999 resultados para dental curing light
Resumo:
The objective of this study was to compare the microhardness of two resin composites (microhybrid and nanoparticles). Light activation was performed with argon ion laser 1.56J (L) and halogen light 2.6J (H) was used as control. Measurements were taken on the irradiated surfaces and those opposite them, at thicknesses of 1, 2 and 3 mm. To evaluate the quality of polymerization, the percentages of maximum hardness were calculated (PMH). For statistical analysis the ANOVA and Tukey tests were used (p <= 0.05). To microhybrid was shown that the hardness with laser was inferior to the hardness achieved with halogen light, for both the 1 mm and 2 mm. The nanoparticles polymerized with laser, presented lower hardness even on the irradiated surface, than the same surface light activated with halogen light. The microhybrid attained a minimum PMH of 80% up to the thickness of 2 mm with halogen light, and with laser, only up to 1 mm. The nanoparticles attained a minimum PMH of 80% up to 3 mm thickness with halogen light and with laser this minimum was not obtained at any thickness. Based on these results, it could be concluded that light activation with argon ion laser is contra-indicated for the studied nanoparticles. Published by Elsevier GmbH.
Resumo:
Background. The use of external sources of energy may accelerate the setting rate of glass ionomer cements (GICs) allowing better initial mechanical properties. Aim. To investigate the influence of ultrasound and halogen light on the microleakage and hardness of enamel adjacent to GIC restorations, after artificial caries challenge. Design. Cavities were prepared in 60 primary canines, restored with GIC, and randomly distributed into three groups: control group (CG), light group (LG) - irradiation with a halogen lightcuring unit for 60 s, and ultrasonic group (UG) application of ultrasonic scaler device for 15 s. All specimens were then submitted to a cariogenic challenge in a pH cycling model. Half of sample in each group were immersed in methylene blue for 4 h and sectioned for dye penetration analysis. The remaining specimens were submitted to Knoop cross-sectional microhardness assessments, and mineral changes were calculated for adjacent enamel. Results. Data were compared using Kruskal-Wallis test and two- way ANOVA with 5% significance. Higher dye penetration was observed for the UG (P < 0.01). No significant mineral changes were observed between groups (P = 0.844). Conclusion. The use of halogen light- curing unit does not seem to interfere with the properties of GICs, whereas the use of ultrasound can affect its marginal sealing.
Resumo:
As várias opções para a realização de tratamentos estéticos conservadores permitem ao profissional a escolha de materiais e técnicas apropriados, que melhor se enquadrem nas características individuais de cada paciente e na realidade de seu consultório. No caso clínico apresentado, a técnica de clareamento dental em consultório com peróxido de hidrogênio a 35% (Total Blanc Office, DFL), ativado com luz híbrida LED/LASER e a microabrasão de esmalte com pasta de acido fosfórico a 37% e pedra pomes, foram associados. Os resultados com o clareamento em consultório são imediatos, de forma que o profissional dispõe de total controle sobre aplicação do gel clareador em áreas e dentes específicos. A microabrasão do esmalte é um tratamento simples e custo relativamente baixo, remove as manchas superficiais do esmalte com preservação de estrutura dental. No caso apresentado, a associação das duas técnicas proporcionou a obtenção de excelente resultado estético em apenas uma sessão de atendimento.
