861 resultados para Denture Stomatitis
Resumo:
Membrane fusion is an essential step in the entry of enveloped viruses into their host cells triggered by conformational changes in viral glycoproteins. We have demonstrated previously that modification of vesicular stomatitis virus (VSV) with diethylpyrocarbonate (DEPC) abolished conformational changes on VSV glycoprotein and the fusion reaction catalyzed by the virus. In the present study, we evaluated whether treatment with DEPC was able to inactivate the virus. Infectivity and viral replication were abolished by viral treatment with 0.5 mM DEPC. Mortality profile and inflammatory response in the central nervous system indicated that G protein modification with DEPC eliminates the ability of the virus to cause disease. In addition, DEPC treatment did not alter the conformational integrity of surface proteins of inactivated VSV as demonstrated by transmission electron microscopy and competitive ELISA. Taken together, our results suggest a potential use of histidine (His) modification to the development of a new process of viral inactivation based on fusion inhibition. © 2006 Elsevier B.V. All rights reserved.
Resumo:
Purpose: To evaluate the effects of disinfection treatments with chemical solutions (2% glutaraldehyde, 5% sodium hypochlorite, and 5% chlorhexidine) and microwave energy on the hardness of four long-term soft denture liners. Materials and Methods: Forty rectangular specimens of four soft lining materials (Molloplast-B, Ufi Gel P, Eversoft, and Mucopren soft) were made for each material. Ten samples of each material were immersed in different disinfectant solutions for 10 minutes or placed in a microwave oven for 3 minutes at 500 W. The hardness values were obtained with a Shore A durometer, before the first disinfection cycle (control), and also after two cycles of disinfection. Data were submitted to analysis of variance and Tukey's test (p < 0.01). Results: The highest value of hardness was obtained for Molloplast-B, independent of the disinfection technique. Mucopren soft demonstrated intermediate values and Ufi Gel P and Eversoft the lowest values of Shore A hardness. For Molloplast-B, the disinfection using glutaraldehyde demonstrated the highest value of hardness. The number of disinfections had no effect on the hardness values for all the materials studied and disinfection techniques. Conclusions: The application of two disinfection cycles did not change the Shore A hardness values for all the materials. The glutaraldehyde solution demonstrated the highest values of Shore A hardness for the Molloplast-B, Mucopren soft, and Ufi Gel P materials, while Eversoft did not present any differences in hardness when submitted to different disinfection treatments. Copyright © 2007 by The American College of Prosthodontists.
Resumo:
This study aimed to evaluate the durability of adhesion between acrylic teeth and denture base acrylic resin. The base surfaces of 24 acrylic teeth were flatted and submitted to 4 surface treatment methods: SM1 (control): No SM; SM2: application of a methyl methacrylate-based bonding agent (Vitacol); SM3: air abrasion with 30-μm silicone oxide plus silane; SM4: SM3 plus SM2. A heat-polymerized acrylic resin was applied to the teeth. Thereafter, bar specimens were produced for the microtensile test at dry and thermocyled conditions (60 days water storage followed by 12,000 cycles). The results showed that bond strength was significantly affected by the SM (P < .0001) (SM4 = SM2 > SM3 > SM1) and storage regimens (P < .0001) (dry > thermocycled). The methyl methacrylate-based adhesive showed the highest bond strength.
Resumo:
The effect of post-polymerization treatments (MW-microwave irradiatron and WB-water-bath) on the degree of conversion (DC) of three reline resins (Ufi Gel hard-U, Kooliner-K, and Tokuso Rebase Fast-T) and one denture base resin (Lucitone 550-L), submitted to two polymerization cycles (LS-short and LL-long), was evaluated by using FT-Raman spectroscopy (n = 5). The molecular weight (Mw) of the powder of all materials and of K polymerized specimens (control; MW; and WB; n = 3) was analyzed using GPC. DC data were analyzed using Kruskal-Wallis test (α = .05). For control specimens, there were no significant differences between U (68%) and LL (77%) and among LL, K (81%), and T (84%). LS (92%) had the highest DC (P<0.05). Only material K exhibited an increased DC after WB (P<0.05). All powders had Mw from 4.0 × 105 to 6.5 × 105 and narrow Mw distributions (2.1 to 3.6). Polymerization and post-polymerization produced K specimens with Mw similar to that of K powder.
