944 resultados para Aluminium-scandium alloys
Resumo:
The Raman spectrum of guanidinium aluminium sulphate hexahydrate also known as ‘GASH’ which is a ferro-electric crystal and has strong hydrogen bonds has been recorded. 38 Raman lines have been identified in the spectra of GASH. The O-H stretching mode is found to be very much influenced by the hydrogen bond and they appear over a widely extended region from 2240–3600 cm.−1 It can therefore be concluded that all the O-H bonds are hydrogen bonded and some of them are quite strong. The Raman lines due to the N-H vibrations appear with the normal frequency shifts indicating thereby that N-H bonds are not hydrogen bonded. These conclusions are fully supported by the results obtained from the X-ray crystal structure analysis of GASH. The principal vibrations of the Al-(OH2)6 groups have also been identified.
Resumo:
Superplastic materials exhibit very large elongations to failure,typically >500%, and this enables commercial forming of complex shaped components at slow strain rates of similar to 10(-4) s(-1). We report extraordinary record superplastic elongations to failure of up to 5300% at both high strain rates and low temperature in electrodeposited nanocrystalline Ni and some Ni alloys. Superplasticity is not related to the presence of sulfur or a low melting phase at grain boundaries. (C) 2010 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
The mechanism of sub-microscopic precipitation in an Al-Zn-Mg alloy selected for its maximum response to ageing has been studied by a standardized oxide-replica technique in a 100 kV. Philips Electron Microscope. Contrary to earlier conclusions, examination of the oxide replicas has been shown to reveal details of the precipitation process almost as clearly as the thin-foil transmission technique. The reported formation of spherical Guinier-Preston zones followed by the development of a Widmanstaetten pattern of precipitated platelets has been confirmed. The zones have, however, been shown to grow into the platelets and not to dissolve in the matrix as reported earlier. The precipitation process has been correlated with the Hardness/Ageing Time curve and the structure of the precipitates has also been discussed.
Resumo:
Polarisation characters of the Raman lines of calcium fluoride (fluorspar) and potassium aluminium sulphate (alum) were investigated under the following conditions. Unpolarised light was incident normally on a face of the crystal making an angle 22.5° with a cubic face and the light scattered transversely along a cubic axis was analysed by a double image prism kept with its principal axes inclined at 45° to the vertical. Under these conditions the depolarisation factors of the Raman lines belonging to the totally symmetric (A), the doubly degenerate (E) and the triply degenerate (F) modes should be respectively =1, >1 and <1. The characteristic Raman line of CaF2 at 322 cm-1 exhibited a depolarisation value less than 1, showing thereby that the corresponding mode is a triply degenerate one (F). The Raman lines observed in the spectrum of K-alum were also classified and the results were compared with those given by previous investigators using standard crystal orientations.
Resumo:
1. Anhydrous aluminium chloride reacts with phosphorus oxychloride to give a complex with a composition AlCl3.2 POCl3 which can be prepared in the form of a free flowing powder. 2. The phosphorus oxychloride-aluminium chloride complex in nitrobenzene dissociates into AlCl3.POCl3 and POCl3 as indicated by the cryoscopic measurements. 3. The solution of the complex in nitrobenzene has a higher specific conductivity than the corresponding electrical conductivities of individual components. Similar higher electrical conductance is observed when the two components are mixed in nitrobenzene in different proportions. 4.When a solution of anhydrous aluminium chloride in nitrobenzene is titrated conductometrically against a solution of phosphorus oxychloride in nitrobenzene, a limiting value in the conductivity is reached at point corresponding to the molecular composition, the components in the ratio of 1:2 AlCl3: POCl3 in solution. 5. The absorption maxima of the complex in nitrobenzene solution differ from the absorption maximum of the individual components.
