996 resultados para 95-603
Resumo:
The effect of growth texture on the magnetostriction of ternary Tb0.3Dy0.7Fe1.95 was studied by conducting unidirectional solidification experiments using a zoning set-up. Detailed texture evolutions were studied using X-ray diffraction on samples obtained by varying growth rates from 18 to 72 cm/h, under a temperature gradient of 100 degrees C/cm. The estimated texture co-efficient and pole figures of the samples indicate that during the onset of the solidification, < 110 > and < 331 >/'rotated < 110 >' texture components nucleate and grow in all the samples. However, as the solidification progresses, < 112 > texture component becomes dominant at higher growth rate. This results in an improvement of magnetostriction from 1000 to 1300 microstrains for samples grown at growth rates of 18 and 72 cm/h respectively. The transition of preferred growth direction occurs through intermediate orientations < 123 >. An attempt has been made in this paper to explain the occurrence of different growth texture by considering the stability of growing interface, its planar packing fraction and atomic stacking sequence of several low index planes. (C) 2010 Elsevier Ltd. All rights reserved.
Resumo:
Hydrogen is a clean energy carrier and highest energy density fuel. Water gas shift (WGS) reaction is an important reaction to generate hydrogen from steam reforming of CO. A new WGS catalyst, Ce(1-x)Ru(x)O(2-delta) (0 <= x <= 0.1) was prepared by hydrothermal method using melamine as a complexing agent. The Catalyst does not require any pre-treatment. Among the several compositions prepared and tested, Ce(0.95)Ru(0.05)O(2-delta) (5% Ru(4+) ion substituted in CeO(2)) showed very high WGS activity in terms of high conversion rate (20.5 mu mol.g(-1).s(-1) at 275 degrees C) and low activation energy (12.1 kcal/mol). Over 99% conversion of CO to CO(2) by H(2)O is observed with 100% H(2) selectivity at >= 275 degrees C. In presence of externally fed CO(2) and H(2) also, complete conversion of CO to CO(2) was observed with 100% H(2) selectivity in the temperature range of 305-385 degrees C. Catalyst does not deactivate in long duration on/off WGS reaction cycle due to absence of surface carbon and carbonate formation and sintering of Ru. Due to highly acidic nature of Ru(4+) ion, surface carbonate formation is also inhibited. Sintering of noble metal (Ru) is avoided in this catalyst because Ru remains in Ru(4+) ionic state in the Ce(1-x)Ru(x)O(2-delta) catalyst.
Resumo:
Temperature dependence of the energy gap and free carrier absorption in a high-quality InAs0.05Sb0.95 single crystal was studied between 90 K and 430 K through the absorption spectra. At this alloy concentration, the room-temperature energy gap was measured to be 0.15 eV. Varshni- and the Bose–Einstein-type fit parameters were obtained from the measured temperature dependence of the energy gap, and the latter gave the zero-temperature gap to be 0.214 eV. It was found that although Weider’s empirical formula for the dependence of the energy gap on temperature and the alloy concentration agrees with the value of the gap at room temperature, it is inaccurate in describing its temperature dependence. From the free carrier absorption measurements, the phonon limited cross section of 7.35×10−16 cm2 at 15 μm was deduced at room temperature.
Resumo:
Barium zirconium titanate [Ba(Zr0.05Ti0.95)O3, BZT] thin films were prepared by pulsed laser ablation technique and dc leakage current conduction behavior was extensively studied. The dc leakage behavior study is essential, as it leads to degradation of the data storage devices. The current-voltage (I-V) of the thin films showed an Ohmic behavior for the electric field strength lower than 7.5 MV/m. Nonlinearity in the current density-voltage (J-V) behavior has been observed at an electric field above 7.5 MV/m. Different conduction mechanisms have been thought to be responsible for the overall I-V characteristics of BZT thin films. The J-V behavior of BZT thin films was found to follow Lampert’s theory of space charge limited conduction similar to what is observed in an insulator with charge trapping moiety. The Ohmic and trap filled limited regions have been explicitly observed in the J-V curves, where the saturation prevailed after a voltage of 6.5 V referring the onset of a trap-free square region. Two different activation energy values of 1.155 and 0.325 eV corresponding to two different regions have been observed in the Arrhenius plot, which was attributed to two different types of trap levels present in the film, namely, deep and shallow traps.
