975 resultados para ALKALI BORATE GLASSES
Resumo:
A new lead fluoroborate glass (PbO-PbF2-B2O3) doped with ytterbium (Yb:PbFB) is presented. Samples with different concentrations of Yb3+ were produced and had their emission cross-sections, fluorescence lifetimes and minimum pump intensities determined. They have high refractive index of 2.2 and a density of 4.4 g/cm(3). For a doping level of 1.153x10(20) ions/cm(3), the fluorescence lifetime, after excitation at 968 nm, is 0.81 ms, which is comparable to Yb:tellurite laser glass. Also, an emission band at 1022 nm is measured with emission cross-section of approximately 1.07x10(-20) cm(2) and fluorescence effective linewidth of 60 nm, which is comparable to Yb:phosphate laser glass. (C) 2001 Optical Society of America.
Resumo:
The synthesis, characterization and ethylene polymerization behavior of a set of Tp'MCl3 complexes (4, M = Ti, Tp' HB(3-neopentyl-pyrazolyl)(3)(-) (Tp(NP)); 5, M = Ti, Tp'= HB(3-tert-butyl-pyrazolyl)(3)(-) (Tp(tBu)); 6, M = Ti, Tp' = HB(3-phenyl-pyrazolyl)(3)(-) (Tp(Ph)); 7, M = Zr, Tp' = HB(3-phenyl-pyrazolyl)(3)(-) (Tp(ph)); 8, M = Zr, Tp' = HB(3-tert-butyl-pyrazolyl)(3)(-) (Tp(tBu))) is described. Treatment of these tris(pyrazolyl)borate Group IV compounds with methylalumoxane (MAO) generates active catalysts for ethylene polymerization. For the polymerization reactions performed in toluene at 60 degreesC and 3 atm of ethylene pressure, the activities varied between 1.3 and 5.1 X 10(3) g of PE/mol[M](.)h. The highest activity is reached using more sterically open catalyst precursor 4. The viscosity-average molecular weights ((M-v) over bar) of the PE's produced with these catalyst precursors varying from 3.57 to 20.23 x 10(5) gmol(-1) with melting temperatures in the range of 127-134 degreesC. Further polymerization studies employing 7 varying Al/Zr molar ratio and temperature of polymerization showed that the activity as well as the polymer properties are dependent on these parameters. In that case, higher activity was attained at 60 degreesC. The viscosity-average molecular weights of the polyethylene's decreases with increasing AI/Zr molar ratio. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
The mechanism involved in the Tm3+ (F-3(4))-->Ho3+ (I-5(7)) energy transfer and Tm3+ (H-3(4), H-3(6))-->Tm3+ (F-3(4), F-3(4)) cross relaxation as a function of the donor and acceptor concentrations was investigated in Tm-Ho-codoped fluorozirconate glasses. The experimental transfer rates were determined for the Tm-->Ho energy transfer from the best fit of the acceptor luminescence decay using an expression which takes into account the Inokuti-Hirayama model and localized donor-to-acceptor interaction solution. The original acceptor solution derived from the Inokuti-Hirayama model fits well the acceptor luminescence transient only for low-concentrated systems. The results showed that a fast excitation diffusion that occurs in a very short time (t<
Resumo:
Solid-state M-4-Cl-BP compounds, where M stands for bivalent Mg, Ca, Sr, Ba and 4-Cl-BP is 4-chlorobenzylidenepyruvate, have been synthesized. Simultaneous thermogravimetry-differential thermal analysis (TG-DTA), differential scanning calorimetry (DSC), infrared spectroscopy, elemental analysis and complexometry were used to characterize and to study the thermal behaviour of these compounds. The results led to informations about the composition, dehydration, thermal stability and thermal decomposition of the isolated complexes.
