921 resultados para polymer single-chains


Relevância:

30.00% 30.00%

Publicador:

Resumo:

The banded textures in the films of a thermotropic liquid crystalline poly(aryl ether ketone) containing a lateral chloro group have been studied by means of transmission electron microscopy(TEM), electron diffraction(ED) and atomic force microscopy (AFM). The crystallization-induced Landed texture without external shear can be formed when the thin films were annealed at the temperature range(320-330 degrees C) of the liquid crystalline state from the melt, The results show that the banded regions have high orientation of single crystal based on the orthorhombic packing and the growing direction of the Lands is along the b axis of the crystals, This kind of single crystal-like bands is due to the different orientation of the packing molecular chains, The molecular chains of the dark bands in the bright field electron micrograph are perpendicular to the film plane, while the ones of the bright Lands are tilt along the b axis with the tilt angle upto +/-20 degrees.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Using poly(styrene-co-maleic anhydride) as the backbone and poly(ethylene glycol) methyl ether as side chains,three kinds of comblike polymers of different side chain length were synthesized. The Li-salt complexes and their firms were prepared. The dynamic mechanical properties were investigated. It was found that the main chain was rigid and the side chain was flexible in this comblike polymer system. Based on the time-temperature equivalence principle, a master curve was constructed. By selecting T-alpha as reference temperature, Arrhenius plots of shift factor and iso-free-volume plots were attained. The values of WLF parameters C-1 and C-2 increase with increasing salt concentration. By reference to T-0 = 50 degrees C, the relation between the average relaxation time 1g tau(c) and Li-salt concentration C is linear. The master curves are displaced progressively to higher frequencies as the M-w of side chains is increased. The relation between the average relaxation time 1g tau(n) and M-w of side chains is also linear. And the master curves are movable with the change of salts. It shows the effect of different kinds of salt on relaxation time.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The crystal of the title compound (C10H18N2O9SZn M-r=407.69) belongs to the hexagonal system, space group P 6(5) with cell parameters: a=11.411 (2), c=20.908(4) Angstrom, V=2357.7(7) Angstrom(3), Z=6, D-c=1.723g/cm(3), F(000)=1260, mu(MoKa)=1.743mm(-1). The final R and omega R factors are 0.072 and 0.178 respectively for 1335 observed reflections. in the structure, zinc ions are bridged by 4,4'-bipyridine to form infinite chains. The sheets containing parallel chains stack along a 65 screw axis to give a helical staircase motif. The helical structure is mainly controlled by the hydrogen bonds.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The present report deals with some results on phase behavior, miscibility and phase separation for several polymer blends casting from solutions. These blends are grouped as the amorphous polymer blends, blends containing a crystalline polymer or two crystalline polymers. The blends of PMMA/PVAc were miscible and underwent phase separation at elevated temperature, exhibited LCST behavior. The benzoylated PPO has both UCST and LCST nature. For the systems composed of crystalline polymer poly(ethylene oxide) and amorphous polyurethane, of two crystalline polymers poly(epsilon-caprolactone) and poly[3,3,-bis-(chloromethyl) oxetane], appear a single T-g, indicating these blends are miscible. The interaction parameter B's were determined to be -14 J cm(-3), -15 J cm(-3) respectively. Phase separation of phenolphthalein poly(ether ether sulfone)/PEO blends were discussed in terms of thermal properties, such as their melting and crystallization behavior.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The comblike polymers based on poly (styrene-co-maleic anhydride) backbone with poly (ethylene glycol) methyl ether as side chains were synthesized and characterized by H-1 NMR. with the result compared with that of 1R. It is found that it is both feasible and simple to synthesize this kind of compounds with the help of H-1 NMR.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The effect of entanglements on the glass transition and structural relaxation behaviors has been studied for polystyrene (PS) and phenolphthalein poly(ether sulfone) (PES-C) samples by fast evaporation of the solution of concentrations varying from above the overlapping concentration to far below it, and compared to the results we have studied previously in PC. It has been found that for all the polymers we have studied, in the concentrated solution region, the T-g of the samples obtained from solution are independent of the change of concentration and are very close to that of normal bulk samples, whereas in the dilute solution region the T-g of the samples decrease with the logarithm of decreasing concentration. The critical concentrations that divide the two distinct regions for the three polymers are 0.9% g/mL for PC, 0.1% g/mL for PS, and 1% g/mL for PES-C. The decrease of T-g of the samples is interpreted by the decrease of intermolecular entanglements as the isolation of polymer chains, and the entanglement of polymer chains restrained the mobility of the segments. The structural relaxation behavior of the polymers is also found to be different from that of normal bulk samples. The enthalpies of single-chain samples are lower than that of the bulk ones, which correspond to the lower glass transition temperature; the peaks are lower and broader, and the relaxed enthalpy is much lower as compared to that of bulk samples. In the three polymers we have studied, the influence of change of entanglements on both the decrease in glass transition temperature and relaxed enthalpy is the most significant for PS and the least for PES-C. It is indicated that the interactions in the flexible polymers are weak; thus, the restraint of the entanglements on the mobility of the segments plays a more important role in the flexible polymers, and the change of entanglement in the flexible polymers has a more significant influence on the physical properties.