Resumo:
The aim of this study was to evaluate the influence of microstructure and composition of basic alloys on their microshear bond strength (µSBS) to resin luting cement. The alloys used were: Supreme Cast-V (SC), Tilite Star (TS), Wiron 99 (W9), VeraBond II (VBII), VeraBond (VB), Remanium (RM) and IPS d.SIGN 30 (IPS). Five wax patterns (13mm in diameter and 4mm height) were invested, and cast in a centrifugal casting machine for each basic alloy. The specimens were embedded in resin, polished with a SiC paper and sandblasted. After cleaning the metal surfaces, six tygon tubes (0.5 mm height and 0.75 mm in diameter) were placed on each alloy surface, the resin cement (Panavia F) was inserted, and the excess was removed before light-curing. After storage (24 h/37°C), the specimens were subjected to µSBS testing (0.5 mm/min). The data were subjected to a one-way repeated measures analysis of variance and Turkey's test (α=0.05). After polishing, their microstructures were revealed with specific conditioners. The highest µSBS (mean/standard deviation in MPa) were observed in the alloys with dendritic structure, eutectic formation or precipitation: VB (30.6/1.7), TS (29.8/0.9), SC (30.6/1.7), with the exception of IPS (31.1/0.9) which showed high µSBS but no eutectic formation. The W9 (28.1/1.5), VBII (25.9/2.0) and RM (25.9/0.9) showed the lowest µSBS and no eutectic formation. It seems that alloys with eutectic formation provide the highest µSBS values when bonded to a light-cured resin luting cement.
Resumo:
Aiming to compare the effect of different light sources for dental bleaching on vascular permeability of dental pulps, forty-eight incisors were used. The bleaching agent (35 % hydrogen peroxide) was activated by halogen light; LED (Light Emitting Diode) or LED, followed by laser phototherapy (LPT) (λ = 780 nm; 3 J/cm²). After the bleaching procedures, the animals received an intra-arterial dye injection and one hour later were sacrificed. The teeth were diaphanized and photographed. The amount of blue stain content of each dental pulp was quantified using a computer imaging program. The data was statistically compared (p < 0.05). The results showed a significant higher (p < 0.01) dye content in the groups bleached with halogen light, compared with the control, LED and LED plus LPT groups. Thus, tooth bleaching activated by LED or LED plus LPT induces lesser resulted in increased vascular permeability than halogen light.
Resumo:
To investigate the surface hardness (Vickers hardness, HVN) of one light-curing flowable resin composite and five dual-curing resin cements after different polymerization procedures.
Resumo:
The first part of this three-part review on the relevance of laboratory testing of composites and adhesives deals with approval requirements for composite materials. We compare the in vivo and in vitro literature data and discuss the relevance of in vitro analyses. The standardized ISO protocols are presented, with a focus on the evaluation of physical parameters. These tests all have a standardized protocol that describes the entire test set-up. The tests analyse flexural strength, depth of cure, susceptibility to ambient light, color stability, water sorption and solubility, and radiopacity. Some tests have a clinical correlation. A high flexural strength, for instance, decreases the risk of fractures of the marginal ridge in posterior restorations and incisal edge build-ups of restored anterior teeth. Other tests do not have a clinical correlation or the threshold values are too low, which results in an approval of materials that show inferior clinical properties (e.g., radiopacity). It is advantageous to know the test set-ups and the ideal threshold values to correctly interpret the material data. Overall, however, laboratory assessment alone cannot ensure the clinical success of a product.
Resumo:
PURPOSE: To investigate the effect of curing rate on softening in ethanol, degree of conversion, and wear of resin composites. METHOD: With a given energy density and for each of two different light-curing units (QTH or LED), the curing rate was reduced by modulating the curing mode. Thus, the irradiation of resin composite specimens (Filtek Z250, Tetric Ceram, Esthet-X) was performed in a continuous curing mode and in a pulse-delay curing mode. Wallace hardness was used to determine the softening of resin composite after storage in ethanol. Degree of conversion was determined by infrared spectroscopy (FTIR). Wear was assessed by a three-body test. Data were submitted to Levene's test, one and three-way ANOVA, and Tukey HSD test (alpha = 0.05). Results: Immersion in ethanol, curing mode, and material all had significant effects on Wallace hardness. After ethanol storage, resin composites exposed to the pulse-delay curing mode were softer than resin composites exposed to continuous cure (P< 0.0001). Tetric Ceram was the softest material followed by Esthet-X and Filtek Z250 (P< 0.001). Only the restorative material had a significant effect on degree of conversion (P< 0.001): Esthet-X had the lowest degree of conversion followed by Filtek Z250 and Tetric Ceram. Curing mode (P= 0.007) and material (P< 0.001) had significant effect on wear. Higher wear resulted from the pulse-delay curing mode when compared to continuous curing, and Filtek Z250 showed the lowest wear followed by Esthet-X and Tetric Ceram.
