915 resultados para NONLINEAR-OPTICAL PROPERTIES
Resumo:
Pure ZnO and co-doped (Mn, Ag) ZnO nanoparticles have been successfully prepared by chemical co-precipitation method without using a capping agent. X-ray diffraction (XRD) studies confirms the presence of wurtzite (hexagonal) crystal structure similar to undoped ZnO, suggesting that doped Mn, Ag ions are substituted to the regular Zn sites. The morphology of the samples were studied by scanning electron microscopy (SEM). The chemical composition of pure and co-doped ZnO nanoparticles were characterized by energy dispersive X-ray analysis spectroscopy (EDAX). Optical absorption properties were determined by UV-vis Diffuse Reflectance Spectrophotometer. The incorporation of Ag+, Mn2+ in the place of Zn2+ provoked to decrease the size of nanocrystals as compared to pure ZnO. Optical absorption measurements indicates blue shift in the absorption band edge upon Ag, Mn ions doped ZnO nanoparticles.
Resumo:
The seasonality and mutual dependence of aerosol optical properties and cloud condensation nuclei (CCN) activity under varying meteorological conditions at the high-altitude Nainital site (2km) in the Indo-Gangetic Plains were examined using nearly year-round measurements (June 2011 to March 2012) at the Atmospheric Radiation Measurement mobile facility as part of the Regional Aerosol Warming Experiment-Ganges Valley Aerosol Experiment of the Indian Space Research Organization and the U.S. Department of Energy. The results from collocated measurements provided enhanced aerosol scattering and absorption coefficients, CCN concentrations, and total condensation nuclei concentrations during the dry autumn and winter months. The CCN concentration (at a supersaturation of 0.46) was higher during the periods of high aerosol absorption (single scattering albedo (SSA)<0.80) than during the periods of high aerosol scattering (SSA>0.85), indicating that the aerosol composition seasonally changes and influences the CCN activity. The monthly mean CCN activation ratio (at a supersaturation of 0.46) was highest (>0.7) in late autumn (November); this finding is attributed to the contribution of biomass-burning aerosols to CCN formation at high supersaturation conditions.
Resumo:
A new triarylborane-aza-BODIPY conjugate is reported. The compound consists of two blue emissive dimesitylarylborane moieties and a near-infrared (NIR) emissive aza-BOIDPY core and shows panchromatic absorption spanning approximately 300-800 nm. DFT computational studies suggest limited electronic communication between the individual fluorophore units. Hence, the partial energy transfer from blue fluorophore triarylborane to NIR chromophore aza-BODIPY unit leads to a broad dual-emissive feature covering a large part of visible and NIR region. Furthermore, the broadband emissive compound can act as a selective sensor for fluoride anion as a result of fluorescence quenching response in both visible and NIR spectral regions.
Resumo:
The exposure with band gap light of thermally evaporated As40Sb15Se45 amorphous film of 800 nm thickness, were found to be accompanied by optical changes. The as-prepared and illuminated thin films were studied by X-ray diffraction, Fourier Transform Infrared Spectroscopy and X-ray Photoelectron Spectroscopy and Raman spectroscopy. The optical band gap was reduced due to photo induced effects along with the increase in disorder. These optical properties changes are due to the change of homopolar bond densities. The core level peak shifting in XPS spectra and Raman shift supports the optical changes happening in the film due to light exposure.
Resumo:
Undoped and Ln(3+) (Eu and Tb)-doped crystalline nanobundles of YPO4 were prepared by a facile microwave-assisted route with water as a solvent and without using any surfactant. TEM investigations reveal that the as-prepared powder consists of lenticular-shaped nanobundles (similar to 100 nm in diameter) made of very small nanorods with diameter less than 10 nm and length varying from 20 to 50 nm. Each nanorod in turn is single crystalline, as revealed by HRTEM imaging. The as-prepared nanobundles are easily dispersible in various solvents, especially water, without any surface functionalization, which is critical for various bio-probe applications like cell and tissue imaging. The Eu- and Tb-doped YPO4 nanobundles show good photoluminescence properties and were further evaluated for their use as fluorescent biolabels. Our results show that HeLa cells labelled with Eu- and Tb-doped YPO4 nanobundles show bright red (Eu) and green (Tb) intracellular luminescence under a confocal microscope. Concentration-and time-dependent MTT cell viability assays show that the nanobundles show low toxicity towards cells which makes them promising in bioimaging field.
Resumo:
The change in photo-induced optical properties in thermally evaporated Ge12Sb25Se63 chalcogenide thin film under 532-nm laser illumination has been reported in this paper. The structure and composition of the film have been examined by X-ray diffraction and energy dispersive X-ray analysis, respectively. The optical properties such as refractive index, extinction coefficient and thickness of the films have been determined from the transmission spectra based on inverse synthesis method and the optical band gap has been derived from optical absorption spectra using the Tauc plot. It has been found that the mechanism of the optical absorption is due to allowed indirect transition. The optical band gap increases by 0.05 eV causing photo-bleaching mechanism, while refractive index decreases because of reduction in structural disordering. Deconvolution of Raman and X-ray photoelectron spectra into several peaks provides different structural units, which supports the optical photo-bleaching.
