998 resultados para Dental adhesive systems


Relevância:

80.00% 80.00%

Publicador:

Resumo:

The aim of this study was to assess, using the DPPH assay, the antioxidant activity of several substances that could be proposed to immediately revert the problems caused by bleaching procedures. The percentage of antioxidant activity (AA%) of 10% ascorbic acid solution (AAcidS), 10% ascorbic acid gel (AAcidG), 10% sodium ascorbate solution (SodAsS), 10% sodium ascorbate gel (SodAsG), 10% sodium bicarbonate (Bicarb), Neutralize® (NE), Desensibilize® (DES), catalase C-40 at 10 mg/mL (CAT), 10% alcohol solution of alpha-tocopherol (VitE), Listerine® (LIS), 0.12% chlorhexidine (CHX), Croton Lechleri (CL), 10 % aqueous solution of Uncaria Tomentosa (UT), artificial saliva (ArtS) and 0.05% sodium fluoride (NaF) was assessed in triplicate by 2,2-diphenyl-1-picryl-hydrazyl-hydrate (DPPH) free radical assay. All substances exhibited antioxidant activity, except for CL. AAcidS, AAcidG and VitE exhibited the highest AA% (p<0.05). On the contrary, CHX, NE, LIS and NaF showed the lowest AA% (p<0.05). In conclusion, AAcidS, AAcidG, SodAsS, SodAsG and VitE presented the highest antioxidant activity among substances tested in this study. The DPPH assay provides an easy and rapid way to evaluate potential antioxidants.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The purpose of this study was to determine the effects of contamination with smoker's and non-smoker's saliva on the bond strength of resin composite to superficial dentin using different adhesive systems. The interfacial structure between the resin and dentin was evaluated for each treatment using environmental scanning electron microscopy (ESEM). Freshly extracted human molars were ground with 600-grit SiC paper to expose the superficial dentin. Adhesives [One-Up-Bond-F-Plus (OUFP) and Adper-Prompt-L-Pop (APLP)] and resin composite (TPHSpectrum) were bonded to the dentin (n = 8/group, 180 total specimens) under five surface conditions: control (adhesive applied following manufacturers' instructions); saliva, then 5-s air dry, then adhesive; adhesive, saliva, 5-s air dry; adhesive, saliva, 5-s water rinse, 5-s air dry (ASW group); and adhesive, saliva, 5-s water rinse, 5-s air dry, reapply adhesive (ASWA group). After storage in water at 37 degrees C for 24 h, the specimens were debonded under tension at a speed of 0.5 mm/min. ESEM photomicrographs of the dentin/adhesive interfaces were taken. Mean bond strength ranged from 8.1 to 24.1 MPa. Fisher's protected least significant difference (P = 0.05) intervals for critical adhesive, saliva, and surface condition differences were 1.3, 1.3, and 2.1 MPa, respectively. There were no significant differences in bond strength to dentin between contamination by smoker's and nonsmoker's saliva, but bond strengths were significantly different between adhesive systems, with OUFP twice as strong as APLP under almost all conditions. After adhesive application and contamination with either smoker's or nonsmoker's saliva followed by washing and reapplication of the adhesive (ASWA group), the bond strength of both adhesive systems was the same as that of the control group.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