Resumo:
Sodium phosphoniobate glasses with the composition (mol%) 75NaPO(3)-25Nb(2)O(5) and containing 2 mol% Yb3+ and x mol% Er3+ (0.01 <= x <= 2) were prepared using the conventional melting/casting process. Er3+ emission at 1.5 mu m and infrared-to-visible upconversion emission, upon excitation at 976 nm, are evaluated as a function of the Er3+ concentration. For the lowest Er3+ content, 1.5 mu m emission quantum efficiency was 90%. Increasing the Er3+ concentration up to 2 mol%, the emission quantum efficiency was observed to decrease to 37% due to concentration quenching. The green and red upconversion emission intensity ratio was studied as a function of Yb3+ co-doping and the Er3+-Er3+ energy transfer processes. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Glass ionomer cements (GICs) are glass and polymer composite materials. These materials currently find use in the dental field. The purpose of this work is to obtain systems based on composition 4.5SiO(2)-3Al(2)O(3)-XNb2O5-2CaO to be used in Dentistry. The systems were prepared by chemical route at 700 degrees C. The results obtained by XRD and DTA showed that all systems prepared are glasses. The structures of the obtained glasses were compared to commercial material using Al-27 and Si-29 MAS NMR. The analysis of MAS NMR spectra indicated that the systems developed and commercial material are formed by SiO4 and AlO4 linked tetrahedra. The properties of glass ionomer cements based on the glasses prepared with several niobium contents were studied. Setting and working times of the cement pastes, microhardness and diametral tensile strength were evaluated for the experimental GICs and commercial luting cements. It was concluded that setting time of the cement pastes increased with increasing niobium content of the glasses (X). The properties to the GICs such as setting time and microhardness were influenced by niobium content. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
\A new class of tungstate fluorophosphate glasses was identified in the NaPO3-BaF2-WO3 ternary system. The variation of several physical properties was determined with respect to chemical composition. Characteristic temperatures, density and refractive index increase as tungsten oxide content increases. The optical transmission range and specially the energy bandgap depend of the WO3 amount. No crystallization could be observed for the Most WO3 concentrated vitreous samples (greater than or equal to20% molar). Color and optical properties of the glasses depend of the melting time because of the presence of reduced tungsten species like W5+ and W4+. In addition, photodarkening is observed in tungsten rich glass samples under UV laser illumination and this phenomenon can be reversible by heat treatment near the glass transition temperature. (C) 2004 Published by Elsevier B.V.
Resumo:
The presence of tin in the network of silicate glasses produces changes in several of their physico-chemical properties. Glasses with the composition (mol%) 22Na(2)O (.) 8CaO (.) 70SiO(2) containing up to 5 wt% of SnO2 were analyzed under several experimental techniques. Dilatometric measurements showed an increase of the glass transition temperature with increasing tin content, while the average thermal expansion coefficient is reduced. Vickers microhardness, density, and refractive index also increase with the tin content. Diffuse reflectance spectra in the infrared (DRIFT) showed that the presence of tin, even at low concentrations, is responsible for some structural changes since there is an increase of the bridging oxygen concentration. The doped glasses present a brown color and optical absorption spectra measurements are interpreted as being due to precipitation of tin in the form of colloidal particles during cooling of the melted glass. In the Na+ <-> K+ ion exchange process the presence of tin in the glass network hinders the diffusion of these ions. The diffusion coefficients of those ions were calculated by the Boltzmann-Matano technique, after concentration profiles obtained by EDS measurements. All results obtained present evidences that Sn4+ cation acts as a glass network former. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Luminescence data for Eu3+ and Gd3+ in fluoroindate glasses are compared to those of a fluorozirconate glass. Emission is observed from Eu3+ 5D(J) (J = 0, 1, 2 and 3) and Gd3+ P-6(7/2) excited-state levels and the results put in evidence Eu-Eu and Gd-Eu energy transfer processes. Vibronic bands related to a 320 cm-1 vibrational mode could be observed for Eu3+ luminescent transitions with DELTAJ = 0, 1 and 2 and also for the P-6(7/2) --> S-8(7/2) transition of Gd3+. Lanthanide ion site symmetry is closer to an inversion center in fluoroindate glasses than it is in fluorozirconate.
Resumo:
We study e+-Na, e+-K, and e+-Rb scattering using the close coupling approach in the static and coupled static expansion schemes. We calculate partial wave elastic scattering phase shifts and total elastic and Ps formation cross sections up to an incident positron energy of 100 eV. The effect of the positronium formation channel on the elastic channel is found to be strong in all cases up to an incident positron energy of 10 eV. We also make an estimate of the total cross section which exhibits a minimum as a function of energy at low energies.
Resumo:
SnO2 coatings were deposited by a sol-gel dip-coating process to shield fluoroindate glasses (40In-F-3:16BaF(2):20SrF(2):20ZnF(2):2NaF:2GaF(3)) against corrosion in aqueous environments. The effect of the number of coating applications and of the withdrawal speed on the thickness, density and roughness of tin oxide films was investigated by X-ray reflectivity. Film thickness increases both with the number of coating applications and the withdrawal speed. The aqueous leaching of uncoated and SnO2-coated fluoroindate glasses was studied by scanning electron microscopy (SEM) and infrared spectroscopy (FTIR), showing that the glass surface was protected against hydrolytic attack. (C) 1999 Elsevier B.V. B.V. All rights reserved.
