Relevância:

90.00% 90.00%

Publicador:

Resumo:

Crystals of a new nonlinear optical (NLO) material, viz., L-histidinium 2-nitrobenzoate (LHNB) (1) were grown by slow evaporation of an aqueous solution containing equimolar concentrations of L-histidine and 2-nitrobenzoic acid. The structure of the title compound which crystallizes in the non-centrosymmetric monoclinic space group P2(1) was elucidated using single crystal X-ray intensity data. The UV-Vis-NIR spectrum of 1 reveals its transparent nature while the vibrational spectra confirm the presence of the functional groups in 1. The thermal stability and second harmonic generation (SHG) conversion efficiency of 1 were also investigated. (C) 2012 Elsevier GmbH. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The present study demonstrates a simple protocol for the preparation of one dimensional (1D) oxidized titanium carbide nanowires and their opto-electronic properties. The oxidized titanium carbide nanowires (Ox-TiC-NW) are prepared from TiC nanowires (TiC-NW) that are in turn synthesized from micron sized TiC particles using the solvothermal technique. The Ox-TiC-NW is characterized by X-ray diffraction, UV-Vis spectroscopy, transmission electron microscopy (TEM), scanning electron microscopy (SEM) and Raman spectroscopy. Thermal oxidation of TiC-NW yields carbon doped TiO2-NW (C-TiO2-NW), a simple methodology to obtain 1D C-TiO2-NW. Temperature dependent Raman spectra reveal characteristic bands for TiO2-NW. Electrical characterization of individual C-TiO2-NW is performed by fabricating a device structure using the focused ion beam deposition technique. The opto-electronic properties of individual C-TiO2-NW demonstrate visible light activity and the parameters obtained from photoconductivity measurements reveal very good sensitivity. This methodology opens up the possibility of using C-TiO2-NW in electronic and opto-electronic device applications.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Efficient ZnO:Eu3+ (1-11 mol%) nanophosphors were prepared for the first time by green synthesis route using Euphorbia tirucalli plant latex. The final products were well characterized by powder X-ray diffraction (PXRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), UV-visible spectroscopy (UV-Vis), Fourier transform infrared spectroscopy (FTIR), etc. The average particle size of ZnO:Eu3+ (7 mol%) was found to be in the range 27-47 nm. With increase of plant latex, the particle size was reduced and porous structure was converted to spherical shaped particles. Photoluminescence (PL) spectra indicated that the peaks situated at similar to 590, 615, 648 and 702 nm were attributed to the D-5(0) -> F-7(j(j=1,2,3,4)) transitions of Eu3+ ions. The highest PL intensity was recorded for 7 mol% with Eu3+ ions and 26 ml plant latex concentration. The PL intensity increases with increase of plant latex concentration up to 30 ml and there after it decreases. The phosphor prepared by this method show spherical shaped particles, excellent chromaticity co-ordinates in the white light region which was highly useful for WLED's. Further, present method was reliable, environmentally friendly and alternative to economical routes. (c) 2013 Elsevier B.V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Undoped and Tb3+ (1-10 mol%) doped CeO2 nanophosphors were synthesized by low temperature solution combustion method. The combustion derived products were well studied by Powder X-ray diffraction (PXRD), Scanning electron microscopy (SEM), transmission electron microscopy (TEM), Fourier transform infrared spectroscopy (FTIR) and Ultraviolet visible (UV-Vis) characterizations. The thermoluminescence (TL) glow curves of CeO2: Tb3+ (1-10 mol%) nanophosphors exposed to c source (60Co) for various doses were discussed for the first time. Two TL glow peaks recorded at 182 and 262 degrees C respectively. The TL intensity at 262 degrees C peak increases linearly in the dose range 0.5-7 kGy. Further, this peak was well defined, intense and glow peak structure does not change with c-dose as a result, it was quite useful in TL dosimetry of ionizing radiations. The kinetic parameters associated with the glow peak were estimated using Chen's half width method. The photoluminescence emission (PLE) spectra consists of characteristic peaks at 544 and 655 nm which were attributed to D-5(4) -> F-7(5) and D-5(4) -> F-7(2) transitions of Tb3+ ions. The optimal concentration of Tb3+ ions was found to be 7 mol%. The color co-ordinates of CeO2: Tb3+ (1-10 mol%) located in green region. Hence, this phosphor was quite useful for display applications. (C) 2013 Elsevier B. V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The dihexyl substituted poly (3,4-propylenedioxythiophene) (PProDOT-Hx(2)) thin films uniformly deposited by cost effective spray coating technique on transparent conducting oxide coated substrates. The electro-optical properties of PProDOT-Hx(2) films were studied by UV-Vis spectroscopy that shows the color contrast about 45% with coloration efficiency of approximate to 185cm(2)/C. The electrochemical properties of PProDOT-Hx(2) films were studied by cyclic voltammetry and AC impedance techniques. The cyclic voltammogram shows that redox reaction of films are diffusion controlled and ions transportation will be faster on the polymer film at higher scan rate. Impedance spectra indicate that polymer films are showing interface charge transfer process as well as capacitive behavior between the electrode and electrolyte. The XRD of the PProDOT-Hx(2) thin films revealed that the films are in amorphous nature, which accelerates the transportation of ions during redox process.