This project was comparing the accuracy of capturing the oral pathology diagnoses among different coding systems. 55 diagnoses were selected for comparison among 5 coding systems. The results of accuracy in capturing oral diagnoses are: AFIP (96.4%), followed by Read 99 (85.5%), SNOMED 98 (74.5%), ICD-9 (43.6%), and CDT-3 (14.5%). It shows that the currently used coding systems, ICD-9 and CDT-3, were inadequate, whereas the AFIP coding system captured the majority of oral diagnoses. In conclusion, the most commonly used medical and dental coding systems lack terms for the diagnosis of oral and dental conditions.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Laser irradiation has numerous favorable characteristics, such as ablation or vaporization, hemostasis, biostimulation (photobiomodulation) and microbial inhibition and destruction, which induce various beneficial therapeutic effects and biological responses. Therefore, the use of lasers is considered effective and suitable for treating a variety of inflammatory and infectious oral conditions. The CO2 , neodymium-doped yttrium-aluminium-garnet (Nd:YAG) and diode lasers have mainly been used for periodontal soft-tissue management. With development of the erbium-doped yttrium-aluminium-garnet (Er:YAG) and erbium, chromium-doped yttrium-scandium-gallium-garnet (Er,Cr:YSGG) lasers, which can be applied not only on soft tissues but also on dental hard tissues, the application of lasers dramatically expanded from periodontal soft-tissue management to hard-tissue treatment. Currently, various periodontal tissues (such as gingiva, tooth roots and bone tissue), as well as titanium implant surfaces, can be treated with lasers, and a variety of dental laser systems are being employed for the management of periodontal and peri-implant diseases. In periodontics, mechanical therapy has conventionally been the mainstream of treatment; however, complete bacterial eradication and/or optimal wound healing may not be necessarily achieved with conventional mechanical therapy alone. Consequently, in addition to chemotherapy consisting of antibiotics and anti-inflammatory agents, phototherapy using lasers and light-emitting diodes has been gradually integrated with mechanical therapy to enhance subsequent wound healing by achieving thorough debridement, decontamination and tissue stimulation. With increasing evidence of benefits, therapies with low- and high-level lasers play an important role in wound healing/tissue regeneration in the treatment of periodontal and peri-implant diseases. This article discusses the outcomes of laser therapy in soft-tissue management, periodontal nonsurgical and surgical treatment, osseous surgery and peri-implant treatment, focusing on postoperative wound healing of periodontal and peri-implant tissues, based on scientific evidence from currently available basic and clinical studies, as well as on case reports.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Purpose: To investigate the effect of airborne-particle abrasion or diamond bur preparation as pretreatment steps of non-carious cervical root dentin regarding substance loss and bond strength. Methods: 45 dentin specimens produced from crowns of extracted human incisors by grinding the labial surfaces with silicon carbide papers (control) were treated with one of three adhesive systems (Group 1A-C; A: OptiBond FL, B: Clearfil SE Bond, or C: Scotchbond Universal; n=15/adhesive system). Another 135 dentin specimens (n=15/group) produced from the labial, non-carious cervical root part of extracted human incisors were treated with one of the adhesive systems after either no pre-treatment (Group 2A-C), pre-treatment with airborne-particle abrasion (CoJet Prep and 50 µm aluminum oxide powder; Group 3A-C), or pre-treatment with diamond bur preparation (40 µm grit size; Group 4A-C). Substance loss caused by the pre-treatment was measured in Groups 3 and 4. After treatment with the adhesive systems, resin composite was applied and all specimens were stored (37°C, 100% humidity, 24 hours) until measurement of microshear bond strength (µSBS). Data were analyzed with a nonparametric ANOVA followed by Kruskal-Wallis and Wilcoxon rank sum tests (level of significance: alpha=0.05). Results: Overall substance loss was significantly lower in Group 3 (median: 19 µm) than in Group 4 (median: 113 µm; p<0.0001). There were no significant differences in µSBS between the adhesive systems (A-C) in Group 1, Group 3, and Group 4 (p>=0.133). In Group 2, OptiBond FL (Group 2A) and Clearfil SE Bond (Group 2B) yielded significantly higher µSBS than Scotchbond Universal (Group 2C; p<=0.032). For OptiBond FL and Clearfil SE Bond, there were no significant differences in µSBS between the ground crown dentin and the non-carious cervical root dentin regardless of any pre-treatment of the latter (both p=0.661). For Scotchbond Universal, the µSBS to non-carious cervical root dentin without pre-treatment was significantly lower than to ground crown dentin and to non-carious cervical root dentin pre-treated with airborne-particle abrasion or diamond bur preparation p<=0.014).

Relevância:

80.00% 80.00%

Publicador:

Resumo:

A utilização de espigões em dentes tratados endodonticamente é um dos temas mais estudados em Medicina Dentária. As opiniões são divergentes em relação aos procedimentos clínicos e materiais a serem utilizados para a colocação e remoção de espigões. O objetivo deste trabalho foi realizar uma revisão bibliográfica de forma a organizar conceitos e princípios clínicos para melhor esclarecer os fatores que determinam a necessidade de colocação, utilização e escolha do tipo de espigão, sua cimentação e técnicas para a remoção. Foram analisadas as características e propriedades dos cimentos de fosfato de zinco, ionômero de vidro, cimentos resinosos de polimerização química, polimerização dupla, foto-polimerizável e os sistemas adesivos etch and rinse, self etch e autoadesivos, bem como as técnicas para a remoção de espigões cimentados com diferentes cimentos e sistemas adesivos para depois acessar o remanescente de guta percha para o retratamento endodôntico. Foi feita uma pesquisa bibliográfica na base de dados electrónica PubMed, Google Scholar e RCAAP com as seguintes palavras chave: “Espigões”; “Retratamento Endodôntico”; “Ionómero de Vidro”; “Fosfato de Zinco”; “Cimentos Resinosos”; “Posts”; “Endodontic Retreatment”; “Glass Ionomer”; Zinc-phosphate”; “Resin Cements"; “Push Out Test”; “Posts AND Removal”. Concluiu-se que a cimentação de espigões pré-fabricados de fibra de vidro com cimentos resinosos de dupla polimerização associados aos sistemas adesivos self etch estão gradualmente substituindo os outros tipos de espigões e demais cimentos e possibilitam restaurar o dente de forma adequada e duradoura. E o uso de ultrassons apresenta maior eficácia e segurança na remoção dos espigões.

