Resumo:
The selective hydrogenation of nitrobenzene (NB) over Ni/gamma-Al2O3 Catalysts Was investigated using different media of dense phase CO2, ethanol, and n-hexane. In dense phase CO2, the total rate of NB hydrogenation was larger than that in organic solvents under similar reaction conditions; the selectivity to the desired product, aniline, was almost 100% over the whole conversion range of 0-100%. The phase behavior of the reactant mixture in/under dense phase CO2 was examined at reaction conditions. In situ high-pressure Fourier transform infrared measurements were made to study the molecular interactions Of CO2 with the following reactant and reaction intermediates: NB, nitrosobenzene (NSB), and N-phenylhydroxylamine (PHA). Dense phase CO2 strongly interacts with NB, NSB, and PHA, modifying the reactivity of each species and contributing to positive effects on the reaction rate and the selectivity to aniline. A possible reaction pathway for the hydrogenation of NB in/under dense phase CO2 over Ni/gamma-Al2O3 is also proposed.
Resumo:
The surface structure of the iron oxide nanoparticles obtained by the co-precipitation method has been investigated, and a thin layer of alpha-FeOOH absorbed on surface of the nanoparticle is confirmed by analyses of Fourier transform infrared (FTIR), X-ray photoelectron spectra (XPS) and surface photovoltage spectroscopy (SPS). After annealed at 400 degrees C, the alpha-FeOOH can be converted to gamma-Fe2O3. The simple-annealed procedure resulted in the formation of Fe3O4@gamma-Fe2O3 core/shell structure with improved stability and a higher magnetic saturation value, and also the simple method can be used to obtain core/shell structure in other similar system.
Resumo:
Water-soluble supramolecular inclusion complexes of alpha-, beta-, and gamma-cyclodextrin-bicapped C-60 (CD/C-60) have been investigated for their photoinduced DNA cleavage activities, with the aim to assess the potential health risks of this class of compounds and to understand the effect of host cyclodextrins having different cavity dimensions. Factors such as incubation temperature, irradiation time, and concentration of NADH or CDs/C-60 supramolecular inclusion complexes have been examined. The results show that alpha-, beta-, and gamma-CDs/C-60 are all able to cleave double-stranded DNA under visible light irradiation in the presence of NADH. However, a difference in the photoinduced DNA cleavage efficiency is observed, where the cleavage efficiency increases in the order of alpha-, beta-, and gamma-CD/C-60. The difference is attributed to the different aggregation behavior of the inclusion complexes in aqueous solution, which is correlated to the cavity dimension of the host cyclodextrin molecules.
Resumo:
Poly(epsilon-caprolactone) was crosslinked by gamma radiation in the presence of triallyl isocyanurate. The influence of gamma-radiation crosslinking on the thermal and mechanical properties of poly(epsilon-caprolactone)/triallyl isocyanurate was investigated. Differential scanning calorimetry analyses showed differences between the first and second scans. Dynamic mechanical analysis showed an increase in the glass-transition temperature as a result of the radiation crosslinking of poly(epsilon-caprolactone). Thermogravimetric analysis showed that gamma-radiation crosslinking slightly improved the thermal stability of poly(epsilon-caprolactone). The 7 radiation also strongly influenced the mechanical properties. At room temperature, crosslinking by radiation did not have a significant influence on the Young's modulus and yield stress of poly(E-caprolactone). However, the tensile strength at break and the elongation at break generally decreased with an increase in the crosslinking level. When the temperature was increased above the melting point, the tensile strength at break, elongation at break, and Young's modulus of poly(epsilon-caprolactone) were also reduced with an increase in the crosslinking level. The yield stress disappeared as a result of the disappearance of the crystallites.
