Our concern here is to rationalize experimental observations of failure modes brought about by indentation of hard thin ceramic films deposited on metallic substrates. By undertaking this exercise, we would like to evolve an analytical framework that can be used for designs of coatings. In Part I of the paper we develop an algorithm and test it for a model system. Using this analytical framework we address the issue of failure of columnar TiN films in Part II [J. Mater. Res. 21, 783 (2006)] of the paper. In this part, we used a previously derived Hankel transform procedure to derive stress and strain in a birefringent polymer film glued to a strong substrate and subjected to spherical indentation. We measure surface radial strains using strain gauges and bulk film stresses using photo elastic technique (stress freezing). For a boundary condition based on Hertzian traction with no film interface constraint and assuming the substrate constraint to be a function of the imposed strain, the theory describes the stress distributions well. The variation in peak stresses also demonstrates the usefulness of depositing even a soft film to protect an underlying substrate.
Resumo:
Under senare tid har förekomsten av samarbete mellan konkurrerande sm-företag ökat. Forskningen kring ämnet har dock bedrivits i mindre skala, framför allt om man beaktar finländska (nordiska) förhållanden. Syftet med denna undersökning är att kartlägga förekomsten av samarbete mellan konkurrerande sm-företag i Österbotten (Finland), samt beskriva dessa. Gällande demografiska variabler jämförs dessa företag även med sm-företag som inte samarbetar. Data insamlades genom en enkät utskickad i november 2001 till 345 sm-företag i Österbotten. Svarsprocenten var 35.1. Av de respondenter som besvarade enkäten, var 47.9 procent involverade i ett eller flera samarbeten med ett eller flera företag som var deras konkurrenter. Samarbete mellan konkurrenter är således inte ett ovanligt fenomen, utan innefattar allt från informella, operativa samarbeten till formella, strategiskt viktiga samarbeten. Samarbete inom produktion var den mest vanligt förekommande formen av samarbete. Partnern kom från Finland, även om målmarknaderna för samarbetet fanns både i Finland och i utlandet. Denna undersökning kunde inte identifiera någon större skillnad mellan de sm-företag som samarbetade med konkurrenter och de sm-företag som inte samarbetade. Det intressanta är således att det inte verkar finnas några skillnader vad gäller ålder, omsättning, omsättningsökning, underleverans- och exportverksamhet mellan de samarbetande och de icke samarbetande företagen. Skillnaderna bör således sökas i andra variabler. Den enda signifikanta skillnaden kunde upptäckas i upplevelsen av konkurrens. Tidigare forskning har identifierat att osäkerhet i konkurrensen är ett incitament till att börja samarbeta med konkurrenter. Denna undersökning förstärker detta antagande. De samarbetande företagen upplevde att konkurrensen var hårdare än de icke samarbetande företagen. Bland de samarbetande företagen var det speciellt de mindre (med en personalstyrka mellan 10 och 50 arbetstagare) som upplevde att konkurrensen var hård. Undersökningen har finansierats med stipendiemedel från Sparbanksstiftelsen i Vasa och Handlande Gustav Svanljungs fond.
Resumo:
Direct writing of patterns is being widely attempted in the field of microelectronic circuit/device manufacture. Use of this technique eliminates the need for employing photolithographic process. Laser induced direct writing can be achieved by (i) Photochemical reaction [i] , (ii) Evaporation from target material [2], and (iii) decomposition.Micron size features of palladium and copper through decomposition of palladium acetate and copper formate respectively on quartz and silicon using Argon ion laser have been reported [3,4] .In this commuication we report a technique for both single line and large area depositon of copper through decomposition of copper acetate,(CH3COO)2Cu, on alumina substrates.Nd:YAG laser known for its reliability and low maintenance cost as compared to excimer and other gas lasers is used. This technique offers an attractive and economical alternative for manufacture of thin film microcircuits.