Resumo:
Purpose: The effect of water immersion on the shear bond strength (SBS) between 1 heat-polymerizing acrylic resin (Lucitone 550-L) and 4 autopolymerizing reline resins (Kooliner-K, New Truliner-N, Tokuso Rebase Fast-T, Ufi Gel Hard-U) was investigated. Specimens relined with resin L were also evaluated. Materials and Methods: One hundred sixty cylinders (20 × 20 mm) of L denture base resin were processed, and the reline resins were packed on the prepared bonding surfaces using a split-mold (3.5 × 5.0 mm). Shear tests (0.5 mm/min) were performed on the specimens (n = 8) after polymerization (control), and after immersion in water at 37°C for 7, 90, and 180 days. All fractured surfaces were examined by scanning electron microscopy (SEM) to calculate the percentage of cohesive fracture (PCF). Shear data were analyzed with 2-way ANOVA and Tukey's test; Kruskall-Wallis test was used to analyze PCF data (α = 0.05). Results: After 90 days water immersion, an increase in the mean SBS was observed for U (11.13 to 16.53 MPa; p < 0.001) and T (9.08 to 13.24 MPa, p = 0.035), whereas resin L showed a decrease (21.74 MPa to 14.96 MPa; p < 0.001). The SBS of resins K (8.44 MPa) and N (7.98 MPa) remained unaffected. The mean PCF was lower than 32.6% for K, N, and T, and higher than 65.6% for U and L. Conclusions: Long-term water immersion did not adversely affect the bond of materials K, N, T, and U and decreased the values of resin L. Materials L and U failed cohesively, and K, N, and T failed adhesively. © 2007 by The American College of Prosthodontists.
Resumo:
Fracture of dentures is a common clinical finding in daily prosthodontic practice, resulting in great inconvenience to both patient and dentist. A satisfactory repair should be cost-effective, simple to perform, and quick; it should also match the original color and not cause distortion to the existing denture. Different repair materials, surface designs, and mechanical and chemical surface treatments have been recommended in order to obtain stronger repairs. This article reviews some of the available literature with regard to the most important factors that may influence the strength of denture repairs. © 2007 by The American College of Prosthodontists.
Resumo:
This study evaluated the effect of water-bath and microwave post-polymerization treatments on the flexural strength and Vickers hardness of four autopolymerizing reline resins (Duraliner II-D, Kooliner-K, Tokuso Rebase Fast-TR and Ufi Gel Hard C-UGH) and one heat-polymerized acrylic resin (Lucitone 550-L), processed using two polymerization cycles (short cycle - 90 minutes at 73°C and 100°C for 30 minutes; and long cycle - 9 hours at 71°C). For each material, thirty specimens (64 x 10 x 3.3 mm) were made and divided into 3 groups (n=10). Specimens were tested after: processing (control group); water-bath at 55°C for 10 minutes (reline materials) or 60 minutes (L); and microwave irradiation. Flexural strength tests were performed at a crosshead speed of 5 mm/min using a three-point bending device with a span of 50 mm. The flexural strengths values were calculated in MPa. One fragment of each specimen was submitted to Vickers hardness test. Data were analyzed by 2-way ANOVA followed by Tukey's HSD test (α=0.05). L microwaved specimens (short cycle) exhibited significantly higher flexural strength means than its respective control group (p<0.05). Water-bath promoted a significant increase (p<0.05) in flexural strength of K and L (long cycle). The hardness of the tested materials was not influenced by the post-polymerization treatments. Post-polymerization treatments could be used to improve the flexural strength of some materials tested.
Resumo:
The restoration of masticatory function and esthetics is an important aim in dentistry mainly when patients present with extensive tooth loss. The aim of mastication is to reduce food size to produce a homogeneous bolus appropriate to be swallowed. For edentulous patients, chewing efficiency is reduced because dental arches are replaced by artificial teeth. The aim of this study is to present factors related to chewing efficiency for the edentulous patient.
Resumo:
The dual path of insertion concept for removable partial denture (RPD) design may be used in esthetically demanding situations. When compared to conventional RPDs, the main advantage of this design is the minimal use of clasps. This clinical report describes the treatment of a patient with an anterior maxillary edentulous area using a dual path RPD. The diagnostic cast was surveyed to ensure the adequacy of the undercuts on the mesial surfaces of the anterior abutments, where rigid minor connectors were placed. Inverted V-shaped canine cingulum rest seats were prepared to provide resistance to tooth movement during function. The dual path RPD concept allows excellent esthetic results, minimizes tooth preparation, and reduces the tendency toward plaque accumulation in a Kennedy class IV partially edentulous arch. © 2008 by The American College of Prosthodontists.