Resumo:
A new vinyl acyl azide monomer, 4-(azidocarbonyl) phenyl methacrylate, has been synthesized and characterized by NMR and FTIR spectroscopy. The thermal stability of the new monomer has been investigated with FTIR and thermal gravimetry/differential thermal analysis (TG/DTA), and the monomer has been demonstrated to be stable below 50 degrees C in the solid state. The copolymerizations of the new monomer with methyl acrylate have been carried out at room temperature under Co-60 gamma-ray irradiation in the presence of benzyl 1-H-imidazole-1-carbodithioate. The results show that the polymerizations bear all the characteristics of controlled/living free-radical polymerizations, such as the molecular weight increasing linearly with the monomer conversion, the molecular weight distribution being narrow (< 1.20), and a linear relationship existing between In([M](0)/[M]) and the polymerization time. The data from H-1 NMR and FTIR confirm that no change in the acyl azide groups has occurred in the polymerization process and that acyl azide copolymers have been obtained. The thermal stability of the polymers has also been investigated with TG/DTA and FTIR.
Resumo:
An efficient enantioselective catalyst of 5 wt.% Ru/-gamma-Al2O3 modified with R,R-1,2-diphenylethylene-diamine ((R,R)-DPEN) for the hydrogenation of a non-activated aromatic ketone of acetophenone has been investigated, a relatively high enantiomeric excess (ee) of 60.5% was obtained at both the conversion and selectivity larger than 99%, it was about three times higher than the ee values reported up to now for acetophenone hydrogenation with the supported transition metal catalysts modified by chiral reagents. The influences of some reaction parameters such as phosphine ligand, substrate/catalyst/modifier molar ratios, base, solvent, pressure and reaction temperature have been discussed. The chiral modifier of (R,R)-DPEN was very important in controlling the enantioselectivity through adsorption competing with other substrates on the surface of active metal species. The phosphine ligand and base were also important and indispensable in the present reaction.
Resumo:
Herein we report the spectroscopic, electrochemical, TEM and DLS characterizations Of C-60 supramolecular inclusion complexes with alpha-, beta- and gamma-cyclodextrins prepared using anionic C-60. The results indicate that the cyclodextrin itself has little effect on the encapsulated C-60 or on the properties of the inclusion complex. Instead, the cyclodextrin has a significant influence on the aggregation behavior of individual complex in aqueous solution, which in turn affects the property of the supramolecular complex of cyclodextrin and C-60 greatly, As the cavity dimension of cyclodextrin becomes smaller as it changes from gamma-CD to beta-CD, and finally to alpha-CD, it is observed that more aggregation occurs for the corresponding inclusion complex in aqueous solution.
Resumo:
The effect of the gamma-form crystal on the thermal fractionation of a commercial poly(propylene-co-ethylene) (PPE) has been studied by differential scanning calorimetry (DSC) and wide-angle X-ray diffraction (WAXD) techniques. Two thermal fractionation techniques, stepwise isothermal crystallization (SIC) and successive self-nucleation and annealing (SSA), have been used to characterize the molecular heterogeneity of the PPE. The results indicate that the SSA technique possesses a stronger fractionation ability than that of the SIC technique. The heating scan of the SSA fractionated sample exhibits 12 endothermic peaks, whereas the scan of the SIC fractionated sample only shows eight melting peaks. The WAXD observations of the fractionated PPE samples prove that the content of the gamma-form crystals formed during the thermal treatment of the SIC technique is much higher than that of the SSA treatment. The former is 57.4%, whereas the later is 12.6%. The effect of they-form crystals on thermal fractionation ability is discussed.
Resumo:
The results obtained for poly(butylene succinate) (PBS) after Co-60 gamma-ray irradiation, studied by wide-angle X-ray diffraction (WAXD), differential scanning calorimeter (DSC) and polarizing optical microscopy (POM), revealed that the degree of crystallinity, melting temperature and enthalpy decreased with increasing irradiation dose, but that the crystal structure of PBS did not vary when compared to non-irradiated PBS. By using Scherrer equation, small changes occurred in the crystal sizes of L-020, L-110 and L-111. The spherulitic morphology of PBS was strongly dependent on irradiation dose and changed significantly at higher irradiation dosages. The crystallization kinetics of PBS indicated that the Avrami exponent (n) for irradiated PBS was reduced to 2.3, when compared to non-irradiated PBS (3.3).