Resumo:
The purpose of this study is to experimentally investigate the interaction of inelastic deformation and microstructural changes of two Zr-based bulk metallic glasses (BMGs): Zr41.25Ti13.75Cu12.5Ni10Be22.5 (commercially designated as Vitreloy 1 or Vit1) and Zr46.75Ti8.25Cu7.5Ni10Be27.5 (Vitreloy 4, Vit4). High-temperature uniaxial compression tests were performed on the two Zr alloys at various strain rates, followed by structural characterization using differential scanning calorimetry (DSC) and transmission electron microscopy (TEM). Two distinct modes of mechanically induced atomic disordering in the two alloys were observed, with Vit1 featuring clear phase separation and crystallization after deformation as observed with TEM, while Vit4 showing only structural relaxation with no crystallization. The influence of the structural changes on the mechanical behaviors of the two materials was further investigated by jump-in-strain-rate tests, and flow softening was observed in Vit4. A free volume theory was applied to explain the deformation behaviors, and the activation volumes were calculated for both alloys.
Resumo:
Understanding material flow in friction stir welding is important for production of sound dissimilar metal welding that control the intermixing of two alloys being welded and consequent formation of new constituents which influences the weld properties. In the present experimental investigation material flow patterns are visualised using dissimilar and similar aluminium alloys using a simple innovative ,experiment. The experimental results reveal that only a portion of material transported from the leading edge undergoes chaotic flow and the remaining is deposited systematically in the trailing edge of the weld. Using this information it is shown that the formation of a friction stir welding defect, joint line remnant, does not occur only when the weld interface is on the advancing side. The material flow visualisation study has been utilised to analyse the mechanism of weld formation and its usefulness in improving fatigue properties and for dissimilar metal welds.
Resumo:
We control the stiffnesses of two dual double cantelevers placed in series to control penetration into a perflurooctyltrichlorosilane monolayer self assembled on aluminium and silicon substrates. The top cantilever which carries the probe is displaced with respect to the bottom cantilever which carries the substrate, the difference in displacement recorded using capacitors gives penetration. We further modulate the input displacement sinusoidally to deconvolute the viscoelastic properties of the monolayer. When the intervention is limited to the terminal end of the molecule there is a strong viscous response in consonance with the ability of the molecule to dissipate energy by the generation of gauche defects freely. When the intervention reaches the backbone, at a contact mean pressure of 0.2GPa the damping disappears abruptly and the molecule registers a steep rise in elastic modulus and relaxation time constant, with increasing contact pressure. We offer a physical explanation of the process and describe this change as due to a phase transition from a liquid like to a solid like state.
Resumo:
This paper deals with the simulation-driven study of the impact of hardened steel projectiles on thin aluminium target plates using explicit finite element analysis as implemented in LS-DYNA. The evaluation of finite element modelling includes a comprehensive mesh convergence study using shell elements for representing target plates and the solid element-based representation of ogivalnosed projectiles. A user-friendly automatic contact detection algorithm is used for capturing interaction between the projectile and the target plate. It is shown that the proper choice of mesh density and strain rate-dependent material properties is crucial as these parameters significantly affect the computed residual velocity. The efficacy of correlation with experimental data is adjudged in terms of a 'correlation index' defined in the present study for which values close to unity are desirable.By simulating laboratory impact tests on thin aluminium plates carried out by earlier investigators, extremely good prediction of experimental ballistic limits has been observed with correlation indices approaching unity. Additional simulation-based parametric studies have been carried out and results consistent with test data have been obtained. The simulation procedures followed in the present study can be applied with confidence in designing thin aluminium armour plates for protection against low calibre projectiles.
Resumo:
The activity of gallium in liquid Ga-Te alloys has been measured at 1120 K using a solid state galvanic cell incorporating yttria-stabilized thoria as the solid electrolyte. The cell can be schematically represented as (−) W,Re,Ga(1)+Ga2O3(s)|(Y2O3) ThO2|Ga-Te(1) + Ga2O3(s), Re, W (+) The activity of tellurium was derived by Gibbs-Duhem integration. The activity of gallium shows negative deviation from Raoult's law for XGa < 0.6 and positive deviation from ideality for XGa > 0.6. The activity of gallium was constant in the composition range 0.73 < XGa < 0.89, indicating liquid state immiscibility in this region. The Gibbs energy of mixing and the concentration-concentration structure factor at long wavelength limit show a minimum at XGa ≈ 0.4, suggesting strong interactions in the liquid phase with formation of ‘Ga2Te3‘-type complexes