Resumo:
Base metal substituted Sn(0.95)M(0.05)O(2-delta) (M = Cu, Fe, Mn, Co) catalysts were synthesized by the solution combustion method and characterized by XRD, XPS, TEM and BET surface area analysis. The catalytic activities of these materials were investigated by performing CO oxidation. The rates and the apparent activation energies of the reaction for CO oxidation were determined for each catalyst. All the substituted catalysts showed high rates and lower activation energies for the oxidation of CO as compared to unsubstituted SnO(2). The rate was found to be much higher over copper substituted SnO(2) as compared to other studied catalysts. 100% CO conversion was obtained below 225 degrees C over this catalyst. A bifunctional reaction mechanism was developed that accounts for CO adsorption on base metal and support ions and O(2) dissociation on the oxide ion vacancy. The kinetic parameters were determined by fitting the model to the experimental data. The high rates of the CO oxidation reactions at low temperatures were rationalized by the high dissociative chemisorption of adsorbed O(2) over these catalysts.
Resumo:
The effect of Tb/Dy ratio on the structural and magnetic properties of (Tb,Dy)Fe-2 class of alloys has been investigated using nine alloys of TbxDy1-xFe1.95 (x = 0-1) covering the entire range. Our results indicate that the three phases viz. (Tb,Dy)Fe-2 (major phase), (Tb,Dy)Fe-3 and(Tb,Dy)-solid solution (minor phases) coexist in all the alloys. The volume fraction of pro-peritectic (Tb,Dy)Fe-3 phase however, has a minimum at x = 0.4 and a maximum at x = 0.6 compositions. The volume fraction of this phase decreases upon heat treatment at 850 degrees C and 1000 degrees C. A Widmanstatten type precipitate of (Tb,Dy)Fe-3 was observed for Dy-rich compositions (0 <= x <= 0.5). The microstructural investigations indicate that the ternary phase equilibria of Tb-Dy-Fe are sensitive to Tb/Dy ratio including the expansion of (Tb,Dy)Fe-2 phase field which is in contrast to the pseudo-binary assumption that is followed in available literature to date. The lattice parameter, Curie temperature and coercivity are found to increase with Tb addition. Split of (440) peak of (Tb,Dy)Fe-2 observed in x >= 0.3 alloys indicate, a spin reorientation transition from 100] to 111] occurs with Tb addition. (C) 2012 Elsevier B. V. All rights reserved.
Resumo:
The frequency-dependent dielectric relaxation of Pb0.94Sr0.06](Mn1/3Sb2/3)(0.05)(Zr0.52Ti0.48)(0.95)]O-3 ceramics, synthesized in pure perovskite phase by a solid-state reaction technique is investigated in the temperature range from 303 to 773 K by alternating-current impedance spectroscopy. Using Cole-Cole model, an analysis of the imaginary part of the dielectric permittivity with frequency is performed assuming a distribution of relaxation times. The scaling behavior of the imaginary part of the electric modulus suggests that the relaxation describes the same mechanism at various temperatures. The variation of dielectric constant with temperature is explained considering the space-charge polarization. The SEM indicates that the sample has single phase with an average grain size similar to 14.2 mu m. The material exhibits tetragonal structure. A detailed temperature dependent dielectric study at various frequencies has also been performed. (C) 2013 Elsevier B.V. All rights reserved.
Structural refinement, optical and electrical properties of Ba1-x Sm-2x/3](Zr0.05Ti0.95)O-3 ceramics
Resumo:
Samarium doped barium zirconate titanate ceramics with general formula Ba1-x Sm-2x/3](Zr0.05Ti0.95)O-3 x = 0, 0.01, 0.02, and 0.03] were prepared by high energy ball milling method. X-ray diffraction patterns and micro-Raman spectroscopy confirmed that these ceramics have a single phase with a tetragonal structure. Rietveld refinement data were employed to model BaO12], SmO12], ZrO6], and TiO6] clusters in the lattice. Scanning electron microscopy shows a reduction in average grain size with the increase of Sm3+ ions into lattice. Temperature-dependent dielectric studies indicate a ferroelectric phase transition and the transition temperature decreases with an increase in Sm3+ ion content. The nature of the transition was investigated by the Curie-Weiss law and it is observed that the diffusivity increases with Sm3+ ion content. The ferroelectric hysteresis loop illustrates that the remnant polarization and coercive field increase with an increase in Sm3+ ions content. Optical properties of the ceramics were studied using ultraviolet-visible diffuse reflectance spectroscopy.