Resumo:
The aim of this study was to evaluate the dimensional changes of denture bases made from different resins after different storage periods. For this purpose, 25 sets of plaster models/resin bases were prepared using 4 acrylic resins submitted to two types of polymerization: 1- QC-20 submitted to polymerization by microwave energy; 2- QC-20 submitted to polymerization by water hot bath; 3- Vipi Cril submitted to polymerization by water hot bath; 4- Vipi Wave submitted to polymerization by microwave energy; and 5- Onda Cryl submitted to polymerization by microwave energy. After polymerization, the specimens were sectioned for accuracy readings using a comparison microscope. Readings were taken at 3 points: the crests of the right (A) and left (B) ridges, and the median region of the palate, in 4 different periods. The data obtained were submitted to two-way ANOVA and Tukey's test at 5% significance level. The greatest distortions were found in the posterior palatal region of the base (M), with statistically significant difference (p<0.05) for the studied resins. All acrylic resins presented dimensional changes and the storage period influenced these alterations.
Resumo:
The technique presented in this article presents a protocol for treatment that reduces the time required for the fabrication and placement of an implant supported prosthesis. It also offers improved patient comfort at a lower cost when compared to conventional technology.
Resumo:
The purpose of this study was to evaluate the effect of 5% sodium bicarbonate on the adherence of Candida albicans to thermally activated acrylic resin. Fifty 4 mm specimens of acrylic resin were obtained using a metallic matrix. The specimens received chemical polishing, were sterilized and then immersed in Sabouraud broth, inoculated with Candida albicans standardized suspension. After 24 hours of incubation at 37°C, the specimens were divided into four groups according to the substance used for disinfection (5% sodium bicarbonate, 0.12% digluconate chlorhexidine, vinegar and Corega Tabs). A control group was included, in which distilled water was used. The adhered microorganisms were dispersed, diluted and plated onto culture media to determine the number of colony-forming units (cfu/mL). The results were analyzed through the Mann-Whitney statistical test at the 5% level of significance. Only 0.12% digluconate chlorhexidine and 5% sodium bicarbonate presented a statistically significant difference (p = 0.0010 and p = 0.0156, respectively) compared to the control group, decreasing the number of cfu/mL. However, when the different disinfecting solutions were compared with each other, only 0.12% digluconate chlorhexidine presented a statistically significant difference in the reduction of cfu/mL. It was concluded that although 0.12% digluconate chlorhexidine was more effective in the reduction of Candida albicans adherence values to thermally activated acrylic resin, 5% sodium bicarbonate also proved to be a viable alternative.
Resumo:
Oral stomatitis induced by endogenous progesterone is a rare clinical condition which may be associated with cutaneous involvement. That is probably due to the peak of progesterone production during the luteal phase of the menstrual cycle. In the present case report, a 21-year-old patient displayed recurrent ulcerative lesions located on the buccal mucosa or the upper lip, on a monthly basis since the age of 15. Such lesions would always manifest themselves on the second day until the end of the menstrual cycle. © 2009 Informa UK Ltd All rights reserved.
Resumo:
This study evaluated the effect of denture base polymer type (heat- and microwave-polymerized), ridge lap surface treatment (with and without methyl methacrylate-MMA etching) and thermocycling on the microtensile bond strength (mTBS) of Biotone acrylic teeth. Flat-ground, ridge-lap surface of posterior artifcial teeth were bonded to cylinders of each denture base resin, resulting in the following groups (n=6): G1a - Clássico/with MMA etching; G1b - Clássico/without MMA etching; G2a - OndaCryl/with MMA etching; G2b - OndaCryl/without MMA etching. Rectangular bar specimens with a cross-sectional area of 1 mm 2 were prepared. Half of the bars in each group were thermocycled (5,000 cycles between 4°C and 60°C). mTBS testing was performed in an universal testing machine at a crosshead speed of 0.5 mm/min. Data were analyzed statistically by three-way ANOVA (a=0.05). There was no statisti-caly signifcant difference (p>0.05) for the factors (resin, surface treatment,and thermocycling) or their interactions. The mean mTBS values (MPa) and standard deviations were as follows: Thermocycling - G1a: 41.00 (14.00); G1b: 31.00 (17.00); G2a: 50.00 (27.00); G2b: 40.00 (18.00); No thermocycling - G1a: 37.00 (14.00); G1b: 43.00 (25.00); G2a: 43.00 (14.00); G2b: 40.00 (27.00). The mTBS of Biotone artifcial teeth to the denture base acrylic resins was not infuenced by the polymer type, surface treatment or thermocycling.