932 resultados para heterogeneous polymerization
Resumo:
Vanadium(III) complexes bearing salicylaldiminato ligands (2a-k) [RN=CH(Ar0)]VCl2(THF)2 (Ar C61714, R = Ph, 2a; p-CF3Ph, 2b; p-CH3Ph, 2c; 2,6-Me2Ph, 2d; 2,6-iPr2Ph, 2e; cyclohexyl, 2f; Ar = C6H3tBu(2), R = Ph, 2g; 2,6-iPr2Ph, 2h; Ar = C6H2tBU2(2,4), R = Ph, 2i; 2,6-iPr2Ph, 2j; Ar = C6H2Br2, R = Ph, 2k) were prepared from VC13(THF)3 by treating with 1.0 equiv of (RN=CH)ArOH in tetrahydrofuran (THF) in the presence of excess triethylamine (TEA).
Resumo:
A series of new titanium complexes with two asymmetric bidentate beta-enaminoketonato (N,O) ligands (4b-t), [RN=CCF3)CHC(t-BU)O](2)TiCl2 (4b, R = -C6H4F(o); 4c, R = -C6H4F(m);4d, R = -C6H4F(p); 4e, R = - C6H3F2(2,3); 4f, R = -C6H3F2(2,4); 4g, R = -C6H3F2(2,5); 4h, R = -C6H3F2(2,6); 4i, R = -C6H3F2(3,4); 4j, R = -C6H3F2(3,5); 4k, R = -C6H2F3(2,3,4); 4l, R = -C6H2F3(3,4,5); 4m, R = -C6H4CF3(o); 4n, R =-C6H4CF3(m); 4o, R = -C6H4CF3(p); 4p, R = -C6H4Cl(p); 4q, R = -C6H4I(p); 4r, R = -C6H4NO2(P); 4s, R = -CH2C6H5; 4t, R = -C6H11), have been synthesized and characterized.
Resumo:
Fe3O4-polylactide (PLA) core-shell nanoparticles were perpared by surface functionalization of Fe3O4 nanoparticles and subsequent surface-initiated ring-opening polymerization of L-lactide. PLA was directly connected onto the magnetic nanoparticles surface through a chemical linkage. Fourier transform infrared (FT-IR) spectra directly provided evidence of the PLA on the surface of the magnetic nanoparticles. Transmission electron microscopy images (TEM) showed that the magnetic nanoparticles were coated by PLA with a 3-nm-thick shell.
Resumo:
A series of phosphoryl (P=O) contained compounds: triethylphosphate (a), diethyl phenyl phosphate (b), ethyldiphenylphosphate (c) triarylphosphates (d and h-m), triphenylphosphine oxide (e), phenyl diphenylphosphinate (f) and diphenyl phenylphosphonate (g) have been prepared. Iron catalysts, which are generated in situ by mixing the compounds with Fe(2-EHA)(3) and (AlBu3)-Bu-i in hexane, are tested for butadiene polymerization at 50 degrees C. Phosphates donated catalysts have been, unprecedently, found to conduct extremely high syndiotactically (pentad, rrrr=46.1-94.5%) enriched 1,2-selective (1,2-structure content=56.2-94.3%) polymerization of butadiene.
Resumo:
Living characteristics of facilely prepared Ziegler-Natta type catalyst system consisting of iron(III) 2-ethylhexanoate, triisobutylaluminum and diethyl phosphite have been found in the polymerization of 1,3-butadiene in hexane at 40 degrees C. The characteristics have been well demonstrated by: a first-order kinetics with respect to monomer conversion, a narrow molecular weight distribution (M-w/M-n = 1.48-1.52) of polybutadiene in the entire range of polymerization conversion and a good linearity between M-n and the yield of polymer. Feasible post-polymerization of 1,3-butadiene and block co-polymerization of 1,3-butadiene and isoprene further support the living natures of the catalyst bestowed with.
Resumo:
Fe(III), Cr(III), Fe(II), Co(II) and Ni(II) chloride complexes supported by 2,6-bis[1-(iminophenyl)ethyl]pyridine have been synthesized and characterized along with single crystal X-ray diffraction. These complexes, in combination with MAO, have been examined in butadiene polymerization. The catalytic activity and regioselectivity are strongly controlled by metal center and cocatalyst (MAO/Co ratio dependent in the case of Co(II) complex). The activity decreases in the order of Fe(III) > Co(II) > Cr(III) approximate to Ni (II) complexes, in consistent with the space around the metal center. Polybutadiene with different microstructure content, from high trans-1,4 units (88-95% for iron(III) and Cr(III)), medium trans-1,4 and cis-1,4 units (55% and 35%, respectively, for iron(II)) to high cis-1,4 units 79% for Co(II) and 97% for Ni(II) call be easily achieved by varying of the metal center.
