975 resultados para CVD diamond films
Resumo:
A new idea of power device, which contains highly nitrogen-doped CVD diamond and Schottky contact, is proposed to actualise a power device with diamond. Two-dimensional simulation is conducted using ISE TCAD device simulator. While comparably high current is obtained in a transient simulation as expected, this current does not contribute to the drain-source current because of the symmetry of the device. Using an asymmetric structure or bias conditions, the device has high potential as an electric device for extremely high power, high frequency and high temperature. © 2003 Elsevier Science B.V. All rights reserved.
Resumo:
A technique for pattern transfer onto carbon-diamond films deposited by radio-frequency plasma-enhanced chemical vapour deposition is reported. Such a technique involves standard photolithography processes and reactive ion etching by oxygen and is compatible with present day microelectronic technology. The patterns transferred are well defined with very good resolution. © 1992.
Resumo:
Field emissions (FE) from La-doped zinc oxide (ZnO) films are both experimentally and theoretically investigated. Owing to the La-doped effect, the FE characteristic of ZnO films is remarkably enhanced compared with an undoped sample, and a startling low turn-on electric field of about 0.4 V/mu m (about 2.5 V/mu m for the undoped ZnO films) is obtained at an emission current density of 1 mu A/cm(2) and the stable current density reaches 1 mA/cm(2) at an applied field of about 2.1 V/mu m. A self-consistent theoretical analysis shows that the novel FE enhancement of the La-doped sample may be originated from its smaller work function. Due to the effect of doping with La, the Fermi energy level lifts, electrons which tunnelling from surface barrier are consumedly enhancing, and then leads to a huge change of field emission current. Interestingly, it suggests a new effective method to improve the FE properties of film materials.
Resumo:
Diamond films were prepared by microwave plasma chemical vapor deposition (MWPCVD). In order to obtain better field emission properties, the samples coated with different metals were prepared. The results showed that the field emission properties of diamond coated with metals could be greatly improved in comparison to pure diamond film and the different kinds of coated metals have different influences on the field emission properties. The possible reasons of effects on the field emission properties are discussed, which were probably due to the reduced effective surface work function by metal coatings; but the detail of the mechanism should be studied further. The surface morphology and microstructure of the sample were characterized by Atomic Force Microscope (AFM), X-ray photoelectron spectroscopy (XPS), X-ray Diffraction (XRD) and Raman spectrum tests. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
The quality of single crystal diamond obtained by microwave CVD processes has been drastically improved in the last 5 years thanks to surface pretreatment of the substrates [A. Tallaire, J. Achard, F. Silva, R.S. Sussmann, A. Gicquel, E. Rzepka, Physica Status Solidi (A) 201, 2419-2424 (2004); G. Bogdan, M. Nesladek, J. D'Haen, J. Maes, V.V. Moshchalkov, K. Haenen, M. D'Olieslaeger, Physica Status Solidi (A) 202, 2066-2072 (2005); M. Yamamoto, T. Teraji, T. Ito, Journal of Crystal Growth 285, 130-136 (2005)]. Additionally, recent results have unambiguously shown the occurrence of (110) faces on crystal edges and (113) faces on crystal corners [F. Silva, J. Achard, X. Bonnin, A. Michau, A. Tallaire, O. Brinza, A. Gicquel, Physica Status Solidi (A) 203, 3049-3055 (2006)]. We have developed a 3D geometrical growth model to account for the final crystal morphology. The basic parameters of this growth model are the relative displacement speeds of (111), (110) and (113) faces normalized to that of the (100) faces, respectively alpha, beta, and gamma. This model predicts both the final equilibrium shape of the crystal (i.e. after infinite growth time) and the crystal morphology as a function of alpha, beta, gamma, and deposition time.
