969 resultados para In-doping
Resumo:
We report the observation of intense frequency up-conversion in Nd3+-doped fluoroindate glasses pumped by the second harmonic of a cw mode-locked Nd: YAG laser. Mechanisms for generating the observed emissions are discussed.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
The evolution of Eu3+ doped SnO2 xerogels to the cassiterite structure observed during sintering was studied by means of Eu3+ spectroscopy, XRD and EXAFS at the Sn K-edge. Eu3+ ions adsorbed at the surface of colloidal particles present a broad distribution of sites, typical of oxide glasses. With sintering at 300°C, this distribution is still broadened. Crystallization is clearly observed by the three techniques with increasing sintering temperature. It is found that the addition of Eu3+ limits the crystallite growth.
Resumo:
The anelastic spectrum (dynamic Young's modulus and elastic energy absorption) of La2CuO4+δ has been measured between 1 and 700 K with 0<δ<0.02. The spectrum of stoichiometric La2CuO4 in the low-temperature orthorhombic (LTO) phase is dominated by two intense relaxation processes which cause softenings of 16% around 150 K and 9% below 30 K at f∼1 kHz. The relaxation at 150 K is attributed to the presence of a fraction of the CuO6 octahedra which are able to change their tilted configuration by thermal activation between orientations which are nearly energetically equivalent, possibly within the twin boundaries. The relaxation below 30 K is governed by tunneling, and involves a considerable fraction of the lattice atoms. It is proposed that the double-well potentials for the low-temperature relaxation are created by the tendency of the LTO phase to form low-temperature tetragonal (LTT) domains, which however are not stabilized like when La is partially substituted with Ba. On doping with excess O, the relaxation rates of these processes are initially enhanced by hole doping, while their intensities are depressed by lattice disorder; an explanation of this behavior is provided. Excess O also causes two additional relaxation processes. The one appearing at lower values of δ is attributed to the hopping of single interstitial O2- ions, with a hopping rate equal to τ-1=2×10-14exp(-5600/T) s. The second process is slower and can be due to O pairs or other complexes containing excess O.
Resumo:
The present work reports the study of KCl thin films doped with In+ or Tl+. Both systems show optical absorption bands similar to single crystals. As the impurity concentration increases, so does the absorption as also the half band width, unlike in KCl: Cu+ films. Further experimental techniques such as X-ray diffraction, scanning electron micrographs and energy dispersive X-ray observations were used and comparative analysis with KCl : Cu+ films reveals new conditions for better crystallinity of the samples.
Resumo:
We report the observation of cooperative frequency upconversion in a fluoroindate glass. The experiments were performed by exciting Yb3+-Tb3+ codoped samples with an infrared diode laser. The process is monitored through the green fluorescence emitted by Tb3+ ions due to a cooperative energy transfer from a pair of excited Yb3+ ions. © 1998 Elsevier Science B.V. All rights reserved.
Resumo:
Non-linear absorption is observed in Er3+-doped fluoroindate glass (in mol% 37InF2:20ZnF2:20SrF2:16BaF2:2GdF2: 2NaF:1GaF3:2ErF3) when the sample is irradiated with a CW laser emitting at 650 nm. An intensity dependence of the optical transmittance is detected. Saturation and sequential absorption of two photons are responsible for the decrease of 50% in the transmittance. The results are explained by simple models which are solved based on rate-equations for the populations of energy levels.
Resumo:
Thin films of undoped and Sb-doped SnO2 have been prepared by a sol-gel dip-coating technique. For the high doping level (2-3 mol% Sb) n-type degenerate conduction is expected, however, measurements of resistance as a function of temperature show that doped samples exhibit strong electron trapping, with capture levels at 39 and 81 meV. Heating in a vacuum and irradiation with UV monochromatic light (305 nm) improve the electrical characteristics, decreasing the carrier capture at low temperature. This suggests an oxygen related level, which can be eliminated by a photodesorption process. Absorption spectral dependence indicates an indirect bandgap transition with Eg ≅ 3.5 eV. Current-voltage characteristics indicate a thermionic emission mechanism through interfacial states.
Resumo:
Ferromagnetic behavior at room temperature is reported in metal-free-conducting polymer samples of poly(3-methylthiophene) doped with ClO 4 -. Magnetic moments associated with spin 1/2 positive polarons are possibly interacting through a Dzialoshinski-Moriya anisotropic superexchange via the dopant anions, giving rise to weak ferromagnetism. © 2001 Elsevier Science B.V. All rights reserved.