Resumo:
Temperature and frequency dependence of the F-19 nuclear spin relaxation of the fluoroindate glass, 40InF(3)-20ZnF(2)- 20SrF(2)-2GaF(3)-2NaF-16BaF(2) and the fluorozirconate glass, 50ZrF(4)-20BaF(2)-21LiF-5LaF(3)-4AlF(3); are reported. Measurements were undertaken on pure and Gd3+ doped samples, in the temperature range of 185-1000 K, covering the region below and above the glass transition temperature, T-g. The temperature and frequency dependence of the spin-lattice relaxation rate, T-1(-1), measured in the glassy state at temperature <300 K, is less than the observed dependence at higher temperatures. At temperatures >T-g, the fluorine mobility increases, leading to a more efficient spins lattice relaxation process. Activation energies, for F- motion, are 0.8 eV for the fluoroindate glass and 1 eV for the fluorozirconate glass. The addition of Gd3+ paramagnetic impurities;at 0.1-wt%, does not alter the temperature and frequency dependence of T-1(-1), but increases its magnitude more than one order of magnitude. At temperatures <400 K, the spin-spin relaxation time, T-2(-1), measured for all samples, is determined by the rigid-lattice nuclear dipole-dipole coupling, and it is temperature independent within the accuracy of the measurements. Results obtained for the pure glass, at temperatures >400 K, show that T-2(-1) decreases monotonically as the temperature increases. This decrease is explained as a consequence of the motional narrowing effect caused by the onset of the diffusive motion of the F- ions, with an activation energy around 0.8 eV. For the doped samples, the hyperfine interaction with the paramagnetic impurities is most effective in the relaxation of the nuclear spin, causing an increase in the T(2)(-1)s observed at temperatures >600 K. (C) 1999 Elsevier B.V. B.V. All rights reserved.
Resumo:
Efficient energy upconversion of cw radiation at 1.064 mum into blue, red, and near infrared emission in Tm3+-doped Yb3+-sensitized 60TeO(2)-10GeO(2)-10K(2)O-10Li(2)O-10Nb(2)O(5) glasses is reported. Intense blue upconversion luminescence at 485 nm corresponding to the Tm3+ (1)G(4)--> H-3(6) transition with a measured absolute power of 0.1 muW for 800 mW excitation power at room temperature is observed. The experimental results also revealed a sevenfold enhancement in the upconversion efficiency when the sample was heated from room temperature to 235 degreesC yielding 0.7 muW of blue absolute fluorescence power for 800 mW pump power. High brightness emission around 800 nm (F-3(4)--> H-3(6)) in addition to a less intense 655 nm ((1)G(4)--> H-3(4) and F-3(2,3)--> H-3(6)) fluorescence is also recorded. The energy upconversion excitation mechanism for thulium emitting levels is assigned to multiphonon-assisted anti-Stokes excitation of the ytterbium-sensitizer followed by multiphonon-assisted sequential energy-transfer processes. (C) 2001 American Institute of Physics.
Resumo:
A soft chemistry route is described to obtain glasses in the P2O5-Na2O-ZnO-H2O. It is based on the addition of zinc salts to coacervates prepared from sodium polyphosphate. The processing of these coacervates leads to polyphosphate glasses with the same properties as those of glasses prepared in the classical way. So far, little work has been implemented in this system using 'coacervate route'. However, it makes an attractive method for coating and joining processes on the industrial scale. As the anion associated to zinc may take part in the adhesion mechanism, coacervate formation has been studied using zinc chloride, nitrate and sulphate as starting materials. The physical properties of the glasses obtained by this method are reported and potential applications of zinc and silver coacervate are described. (C) 2002 Academie des sciences / Editions scientifiques et medicales Elsevier SAS.
Resumo:
Irreversible photoexpansion and photobleaching effect has been observed in amorphous Ga10Ge25S65 glass when its surface was exposed to light with energy greater than the band gap, 3.52 eV. The magnitude of the expansion of GaGeS glasses depends on the exposure conditions. Extended X-ray absorption fine structure (EXAFS) spectroscopy and Rutherford backscattering spectrometry (RBS) have been used to identify the chemical nature of the glass samples before and after illumination. The quantitative analysis of the EXAFS data leads to a two-shell model of 0.5 oxygen atoms at 2.01 Angstrom and 3.6 sulfur atoms at a 2.20 Angstrom. RBS technique demonstrated that chemical composition of the glass surface after irradiation is oxygen rich. The existence of Ge-O bonds in the glass after illumination was also confirmed by infrared measurements. (C) 2002 Elsevier B.V. B.V. All rights reserved.