), hysteresis measurements and laser-intensity-modulation method (LIMM). The pyroelectric coefficient at 343 K was 7x10(-5) C.m(-2) K-1 for the sample poled with 10 MV/m at 373 K for Ih. The results show that this new composite can be used as suitable piezo and pyroelectric sensors.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Flexible piezo- and pyroelectric composite was made in the thin film form by spin coating. Lead Zirconate Titanate (PZT) ceramic powder was dispersed in a castor oil-based polyurethane (PU) matrix, providing a composite with 0-3 connectivity. The dielectric data, measured over a wide range of frequency (10(-5) Hz to 105 Hz), shows a loss peak around 100 Hz related with impurities in the polymer matrix. There is also an evidence of a peak in the range 10(-4) Hz, possibly originating from the glass transition temperature T of the polymer. The pyroelectric coefficient at 34 K is 7.0x10(-5) C(.)m(-2.)K(-1) which is higher than that of P-PVDF (1X10(-5) C(.)m(-2.)K(-1)).

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Thin films of blend made up of castor oil-based polyurethane (PU) and polyaniline (PANI) were obtained by casting. The molecular mobility was studied using dielectric spectroscopy and thermally stimulated depolarization current (TSDC) for blends with two different compositions (90/10, 80/20) and the results were compared with PU pure. The peak located around -60 degrees C in TSDC thermograms of PU/PANI blend has dipolar behavior and might be attributed to the change in the molecular chain due to the interaction between isocyanate and the solvent. Vogel-Fulcher Tammann fits was performed on the observed relaxation and the result shows a alpha-relaxation-like. (c) 2005 Springer Science + Business Media, Inc.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Ferroelectric ceramic particles based on lead titanate zirconate (PZT) were dispersed in a polymer matrix based on castor oil. After the poling process, the pyroelectric activity of this composite was measured using a direct method in which a linear heating rate was applied to the pre-poled samples. The pyroelectric coefficient at 343 K is comparable with that of a PZT-poly(vinylidene fluoride) (PVDF) composite and significantly higher than that of PVDF. © 1998 Kluwer Academic Publishers.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Flexible and free-standing films of piezoelectric composites made up of lead zirconate titanate (PZT) ceramic powder dispersed in a castor oil-based polyurethane (PU) matrix were obtained by spin coating and characterized as materials for sensor applications. The piezoelectric coefficients d 31 and d 33 were measured with the usual technique. The piezoelectric charge constant d 33 yields values up to ≤24 pC/N, even at lower PZT content (33 vol%). Some desirable properties like piezoelectricity, flexibility and good mechanical resistance show this new material to be a good alternative for use as sensors and actuators.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The aim of this study is to compare polyurethanes containing castor oil (soft segment) in granular form compared to cancellous bone autograft applied to a segmental bone defect. Norfolk adult female rabbits - approximately 13 months of age with a mean body weight of 4.5 kg - are used. In both radial diaphyses, 1 cm osteoperiosteal segmental defects are created. The defect in the left radius is filled with the castor-oil-based polyurethane, and the right one, filled with cancellous bone autograft, collected from the left proximal humerus. The rabbits are euthanazed at 15, 30, 60, and 120 days postsurgery (5 animals/ period), for histological analyses. By radiographic analyses, at these time points, the bone regeneration is more evident and accelerated in the bone defects treated with the cancellous bone autograft. At 120 days postsurgery, the segmental bone defects treated with the cancellous bone autograft are totally reconstituted and remodeled, while the bone defects treated with polyurethane polymer have bone formation of 79%. Histological study shows that the polyurethane acts as a space filler, minimizing the local production of fibrous tissue. No granule degradation, resorption or any inflammatory reaction is detected. Thus, it is possible to conclude that the castor-oil-plant-based polyurethane - in the granule presentation - is biocompatible and osteointegrated, but does not show the same bone regeneration capacity as the cancellous bone autograft. © 2007 SAGE Publications.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A simple flow-injection analysis procedure was developed for determining captopril in pharmaceutical formulations employing a novel solid-phase reactor containing silver thiocyanate immobilized in a castor oil derivative polyurethane resin. The method was based on silver mercaptide formation between the captopril and Ag(I) in the solid-phase reactor. During such a reaction, the SCN- anion was released and reacted with Fe3+, which generated the FeSCN2+ complex that was continuously monitored at 480 nm. The analytical curve was linear in the captopril concentration range from 3.0 x 10(-4) mol L-1 to 1.1 x 10(-3) mol L-1 with a detection limit of 8.0 x 10(-5) mol L-1. Recoveries between 97.5% and 103% and a relative standard deviation of 2% for a solution containing 6.0 x 10(-4) mol L-1 captopril (n = 12) were obtained. The sample throughput was 40 h(-1) and the results obtained for captopril in pharmaceutical formulations using this procedure and those obtained using a pharmacopoeia procedure were in agreement at a 95% confidence level.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The need to develop new dental luting agents in order to improve the success of treatments has greatly motivated research. Objective: The aim of this study was to evaluate the diametral tensile strength (DTS) and film thickness (FT) of an experimental dental luting agent derived from castor oil (COP) with or without addition of different quantities of filler (calcium carbonate - CaCO3). Material and Methods: Eighty specimens were manufactured (DTS N=40; FT N=40) and divided into 4 groups: Pure COP; COP 10%; COP 50% and zinc phosphate (control). The cements were mixed according to the manufacturers' recommendations and submitted to the tests. The DTS test was performed in the MTS 810 testing machine (10 KN, 0.5 mm/min). For FT test, the cements were sandwiched between two glass plates (2 cm(2)) and a load of 15 kg was applied vertically on the top of the specimen for 10 min. The data were analyzed by means of one-way ANOVA and Tukey's test (alpha=0.05). Results: The values of DTS (MPa) were: Pure COP- 10.94 +/- 1.30; COP 10%- 30.06 +/- 0.64; COP 50%- 29.87 +/- 0.27; zinc phosphate- 4.88 +/- 0.96. The values of FT (pm) were: Pure COP- 31.09 +/- 3.16; COP 10%- 17.05 +/- 4.83; COP 50%- 13.03 +/- 4.83; Zinc Phosphate- 20.00 +/- 0.12. One-way ANOVA showed statistically significant differences among the groups (DTS - p=1.01E-40; FT - p=2.4E-10). Conclusion: The experimental dental luting agent with 50% of filler showed the best diametral tensile strength and film thickness.