Resumo:
Room-temperature photoluminescence (PL) was observed in undoped and 2 mol% Cr-, Al- and Y-doped amorphous SrTiO3 thin films. Doping increased the PL, and in the case of Cr significantly reduced the associated PL wavelength. The optical bandgaps, calculated by means of UV-vis absorption spectra, increased with crystallinity and decreased with the doping level. It was considered that yttrium and aluminum substituted Sr2+, whereas chromium replaced Ti4+. It is believed that luminescence centers are oxygen-deficient BO6 complexes, or the same centers with some other defects, such as oxygen or strontium vacancies, or BO6 complexes with some other defects placed in their neighborhood. The character of excitation and the competition for negatively charged non-bridging oxygen (NBO) among numerous types of BO6 defect complexes in doped SrTiO3 results in various broadband luminescence peak positions. The results herein reported are an indicative that amorphous titanates are sensitive to doping, which is important for the control of the electro-optic properties of these materials. The probable incorporation of Cr into the Ti site suggests that the existence of a double network former can lead to materials displaying a more intense photoluminescence.
Resumo:
We investigated near-infrared-to-blue upconversion from thulium (Tm 3+) doped in tellurite glasses upon continuous wave excitation near 800 nm. We observed an enhancement of over two orders of magnitude of the upconverted emission at ∼480nm when neodymium (Nd 3+) ions were codoped with Tm 3+ ions. For comparison, using a Tm 3+:Nd 3+ codoped fluorozirconate glass as a reference material we observed a 40-fold enhancement of the blue emission. Analysis of the blue emission for samples with different doping levels of Nd 3+ ions showed that energy transfer between Nd 3+ and Tm 3+ is the mechanism responsible for the enhancement in upconversion. © 2002 American Institute of Physics. © 2002 American Institute of Physics.
Resumo:
Energy transfer processes between Er3+ and Tm3+ were investigated examining the frequency upconversion emissions in a fluoroindate glass pumped at 790 nm. A 60-fold enhancement in the emission at ≈670 nm originating from Er3+ was observed when Tm3+ at concentration of 2% was introduced in a sample containing 2% of Er3+. The results are explained considering the influence of cross-relaxation processes between the active ions. © 2002 Elsevier Science B.V. All rights reserved.
Resumo:
In this work we present results on the preparation of planar waveguides based on HfO2 and HfO2-SiO2. Stable sols containing europium and erbium doped HfO2 nanoparticles have been prepared and characterized. The nanosized sol was either deposited (spin-coating) on quartz substrates or embedded in (3-glycidoxipropil)trimethoxisilane (GPTS) used as a hybrid host for posterior deposition. The refractive index dispersion and luminescence characteristics were determined for the resulting HfO2 films. The optical parameters of the waveguides such as refractive index, thickness and propagation losses were measured for the hybrid composite. The planar waveguides present thickness of a few micra and support well confined propagating modes.
Resumo:
Illumination of photorefractive, iron-doped lithium niobate crystals (LiNbO 3:Fe) with x-rays generates a conductivity that we determine from the speed of hologram erasure. The doping levels of the crystals and the acceleration voltage of our x-ray tube are varied. A theoretical model is presented, which describes the obtained results. A decrease of the conductivity with increasing Fe 2+ concentration can be explained by assuming that holes are the dominant charge carriers for this short-wavelength illumination.
Resumo:
In this work we report on visible upconversion emission in Er 3+-, and Ho3+-doped PbGeO3-PbF 2-CdF2-based transparent glass ceramics under 980 nm infrared excitation. In erbium-doped vitroceramic samples, blue(410 ran), green(530, and 550 nm) and red(660 nm) emission signals were generated, which were identified as due to the 2H9/2, 2H 11/2, 4S3/2, and 4F9/2 transitions to the 4I15/2 ground-state, respectively. Intense red(650 nm) upconversion emission corresponding to the 5F5 - 5I8 transition and very small blue(490 nm) and green(540 nm) signals assigned to the 5F 2,3 - 5I8 and 4S2, 5F4 - 5I8 transitions, respectively, were observed in the holmium-doped samples. The 540 nm is the dominant upconversion signal in Ho3+-doped vitroceramics under 850 nm excitation. The dependence of the upconversion processes upon pump power and doping concentration are also investigated, and the main routes for the upconversion excitation processes are also identified. The comparison of the upconversion process in transparent glass ceramics and the precursor glass was also examined and the results revealed that the former present higher upconversion efficiencies.