Resumo:
Objective: Root canal obliterations may pose esthetic and clinical problems or may even be a risk factor for tooth survival. Microcalcifications in the pulp can be so extensive that the entire root canal system becomes obliterated. Since bone sialoprotein (BSP) and osteopontin (OPN) are involved in both physiological and pathological mineralization processes, our hypothesis was that these two bone-related noncollagenous proteins are present in microcalcifications of the pulp. The purpose of this study was, therefore, to characterize the nature of microcalcifications in the pulp of aged human teeth. Methods: From a large collection of human teeth, 10 were found to exhibit pulpal microcalcifications. The teeth were extracted for periodontal reasons from 39-60 year old patients. After fixation in aldehydes and decalcification, teeth were processed for embedding in LR White resin for analysis in the light and transmission electron microscope. For the detection of BSP and OPN, post-embedding high resolution immunocytochemistry was applied. Results: The microcalcifications were round or elongated, occasionally coalescing, and intensely stained with toluidine blue. Collagen fibrils were found in most but not all microcalcifications. All microcalcifications were immunoreactive for both antibodies and showed an identical labeling pattern. Gold particle labeling was extensively found throughout the interfibrillar ground substance of the microcalcifications, whereas the dentin matrix lacked immunolabeling. Conclusion: BSP and OPN appear to be major matrix constituents of pulp microcalcifications and may thus, like in other mineralized tissues, be involved in their mineralization process.
Resumo:
Grafting of the maxillary sinus in both one- and two-stage protocols has become a highly predictable surgical technique for site development and for the placement of implants to support dentures. However, despite the predictability and high success rates reported for dental implants placed either simultaneously with or after a sinus floor elevation (SFE) procedure, complications have been reported. The aim of the following case report is to present an uncommon complication in a staged SFE procedure: the displacement of a dental implant into the maxillary sinus during insertion. As implant dentistry is becoming more and more popular among practitioners, and ever more demanding procedures for initial site development in jaws with bony deficiencies are being introduced into daily practice, the displacement of dental implants into the maxillary sinus during implant placement may become a more frequent complication. Management of this complication is presented, discussed, and evaluated in light of the current literature.
Resumo:
AIM: The aim of this study was to assess the marginal fit of crowns on the Straumann (ITI) Dental Implant System with special consideration of different casting dental materials. MATERIAL AND METHODS: Sixty porcelain-fused-to-metal crowns were fabricated: 18 crowns on standard cone abutments with an impression cylinder, partially prefabricated analogs, no coping and screw-retained (A); 18 crowns on solid abutments without an impression device, no analogs, no coping and cemented (B); and 18 crowns on solid abutments using an impression transfer cap, an analog with a shoulder, no coping and cemented (C). In each group, six crowns were made on epoxy mastercasts (Bluestar), six on synthetic plaster (Moldasynt) and six on super hard stone (Fujirock). Six additional crowns were fabricated with the transversal screw retention system onto the Octa system with impression transfer caps, metal analogs, gold copings and screw-retained (D). Impregum was used as impression material. Crowns of B and C were cemented with KetacCem. Crowns of A and D were fixed with an occlusal screw torqued at 15 N cm. Crowns were embedded, cut and polished. Under a light microscope using a magnification of x 100, the distance between the crown margin (CM) and the shoulder (marginal gap, MG) and the distance between the CM and the end of the shoulder (crown length, CL) was measured. RESULTS: MGs were 15.4+/-13.2 microm (A), 21.2+/-23.1 microm (B), 11+/-12.1 microm (C) and 10.4+/-9.3 microm (D). No statistically significantly differences using either of the casting materials were observed. CLs were -21.3+/-24.8 microm (A), 3+/-28.9 microm (B), 0.5+/-22 microm (C) and 0.1+/-15.8 microm (D). Crowns were shorter on synthetic casting materials compared with stone casts (P<0.005). CONCLUSIONS: CMs fit precisely with both cemented and screw-retained versions as well as when using no, partial or full analogs.