Relevância:

50.00% 50.00%

Publicador:

Resumo:

Stress distributions in torsion and wire-loop shear tests were compared using three-dimensional (3-D) linear-elastic finite element method, in an attempt to predict the ideal conditions for testing adhesive strength of dental resin composites to dentin. The torsion test presented lower variability in stress concentration at the adhesive interface with changes in the proportion adhesive thickness/resin composite diameter, as well as lower variability with changes in the resin composite elastic modulus. Moreover, the torsion test eliminated variability from changes in loading distance, and reduced the cohesive fracture tendency in the dentin. The torsion test seems to be more appropriate than wire-loop shear test for testing the resin composite-tooth interface strength. (c) Koninklijke Brill NV, Leiden, 2009

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The development and maintenance of the sealing of the root canal system is the key to the success of root canal treatment. The resin-based adhesive material has the potential to reduce the microleakage of the root canal because of its adhesive properties and penetration into dentinal walls. Moreover, the irrigation protocols may have an influence on the adhesiveness of resin-based sealers to root dentin. The objective of the present study was to evaluate the effect of different irrigant protocols on coronal bacterial microleakage of gutta-percha/AH Plus and Resilon/Real Seal Self-etch systems. One hundred ninety pre-molars were used. The teeth were divided into 18 experimental groups according to the irrigation protocols and filling materials used. The protocols used were: distilled water; sodium hypochlorite (NaOCl)+eDTA; NaOCl+H3PO4; NaOCl+eDTA+chlorhexidine (CHX); NaOCl+H3PO4+CHX; CHX+eDTA; CHX+ H3PO4; CHX+eDTA+CHX and CHX+H3PO4+CHX. Gutta-percha/AH Plus or Resilon/Real Seal Se were used as root-filling materials. The coronal microleakage was evaluated for 90 days against Enterococcus faecalis. Data were statistically analyzed using Kaplan-Meier survival test, Kruskal-Wallis and Mann-Whitney tests. No significant difference was verified in the groups using chlorhexidine or sodium hypochlorite during the chemo-mechanical preparation followed by eDTA or phosphoric acid for smear layer removal. The same results were found for filling materials. However, the statistical analyses revealed that a final flush with 2% chlorhexidine reduced significantly the coronal microleakage. A final flush with 2% chlorhexidine after smear layer removal reduces coronal microleakage of teeth filled with gutta-percha/AH Plus or Resilon/Real Seal SE.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