Resumo:
Three new triarylborane conjugated dicyanovinyl chromophores (Mes(2)B-pi-donor-DCV); donor: N-methyldiphenylamine (1) and triphenylamine (2 and 3 with two BMes(2) substitutions]) of type A-D-A (acceptor-donor- acceptor) are reported. Compounds 1-3 exhibit intense charge transfer (CT) absorption bands in the visible region. These absorption peaks are combination CT bands of the amine donor to both the BMes(2) and DCV units. This inference was supported by theoretical studies. Compound 1 shows weak fluorescence compared to 2 and 3. The discrimination of fluoride and cyanide ions is essential in the case of triarylborane (TAB) based anion sensors as a similar response is given towards both the anions. Anion binding studies of 1, 2 and 3 showed that fluoride ions bind selectively to the boron centre and block the corresponding CT transition (donor to BMes(2)) leaving the other CT transition to be red shifted. On the other hand, cyanide ions bind with both the receptor sites and stop both the CT transition processes and hence a different colorimetric response was noted. The binding of F-/CN- induces colour changes in the visible region of the electronic spectra of 2 and 3, which allows for the naked-eye detection of F- and CN- ions. The anion binding mechanisms are established using NMR titration experiments.
Resumo:
Regular ZnO tetrapods with different morphologies have been obtained on Si(100) substrate via the chemical vapour deposition approach. Varying the growth temperature and gas rate, we have obtained different structured ZnO materials: tetrapods with a large hexagonal crown, a flat top and a small hexagonal crown. The results suggest that these tetrapods are all single crystals with a wurtzite structure that grow along the (0001) direction. However, photoluminescence spectra shows that their optical properties are quite different: for those with large hexagonal crown, the green emission overwhelms that of the near band-edge (NBE) ultraviolet (UV) peak, while others have only a strong NBE UV peak at ~386 nm.
Resumo:
The deposition of CdO center dot nH(2)O On CdTe nanoparticles was studied in an aqueous phase. The CdTe nanocrystals (NCs) were prepared in aqueous solution through the reaction between Cd2+ and NaHTe in the presence of thioglycolic acid as a stabilizer. The molar ratio of the Cd2+ to Te2- in the precursory solution played an important role in the photoluminescence of the ultimate CdTe NCs. The strongest photoluminescence was obtained under 4.0 of [Cd2+]/[Te2-] at pH similar to 8.2. With the optimum dosage of Cd(II) hydrous oxide deposited on the CdTe NCs, the photoluminescence was enhanced greatly. The photoluminescence of these nanocomposites was kept constant in the pH range of 8.0-10.0, but dramatically decreased with an obvious blue-shifted peak while the pH was below 8.0. In addition, the photochemical oxidation of CdTe NCs with cadmium hydrous oxide deposition was markedly inhibited.
Resumo:
The InAsxSb1-x films were grown on (100) GaSb substrates by liquid-phase epitaxy, and their structural, electrical, and optical properties were investigated. The high-resolution x-ray diffraction results reveal that the single crystalline InAsxSb1-x films with a midrange composition are epitaxially grown on the GaSb substrates. Temperature dependence of the Hall mobility was theoretically modeled by considering several predominant scattering mechanisms. The results indicate that ionized impurity and dislocation scatterings dominate at low temperatures, while polar optical phonon scattering is important at room temperature (RT). Furthermore, the InAsxSb1-x films with the higher As composition exhibit the better crystalline quality and the higher mobility. The InAs0.35Sb0.65 film exhibits a Hall mobility of 4.62x10(4) cm(2) V-1 s(-1). The cutoff wavelength of photoresponse is extended to about 12 mu m with a maximum responsivity of 0.21 V/W at RT, showing great potential for RT long-wavelength infrared detection. (C) 2008 American Institute of Physics. [DOI: 10.1063/1.2989116]
Resumo:
The deposition of CdO center dot nH(2)O On CdTe nanoparticles was studied in an aqueous phase. The CdTe nanocrystals (NCs) were prepared in aqueous solution through the reaction between Cd2+ and NaHTe in the presence of thioglycolic acid as a stabilizer. The molar ratio of the Cd2+ to Te2- in the precursory solution played an important role in the photoluminescence of the ultimate CdTe NCs. The strongest photoluminescence was obtained under 4.0 of [Cd2+]/[Te2-] at pH similar to 8.2. With the optimum dosage of Cd(II) hydrous oxide deposited on the CdTe NCs, the photoluminescence was enhanced greatly. The photoluminescence of these nanocomposites was kept constant in the pH range of 8.0-10.0, but dramatically decreased with an obvious blue-shifted peak while the pH was below 8.0. In addition, the photochemical oxidation of CdTe NCs with cadmium hydrous oxide deposition was markedly inhibited.