Resumo:
INTRODUCTION Light cure of resin-based adhesives is the mainstay of orthodontic bonding. In recent years, alternatives to conventional halogen lights offering reduced curing time and the potential for lower attachment failure rates have emerged. The relative merits of curing lights in current use, including halogen-based lamps, light-emitting diodes (LEDs), and plasma arc lights, have not been analyzed systematically. In this study, we reviewed randomized controlled trials and controlled clinical trials to assess the risks of attachment failure and bonding time in orthodontic patients in whom brackets were cured with halogen lights, LEDs, or plasma arc systems. METHODS Multiple electronic database searches were undertaken, including MEDLINE, EMBASE, and the Cochrane Oral Health Group's Trials Register, CENTRAL. Language restrictions were not applied. Unpublished literature was searched on ClinicalTrials.gov, the National Research Register, Pro-Quest Dissertation Abstracts, and Thesis database. Search terms included randomized controlled trial, controlled clinical trial, random allocation, double blind method, single blind method, orthodontics, LED, halogen, bond, and bracket. Authors of primary studies were contacted as required, and reference lists of the included studies were screened. RESULTS Randomized controlled trials and clinical controlled trials directly comparing conventional halogen lights, LEDs, or plasma arc systems involving patients with full arch, fixed, or bonded orthodontic appliances (not banded) with follow-up periods of a minimum of 6 months were included. Using predefined forms, 2 authors undertook independent extraction of articles; disagreements were resolved by discussion. The assessment of the risk of bias of the randomized controlled trials was based on the Cochrane Risk of Bias tool. Ten studies met the inclusion criteria; 2 were excluded because of high risk of bias. In the comparison of bond failure risk with halogen lights and plasma arc lights, 1851 brackets were included in both groups. Little statistical heterogeneity was observed in this analysis (I(2) = 4.8%; P = 0.379). There was no statistical difference in bond failure risk between the groups (OR, 0.92; 95% CI, 0.68-1.23; prediction intervals, 0.54, 1.56). Similarly, no statistical difference in bond failure risk was observed in the meta-analysis comparing halogen lights and LEDs (OR, 0.96; 95% CI, 0.64-1.44; prediction intervals, 0.07, 13.32). The pooled estimates from both comparisons were OR, 0.93; 95% CI, 0.74-1.17; and prediction intervals, 0.69, 1.17. CONCLUSIONS There is no evidence to support the use of 1 light cure type over another based on risk of attachment failure.
Resumo:
AIMS The aims of this double-blind, controlled, crossover study were to assess the influence of food preservatives on in situ dental biofilm growth and vitality, and to evaluate their influence on the ability of dental biofilm to demineralize underlying enamel over a period of 14 days. MATERIALS AND METHODS Twenty volunteers wore appliances with six specimens each of bovine enamel to build up intra-oral biofilms. During four test cycles of 14 days, the subjects had to place the appliance in one of the assigned controls or active solutions twice a day for a minute: negative control 0.9 % saline, 0.1 % benzoate (BA), 0.1 % sorbate (SA) and 0.2 % chlorhexidine (CHX positive control). After 14 days, the biofilms on two of the slabs were stained to visualize vital and dead bacteria to assess biofilm thickness (BT) and bacterial vitality (BV). Further, slabs were taken to determine mineral loss (ML), by quantitative light-induced laser fluorescence (QLF) and transversal microradiography (TMR), moreover the lesion depths (LD). RESULTS Nineteen subjects completed all test cycles. Use of SA, BA and CHX resulted in a significantly reduced BV compared to NaCl (p < 0.001). Only CHX exerted a statistically significant retardation in BT as compared to saline. Differences between SA and BA were not significant (p > 0.05) for both parameters. TMR analysis revealed the highest LD values in the NaCl group (43.6 ± 44.2 μm) and the lowest with CHX (11.7 ± 39.4 μm), while SA (22.9 ± 45.2 μm) and BA (21.4 ± 38.5 μm) lay in between. Similarly for ML, the highest mean values of 128.1 ± 207.3 vol% μm were assessed for NaCl, the lowest for CHX (-16.8 ± 284.2 vol% μm), while SA and BA led to values of 83.2 ± 150.9 and 98.4 ± 191.2 vol% μm, respectively. With QLF for both controls, NaCl (-33.8 ± 101.3 mm(2) %) and CHX (-16.9 ± 69.9 mm(2) %), negative values were recorded reflecting a diminution of fluorescence, while positive values were found with SA (33.9 ± 158.2 mm(2) %) and BA (24.8 ± 118.0 mm(2) %) depicting a fluorescence gain. These differences were non-significant (p > 0.05). CONCLUSION The biofilm model permited the assessment of undisturbed oral biofilm formation influenced by antibacterial components under clinical conditions for a period of 14 days. An effect of BA and SA on the demineralization of enamel could be demonstrated by TMR and QLF, but these new findings have to be seen as a trend. As part of our daily diet, these preservatives exert an impact on the metabolism of the dental biofilm, and therefore may even influence demineralization processes of the underlying dental enamel in situ.
