317 resultados para 12E-diene
Resumo:
A super-tough polycarbonate (PC) blend was obtained by using epoxidized ethylene propylene diene (eEPDM) rubber as modifier. The notched Izod impact strength of PC/eEPDM (96/4) blend shows a great improvement, with a value about 25 times of that of pure PC. Finely and homogeneously dispersed rubber particles (0.2-0.8 mu m) in the PC matrix indicated good adhesion between the eEPDM rubber phase and the PC matrix. (C) 1997 Elsevier Science Ltd.
Resumo:
In this paper, epoxidation of ethylene propylene diene rubber by in situ generated performic acid is discussed. The samples have been characterized by infra-red and H-1-nuclear magnetic resonance analyses. Quantitative analysis of the reaction products is made possible by using the methyl deformation band at 1377 cm(-1) as internal standard. The conversion of double bonds increases rapidly within the first 1 h, then gradually, over 2 h, has only a slight increase. The maximum conversion ratio of double bonds is about 70%. The relative content of epoxy groups has a top value at about 7 h. The side reactions are also discussed. (C) 1997 Elsevier Science Ltd.
Resumo:
In this paper, unepoxidized ethylene propylene diene rubber (uEPDM) was first epoxidized with formic acid and H2O2, and then the epoxidized ethylene propylene diene rubber (eEPDM) was melt-mixed with PET resin in a Brabender-like apparatus. Toughening of PET matrix was achieved by this method. The dispersion of rubber particles and phase structure of the blends were also observed by SEM. It has been suggested that the epoxy groups in the eEPDM could react with PET end groups to form a graft copolymer which could act as an interfacial compatibilizer between the PBT matrix and eEPDM rubber dispersed phase. This is beneficial to the improvement of the impact performance of PBT. (C) 1997 Elsevier Science Ltd.
Resumo:
Blends of poly (butylene terephthalate) (PBT) and epoxided ethylene-propylene-diene terpolymer (EEPDM) were prepared. Their mechanical properties and morphology were studied by Izod impact test machine and scanning electronic microscope respectively, It was found that the notched Izod impact strength of blend PBT/EEPDM was as about 23 times as that of pure PET and about 10 times as that of blend PBT/EPDM at room temperature, The dispersed rubber particles were much smaller and the phase boundary was more blurred in blend PBT/EEPDM than in blend PBT/EPDM. The toughness of blend PBT/EEPDM was much more better than that of blend PET and PBT/EPDM, which was in good agreement with the difference between their morphologies.
Resumo:
Absolute configurations of a number of cis-dihydrodiols (cis-1,2-dihydroxy-3,5-cyclohexadienes), synthetically useful products of TDO-catalyzed dihydroxylations of 1,2- and 1,3-disubstituted benzene derivatives, have been determined by a comparison of calculated and experimental CD spectra and optical rotations and by methods involving X-ray crystallography, H-1 NMR spectra of diastereoisomeric derivatives, and by stereochemical correlations. The computations disclosed a significant effect of the substituents on conformational equilibria of cis-dihydrodiols and chiroptical properties of individual conformers. The assigned absolute configurations of cis-dihydrodiols have allowed the validity of a simple predictive model for TDO-catalyzed arene dihydroxylations to be extended.
Resumo:
Palladium catalysed reductive cyclisation of a 1,1-dibromoalkene to an acetylene gives the core unit of the quinolizidine based diene homopuniliotoxin alkaloids with complete control of stereochemistry of the exocyclic double bond. Copyright (C) 1996 Elsevier Science Ltd
Resumo:
Référence bibliographique : Rol, 61307