Resumo:
A novel structural triblock copolymer of poly(gamma-benzyl-L-glutamic acid)-b-poly(ethylene oxide)-b-poly(epsilon-caprolactone) (PBLG-PEO-PCL) was synthesized by a new approach in the following three steps: (1) sequential anionic ring opening polymerization (ROP) of ethylene oxide and epsilon-caprolactone with an acetonitrile/potassium naphthalene initiator system to obtain a diblock copolymer CN-PEO-PCL with a cyano end-group; (2) conversion of the CN end-group into NH2 end-group by hydrogenation to obtain NH2-PEO-PCL; (3) ROP of gamma-benzyl-L-glutamate-N-carboxyanhydrides (Bz-L-GluNCA) with NH2-PEO-PCL as macroinitiator to obtain the target triblock copolymer. The structures from CN-PEO precursor to the triblock copolymers were confirmed by FT-IR and H-1 NMR spectroscopy, and their molecular weights were measured by gel permeation chromatography. The monomer of Bz-L-GluNCA can react almost quantitatively with the amino end-groups of NH2-PEO-PCL macroinitiator by ROP.
Resumo:
A biodegradable two block copolymer, poly(epsilon-caprolactone)-b- poly(gamma-benzyl-L-glutamic acid) (PCL-PBLG) was synthesized successfully by ring-opening polymerization of N-carboxyanhydride of gamma-benzyl-L-glutamate (BLG-NCA) with aminophenyl-terminated PCL as a macroinitiator. The aminophenethoxyl-terminated PCL was prepared via hydrogenation of a 4-nitrophenethoxyl-teminated PCL, which was novelly obtained from the polymerization of c-caprolactone (CL) initiated by amino calcium 4-nitrobenzoxide. The structures of the block copolymer and its precursors from the initial step of PCL were confirmed and investigated by H-1 NMR, FT-IR, GPC, and FT-ICRMS analyses and DSC measurements.
Resumo:
CdS nanocrystals were synthesized through AOT/heptane/H2O reverse micelles. New stable reverse mikelles were obtained by adding an appropriate amount of acrylic. acid monomer, CdS nanocrystal-poly(acrylic acid) composites were synthesized by gamma-radiation with a reverse mi'celle route at room temperature. The US nanocrystals with narrow size distribution were, found to be dispersed homogeneously in the poly(acrylic acid) matrix. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
Mossbauer spectra of Fe-57 in a thick film YBa2(Cu0.97Fe0.03)(3)O7-x irradiated by a large dose of gamma-rays from Co-60 have been measured. The variation of the relative intensities of some subspectra of Fe-57 in the. Mossbauer spectra of the thick film YBa2(Cu0.97Fe0.03)(3)O7-x after irradiation can be observed. This variation indicates that the change of the coordination environment around some Fe atoms in the lattice occurs due to irradiation. The relative intensity of subspectrum D1(Fe) at the Cu(1) site decreases and that of subspectrum D4(Fe) at the Cu(1) site increases. This may be because of the possible oxygen atom hopping between the coordination environments of D1(Fe) and D4(Fe) in the lattice caused by irradiation. The effect of irradiation on the coordination environment around the Fe atom at the Cu(2) site is not appreciable. (C) 1997 Elsevier Science B.V.
Resumo:
Irradiation can be applied to crosslink the dispersed elastomer phase to increase the modulus and decrease the voiding ability of the elastomer, which results in increasing critical brittle-tough transition elastomer content at constant temperature. The experimental results show that at 25 degrees C the critical elastomer content of EPDM shifts to higher composition (shift of about 4 wt%) for PBT/EPDM blends after 100 kGy gamma-irradiation. (C) 1997 Elsevier Science Ltd.