Resumo:
O presente trabalho teve por foco prover uma revisão de conceitos relacionados às resinas dentais fotopolimeráveis e, também, analisar como diferentes concentrações de fotoiniciadores de uso comum em odontologia podem influenciar no desempenho mecânico e na cor de resinas dentais. Concentrações de 0,01%, 0,10%, 0,25% 0,50%, 0,75%, 1,00% e 10% em massa de fotoiniciador foram adicionadas em uma matriz polimérica composta por TEGDMA/BisGMA 50%/50% em massa de forma que, fixando variáveis externas referentes à fonte de luz e à preparação das amostras, foi possível avaliar o efeito da concentração de fotoiniciador nas propriedades mecânicas de resistência à fratura por compressão, resistência à fratura pela aplicação de tensão diametral e dureza Barcol. Por fim, o efeito da concentração na cor aferida através do método CIELab foi investigada. Os fotoiniciadores utilizados foram o Irgacure® 819, a 1-fenil-1,2-propanodiona (PPD) e a Canforoquinona a qual foi utilizada juntamente com ocoiniciador Etil-4 dimetilaminobenzoato (EDB) na concentração constante de 1% em massa. Os resultados mecânicos e de cor foram comparados entre as diferentes amostras através de análises estatísticas (ANOVA) e, especificamente para cor, o parâmetro de diferença de cor (ΔE) foi interpretado verificar se as alterações observadas são perceptíveis ao olho humano. Para fundamentar os estudos, análises do espectro de absorção das amostras, do espectro de irradiação da fonte de luz e do grau de conversão das amostras foram realizadas. Os resultados revelaram que, independentemente do fotoiniciador, graus de conversão da mesma ordem de grandeza de um adesivo comercial foram obtidos, porém as velocidades de reação foram diferentes (maior velocidade para as amostras de CQ e menor para PPD). Curvas características foram obtidas para os espectros de absorção e de irradiação confirmando, pela sobreposição das curvas, que a fonte de luz é efetiva para iniciação da polimerização das amostras. As análises de resistência à fratura revelaram que a quebra catastrófica do material ocorrerá preferencialmente quando a força é aplicada ao longo do diâmetro para os corpos de prova preparados. Quanto à dureza, verificou-se que que para a CQ houve um máximo, para Irgacure um comportamento assintótico com aumento da concentração e, para a PPD, não foi possível a obtenção de amostras (verificado que a PPD necessita de tempo de irradiação superior ao convencionalmente utilizado na prática odontológica). Os testes de ANOVA permitiram verificar que o Irgacure é capaz de fornecer resultados mecânicos semelhante em relação à CQ ocasionando, em contrapartida, um menor escurecimento e amarelamento. Analisando o parâmetro ΔE, confirmou-se que a alteração na cor se torna evidente à medida que ocorre o aumento da concentração de fotoiniciador independentemente do fotoiniciador utilizado, porém a alteração é maior para a CQ.