Resumo:
Most nanofiltration (NF) membranes are composite and have a polyamide thin film prepared by interfacial polymerization. Their performances mainly correlate the structure of the thin film and monomers used for its preparation. In this work, a novel thin-film composite (TFC) nanofiltration membrane was successfully prepared from 3,3',5,5'-biphenyl tetraacyl chloride (mm-BTEC) and piperazine (PIP) through interfacial polymerization. Attenuated reflectance infrared (ATR-IR) and X-ray photoelectronic spectroscopy (XPS) were used to characterize the chemical composition of the membrane surface. The membrane performance was optimized by studying preparation parameters including monomer concentration, reaction time, and pH of aqueous phase.
Resumo:
Synthetic routes to aluminium ethyl complexes supported by chiral tetradentate phenoxyamine (salan-type) ligands [Al(OC6H2(R-6-R-4)CH2)(2){CH3N(C6H10)NCH3}-C2H5] 7: R = H ; 5, 8: R = Cl; 6, 9: R = CH3) are reported. Enantiornerically pure salan ligands 1-3 with (R,R) configurations at their cyclohexane rings afforded the complexes 4, 5, and 6 as mixtures of two diastereoisomers (a and b). Each diastereoisomer a was, as determined by X-ray analysis, monomeric with a five-coordinated aluminium central core in the solid state, adopting a cis-(O,O) and cis-(Me,Me) ligand geometry. From the results of variable-temperature (VT) H-1 NMR in the temperature range of 220-335 K, H-1-H-1 NOESY at 220 K, and diffusion-ordered spectroscopy (DOSY), it is concluded that each diastereoisomer b is also monomeric with a five-coordinated aluminium central core.
Resumo:
A series of aluminum ethyls and isopropoxides based on a bis(pyrrolidene) Schiff base ligand framework has been prepared and characterized. NMR studies of the dissolved complexes indicate that they adopt a symmetric structure with a monomeric, five-coordinated aluminum center core. The aluminum ethyls used as catalysts in the presence of 2-propanol as initiator and the aluminum isopropoxides were applied for lactide polymerization in toluene to test their activities and stereoselectivities. All polymerizations are living, as evidenced by the narrow polydispersities and the good fit between calculated and found number-average molecular weights of the isolated polymers. All of these aluminum complexes polymerized (S,S)-lactide to highly isotactic PLA without epimerization of the monomer, furnished isotactic-biased polymer from rac-lactide, and gave atactic polymer from meso-lactide.
Resumo:
The surface modification of hydroxyapatite (HA) nanoparticles by the ring opening polymerization (ROP) of gamma-benzyl-L-glutamate N-carboxyanhydride (BLG-NCA) was proposed to prepare the poly(gamma-benzyl-L-glutamate) (PBLG)-grafted HA nanoparticles (PBLG-g-HA) for the first time. HA nanoparticles were firstly treated by 3-aminopropylthriethoxysilane (APS) and then the terminal amino groups of the modified HA particles initiated the ROP of BLG-NCA to obtain PBLG-g-HA. The process was monitored by XPS and FT-IR. The surface grafting amounts of PBLG on HA ranging from 12.1 to 43.1% were characterized by thermal gravimetric analysis (TGA). The powder X-ray diffraction (XRD) analysis confirmed that the ROP only underwent on the surface of HA nanoparticles without changing its bulk properties. The SEM measurement showed that the PBLG-g-HA hybrid could form an interpenetrating net structure in the self-assembly process.
Resumo:
The Heck reaction of iodobenzene and methyl acrylate was investigated with CO2-philic Pd complex catalysts having fluorous ponytails and the organic base triethylamine (Et3N) in the presence of CO2 under solventless conditions at 80 degrees C. The catalysts are not soluble in the organic phase in the absence Of CO2 and the reaction occurs in a solid-liquid biphasic system. When the organic liquid mixture is pressurized by CO2, CO2 is dissolved into the organic phase and this promotes the dissolution of the I'd complex catalysts. As a result, the Heck reaction occurs homogeneously in the organic phase, which enhances the rate of reaction. This positive effect Of CO2 pressurization competes with the negative effect that the reacting species are diluted by an increasing amount of CO2 molecules dissolved. Thus, the maximum conversion appears at a CO2 pressure of around 4 MPa under the present reaction conditions. The catalysts are separated in the solid granules by depressurization and are recyclable without loss of activity after washing with n-hexane and/or water.