Resumo:
Tb0.3Dy0.7Fe1.95 alloy was directionally solidified by using a modified Bridgman technique at a wide range of growth rates of 5 to 100 cm/h. The directionally grown samples exhibited plane front solidification morphology up to a growth rate of 90 cm/h. Typical island banding feature was observed closer to the chilled end, which eventually gave rise to irregular peritectic coupled growth (PCG). The PCG gained prominence with an increase in the growth rate. The texture study revealed formation of strong aOE (c) 311 > texture in a lower growth rate regime, aOE (c) 110 > and ``rotated aOE (c) 110 > aEuroe in an intermediate growth regime, and aOE (c) 112 > in a higher growth rate regime. In-depth analysis of the atomic configuration of a solid-liquid interface revealed that the growth texture is influenced by the kinetics of atomic attachment to the solid-liquid interface, which is intimately related to a planar packing fraction and an atomic stacking sequence of the interfacial plane. The mechanism proposed in this article is novel and will be useful in addressing the orientation selection mechanism of topologically closed packed intermetallic systems. The samples grown at a higher growth rate exhibit larger magnetostriction (lambda) and d lambda/dH owing to the absence of pro-peritectic (Tb,Dy)Fe-3 and formation of aOE (c) 112 > texture, which lies closer to the easy magnetization direction (EMD).
Resumo:
El café(Coffea arabica L) es un componente importante del paisaje y la economía nacional, los arboles de sombra y el manejo agronómico influyen en la ecofisiología y calidad del café,mejorando la sostenibilidad de las fincas cafetaleras y su viabilidad económica; por tal razón es de suma importancia el estudio de diferentes sistemas de manejo agronómico del cafeto asociados o no con arboles de sombra. El presente estudio se realizó en la Finca San Francisco de Inversiones Generales S. A., ubicada en el km 39 ½ de la carretera San Marcos,Las Esquinas, en el departamento de Carazo, en un periodo comprendido de Agosto del 2002 hasta Junio del 2003.Los suelos pertenecen a la serie San Marcos del orden de los Andisoles, la finca tiene una altitud de 670 msnm, precipitación anual de 1400 mm, con temperatura promedio anual de 24 ºC y humedad relativa de 80 %. El objetivo general del experimento fue evaluar tres sistemas de manejo del café sobre el crecimiento, estructura productiva, acumulación de biomasa y nitrógeno en la raíz,tallo,ramas, hojas y frutos;producción y calidad del café oro de los cafetos. El diseño utilizado fue de bloques completos al azar (BCA), con tres tratamientos que consistieron en: a)Café(Coffea arabica L cv. Costa Rica 95) bajo sombra de madero negro (Gliricidia sepium(Jacquin) Kunth ex Walpers) y fertilización química,b)Café a plena explosión solar y fertilización química y c) Café bajo sombra sin fertilización.En cada parcela se seleccionaron 8 plantas a las cuales se les tomaron los datos de altura,diámetro, proyección de copa,nudos totales en el tallo principal, numero de ramas primarias,secundarias y terciarias tanto totales como productivas de la planta y rendimiento de café oro por parcela.Una muestra por tratamiento de café oro en cada una de las cuatro cosechas fue tomada y enviada a CERCAFENIC de UNICAFE en Managua para determinar los aspectos físicos y organolépticos de cada una de las muestras de café oro.Empleando el método destructivo se midió la biomasa y cantidad de nitrógeno acumulado en la raíz, tallo,ramas, hojas y frutos por planta. A cada una de las variables estudiadas se le realizó un análisis de varianza (ANDEVA) y separación de medias por rangos múltiples de Tukey al 5 % de margen de error.En Agosto del 2002 las plantas de café bajo sombra sin fertilizante,presentaron la mayor biomasa de raíces (Pr = 0.0065) y el mayor contenido de nitrógeno en raíces (Pr = 0.0084), tallo (Pr = 0.0023) y hojas (Pr = 0.0177); el sistema de café a pleno sol y fertilizante obtuvo la mayor biomasa de tallo (Pr = 0.0165), en las variables restantes no se encontró diferencia significativa. Para el mes de Diciembre del 2002 el sistema café a pleno sol y fertilización presentó el