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This paper studies the radiation properties of the immiscible blend of nylon1010 and HIPS. The gel fraction increased with increasing radiation dose. The network was found mostly in nylon1010, the networks were also found in both nylon1010 and HIPS when the dose reaches 0.85 MGy or more. We used the Charleby-Pinner equation and the modified Zhang-Sun-Qian equation to simulate the relationship with the dose and the sol fraction. The latter equation fits well with these polymer blends and the relationship used by it showed better linearity than the one by the Charleby-Pinner equation. We also studied the conditions of formation of the network by the mathematical expectation theorem for the binary system. Thermal properties of polymer blend were observed by DSC curves. The crystallization temperature decreases with increasing dose because the cross-linking reaction inhibited the crystallization procession and destroyed the crystals. The melting temperature also reduced with increasing radiation dose. The dual melting peak gradually shifted to single peak and the high melting peak disappeared at high radiation dose. However, the radiation-induced crystallization was observed by the heat of fusion increasing at low radiation dose. On the other hand, the crystal will be damaged by radiation. A similar conclusion may be drawn by the DSC traces when the polymer blends were crystallized. When the radiation dose increases, the heat of fusion reduces dramatically and so does the heat of crystallization. (C) 1999 Elsevier Science Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The structures of single crystals of syndiotactic poly(butene-1) in form I, produced by thin-film growth, are studied by transmission electron microscopy and electron diffraction. Bright-field electron microscopy observation shows that the single crystal exhibits a regular rectangular shape with the long axis along its crystallographic b-axis. Electron diffraction results indicate an isochiral C-centered packing of a-fold helical chains in an orthorhombic unit cell corresponding to the C222(1) space group, according to the model proposed in the literature. The differences with the polymorphic behavior of syndiotactic polypropylene concerning the formation and the stability of the isochiral mode of packing are outlined.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Using poly(styrene-co-maleic anhydride) as a backbone and poly(ethylene glycol) methyl ether (PEGME) with different molecular weights as side chains, three comb-like polymers and their Li salt complexes were synthesized. The dynamic mechanical properties and conductivities were investigated. Results showed that the polymer electrolytes possess two glass transitions: alpha -transition and beta -transition, and the temperature dependence of the ionic conductivity shows WLF (Williams-Landel-Ferry) behavior. Based on the time-temperature equivalence principle, a master curve was constructed by selecting T-beta as reference temperature. The values of the WLF parameters (C-1 and C-2) were obtained and were found to be almost independent of the length of the PEGME side chain and the content of Li salt. By reference to T-0 = 50 degreesC. the relation between log tau (c) and c was found to be linear. The master curves are displaced progressively to higher frequencies as the molecular weight of the side chain is increased. The relation between log tau (n) and the molecular weight of the side chain is also linear. (C) 2001 Elsevier Science B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Metallocene-catalyzed short chain branched polyethylene single crystals, formed from the melt at a higher crystallization temperature of 114 degreesC, were obtained. Highly elongated lamellae were formed, which are different from truncated lozenge or lenticular shaped single crystals formed at a lower crystallization temperature. It was found that there existed a definite line in the lamellae along the longitudinal growth direction and two regions were separated by the definite line. The lateral habits of both the regions were asymmetrical about the b-axis due to the chain tilting, which was the same as that at a lower crystallization temperature. Generally, the highly elongated lamellae were not straight, but curved towards the opposite direction with chain tilting direction due to a series of edge dislocation within a lamella. The inner side of a lamella was serrated and the outer side was smooth due to the lamellar curvature. The thickness of both regions of a lamella was different, the broader region was thicker than the narrower region, which was different from the uniform thickness of the lamellae formed at a lower crystallization temperature. The different thicknesses within a lamella were considered as the result of the initial thickness difference and the impact of isothermal thickening. (C) 2001 Elsevier Science Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A new solvent, dimethylformamide (DMF), and the traditional solvent, 1,4-butanediol, were used to prepare single crystals of nylon-10,10 from a dilute solution. The lamellae grown from DMF inhabited a more perfect structure and regular shape than those crystals crystallized from traditional solvents such as 1,4-butanediol and glycerin. These thin and perfect lamellar crystals demonstrated patterns of variation in spacing different from those of melt-crystallized spherulites on heating. Specifically, the two main spacings slightly separated rather than continuously approaching each other when the temperature was greater than 180 degreesC. This is a novel phenomenon observed in nylons. Nevertheless, the usual pattern of change in spacing was observed during the cooling process. These lamellar crystals showed more compact spacing of the (002) and (010/100) planes than spherulites at room temperature. (C) 2001 John Wiley & Sons, Inc.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