A study was performed in order to determine the efficiency of the simultaneous use of the photoinitiators phenylpropanedione (PPD) and camphorquinone (CQ) in the polymerization of acrylic polymers and evaluate possible mechanisms leading to synergism or antagonism. It was found that efficiencies of both initiators taken individually are higher than that of their mixture, indicating that when both dyes are used simultaneously there will be an energy transfer from the more efficient initiator (CQ) to the less efficient one (PPD). Also, there was no proof of any reaction between the amine present in the CQ formulation and the PPD excited state.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The present study investigated the distribution profile of dental caries and its association with areas of social deprivation at the individual and contextual level. The cluster sample consisted of 1,002 12-year-old schoolchildren from Piracicaba, SP, Brazil. The DMFT Index was used for dental caries and the Care Index was used to determine access to dental services. On the individual level, variables were associated with a better oral status. On the contextual level, areas were not associated with oral status. However, maps enabled determining that the central districts have better social and oral conditions than the deprived outlying districts.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Purpose: The aim of this study was to detect the influence of (1) storage period of heparinized blood, (2) type of blood and presence of contaminant, (3) application mode of cleansing agents, and (4) efficacy of cleansing agents on contaminated enamel and dentin during the adhesion process of a one-step adhesive system. Materials and Methods: One hundred four human molars were sectioned into halves along the long axis for enamel and dentin tests. Heparinized and fresh blood were obtained from the same donor, applied and dried to maintain a layer of dry blood on the top of samples. The cleansing agents used were hydrogen peroxide, anionic detergent, and antiseptic solution. A one-step adhesive system (Clearfil S3 Bond) was applied on the dental surface, and composite resin cylinders were built up using Tygon tubing molds. After 24 h, the mu SBS test (1 mm/min) and fracture analysis were performed. Results: There was no statistically significant difference in bond strength values regarding the storage period of heparinized blood and the types of blood. Groups without contamination presented higher bond strengths than contaminated groups. The application mode of the cleansing agents had no influence on bond strength results. There was no statistically significant difference among cleansing agents and they were as effective as a water stream in counteracting the effect of blood contamination. Conclusion: Heparinized blood can be used as a contaminant for up to one week, and it is a reliable procedure to standardize the contaminant. The cleansing agents can be used without friction. A water stream is sufficient to remove blood contamination from dental tissues, before the application of a one-step adhesive system.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Purpose: To evaluate the flexural strength of two fixed dental prosthesis (FDP) designs simulating frameworks of adhesive fixed partial prostheses, reinforced or not by glass fiber.Materials and Methods: Forty specimens, made with composite resin, were divided into 4 groups according to the framework design and the presence of fiber reinforcement: A1 - occlusal support; A2: occlusal support + glass fiber; B1: occlusal and proximal supports; B2: occlusal and proximal supports + glass fiber. The specimens were subjected to the three-point bending test, and the data were submitted to two-way ANOVA and Tukey's test (5%).Results: Group A2 (97.9 +/- 38 N) was statistically significantly different from all other experimental groups, presenting a significantly lower mean flexural strength.Conclusion: The use of glass fibers did not improve the flexural strength of composite resin, and designs with occlusal and proximal supports presented better results than designs simulating only occlusal support.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Purpose: This study evaluated the efficacy of the union between two new self-etching self-adhesive resin cements and enamel using the microtensile bond strength test.Materials and Methods: Buccal enamel of 80 bovine teeth was submitted to finishing and polishing with metallographic paper to a refinement of #600, in order to obtain a 5-mm(2) flat area. Blocks (2 x 4 x 4 mm) of laboratory composite resin were cemented to enamel according to different protocols: (1) untreated enamel + RelyX Unicem cement (RX group); (2) untreated enamel + Bifix SE cement (BF group); (3) enamel acid etching and application of resin adhesive Single Bond + RelyX Unicem (RXA group); (4) enamel acid etching and application of resin adhesive Solobond M + Bifix SE (BFA group). After 7 days of storage in distillated water at 37 degrees C, the blocks were sectioned for obtaining microbar specimens with an adhesive area of 1 mm(2) (n = 120). Specimens were submitted to the microtensile bond strength test at a crosshead speed of 0.5 mm/min. The results (in MPa) were analyzed statistically by ANOVA and Tu key's test.Results: Enamel pre-treatment with phosphoric acid and resin adhesive (27.9 and 30.3 for RXA and BFA groups) significantly improved (p <= 0.05) the adhesion of both cements to enamel compared to the union achieved with as-polished enamel (9.9 and 6.0 for RX and BF).Conclusion: Enamel pre-treatment with acid etching and the application of resin adhesive significantly improved the bond efficacy of both luting agents compared to the union achieved with as-polished enamel.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Objectives. This study compared the durability of repair bond strength of a resin composite to a reinforced ceramic after three repair systems.Methods. Alumina-reinforced feldspathic ceramic blocks (Vitadur-alpha(R)) (N=30) were randomly divided into three groups according to the repair method: PR-Porcelain Repair Kit (Bisco) [etching with 9.5% hydrofluoric acid + silanization + adhesive]; CJ-CoJet Repair Kit (3M ESPE) [(chairside silica coating with 30 mu m SiO2 + silanization (ESPE(R)-Sil) + adhesive (Visio(TM)-Bond)]; CL-Clearfil Repair Kit [diamond surface roughening, etching with 40% H3PO4 + Clearfil Porcelain Bond Activator + Clearfil SE Bond)]. Resin composite was photo-polymerized on each conditioned ceramic block. Non-trimmed beam specimens were produced for the microtensile bond strength (mu TBS) tests. In order to study the hydrolytic durability of the repair methods, the beam specimens obtained from each block were randomly assigned to two conditions. Half of the specimens were tested either immediately after beam production (Dry) or after long-term water storage (37 degrees C, 150 days) followed by thermocyling (12,000 cycles, 5-55 degrees C) in a universal testing machine (1 mm/min). Failure types were analyzed under an optical microscope and SEM.Results. mu TBS results were significantly affected by the repair method (p=0.0001) and the aging conditions (p=0.0001) (two-way ANOVA, Tukey's test). In dry testing conditions, PR method showed significantly higher (p < 0.001) repair bond strength (19.8 +/- 3.8 MPa) than those of CJ and CL (12.4 +/- 4.7 and 9.9 +/- 2.9, respectively). After long-term water storage and thermocycling, CJ revealed significantly higher results (14.5 +/- 3.1 MPa) than those of PR (12.1 +/- 2.6 MPa) (p < 0.01) and CL (4.2 +/- 2.1 MPa) (p < 0.001). In all groups when tested in dry conditions, cohesive failure in the composite accompanied with adhesive failure at the interface (mixed failures), was frequently observed (76%, 80%, 65% for PR, CJ and CL, respectively). After aging conditions, while the specimens treated with PR and CJ presented primarily mixed failure types (52% and 87%, respectively), CL group presented mainly complete adhesive failures at the interface (70%).Significance. Hydrolytic stability of the repair method based on silica coating and silanization was superior to the other repair strategies for the ceramic tested. (C) 2009 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.