mayor número de ramas terciarias totales (Pr =0.0166), en las variables restantes no se encontró diferencia significativa. Los datos del mes de Junio del 2003 presentan al sistema café bajo sombra y fertilizante con la mayor altura (Pr =0.0001) y el mayor número de ramas primarias totales (Pr = 0.0137) y el sistema café a pleno sol y fertilizante con el mayor número de ramas terciarias productivas (Pr = 0.0303)para las demás variables no se encontró diferencia estadística. El sistema de café bajo sombra sin fertilización obtuvo el mejor rendimiento con 438 kg oro ha–1. La calidad del café fue mejor en el sistema café bajo sombra con fertilizante en la cosecha cuatro y cinco presentando una taza OK, tipo GW y calidad como café lavado Nicaragua. Por ser el primer año de estudio, al no presentarse diferencia significativa en la mayoría de las variables se afirma que se inició con una población altamente homogénea lo cual seria de mucha utilidad para los datos que se tomaran en la continuidad de esta investigación.
Resumo:
El ensayo se realizó en la Finca San Francisco, propiedad de Inversiones Generales S. A., ubicada en el km 39 ½ de la carretera San Marcos, Carazo, desde agosto del 2002 hasta junio del 2004, un estudio cuyo objetivo general fue evaluar tres sistemas de manejo del café sobre el crecimiento, estructura productiva, acumulación de biomasa y nitrógeno en la planta; producción y calidad del grano de café. El ensayo se estableció en tres franjas cuyos tratamientos correspondieron a: a) Café bajo sombra de madero negro (Glericidia sepium jacquin kunth ex walpers) y fertilización química, b) Café a plena explosión solar y fertilización química y c) Café bajo sombra sin fertilización. En cada parcela se seleccionaron 48 plantas de las cuales se tomaron 8 plantas en cada una de las 6 fechas para realizar las mediciones correspondientes. Una muestra de café oro por tratamiento de cada una de las cosechas de cada año fue tomada y enviada a laboratorio de CERCAFENIC de UNICAFE en Managua para determinar los aspectos físicos y organolépticos.Empleando el método destructivo se midió la biomasa y cantidad de Nitrógeno acumulado en laraíz, tallo, ramas, hojas y frutos de cada una de las 8 plantas seleccionadas por fecha. Las variables de crecimiento y rendimiento se presentan a través de figuras y la acumulación de biomasa en los diferentes componentes de la planta de café se explica de acuerdo a resultados de la prueba de t-stundent.Para los meses junio 2003, septiembre 2003, diciembre 2003, y junio 2004 el sistema café sombra con fertilizante obtuvo la mayor altura con 166, 170.25, 179.87 y 204 cm respectivamente mientras este mismo tratamiento en el mes de diciembre 2003 obtuvo el mayor diámetro con 4.87 cm, en septiembre y diciembre 2003 obtuvo una mayor proyección de copa con 2.63 y 2.46m, el mayor números de nudos totales lo obtuvo en diciembre 2003 con 42.50 el mayor número de ramas primarias totales se encontraron en diciembre 2003 con 74.87 y las terciarias totales en diciembre 2002 con 11.50, el mayor número de ramas terciarias productivas se encontraron en junio 2003 con 6, estas en el sistema café a pleno sol. En agosto del 2002 las plantas del sistema café sombra sin fertilizante presentaron la mayor biomasa de raíces con 21.75%; mayor contenido de nitrógeno en raíces con 19.73%; en hojas con 52.02% y en tallos con 8.71% el sistema café a pleno sol obtuvo la mayor biomasa del tallo con 18.87%, en septiembre 2003, el sistema a pleno sol obtuvo la mayor biomasa de raíces con 20.49% en cambio para el junio 2004 el mayor contenido de biomasa fue para el tallo en el sistema café sombra sin fertilizante con 27.63% y el mayor cantidad total de nitrógeno fue para las hojas en el sistema café sombra con fertilizante con 38.41%. El sistema de café sombra sin fertilizante obtuvo el mayor rendimiento en el 2002 con 438 kg oro ha–1 y el sistema a pleno sol obtuvo el mayor rendimiento en 2003 con 2952 kg oro ha–1 . La calidad 2003 fue buena en los tres sistemas pero la cosecha seis para los tres tratamientos presento una taza OK, tipo SHG y calidad como café lavado Matagalpa /Jinotega o estrictamente de altura.
