921 resultados para floristic and structural comparisons
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Pb1-xCaxTiO3 (0.10less than or equal toxless than or equal to0.40) thin films on Pt/Ti/SiO2/Si(100) substrates were prepared by the soft solution process and their characteristics were investigated as a function of the calcium content (x). The structural modifications in the films were studied using x-ray diffraction and micro-Raman scattering techniques. Lattice parameters calculated from x-ray data indicate a decrease in lattice tetragonality with the increasing content of calcium in these films. Raman spectra exhibited characteristic features of pure PbTiO3 thin films. Variations in the phonon mode wave numbers, especially those of lower wave numbers, of Pb1-xCaxTiO3 thin films as a function of the composition corroborate the decrease in tetragonality caused by the calcium doping. As the Ca content (x) increases from 0.10 to 0.40, the dielectric constant at room temperature abnormally increased at 1 kHz from 148 to 430. Also calcium substitution decreased the remanent polarization and coercive field from 28.0 to 5.3 muC/cm(2) and 124 to 58 kV/cm, respectively. These properties can be explained in terms of variations of phase transition (ferroelectric-paraelectric), resulting from the substitution the lead site of PbTiO(3)for the nonvolatile calcium. (C) 2002 American Institute of Physics.
Resumo:
The structural and electronic properties of ZnO (10 (1) over bar0) and (11 (2) over bar0) surfaces were investigated by means of density functional theory applied to periodic calculations at B3LYP level. The stability and relaxation effects for both surfaces were analyzed. The electronic and energy band properties were discussed on the basis of band structure as well as density of states. There is a significant relaxation in the (10 (1) over bar0) as compared to the (11 (2) over bar0) terminated surfaces. The calculated direct gap is 3.09, 2.85, and 3.09 eV for bulk, (10 (1) over bar0), and (11 (2) over bar0) surfaces, respectively. The band structures for both surfaces are very similar.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
The bis(1,10-phenanthrolinethiocyanatemercury)tetracarbonyliron was prepared from bis(thiocyanatemercury)tetracarbonyliron and 1,10-phenanthroline and crystallized from hot acetone solution as [Fe(CO)4(HgSCN)2(phen)2]·C3H6O, which was subjected to a full IR and X-ray crystallographic characterization. The iron atom is octahedrally coordinated by four carbonyl groups and two mercury atoms in cis positions. The coordination geometry of the mercury atoms is a distorted square-based pyramid since each one is coordinated to one iron, one sulphur, one mercury and two nitrogen atoms. The FeHg distances are 2.549(3) and 2.564(3) Å, and the HgFeHg angle is 78.01(9)°. © 1992.
Resumo:
The compound (3,5-dinitrobenzoate)bis(triphenylphosphine)copper(I) was synthesized and studied by IR spectroscopy and X-ray diffraction techniques. It is monomeric with the carboxylato acting as a monodentate ligand. The copper atom shows a trigonal planar coordination geometry. © 1993.
Resumo:
In the present investigation we analyzed both histology and area of secretory cells from workers, virgin and physogastric queen mandibular glands of Melipona bicolor bicolor Lepeletier. The histological differences observed include the number of vacuoles present in the cell cytoplasm and the quantity and distribution of the secretion. The morphometry results demonstrated the occurrence of significative differences in the cell area values that were related to the secretory cell activity level, which is higher in the physogastric queens. Worker and queen glands have histological patterns quite similar, but the morphometric data indicated cast-specific differences, as well as differences between the queens, which were related to the posture activity.
Resumo:
The effect of bath composition and electroplating conditions on structure, morphology and composition of amorphous Fe-Cr-P-Ni-C deposits on Cu substrate was investigated. The deposition efficiency of Fe-Ni-P-C alloy increased significantly with the addition of formic acid, but decreased with the addition of Cr to the plating bath. The increase of charge density activates the inclusion of Cr in the deposit. However, above a specific value of charge density, which depends on deposition current density, the Cr content in the deposit decreases. SEM analysis showed that the increase of Ni, Cr or charge deposition promotes susceptibility to microcracking.
Resumo:
Follicle diameters and concentrations of follicular fluid factors were studied in the two largest follicles (F1 and F2) using F1 diameters in increments of 0.2 mm (equivalent to 4 h intervals) and extending from 7.4 to 8.4 mm (12 heifers in each of 6 groups). Changes were compared between follicles using the F2 associated with each F1-diameter group. Diameter deviation began in the 8.2-mm group as indicated by a greater (P < 0.05) diameter difference between F1 and F2 in the 8.4-mm group than in the 8.2-mm group. In the 8.0-mm group, estradiol concentrations began to increase (P < 0.05) differentially in F1 versus F2, and free insulin-like growth factor-1 (IGF-1) began to decrease differentially in F2 (P < 0.06). Combined for F1 and the associated F2, activin-A concentrations increased (P < 0.05) between the 7.6- and 8.2-mm groups and then decreased (P < 0.05). Results supported the hypothesis that estradiol and free IGF-1 concentrations simultaneously become higher in F1 than in the associated F2 by the beginning of diameter deviation. Results did not support the hypothesis that a transient elevation in activin-A is present in F1 but not in the associated F2 at the beginning of the estradiol and IGF-1 changes; instead, a mean transient elevation in activin-A occurred at this time only when data for the two follicles were combined. Comparisons between F1 and F2 also were made by independently grouping F2 and using diameter groups at 0.2-mm increments for F2 as well as for F1. In the diameter groups common to F1 and F2 (7.4, 7.6, 7.8, and 8.0 mm) there was a group effect (P < 0.003) for estradiol involving an increase (P < 0.05) beginning at the 7.6-mm group averaged over F1 and F2. For free IGF-1 concentrations, a fluctuation (a significant increase followed by a significant decrease) occurred independently in F1 between the 7.4-to 7.8-mm groups and independently in F2 between the 7.0- to 7.4-mm groups.
Resumo:
First-principles quantum-mechanical techniques, based on density functional theory (B3LYP level) were employed to study the electronic structure of ordered and deformed asymmetric models for Ba0.5Sr 0.5TiO3. Electronic properties are analyzed and the relevance of the present theoretical and experimental results on the photoluminescence behavior is discussed. The presence of localized electronic levels in the band gap, due to the symmetry break, would be responsible for the visible photoluminescence of the amorphous state at room temperature. Thin films were synthesized following a soft chemical processing. Their structure was confirmed by x-ray data and the corresponding photoluminescence properties measured.
Resumo:
Poly(o-methylaniline) (poly-o-toluidine, PTOL) was synthesized by chemical oxidation of o-toluidine with ammonium peroxydisulfate in an aqueous 1.0 mol L -1 HCl solution. The progress of polymerization was followed by measuring the open-circuit potential (OCP) of a Pt electrode immersed in the reaction medium with the polymerization time. The chemical synthesis of PTOL was carried out at different monomer:oxidant (M:O) molar ratios (4:1, 2:1, 1.5:1, 1:1, and 0.66:1), and the products obtained were characterized by infrared spectroscopy, gel permeation chromatography, and X-ray diffraction. The molecular weight and percentage of crystallinity of PTOL are higher for samples synthesized in an excess of the monomer, i.e. at higher M:O ratios. However, the yield of PTOL prepared at higher M:O ratios is considerably low, in particular at a 4:1 M:O ratio, which is the M:O ratio most commonly used in the literature to synthesize polyaniline and its derivatives.