Resumo:
The increase in optical band gap (photo bleaching) due to light illumination was studied at room temperature as well as at low (4.2 K) temperature for Sb/As2S3 multilayered film of 640 nm thickness by Fourier Transform Infrared Technique. The interdiffusion of Sb into As2S3 matrix results the formation of Sb-As2S3 ternary solid solutions which is explained by the change in optical band gap (E-g), absorption coefficient (alpha), Tauc parameter (B-1/2), Urbach edge (E-e). At the same time, photo darkening phenomena was observed in (As2S3)(0.93)Sb-0.07 film of same thickness both at low and room temperatures. From our X-ray Photoelectron Spectroscopy measurements,we are able to show that some of the As-As, S-S and Sb-Sb bonds are converted into As-S and S-Sb bonds in case of multilayers. We found that the energetically favoured heteropolar bond formation take place by a phonon-assisted mechanism using the lone pair pi electrons of S-2(0). But in case of (As2S3)(0.93)Sb-0.02 film, the homopolar bonds are playing a major role. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Rapid multiplication of axillary meristems and direct shoot development occurred from nodal explants of mature Eucalyptus tereticornis Sm. with 5.3 mgrM NAA, 1.1 mgrM IAA and 4.4 mgrM BA in Murashige-Skoog medium. Repeated subcultures of the second generation shoot cultures into low cytokinin-auxin containing media (0.44�0.88 mgrM BA+0.1 mgrM NAA) yielded axillary microshoots in large numbers. Half-strength MS liquid medium with 4.9 mgrM IBA, 5.5 mgrM IAA and 5.3 mgrM NAA for four days, half-strength semi-solid hormonefree MS medium with charcoal, and MS liquid medium without charcoal and hormones, in sequence, induced rooting of shoots in the dark. This system is suitable for the mass propagation of this difficult-to-root eucalypt.
Resumo:
PbSnS2 thin film has been prepared for the first time by spray pyrolysis technique on FTO substrate at 570K. The preliminary optical and structural characteristics of the film have been reported. The optical studies showed that the value of the fundamental absorption edge lies at 1.47eV and a low energy absorption band tail has been observed. The prepared film is p- type electrical conductivity, polycrystalline in nature and has an orthorhombic crystal structure. The value of an average grain size of the film is 350Å.
Resumo:
The electrochemical properties of the film-covered anode/solution interface in the magnesium/ manganese dioxide dry cell have been evaluated. The most plausible electrical equivalent circuit description of the Mg/solution interface with the passive film intact, has been identified. These results are based on the analysis of ac impedance and voltage transient measurements made on the dry cell under conditions which cause no damage to the protective passive film on the anode. The study demonstrates the complementary character of impedance and transient measurements when widely different frequency ranges are sampled in each type of investigation. The values and temperature dependence of the anode-film resistance, film capacitance, double-layer capacitance and charge-transfer resistance of the film-covered magnesium/solution interface have been determined. The magnitude of these values and its implications in understanding the important performance aspects of the magnesium/manganese dioxide dry cell are discussed. The study may be extended, in principle, to Li, Al and Ca batteries.
Resumo:
The electrochemical properties of the film-covered anode/solution interface in the magnesium/ manganese dioxide dry cell have been evaluated. The most plausible electrical equivalent circuit description of the Mg/solution interface with the passive film intact, has been identified. These results are based on the analysis of ac impedance and voltage transient measurements made on the dry cell under conditions which cause no damage to the protective passive film on the anode. The study demonstrates the complementary character of impedance and transient measurements when widely different frequency ranges are sampled in each type of investigation. The values and temperature dependence of the anode-film resistance, film capacitance, double-layer capacitance and charge-transfer resistance of the film-covered magnesium/solution interface have been determined. The magnitude of these values and its implications in understanding the important performance aspects of the magnesium/manganese dioxide dry cell are discussed. The study may be extended, in principle, to Li, Al and Ca batteries.