It was first found that Ind(2)Y(mu -Et)(2)AlEt2 and Ind(2)LnN(i-Pr)(2) (Ln = Y, Yb) exhibit extremely high catalytic activity in the polymerization of methyl methacrylate. The reactions can be carried out over a quite broad range of polymerization temperatures from -30 to 50 degreesC. PMMA with high molecular weight (7.8 x 10(-5)) and high isotacticity (94%) can be obtained by using Ind(2)Y(mu -Et)(2)AlEt2, and narrow molecular weight distribution (M-w/M-n < 1.5) can be obtained by using Ind(2)LnN(i-Pr)(2) (Ln = Y, Yb).

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Ind(2)Y(mu -Et)(2)AlEt2 and Ind(2)LnN(i-Pr)(2) (Ln = Y, Yb) were used as a single-component catalyst for the polymerization of acrylonitrile (AN) respectively. The regularity of polymerization of AN and stereoregularity of polyacrylonitrile (PAN) were also studied in both cases. Both catalysts can produce PAN with molecular weight from 10,000 to 30,000. In addition, the catalytic activity and molecular weights were increased by the addition of PhONa.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Phase structures and transformation mechanisms of nonracemic chiral biological and synthetic polymers are fundamentally important topics in understanding their macroscopic responses in different environments. It has been known for many years that helical structures and morphologies can exist in low-ordered chiral liquid crystalline (LC) phases. However, when the chiral liquid crystals form highly ordered smectic liquid crystal phases, the helical morphology is suppressed due to the crystallization process. A double-twisted morphology has been observed in many liquid crystalline biopolymers such as dinoflaggellate chromosomes (in Prorocentrum micans) in an in vivo arrangement. Helical crystals grown from solution have been reported in the case of Bombyx mori silk fibroin crystals having the beta modification. This study describes a synthetic nonracemic chiral main-chain LC polyester that is able to thermotropically form helical single lamellar crystals. Flat single lamellar crystals can also be observed under the same crystallization condition. Moreover, flat and helical lamellae can coexist in one single lamellar crystal, within which one form can smoothly transform to the other. Both of these crystals possess the same structure, although translational symmetry is broken in the helical crystals. The polymer chain folding direction in both flat and helical lamellar crystals is determined to be identical, and it is always along the long axis of the lamellae. This finding provides an opportunity to study the chirality effect on phase structure, morphology, and transformation in condensed states of chiral materials. [S0163-1829(99)01042-5].

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The orientational behavior of liquid crystalline polymers with para-nitro azobenzene as side chains under electric field was studied by UV-visible spectroscopy. The results showed that lambda(max) of the poled polymer films was around 394nm, compared to that of the unpoled films, the absorption decreased due to poling. The orientational parameters increased linearly with the increase of the electric field. The temporal stability of the poled polymer film is good at room temperature. This kind of materials showed promise application as nonlinear optical component in photorefractive polymers.