Resumo:
Sulfonated poly(ether ether ketone) (SPEEK) and aminopropyltriethoxysilane (KH550) hybrid membranes doped with different weight ratio of phosphotungstic acid (PWA) were prepared by the casting procedure, as well as PWA as a catalyst for sol-gel process of KH550. The chemical structures of hybrid membranes were characterized by energy dispersive X-ray spectrometry (EDX) and Fourier transform infrared spectroscopy (FTIR). The morphology of hybrid membranes was investigated by scanning electron microscopy (SEM) and atomic force microscopy (AFM). The results had proved the uniform and homogeneous distribution of KH550 and PWA in these hybrid membranes.
Resumo:
A novel selenium source was developed to synthesize the size-controlled CdSe nanocrystals with relatively narrow size distribution successfully in a two-phase thermal approach. A highly reactive and aqueous soluble selenium source was provided by the reduction of selenite, and in this route the size of the nanocrystals can be adjusted by the reaction temperature and time. The size, crystalline structure and optical characteristics of these nanocrystals were investigated by transmission electron microscopy, X-ray powder diffraction, X-ray photoelectron spectroscopy, UV-vis spectroscopy, and photoluminescence spectroscopy. The influence factors for this approach were also discussed.
Resumo:
Langmuir-Blodgett (LB) films of octadecylammonium octadecanoate (C(18)H(37)j7NH(3)(+)C(17)H(35)COO(-),ODASA) and octadecylammonium octadecanoate-d(35) (C18H37+NH3+C17D35COO-, ODASA-d(53)) were prepared and their thermal behaviors were investigated by variable-temperature Fourier transform infrared transmission spectroscopy. It was found that the two hydrocarbon chains of ODASA molecule in LB films are highly ordered while that protonated (H) chain in ODASA-d(35) is partially disordered with some gauche conformers introduced at room temperature.
Resumo:
In this study, melt blends of poly(butylene terephthalate) (PBT) with epoxy resin were characterized by dynamic mechanical analysis, differential scanning calorimetry, tensile testing, Fourier transform infrared spectroscopy, and wide-angle X-ray diffraction. The results indicate that the presence of epoxy resin influenced either the mechanical properties of the PBT/epoxy blends or the crystallization of PBT. The epoxy resin was completely miscible with the PBT matrix. This was beneficial to the improvement of the impact performance of the PBT/epoxy blends.
Resumo:
Porous SnO2 and SnO2-Eu3+ nanorods have been facilely prepared using triphenyltin hydroxide microrods as precursors. The porous structure of SnO2 nanorods, which was aggregated by small SnO2 nanocrystallites, has been confirmed by TEM images and nitrogen adsorption-desorption isotherms. The optical property of the porous SnO2-Eu3+ nanorods was investigated by UV-vis absorption and photoluminescence spectra.
Resumo:
Theoretical researches are performed on the alpha-R2MoO6 (R = Y, Gd, Tb Dy, Ho, Er, Tm and Yb) and pyrochlore-type R2Mo2O7 (R = Y, Nd, Sm, Gd, Tb and Dy) rare earth molybdates by using chemical bond theory of dielectric description. The chemical bonding characteristics and their relationship with thermal expansion property and compressibility are explored. The calculated values of linear thermal expansion coefficient (LTEC) and bulk modulus agree well with the available experimental values. The calculations reveal that the LTECs and the bulk moduli do have linear relationship with the ionic radii of the lanthanides: the LTEC decreases from 6.80 to 6.62 10(-6)/K and the bulk modulus increases from 141 to 154 GPa when R goes in the order Gd, Tb Dy, Ho, Er, Tm, and Yb in the alpha-R2MoO6 series; while in the R2Mo2O7 series, the LTEC ranges from 6.80 to 6.61 10(-6)/K and the bulk modulus ranges from 147 to 163 GPa when R varies in the order Nd, Sm, Gd, Tb and Dy.