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Interaction of adsorbate on charged surfaces, orientation of the analyte on the surface, and surface enhancement aspects have been studied. These aspects have been explored in details to explain the surface-enhanced Raman spectroscopic (SERS) spectra of 2,4,6,8,10,12-hexanitro-2,4,6,8,10,12-hexaazaisowurtzitane (HNIW or CL-20), a well-known explosive, and 2,4,6-trinitrotoluene (TNT) using one-pot synthesis of silver nanoparticles via biosynthetic route using natural precursor extracts of clove and pepper. The biosynthesized silver nanoparticles (bio Ag Nps) have been characterized using UV-vis spectroscopy, scanning electron microscopy and atomic force microscopy. SERS studies conducted using bio Ag Nps on different water insoluble analytes, such as CL-20 and TNT, lead to SERS signals at concentration levels of 400 pM. The experimental findings have been corroborated with density functional computational results, electrostatic surface potential calculations, Fukui functions and potential measurements.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Ligational behaviour of (E)-2-amino-N'-1-(2-hydroxyphenyl)ethylidene]benzohydrazide (Aheb) towards later 3d metal ionscopper(II), cobalt(II), manganese(II), zinc(II), cadmium(II) and nickel(IV)] has been studied. Their structures have been elucidated on the basis of spectral (IR, H-1 NMR, UV-Vis, EPR and FAB-mass), elemental analyses, conductance measurements, magnetic moments, and thermal studies. During complexation Ni(II) ion has got oxidized to Ni(IV). The changes in the bond parameters of the ligand on complexation has been discussed by comparing the crystal structure of the ligand with that of its Ni(IV) complex. The X-ray single crystal analysis of Ni(aheb)(2)]Cl-2 center dot 4H(2)O has confirmed an octahedral geometry around the metal ion. EPR spectra of the Cu(II) complex in polycrystalline state at room (300 K) and liquid nitrogen temperature (77 K) were recorded and their salient features are reported. (C) 2014 Elsevier B.V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Solvent effects play a vital role in various chemical, physical, and biological processes. To gain a fundamental understanding of the solute-solvent interactions and their implications on the energy level re-ordering and structure, UV-VIS absorption, resonance Raman spectroscopic, and density functional theory calculation studies on 9,10-phenanthrenequinone (PQ) in different solvents of diverse solvent polarity has been carried out. The solvatochromic analysis of the absorption spectra of PQ in protic dipolar solvents suggests that the longest (1n-pi(1)*; S-1 state) and the shorter (1 pi-pi(1)*; S-2 state) wavelength band undergoes a hypsochromic and bathochromic shift due to intermolecular hydrogen bond weakening and strengthening, respectively. It also indicates that hydrogen bonding plays a major role in the differential solvation of the S-2 state relative to the ground state. Raman excitation profiles of PQ (400-1800 cm(-1)) in various solvents followed their corresponding absorption spectra therefore the enhancements on resonant excitation are from single-state rather than mixed states. The hyperchromism of the longer wavelength band is attributed to intensity borrowing from the nearby allowed electronic transition through vibronic coupling. Computational calculation with C-2 nu symmetry constraint on the S-2 state resulted in an imaginary frequency along the low-frequency out-of-plane torsional modes involving the C=O site and therefore, we hypothesize that this mode could be involved in the vibronic coupling. (C) 2015 AIP Publishing LLC.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Ho3+ (0.25-7 mol%) doped Sr2CeO4 nanophosphors were synthesized by solution combustion method using urea as fuel. The structural properties of the nanophosphors were investigated by powder X-ray diffraction studies (PXRD), scanning electron microscopy (SEM) and transmission electron microscopy (TEM) techniques. UV-Visible and photoluminescence (PL) spectroscopic techniques were used for analysing the optical properties of the nanoparticles. PXRD and TEM results revealed the formation of Sr2CeO4: Ho3+ nanocrystalline particles with orthorhombic crystal structure. From the UV-Vis studies the optical band gap energy found to decrease from 5.9 to 5.74 eV with increase in dopant concentration. The PL spectra exhibit the broad excitation band from 200 to 400 nm which concurs well with the commercial near UV LED. The PL spectra vary with the dopant content due to energy transfer from the host to the activator. In this present work we demonstrate that color tuning of phosphor can be achieved by merely varying the Ho3+ ions concentration. The CIE and CCT chromaticity coordinates suggests Sr2CeO4: Ho3+ nanophosphors may be potentially applicable as promising single - phased phosphors for lighting applications. (C) 2015 Elsevier B.V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