An optimized operating point, deduced from the model, has been validated experimentally by measuring the growth rate in (100), (111), (110), and (113) orientations. Furthermore, the evolution of alpha, beta, gamma as a function of methane concentration in the gas discharge has been established. From these results, crystal growth strategies can be proposed in order, for example, to enlarge the deposition area. In particular, we will show, using the growth model, that the only possibility to significantly increase the deposition area is, for our growth conditions, to use a (113) oriented substrate. A comparison between the grown crystal and the model results will be discussed and characterizations of the grown film (Photoluminescence spectroscopy, EPR, SEM) will be presented. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
Aim: The aim of this study was to compare the microtensile bond strength of three adhesive systems, using different methods of dentin preparation. Materials and methods: A hundred and eight bovine teeth were used. The dentin from buccal face was exposed and prepared with three different methods, divided in 3 groups: Group 1 (DT)- diamond tip on a high-speed handpiece; Group 2 (CVD)-CVD tip on a ultrasonic handpiece; Group 3 (LA)-Er: YAG laser. The teeth were divided into 3 subgroups, according adhesive systems used: Subgroup 1-Adper Single Bond Plus/3M ESPE (SB) total-etch adhesive; Subgroup 2-Adper Scotchbond SE/3M ESPE (AS) selfetching adhesive; Subgroup 3-Clearfil SE Bond/Kuraray (CS) selfetching adhesive. Blocks of composite (Filtek Z250-3M ESPE) 4 mm high were built up and specimens were stored in deionized water for 24 hours at 37°C. Serial mesiodistal and buccolingual cuts were made and stick-like specimens were obtained, with transversal section of 1.0 mm2. The samples were submitted to microtensile test at 1 mm/min and load of 10 kg in a universal testing machine. Data (MPa) were subjected to ANOVA and Tukey's tests (p < 0.05). Results and conclusion: Surface treatment with Diamond or CVD tips associated with Clearfil SE Bond adhesive produced significantly lower bond strength values compared to other groups. Surface treatment with Er: YAG laser associated with Single Bond Plus or Clearfil SE Bond adhesives and surface treatment with CVD tip associated with Adper Scotchbond SE adhesive produced significantly lower bond strength values compared to surface treatment with diamond or CVD tips associated with Single Bond Plus or Adper Scotchbond SE adhesives. Clinical significance: Interactions between laser and the CVD tip technologies and the different adhesive systems can produce a satisfactory bonding strength result, so that these associations may be beneficial and enhance the clinical outcomes.
Resumo:
Dissipadores de calor recobertos com filmes de diamante CVD foram desenvolvidos para acoplar a semicondutores, utilizando-se do Laboratório de Deposição de Filmes de Diamante CVD, na UNESP - Campus de Guaratinguetá e o Laboratório de Diamantes da Universidade São Francisco, em Itatiba, SP. Analisou-se o filme de diamante CVD sobre o silício, para emprego como dissipador de calor, porque o filme de diamante CVD pode ter o valor da condutividade térmica até cinco vezes superior ao do cobre e de dez vezes a do alumínio. Os filmes foram obtidos via deposição através de reator de filamento quente, trabalhando-se com vários filamentos retilíneos em paralelo, resultando assim em um processo que visou obter um filme mais uniforme e com grande área de deposição. Os dados para análises da composição química superficial dos filmes foram obtidos por Difração de Raios-X, Dispersão de Energia de Raios-X e para a verificação da morfologia e espessura do filme foi utilizada a Microscopia Eletrônica de Varredura. Para a verificação do comportamento da temperatura sobre o dissipador com o filme de diamante CVD foi utilizada uma câmera de imagem termográfica, marca Fluke, modelo Ti 40 FT. Foram obtidos filmes de 2 e 10 ?m sobre o silício. Estas espessuras ainda não oferecem um desempenho mecânico que o torne autosustentado. Do ponto de vista de desempenho térmico as análises mostraram que, mesmo com pequena espessura, o filme de diamante CVD apresentou bom resultado experimental. Os principais desafios de construção para esse dissipador de calor são a obtenção do filme com espessura acima de um mm e a garantia da qualidade do filme com a repetitividade do processo em cujo caso torna-se necessário definir as dimensões do dissipador antes da deposição do filme.
Resumo:
Two polycrystalline diamond surfaces, manufactured by chemical vapour deposition (CVD) technique, are investigated regarding their applicability as charge state conversion surfaces (CS) for use in a low energy neutral atom imaging instrument in space research. The capability of the surfaces for converting neutral atoms into negative ions via surface ionisation processes was measured for hydrogen and oxygen with particle energies in the range from 100 eV to 1 keV and for angles of incidence between 6 deg and 15 deg. We observed surface charging during the surface ionisation processes for one of the CVD samples due to low electrical conductivity of the material. Measurements on the other CVD diamond sample resulted in ionisation efficiencies of ~2 % for H and up to 12 % for O. Analysis of the angular scattering revealed very narrow and almost circular scattering distributions. Comparison of the results with the data of the CS of the IBEX-Lo sensor shows that CVD diamond has great potential as CS material for future space missions.