Resumo:
Con el objetivo de determinar el efecto de la sombra y la aplicación de fertilizantes químicos sobre el desarrollo de algunas variables de crecimiento, la estructura productiva y la calidad, tanto física como organoléptica, del café (Coffea arabicaL.) variedad Costa Rica 95, se realizó el presente estudio en la Finca San Francisco, en el municipio de San Marcos, departamento de Carazo, Nicaragua. Consistió de tres parcelas: una a pleno sol con aplicación de fertilizantes y dos bajo sombra de Madero Negro (Gliricidia sepium (Jacquin) Kunth ex Walpers). Solamente una de estas dos parcelas sombreadas recibió fertilización. Se tomaron ocho plantas de café como parcela útil para la toma de variables de crecimiento, estructura productiva y acumulación de biomasa en cada uno de los muestreos. Las variables medidas fueron: altura del tallo, diámetro del tallo, número de nudos en el tallo principal, número de ramas primarias totales y productivas, número de ramas secundarias totales y productivas, número de ramas terciarias totales y productivas, número de ramas agotadas o muertas, rendimiento y la calidad del café. Además, empleando el método destructivo, se determinó la cantidad de biomasa acumulada en los diferentes componentes de la planta de café y su contenido de nitrógeno. Los datos recopilados fueron sometidos a un análisis T de Student para comparar las medias de los diferentes tratamientos estudiados. Se encontró que la fertilización tiene un efecto muy importante en el crecimiento y en el desarrollo de las estructuras productivas del cafeto; sin embargo la sombra juega un papel mucho más importante en la obtención de un café de calidad. También se encontró que la acumulación de biomasa y nitrógeno es afectada por la fertilización y la luz solar ya que se encontraron diferencias entre las plantas fertilizadas y las no fertilizadas y entre las plantas bajo sombra y las cultivadas a plena exposición solar.
Resumo:
Contenido: Materia y necesidad, espíritu y libertad / Octavio N. Derisi – Sistema y silencio en el “Tractatus” de Ludwig Wittgenstein / Alberto Moreno – Los nombres del ser / Gustavo E. Ponferrada – Una perspectiva iusfilosófica del valor justicia en el derecho constitucional / Germán J. Bidart Campos – Notas y comentarios -- Bibliografía
Resumo:
本文采用三种不同加载方式(单轴拉伸,三点弯曲以及圆盘压缩)研究含微裂纹Al_2O_3的陶瓷的弹性性能及其抗拉强度.微裂纹是通过对材料瞬时突变加热和冷却(简称热冲击)形成的.试验结果表明:1)三点弯曲试验得到的力学性能参数较其它两种加载方式所得到的结果要稳定和集中.单轴拉伸试验结果分散性最大.2)热冲击温度越高,材料的等效弹性模量?和等效泊松比?以及各种加载方式下试件的抗拉强度??都有不同程度的下降.电镜观察证实了力学性能参数下降主要与材料内部微裂纹密度增加有关.3)Budiansky-O'Connell方法被用来估计不同热冲击处理后的圆盘试件在断裂过程中的微裂纹密度变化,结果表明实际材料的微裂纹密度较理想材料的微裂纹密度都有一定的偏差.
Resumo:
Procura identificar as causas das falhas nos procedimentos de alteração das leis e apontar possíveis caminhos para a solução do problema. Para tanto, analisam-se a técnica de alteração das leis estabelecida na Lei Complementar n. 95/1998 e casos de incoerências e controvérsias textuais na legislação federal decorrentes de alterações feitas com descuido da boa técnica legislativa, mesmo após o advento da referida lei complementar.