In the present study, we report the hydrogen content estimation of the hydrogenated amorphous carbon (a-C:H) films using visible Raman spectroscopy in a fast and nondestructive way. Hydrogenated diamondlike carbon films were deposited by the plasma enhanced chemical vapor deposition, plasma beam source, and integrated distributed electron cyclotron resonance techniques. Methane and acetylene were used as source gases resulting in different hydrogen content and sp2/sp3 fraction. Ultraviolet-visible (UV-Vis) spectroscopic ellipsometry (1.5-5 eV) as well as UV-Vis spectroscopy were provided with the optical band gap (Tauc gap). The sp2/sp3 fraction and the hydrogen content were independently estimated by electron energy loss spectroscopy and elastic recoil detection analysis-Rutherford back scattering, respectively. The Raman spectra that were acquired in the visible region using the 488 nm line shows the superposition of Raman features on a photoluminescence (PL) background. The direct relationship of the sp2 content and the optical band gap has been confirmed. The difference in the PL background for samples of the same optical band gap (sp2 content) and different hydrogen content was demonstrated and an empirical relationship between the visible Raman spectra PL background slope and the corresponding hydrogen content was extracted. © 2004 American Institute of Physics.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

380 p. : il., gráf.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Semisynthesis of horse heart cytochrome c and site-directed mutagenesis of Saccharomyces cerevisiae (S. c.) iso-1-cytochrome c have been utilized to substitute Ala for the cytochrome c heme axial ligand Met80 to yield ligand-binding proteins (horse heart Ala80cyt c and S.c. Ala80cyt c) with spectroscopic properties remarkably similar to those of myoglobin. Both species of Fe(II)Ala80cyt c form exceptionally stable dioxygen complexes with autoxidation rates 10-30x smaller and O2 binding constants ~ 3x greater than those of myoglobin. The resistance of O2-Fe(II)Ala80cyt c to autoxidation is attributed in part to protection of the heme site from solvent as exhibited by the exceptionally slow rate of CO binding to the heme as well as the low quantum yield of CO photodissociation.

UV/vis, EPR, and paramagnetic NMR spectroscopy indicate that at pH 7 the Fe(III)Ala80cyt c heme is low-spin with axial His-OH- coordination and that below pH ~6.5, Fe(III)Ala80cyt cis high-spin with His-H2O heme ligation. Significant differences in the pH dependence of the 1H NMR spectra of S.c. Fe(III)Ala80cyt c compared to wild-type demonstrate that the axial ligands influence the conformational energetics of cytochrome c.