Resumo:
The macroscopic mechanical properties of polyaniline (PANI) lie mainly on two factors, the structure of molecular aggregations of polymers and the mechanical properties of a single polymer chain. The former factor is swell revealed; however, the latter is rarely studied. In this article, we have employed atomic force microscopy-based single-molecule force spectroscopy to investigate the mechanical properties of a kind of water-soluble PANI at a single-molecular level. We have carried out the study comparatively on single-chain-stretching experiments of oxidized, reduced, and doped PANI and obtained a full view of the single-chain elasticity of PANI in all these states. It is found that oxidized and reduced PANI chains are rigid, and the oxidized PANI is more rigid than the reduced PANI. Such a difference in single-chain elasticity can be rationalized by the molecular structures that are composed of benzenoid diamine and quinoid diimine its different proportions. The doped PANI has been found to be more flexible than the oxidized and reduced PANI, and the modified freely jointed chain parameters of doped PANI are similar with those of a common flexible-chain polymer.
Resumo:
Ordered hexagonal mesoporous silica material (JLU-30) has been successfully synthesized in alkaline media at high temperature (> 160 degreesC, using cationic (1,3-dimethyl-2-imidazolidin-2-ylidene)hexadecylmethyl-ammonium bromide (DIHAB) as a template, and characterized with X-ray diffraction (XRD), transmission electron microscopy (TEM), nitrogen adsorption-desorption isotherms, differential thermal analysis (DTA), and thermogravimetric analysis (TG), as well as Al-27 and Si-29 nuclear magnetic resonance (NMR) spectroscopy. Mesoporous JLU-30 shows much higher hydrothermal stability than MCM-41. Si-29 NMR spectra indicate that the pore walls of JLU-30 samples synthesized at high temperature (160 degreesC) are fully condensed, giving a Q(4)/Q(3) ratio as high as 6.2. In contrast, MCM-41 synthesized at relatively low temperature (100 degreesC) shows the Q(4)/Q(3) + Q(2) ratio at 1.1. Such unique structural feature might be responsible for the observed highly hydrothermal stability of the mesoporous silica materials (JLU-30).
Resumo:
A new method for syntheses of hyperbranched poly(ester-amide)s from commercially available A(2) and CBx type monomers has been developed on the basis of a series of model reactions. The aliphatic and semiaromatic hyperbranched poly(ester-amide)s with multihydroxyl end groups are prepared by in situ thermal polycondensation of intermediates obtained from dicarboxylic acids (A(2)) and multihydroxyl primary amines (CBx) in N,N-dimethylformamide. Analyses of FTIR, H-1 NMR, and C-13 NMR spectra revealed the structures of the polymers obtained. The MALDI-TOF MS of the polymers indicated that cyclization side reactions occurred during polymerization. The hyperbranched poly(ester-amide) s contain configurational isomers observed by C-13 and DEPT C-13 NMR spectroscopy. The DBs of the polymers were determined to be 0.38-0.62 by H-1 NMR or quantitive C-13 NMR and DEPT 135 spectra. These polymers exhibit moderate molecular weights, with broad distributions determined by size exclusion chromatography ( SEC), and possess excellent solubility in a variety of solvents such as N, N- dimethylacetamide, dimethyl sulfoxide, tetrahydrofuran, and ethanol, and display glass-transition temperatures (T(g)s) between -2.3 and 53.2 degrees C, determined by DSC measurements.
Resumo:
A new solvothermal route has been developed for synthesizing the size-controlled CdSe nanocrystals with relatively narrow size distribution, and the photoluminescence (PL) quantum yields (QYs) of the nanocrystals can reach 5-10%. Then the obtained CdSe nanocrystals served as cores to prepare the core/shell CdSe/CdS nanocrystals via a two-phase thermal approach, which exhibited much higher PL QYs (up to 18-40%) than the CdSe core nanocrystals. The nanocrystal samples were characterized by ultraviolet-visible (UV-vis) absorption spectra, PL spectra, wide-angle Xray diffraction (WAXD), X-ray photoelectron spectroscopy (XPS) and transmission electron microscopy (TEM).