Resumo:
For polyamide used in reverse osmosis (RO) membranes, the content of pendant acid groups is critical to its performance. In this work, FTIR was used to analyze the acid contents in the polyamide films prepared via interfacial polymerization of trimesic acid trichloride (TMC) in hexane and 1,3-phenylenediamine (MPDA) in water, and the effects of reaction conditions, including monomer concentrations, time, and temperature, were studied. It was found that more pendant acid groups are present in the polyramide film at higher TMC concentrations or lower MPDA concentrations, and longer reaction times and lower temperatures also favor the formation of the free acids. These results can be explained by the monomer diffusion in the interfacial polymerization process. This work may help the design and fabrication of RO membranes with different hydrophilicity and target performance.
Resumo:
Deprotonation of (ArNHPPh2NAr2)-N-1 (H[NPN](n), n = 1 - 10) by Ln(CH2SiMe3)(3)(THF)(2) (Ln = Lu, Y, Sc, Er) generated a series of rare-earth metal bis(alkyl) complexes [NPN](n)Ln(CH2SiMe3)(2)(THF)(2) (1-10), which under activation with [Ph3C][B(C6F5)(4)] and AliBu(3) were tested for isoprene polymerization. The correlation between catalytic performances and molecular structures of the complexes has been investigated. Complexes 1-5 and 8, where Ar-1 is nonsubstituted or ortho-alkyl-substituted phenyl, adopt trigonal-bipyramidal geometry. The Ar-1 and Ar-2 rings are perpendicular in 1-4 and 8 but parallel in 5. When Ar-1 is pyridyl, the resultant lutetium and yttrium complexes 9a and 9b adopt tetragonal geometry with the ligand coordinating to the metal ions in a N,N,N-tridentate mode, whereas in the scandium analogue 9c, the ligand coordinates to the Sc3+ ion in a N,N-bidentate mode. These structural characteristics endow the complexes with versatile catalytic performances, With increase of the steric bulkiness of the ortho-substituents Ar-1 and Ar-2, the 3,4-selectivity increased stepwise from 81.6% for lutetium complex 1 to 96.8% for lutetium complex 6 and to 97.8% for lutetium complex 7a. However, further increase of the steric bulk of the ligand led to a slight drop of 3,4-selectivity for the attached complex 5 (95.1%).
Resumo:
A series of lutetium alkyl, amino, and guanidinato complexes based upon an amino-phosphine ligand framework had been prepared. These complexes were applied to initiate ring-opening polymerization of 2,2'-dimethyltrimethylene carbonate (DTC). The type of the initiator significantly influenced the catalytic activity of these complexes in a trend as follows: alkyl approximate to guanidinate > amide, whereas the complexes with flexible backbone between P and N atoms within the ligand exhibited higher activity than those with rigid backbone. The isolated PDTC had bimodal-mode molecular weight distribution. The molecular weights of each fraction increased linearly with the conversion, indicating that there might be two active species. This had been confirmed by analyses of oligomeric DTC living species and oligomer with NMR technique as the metal-alkoxide and the four-membered metallocyclic lactate. Kinetic investigation displayed that the polymerization rate was the first order with the monomer concentration.
Resumo:
Hyperbranched polymers with numerous pendent norbornene functionalities have been synthesized via the radical polymerization of a novel asymmetrical divinyl monomer hearing a higher reactivity methacrylate group and it lower reactivity norbornene group. Mediated by a rapid reversible addition-fragmentation chain transfer (RAFT) equilibrium, the concentration of polymeric chain radicals is decreased, and thus the gelation did not occur until higher monomer conversions (ca. 90%). An increase in reaction temperature call also significantly promote the formation of the hyperbranched structure owing to the decreased stability of the intermediate radicals derived from the norbornene group, which was confirmed by a model copolymerization system of two single vinyl monomers with similar structures to the vinyl groups in the asymmetrical divinyl monomer. Furthermore, Tri-SEC and conventional Sin-SEC as well as H-1 NMR.