1H NMR spectroscopy has been utilized to determine the solution structure of the cyanide derivative of S.c. Fe(III)Ala80cyt c. 82% of the resonances in the 1H NMR spectrum of S.c. CN-Fe(III)Ala80cyt c have been assigned through 1D and 2D experiments. The RMSD values after restrained energy minimization of the family of 17 structures obtained from distance geometry calculations are 0.68 ± 0.11 Å for the backbone and 1.32 ± 0.14 Å for all heavy atoms. The solution structure indicates that a tyrosine in the "distal" pocket of CN-Fe(III)Ala80cyt c forms a hydrogen bond with the Fe(III)-CN unit, suggesting that it may play a role analogous to that of the distal histidine in myoglobin in stabilizing the dioxygen adduct.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

As indústrias consomem volumes elevados de água e outras substâncias químicas na síntese dos seus produtos e geram grande quantidade de rejeitos. Entre os mais importantes poluentes encontrados nos efluentes dessas indústrias estão os corantes sintéticos que representam um problema, pois não são facilmente destruídos por tratamentos convencionais. A fotocatálise heterogênea tem sido considerada como uma alternativa efetiva no tratamento de efluentes contendo esses corantes. Neste trabalho, estudou-se a cinética de descoloração e o grau de mineralização dos corantes sintéticos reativos Yellow 145, Black 5, Red 4 e Blue 21 através da fotocatálise utilizando ZnO puro e impregnado com íons Fe2+ e Co2+. Testes preliminares foram realizados para otimizar a concentração dos corantes e a massa mínima de catalisador a ser utilizado nos experimentos fotocatalíticos. Além da fotocatálise, experimentos individuais de fotólise e adsorção também foram realizados, porém se mostraram poucos eficientes. Através da espectrofotometria UV-Vis, verificou-se o total descoramento individual dos corantes em aproximadamente 30 minutos de irradiação com ZnO. O grau de mineralização de cada corante foi determinado através de análise de carbono orgânico total (COT), atingindo-se cerca de 70 a 80% de mineralização após 240 minutos de tratamento fotocatalítico. Foram comparadas, ainda, as eficiências de cada fotocatalisador ZnO, Fe/ZnO e Co/ZnO na mineralização de uma solução contendo a mistura dos quatro corantes já mencionados após 240 minutos de reação. A eficiência na mineralização da mistura dos corantes seguiu a seguinte ordem: Co/ZnO (32%), ZnO (78%) e Fe/ZnO (87%). A reação de degradação fotocatalítica do corante Black 5 seguiu uma cinética de primeira ordem, enquanto que os corantes Yellow 145, Red 4 e Blue 21 seguiram uma cinética de ordem zero.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

合成了2种新型的可溶性四氮杂卟啉中间体:反式-1,2二氰-(4-乙基苯)乙烯和顺式-1,2-二氰(4-乙基苯)乙烯。通过UV-Vis,FFIR,GC/MS,^1H NMR等方法对这2种化合物的结构进行了表征,给出了它们完整的结构信息。分析比较了顺、反异构体结构上的差异,分析两者的紫外-可见光谱(UV-Vis)、红外光谱(FTIR)和核磁共振光谱(^1H NMR)谱图的差异及其产生原因。

Relevância:

90.00% 90.00%

Publicador:

Resumo:

研究了5种新型的具有不同结构的aα-异噁唑偶氮基-β-二酮类衍生物的红外光谱和紫外光谱,讨论了它们的酮式-烯醇式以及偶氮式.腙式之间的互变异构化现象。结果表明,所有化合物无论以固体形式或在溶液中均以腙式二酮体和偶氮式烯醇体的混合形式存在。各化合物的紫外吸收谱均呈双峰状,峰值分别处于246~262nm和326~339nm之间,其中,高波长吸收峰的强度明显高于低波长吸收峰强度,说明了各化合物中偶氮式烯醇体形式均多于腙式二酮体形式,其原因是由于各化合物中偶氮式烯醇体的异构体较多,且易以分子内氢键形式形成六元环,