Resumo:
Supported nickel catalyst (Ni-Cat) was used as a catalyst to improve the flame retarclancy of intumescent flame-retardants (IFR) systems based on ammonium polyphosphate and pentaerythritol (PETOL) in polypropylene (PP) matrix. Limited oxygen index (LOI), UL-94 rating, and thermogravimetric analysis were used to characterize the flame retardancy and thermal stability of the PP systems, and field emission scanning electron microscopy (FE-SEM) and Fourier transformed infrared spectroscopy (FTIR) were used to analyze the microstructure and composition of the chars formed during measuring LOI value and after combustion at 800 degrees C. The catalytic effect of NiCat was shown in an increase of LOI, a change in the char microstructure, and improvement of the thermal stability in the PP systems, which result from the synergistic effect of Ni-Cat and IFR. The results from FE-SEM and FTIR spectra of the char can explain how this synergistic effect happened.
Resumo:
The modification of high-impact polystyrene (HIPS) was accomplished by melt-grafting glycidyl methacrylate (GMA) on its molecular chains. Fourier transform infrared spectroscopy and electron spectroscopy for chemical analysis were used to characterize the formation of HIPS-g-GMA copolymers. The content of GMA in HIPS-g-GMA copolymer was determined by using the titration method. The effect of the concentrations of GMA and dicumyl peroxide on the degree of grafting was studied. A total of 1.9% of GMA can be grafted on HIPS. HIPS-g-GNU was used to prepare binary blends with poly(buthylene terephthalate) (PBT), and the evidence of reactions between the grafting copolymer and PBT in the blends was confirmed by scanning electron microscopy (SEM), dynamic mechanical analysis, and its mechanical properties. The SEM result showed that the domain size in PBT/HIPS-g-GMA blends was reduced significantly compared with that in PBT/HIPS blends; moreover, the improved strength was measured in PBT/HIPS-g-GMA blends and results from good interfacial adhesion. The reaction between ester groups of PBT and epoxy groups of HIPS-g-GMA can depress crystallinity and the crystal perfection of PBT.
Resumo:
Detailed circular dichroism(CD) and Fourier transform infrared (FTIR) studies have been carried out to monitor thermal unfolding of horseradish peroxidase isoenzyme C(HRP) inhibited by CN(HRP-CN). The results suggest that HRP-CN is quite different from native HRP with different spin states of Fe of heme and different coordinated states. Cyanide becomes the sixth ligand of Fe(I) of heme and the hydrogen-binding network is destroyed partly at the same time, which cause the drastic decrease of thermal stability of HRP. The FTIR and Soret-CD spectra analysis demonstrate that during the heating process there is an intermediate state(I') which has both partly destroyed secondary and tertiary structures of native HRP, then it is the appearance of protein aggregation state(A) after fully unfolding. The unfolding pathway thus can be shown as follows: I -->I'-->U -->A.
Resumo:
Molecular weight of 8 ginsenosides and the component of total saponions in American ginseng have been determined by matrix-assisted laser desorption/ionization mass spectrometry (MALDI-MS). The average error of the molecular weight of each ginsenoside was found less than 0.05%. The results demonstrate that MALDI-MS is a very simple and useful method to measure the molecular weight of some high polar, thermal unstable small molecules with high sensitivity and reproducibility.
Resumo:
The thermal stability and the solid solid phase transitions in Ills compounds with n = 7-12 have been studied by DSC and TG methods. Comparision with CnZn compounds want made. The nature of three phases of CnCu has been discussed in terms of infrared spectroscopy and the assignment of the phase transitions has been given. The thermal stability of CnCu is lower than that of CnZn and presents an obvious odd even effect. All of these compounds exhibit two solid solid phase transitions in the temperature range of 248-337 K. The peak tempe nature of phase transitions changes regularly. The peak temperature or the main phase transition increases with the chain length. The total transition enthalpies and entropies increase with increasing chain length. When n <= 9, the high temperature phase exists in a partial disorder state. When n >= 10, the high temperature phase exists in a conformational disorder state. The main phase transition and the phase transition at 307.7 K of CnCu may mainly are from the change of the packing structure and the change of the partial conformational order-disorder of alkyl chain, respectively.